Krestina V. Aksenova
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Krestina V. Aksenova has a total of 75 co-authors. Here are the top co-authors by number of shared publications:
- Viktor Evgenievich Gromov
Siberian State Industrial University, Novokuznetsk, Russia
38 shared publications - Yurii Fedorovich Ivanov
High Current Electronics Institute, Siberian Branch of the Russian Academy of Sciences, Tomsk, Russia
31 shared publications - Sergey V. Konovalov
Siberian State Industrial University
18 shared publications Olga Semina
Siberian State Industrial University, Novokuznetsk, 654007 Russia
8 shared publications- Dmitrii Zaguliaev
Siberian State Industrial University
6 shared publications Yu F Ivanov
Institute of High Current Electronics, Siberian Brunch of the Russian Academy of Sciences, 2/3 Akademichesky Ave, Tomsk, 634055, Russia
6 shared publications
Latest Publications
- 29 December 2025
- Published by Siberian State Industrial University in Bulletin of the Siberian State Industrial University
- No. 4
MODERN ASPECTS OF STUDYING THE EFFECT OF EXTERNAL MAGNETIC FIELDS ON THE DEFORMATION CHARACTERISTICS OF METALLIC MATERIALS
Сибирский государственный индустриальный университет (Россия, 654007, Кемеровская обл.-Кузбасс, Новокузнецк, ул. Кирова, 42) Аннотация. Проведен анализ влияния постоянных и импульсных магнитных полей различной интенсивности на деформационные характеристики металлических материалов, преимущественно пара-и диамагнетиков. Установлено, что выдержка образцов в магнитных полях с индукцией 0,1-0,5 Тл приводит к перераспределению легирующих атомов, ослаблению связи дислокаций с точечными и протяженными дефектами кристаллической решетки, что обуславливает снижение микротвердости материалов на 15-25 % по сравнению с исходным состоянием. В области слабых полей (10-50 мТл) обнаружена выраженная нелинейная зависимость предела текучести и относительного удлинения от индукции, что указывает на высокую чувствительность макропластических свойств металлов к малым значениям магнитного воздействия. Для сплава Al-Zn-Mg-Cu обработка при поле 1 Тл и в интервале температур 110-140 °C способствует снижению критического напряжения сдвига на 10-15 % и интенсифицирует процесс нуклеации η′-фазы, что связано с уменьшением межфазной энергии и активацией структурно-кинетических процессов. В титановом сплаве Ti-6Al-4V действие поля 2 Тл способствует росту плотности дислокаций до 60 %, увеличению микротвердости на 8 % и относительного удлинения до 13 %, что объясняется участием спинозависимых переходов в механизмах пластической деформации. Воздействие импульсных магнитных полей стимулирует субгранулярную фрагментацию и существенное измельчение зерна, приводя к увеличению пластичности сплавов до 25 %. Полученные данные свидетельствуют о высоком потенциале магнитных полей как управляемого инструмента регулирования кинетики фазовых превращений, динамики дефектов и снижения энергетических барьеров пластического течения, что открывает новые возможности для интеграции магнитной обработки в современные промышленные технологии формоизменения и упрочнения конструкционных материалов различной природы.
- 29 December 2025
- Published by Siberian State Industrial University in Bulletin of the Siberian State Industrial University
- No. 4
MODERN ASPECTS OF STUDYING THE EFFECT OF EXTERNAL MAGNETIC FIELDS ON THE DEFORMATION CHARACTERISTICS OF METALLIC MATERIALS
Сибирский государственный индустриальный университет (Россия, 654007, Кемеровская обл.-Кузбасс, Новокузнецк, ул. Кирова, 42) Аннотация. Проведен анализ влияния постоянных и импульсных магнитных полей различной интенсивности на деформационные характеристики металлических материалов, преимущественно пара-и диамагнетиков. Установлено, что выдержка образцов в магнитных полях с индукцией 0,1-0,5 Тл приводит к перераспределению легирующих атомов, ослаблению связи дислокаций с точечными и протяженными дефектами кристаллической решетки, что обуславливает снижение микротвердости материалов на 15-25 % по сравнению с исходным состоянием. В области слабых полей (10-50 мТл) обнаружена выраженная нелинейная зависимость предела текучести и относительного удлинения от индукции, что указывает на высокую чувствительность макропластических свойств металлов к малым значениям магнитного воздействия. Для сплава Al-Zn-Mg-Cu обработка при поле 1 Тл и в интервале температур 110-140 °C способствует снижению критического напряжения сдвига на 10-15 % и интенсифицирует процесс нуклеации η′-фазы, что связано с уменьшением межфазной энергии и активацией структурно-кинетических процессов. В титановом сплаве Ti-6Al-4V действие поля 2 Тл способствует росту плотности дислокаций до 60 %, увеличению микротвердости на 8 % и относительного удлинения до 13 %, что объясняется участием спинозависимых переходов в механизмах пластической деформации. Воздействие импульсных магнитных полей стимулирует субгранулярную фрагментацию и существенное измельчение зерна, приводя к увеличению пластичности сплавов до 25 %. Полученные данные свидетельствуют о высоком потенциале магнитных полей как управляемого инструмента регулирования кинетики фазовых превращений, динамики дефектов и снижения энергетических барьеров пластического течения, что открывает новые возможности для интеграции магнитной обработки в современные промышленные технологии формоизменения и упрочнения конструкционных материалов различной природы.
- 1 January 2025
- Published by Penza State University in University proceedings. Volga region. Physical and mathematical sciences
- No. 3
Influence of constant magnetic field on fatigue life of diamagnetics: the role of the Zeeman effect in the fatigue strength of non-ferrous metals
Background. The relevance of the study is due to the need to study the effect of constant magnetic fields on the fatigue life of commercially pure copper and lead, widely used in industry and sensitive to magnetic effects, which will improve the reliability of products and control their mechanical properties. The purpose of the work is to study the effect of a constant magnetic field with an induction of 0.1-0.5 T on the fatigue life of commercially pure copper and lead. Materials and methods. Samples of commercially pure copper grade M1 and lead grade C2 measuring 4 × 12 × 130 mm were manufactured by electrical discharge cutting on a CNC machine. Fatigue tests were carried out on a setup with cyclic asymmetric cantilever bending at a temperature of (~ 300 K). The mode with a loading amplitude of 2.5 mm was selected. The fracture surface was studied by scanning electron microscopy (KYKY EM6900) with structure analysis in ImageJ, and the elemental composition was studied using Ultim Extreme. Results. The fatigue test results showed that the magnetic field increases the fatigue life of copper M1 by 9–28% and lead C2 by 7% at 0.3 T, but reduces it at 0.4–0.5 T; copper fracture occurs through three zones with the formation of a subgrain structure, while in lead the magnetic field changes the fracture morphology and the fracture mechanism. The Zeeman effect, causing splitting of the electron energy levels, changes the activation energies of dislocation motion in diamagnetic metals, which affects their sliding speed and mechanical properties. Conclusions. 1 The magnetic field (0.1–0.25 T) increases the fatigue life of copper by 9–28%, affecting the fracture mechanism through the formation of a subgrain structure. 2 A magnetic field of 0.3 T increases the fatigue life of lead by 7%, while at 0.4–0.5 T it significantly reduces it due to the effect on dislocation mobility and fracture morphology. 3 The Zeeman effect changes the electronic structure of diamagnetic metals, changing the activation energies of dislocation motion and their slip velocity, which affects mechanical properties.
- 1 January 2025
- Published by Penza State University in University proceedings. Volga region. Physical and mathematical sciences
- No. 3
Influence of constant magnetic field on fatigue life of diamagnetics: the role of the Zeeman effect in the fatigue strength of non-ferrous metals
Background. The relevance of the study is due to the need to study the effect of constant magnetic fields on the fatigue life of commercially pure copper and lead, widely used in industry and sensitive to magnetic effects, which will improve the reliability of products and control their mechanical properties. The purpose of the work is to study the effect of a constant magnetic field with an induction of 0.1-0.5 T on the fatigue life of commercially pure copper and lead. Materials and methods. Samples of commercially pure copper grade M1 and lead grade C2 measuring 4 × 12 × 130 mm were manufactured by electrical discharge cutting on a CNC machine. Fatigue tests were carried out on a setup with cyclic asymmetric cantilever bending at a temperature of (~ 300 K). The mode with a loading amplitude of 2.5 mm was selected. The fracture surface was studied by scanning electron microscopy (KYKY EM6900) with structure analysis in ImageJ, and the elemental composition was studied using Ultim Extreme. Results. The fatigue test results showed that the magnetic field increases the fatigue life of copper M1 by 9–28% and lead C2 by 7% at 0.3 T, but reduces it at 0.4–0.5 T; copper fracture occurs through three zones with the formation of a subgrain structure, while in lead the magnetic field changes the fracture morphology and the fracture mechanism. The Zeeman effect, causing splitting of the electron energy levels, changes the activation energies of dislocation motion in diamagnetic metals, which affects their sliding speed and mechanical properties. Conclusions. 1 The magnetic field (0.1–0.25 T) increases the fatigue life of copper by 9–28%, affecting the fracture mechanism through the formation of a subgrain structure. 2 A magnetic field of 0.3 T increases the fatigue life of lead by 7%, while at 0.4–0.5 T it significantly reduces it due to the effect on dislocation mobility and fracture morphology. 3 The Zeeman effect changes the electronic structure of diamagnetic metals, changing the activation energies of dislocation motion and their slip velocity, which affects mechanical properties.
- 1 April 2024
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 15 (2) , 426-431
Analysis of Hardening Mechanisms of Rail Steel under Plastic Deformation by Uniaxial Compression
Using the methods of scanning and transmission electron microscopy, an analysis was made of the evolution of the structure and defective substructure of rail steel under uniaxial compression up to a degree of 50%. It is revealed that the strain hardening has a multistage nature and is accompanied by a decrease in the scalar and excess dislocation density and fragmentation of pearlite grains, which increases with increasing strain. Fracture of cementite plates proceeding through the mechanisms of their dissolution and cutting by mobile dislocations is revealed. On the basis of data on the structural-phase states and the defective substructure of rail steel obtained by the methods of modern physical materials science, a quantitative analysis of the mechanisms of hardening of rail steel at degrees of compression deformation of 15, 30, and 50% was carried out. It is shown that, at the initial stage (ε = 15%), the main strengthening factor of the steel under study is the presence of lamellar pearlite grains, and at high degrees of deformation (ε = 50%), it is hardening by incoherent particles of the carbide phase. The overall yield strength of steel was estimated in the first approximation based on the additivity principle, which assumes the independent action of each of the hardening mechanisms. A good qualitative agreement between the experimentally obtained and theoretically calculated values of steel strength has been revealed.
- 1 April 2024
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 15 (2) , 426-431
Analysis of Hardening Mechanisms of Rail Steel under Plastic Deformation by Uniaxial Compression
Using the methods of scanning and transmission electron microscopy, an analysis was made of the evolution of the structure and defective substructure of rail steel under uniaxial compression up to a degree of 50%. It is revealed that the strain hardening has a multistage nature and is accompanied by a decrease in the scalar and excess dislocation density and fragmentation of pearlite grains, which increases with increasing strain. Fracture of cementite plates proceeding through the mechanisms of their dissolution and cutting by mobile dislocations is revealed. On the basis of data on the structural-phase states and the defective substructure of rail steel obtained by the methods of modern physical materials science, a quantitative analysis of the mechanisms of hardening of rail steel at degrees of compression deformation of 15, 30, and 50% was carried out. It is shown that, at the initial stage (ε = 15%), the main strengthening factor of the steel under study is the presence of lamellar pearlite grains, and at high degrees of deformation (ε = 50%), it is hardening by incoherent particles of the carbide phase. The overall yield strength of steel was estimated in the first approximation based on the additivity principle, which assumes the independent action of each of the hardening mechanisms. A good qualitative agreement between the experimentally obtained and theoretically calculated values of steel strength has been revealed.
- 1 January 2024
- Published by Pleiades Publishing Ltd in Technical Physics
- Vol. 69 (1) , 57-61
Evolution of the Lamellar Pearlite Structure of Rail Steel under Tension
Methods of modern physical materials science were used to investigate the mechanical properties of rail steel, the defective substructure of pearlite with lamellar morphology, and the fracture surface of rail steel subjected to fracture under uniaxial tensile strain. The ultimate strength was found to vary from 1247 to 1335 MPa and the fracture strain of the specimens to range from 0.22 to 0.26. The deformation of steel is shown to be coupled with the division of ferrite plates into fragments by low-angle boundaries along with a significant increase in the scalar dislocation density up to 7.9 × 1010 cm–2 (the scalar dislocation density of original rail steel being 3.2 × 1010 cm–2). In addition, internal stress fields arise in the form of bend extinction contours. Sources of the stress fields are identified. It was found that cementite plates were fractured by cutting and dissolution with subsequent transfer of carbon by moving dislocations to ferrite plates to form there nanosized (8.3 nm) round particles of tertiary cementite. It is shown that the dissolution of cementite plates is accompanied by fragmentation (division into coherent scattering regions of 9.3 nm on average).
- 1 January 2024
- Published by Pleiades Publishing Ltd in Technical Physics
- Vol. 69 (1) , 57-61
Evolution of the Lamellar Pearlite Structure of Rail Steel under Tension
Methods of modern physical materials science were used to investigate the mechanical properties of rail steel, the defective substructure of pearlite with lamellar morphology, and the fracture surface of rail steel subjected to fracture under uniaxial tensile strain. The ultimate strength was found to vary from 1247 to 1335 MPa and the fracture strain of the specimens to range from 0.22 to 0.26. The deformation of steel is shown to be coupled with the division of ferrite plates into fragments by low-angle boundaries along with a significant increase in the scalar dislocation density up to 7.9 × 1010 cm–2 (the scalar dislocation density of original rail steel being 3.2 × 1010 cm–2). In addition, internal stress fields arise in the form of bend extinction contours. Sources of the stress fields are identified. It was found that cementite plates were fractured by cutting and dissolution with subsequent transfer of carbon by moving dislocations to ferrite plates to form there nanosized (8.3 nm) round particles of tertiary cementite. It is shown that the dissolution of cementite plates is accompanied by fragmentation (division into coherent scattering regions of 9.3 nm on average).
- 1 January 2024
- Published by Pleiades Publishing Ltd in Technical Physics Letters
- Vol. 50 (1) , 13-18
Increasing the Fatigue Life of VT1-0 Titanium under the Influence of a Constant Magnetic Field
High-cycle fatigue tests of VT1-0 titanium samples were carried out under conditions of exposure to a constant magnetic field of various magnitudes and without it. It is shown that the use of a constant magnetic field with induction B = 0.3, 0.4, and 0.5 T leads to a multiple increase in the average number of cycles before the destruction of titanium samples VT1-0 by 64, 123, and 163%, respectively. Using scanning electron microscopy, it was found that the structure of a sample destroyed under fatigue testing conditions, regardless of the test mode, has three characteristic zones: a fatigue crack growth zone, an accelerated crack growth zone, and a fracture zone. It was found that the width of the fatigue crack growth zone depends on the magnetic field induction and reaches its maximum values (h = 264 μm) at B = 0.4 T, and during fatigue tests without a magnetic field, h = 182 μm. This indicates an increase in the critical crack length (the width of the fatigue crack growth zone) by a factor of 1.45. It is shown that the average distance between fatigue striations in titanium samples depends on the value of the magnetic induction of the magnetic field and decreases from 0.78 μm in the absence of a field to 0.49 μm at B = 0.5 T. The formation of a subgrain (fragmented) structure in the zone of fatigue crack growth in a titanium sample was established. The subgrain sizes correspond to the distance between the fatigue striations, which has a retarding effect on the movement of a microcrack. Taken together, the revealed facts indicate a higher resistance of the material to the propagation of a fatigue crack and an increase in its service life during fatigue tests in a magnetic field.
- 1 January 2024
- Published by Pleiades Publishing Ltd in Technical Physics Letters
- Vol. 50 (1) , 13-18
Increasing the Fatigue Life of VT1-0 Titanium under the Influence of a Constant Magnetic Field
High-cycle fatigue tests of VT1-0 titanium samples were carried out under conditions of exposure to a constant magnetic field of various magnitudes and without it. It is shown that the use of a constant magnetic field with induction B = 0.3, 0.4, and 0.5 T leads to a multiple increase in the average number of cycles before the destruction of titanium samples VT1-0 by 64, 123, and 163%, respectively. Using scanning electron microscopy, it was found that the structure of a sample destroyed under fatigue testing conditions, regardless of the test mode, has three characteristic zones: a fatigue crack growth zone, an accelerated crack growth zone, and a fracture zone. It was found that the width of the fatigue crack growth zone depends on the magnetic field induction and reaches its maximum values (h = 264 μm) at B = 0.4 T, and during fatigue tests without a magnetic field, h = 182 μm. This indicates an increase in the critical crack length (the width of the fatigue crack growth zone) by a factor of 1.45. It is shown that the average distance between fatigue striations in titanium samples depends on the value of the magnetic induction of the magnetic field and decreases from 0.78 μm in the absence of a field to 0.49 μm at B = 0.5 T. The formation of a subgrain (fragmented) structure in the zone of fatigue crack growth in a titanium sample was established. The subgrain sizes correspond to the distance between the fatigue striations, which has a retarding effect on the movement of a microcrack. Taken together, the revealed facts indicate a higher resistance of the material to the propagation of a fatigue crack and an increase in its service life during fatigue tests in a magnetic field.
- Open Access
Effect of Thickness of Ti Coating Deposited by Vacuum Arc Melting on Fatigue Behavior of Aluminum Alloy Al–5%Si
Fatigue strength tests of Ti-coated aluminum alloys with a thickness of 1 µm, 3 µm, and 5 µm were conducted to investigate the effect of the coating thickness on fatigue strength. Under the same applied stress amplitude, the optimum thickness with the most-extended fatigue life was around the coating thickness of 5 µm. This may be attributed to the good resistance to surface cracks under repeated loads. The results suggested that a lower fatigue life of a coating thickness of 1 µm results from the fracture of the coating layer under the strong influence of the deformation of the substrate. This could be due to the higher tensile residual stress induced in the substrate near the coating layer and substrate interface. The titanium coating restricted the initiation of offsets and cracks beneath the surface of the specimen, which may be attributed to the high strength of the Al–5%Si substrate, good flexibility, and strong adhesion, which provided sufficient compressive stress to suppress slip band protrusions. The fatigue life and fatigue limit increased proportionally to the thickness of the titanium coating due to changes in the surface roughness and adhesion capability.
Open AccessEffect of Thickness of Ti Coating Deposited by Vacuum Arc Melting on Fatigue Behavior of Aluminum Alloy Al–5%Si
Fatigue strength tests of Ti-coated aluminum alloys with a thickness of 1 µm, 3 µm, and 5 µm were conducted to investigate the effect of the coating thickness on fatigue strength. Under the same applied stress amplitude, the optimum thickness with the most-extended fatigue life was around the coating thickness of 5 µm. This may be attributed to the good resistance to surface cracks under repeated loads. The results suggested that a lower fatigue life of a coating thickness of 1 µm results from the fracture of the coating layer under the strong influence of the deformation of the substrate. This could be due to the higher tensile residual stress induced in the substrate near the coating layer and substrate interface. The titanium coating restricted the initiation of offsets and cracks beneath the surface of the specimen, which may be attributed to the high strength of the Al–5%Si substrate, good flexibility, and strong adhesion, which provided sufficient compressive stress to suppress slip band protrusions. The fatigue life and fatigue limit increased proportionally to the thickness of the titanium coating due to changes in the surface roughness and adhesion capability.
- Open Access
- 14 September 2023
- Published by Altai State University in Izvestiya of Altai State University
- No. 4(132),p. 52-58
Study of Microhardness and Plasticity Parameter of Lead in External Magnetic Fields with Induction up to 0.5 T
Проведены измерения микротвердости образцов технически чистого свинца без воздействия и при воздействии внешнего магнитного поля с индукцией 0.3 Тл, 0.4 Тл, 0.5 Тл. Получены зависимости микротвердости поверхности свинца марки С2 от времени выдержки в магнитном поле, отражающие влияние магнитного поля на пластические характеристики свинца. Выявлено время выдержки, при котором наблюдается максимальный эффект влияния на микротвердость. Дополнительно были проведены испытания на микротвердость образцов технически чистого свинца без воздействия и при воздействии внешнего магнитного поля с индукцией до 0.3, 0.4 и 0.5 Тл и временем обработки 0.25, 0.5 и 1 час. По полученным данным микротвердости вычислен параметр пластичности свинца в исходном состоянии и после обработки во внешнем магнитном поле, показаны зависимости параметра пластичности от времени обработки. Установлен характер изменения параметра пластичности при обработке свинца в магнитном поле с индукцией до 0.5 Тл. Показаны проценты изменения значений микротвердости в зависимости от индукции магнитного поля.
- 14 September 2023
- Published by Altai State University in Izvestiya of Altai State University
- No. 4(132),p. 52-58
Open AccessStudy of Microhardness and Plasticity Parameter of Lead in External Magnetic Fields with Induction up to 0.5 T
Проведены измерения микротвердости образцов технически чистого свинца без воздействия и при воздействии внешнего магнитного поля с индукцией 0.3 Тл, 0.4 Тл, 0.5 Тл. Получены зависимости микротвердости поверхности свинца марки С2 от времени выдержки в магнитном поле, отражающие влияние магнитного поля на пластические характеристики свинца. Выявлено время выдержки, при котором наблюдается максимальный эффект влияния на микротвердость. Дополнительно были проведены испытания на микротвердость образцов технически чистого свинца без воздействия и при воздействии внешнего магнитного поля с индукцией до 0.3, 0.4 и 0.5 Тл и временем обработки 0.25, 0.5 и 1 час. По полученным данным микротвердости вычислен параметр пластичности свинца в исходном состоянии и после обработки во внешнем магнитном поле, показаны зависимости параметра пластичности от времени обработки. Установлен характер изменения параметра пластичности при обработке свинца в магнитном поле с индукцией до 0.5 Тл. Показаны проценты изменения значений микротвердости в зависимости от индукции магнитного поля.
- Open Access
- 28 March 2023
- Published by Altai State University in Izvestiya of Altai State University
- No. 1(129),p. 11-17
Evolution of the Lamellar Pearlite Structure of Rail Steel under Tension
Методами современного физического материаловедения проведены исследования механических свойств, дефектной субструктуры перлита пластинчатой морфологии и поверхности разрушения рельсовой стали, подвергнутой разрушению в условиях деформации одноосным растяжением. Установлено, что предел прочности на разрыв изменяется от 1247 МПа до 1335 МПа; деформация образцов при разрушении — от 0,22 до 0,26. Показано, что деформация стали сопровождается разбиением пластин феррита малоугловыми границами на фрагменты и существенным увеличением скалярной плотности дислокаций до 7,9-1010 см-2 (скалярная плотность дислокаций исходной стали 3,2-1010 см-2). Показано, что деформация сопровождается формированием внутренних полей напряжений, проявляющихся в виде изгибных контуров экстинкции. Отмечены источники полей напряжений. Выявлено разрушение пластин цементита по механизмам разрезания и растворения с последующим выносом углерода движущимися дислокациями в объем пластин феррита с образованием в них наноразмерных (8,3 нм) частиц третичного цементита округлой формы. Показано, что растворение пластин цементита сопровождается их фрагментацией (разделением на области когерентного рассеивания, средние размеры которых 9,3 нм).
- 28 March 2023
- Published by Altai State University in Izvestiya of Altai State University
- No. 1(129),p. 11-17
Open AccessEvolution of the Lamellar Pearlite Structure of Rail Steel under Tension
Методами современного физического материаловедения проведены исследования механических свойств, дефектной субструктуры перлита пластинчатой морфологии и поверхности разрушения рельсовой стали, подвергнутой разрушению в условиях деформации одноосным растяжением. Установлено, что предел прочности на разрыв изменяется от 1247 МПа до 1335 МПа; деформация образцов при разрушении — от 0,22 до 0,26. Показано, что деформация стали сопровождается разбиением пластин феррита малоугловыми границами на фрагменты и существенным увеличением скалярной плотности дислокаций до 7,9-1010 см-2 (скалярная плотность дислокаций исходной стали 3,2-1010 см-2). Показано, что деформация сопровождается формированием внутренних полей напряжений, проявляющихся в виде изгибных контуров экстинкции. Отмечены источники полей напряжений. Выявлено разрушение пластин цементита по механизмам разрезания и растворения с последующим выносом углерода движущимися дислокациями в объем пластин феррита с образованием в них наноразмерных (8,3 нм) частиц третичного цементита округлой формы. Показано, что растворение пластин цементита сопровождается их фрагментацией (разделением на области когерентного рассеивания, средние размеры которых 9,3 нм).
- Open Access
- 1 March 2023
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 66 (1) , 50-56
Transformation of fine structure of lamellar pearlite under deformation of rail steel
The defective substructure of polycrystalline bodies causes substructural hardening and mechanical properties. Perlite, which is the main structural component of rails, undergoes a significant transformation during deformation, which is accompanied by a number of processes. In this paper, the methods of modern physical materials science were used to study and analyze the defective substructure of perlite of lamellar morphology and the properties of rail steel subjected to destruction under deformation conditions by single-axis stretching of flat samples. It was established that the ultimate strength varies from 1247 to 1335 MPa, and the relative deformation to failure – from 0.69 to 0.75. The formation of three zones of the fracture surface was observed: fibrous, radial and shear zones. Their shape and sizes were analyzed. Deformation of rail steel is accompanied by destruction of cementite plates of perlite colonies and repeated release of nanoscale particles of tertiary cementite approximately 8.3 nm in size in the volume of ferrite plates. The main mechanisms of destruction of cementite plates are cutting and dissolution. The dislocation substructure is represented by a chaotic distribution of dislocations and their clusters. The scalar density of dislocations in ferrite increases from 3.2·1010 cm–2 in the initial state to 7.9·1010 cm–2 when it is destroyed. Deformation is accompanied by formation of internal stress fields, manifested in the form of bending extinction contours. The sources of stress fields are the interface of cementite and ferrite plates, as well as grain boundaries. Fragmentation of ferrite and cementite plates was revealed. The average size of cementite fragments is 9.3 nm. In fracture zone of the rail steel sample, rotation of perlite grains was noted, indicating the presence of a rotational mode of deformation. Electron microscopic images of cementite plates show a change in the contrast, which may be associated with the formation of Cottrell’s atmospheres.
- 1 March 2023
- Published by National University of Science and Technology MISiS in Izvestiya. Ferrous Metallurgy
- Vol. 66 (1) , 50-56
Open AccessTransformation of fine structure of lamellar pearlite under deformation of rail steel
The defective substructure of polycrystalline bodies causes substructural hardening and mechanical properties. Perlite, which is the main structural component of rails, undergoes a significant transformation during deformation, which is accompanied by a number of processes. In this paper, the methods of modern physical materials science were used to study and analyze the defective substructure of perlite of lamellar morphology and the properties of rail steel subjected to destruction under deformation conditions by single-axis stretching of flat samples. It was established that the ultimate strength varies from 1247 to 1335 MPa, and the relative deformation to failure – from 0.69 to 0.75. The formation of three zones of the fracture surface was observed: fibrous, radial and shear zones. Their shape and sizes were analyzed. Deformation of rail steel is accompanied by destruction of cementite plates of perlite colonies and repeated release of nanoscale particles of tertiary cementite approximately 8.3 nm in size in the volume of ferrite plates. The main mechanisms of destruction of cementite plates are cutting and dissolution. The dislocation substructure is represented by a chaotic distribution of dislocations and their clusters. The scalar density of dislocations in ferrite increases from 3.2·1010 cm–2 in the initial state to 7.9·1010 cm–2 when it is destroyed. Deformation is accompanied by formation of internal stress fields, manifested in the form of bending extinction contours. The sources of stress fields are the interface of cementite and ferrite plates, as well as grain boundaries. Fragmentation of ferrite and cementite plates was revealed. The average size of cementite fragments is 9.3 nm. In fracture zone of the rail steel sample, rotation of perlite grains was noted, indicating the presence of a rotational mode of deformation. Electron microscopic images of cementite plates show a change in the contrast, which may be associated with the formation of Cottrell’s atmospheres.
- Open Access
Structural Phase Transformation of Rail Steel in Compression
The analysis of structure and defective substructure of rail steel in uniaxial compression to a degree of 50% is carried out. It is revealed that cold hardening has a multi-stage character and is accompanied by fragmentations of pearlite grains which is in field as the degree of deformation increases and reaches ≈ 0.4 volume of the foil studied at ε = 50%. The fragments being formed in ferrite plates are separated by low-angle boundaries. The average size of the fragmented ferrite decreases from 240 nm at ε = 15% to 200 nm at ε = 50%. Concurrently with the ferrite fragmentation, fragments of cementite are also observed. It is found that the sizes of the cementite fragments are in a range of 15 to 20 nm and depend weakly on the degree of sample deformation. The cementite fragmentation is caused by deformation-induced carbon dissolution and dislocation-induced fracture. The carbon atoms diffuse from cementite crystal to dislocations, which move through an interplanar space to form particles of tertiary cementite at nanoscale (2–4 nm). It is found that the increase in the degree of deformation is accompanied by a decrease in the scalar and an excess dislocation density. A physical interpretation of the observations has been given.
Open AccessStructural Phase Transformation of Rail Steel in Compression
The analysis of structure and defective substructure of rail steel in uniaxial compression to a degree of 50% is carried out. It is revealed that cold hardening has a multi-stage character and is accompanied by fragmentations of pearlite grains which is in field as the degree of deformation increases and reaches ≈ 0.4 volume of the foil studied at ε = 50%. The fragments being formed in ferrite plates are separated by low-angle boundaries. The average size of the fragmented ferrite decreases from 240 nm at ε = 15% to 200 nm at ε = 50%. Concurrently with the ferrite fragmentation, fragments of cementite are also observed. It is found that the sizes of the cementite fragments are in a range of 15 to 20 nm and depend weakly on the degree of sample deformation. The cementite fragmentation is caused by deformation-induced carbon dissolution and dislocation-induced fracture. The carbon atoms diffuse from cementite crystal to dislocations, which move through an interplanar space to form particles of tertiary cementite at nanoscale (2–4 nm). It is found that the increase in the degree of deformation is accompanied by a decrease in the scalar and an excess dislocation density. A physical interpretation of the observations has been given.