P. S. Shivakumar Gouda
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
P. S. Shivakumar Gouda has a total of 109 co-authors. Here are the top co-authors by number of shared publications:
- M. A. Umarfarooq
Karpagam Academy of Higher Education
11 shared publications - Maruthi Prashanth B. H.
Department of Mechanical Engineering, AGMR College of Engineering and Technology, Affiliated to Visvesvaraya Technological University Belagavi
11 shared publications - I. Sridhar
Research Center, Department of Mechanical Engineering, SDM College of Engineering & Technology, Dharwad, Visvesvaraya Technological University, Belagavi, Karnataka, India
6 shared publications Abhilash Edacherian
Department of Mechanical Engineering College of Engineering, King Khalid University Abha Saudi Arabia
5 shared publicationsAravind Muddebihal
Research Center, Department of Mechanical Engineering Dayananda Sagar College of Engineering, Bengaluru, Visvesvaraya Technological University Belagavi Karnataka India
4 shared publicationsG.B. Veeresh Kumar
Department of Mechanical Engineering, Amrita School of Engineering, Amrita Vishwa Vidyapeetham, Amrita University, Bangalore Campus, Karnataka, India
4 shared publications
Latest Publications
- Open Access
- 16 October 2025
- Published by Gruppo Italiano Frattura in Fracture and Structural Integrity
- Vol. 20 (75) , 76-87
Realization of introducing non-woven veil on interlaminar radial strength of Glass Epoxy L-Bend composites
This study investigates the effect of interleaving non-woven veils and their surface areal density on the curved beam strength (CBS) and interlaminar radial stress (ILRS) of glass/epoxy L-bend composite laminates. Carbon veils with areal densities of 15, 20, and 30 g/m2 , and glass veils with 25 and 30 g/m2 were used as interleaving materials. The L-bend laminates, both interleaved and non-interleaved, were fabricated using the compression moulding technique. A four-point bending test was employed to evaluate the influence of veil interleaving and areal density on CBS and ILRS. The experimental results demonstrated that interleaving with carbon and glass non-woven veils significantly affects the performance of curved laminates. Notably, the CBS of the glass/epoxy laminate improved by 88% and 17% for specimens interleaved with 15 g/m2 carbon and 30 g/m2 glass veils, respectively. Furthermore, the ILRS of carbon veil-interleaved laminates showed a strong dependence on the veil’s areal density. In contrast, interleaving with glass veils did not exhibit a significant effect on ILRS. Finally, the fracture surfaces of the tested laminates were examined using scanning electron microscopy (SEM) to identify the various failure modes in the curved region and to understand the underlying fracture mechanisms.
- 16 October 2025
- Published by Gruppo Italiano Frattura in Fracture and Structural Integrity
- Vol. 20 (75) , 76-87
Open AccessRealization of introducing non-woven veil on interlaminar radial strength of Glass Epoxy L-Bend composites
This study investigates the effect of interleaving non-woven veils and their surface areal density on the curved beam strength (CBS) and interlaminar radial stress (ILRS) of glass/epoxy L-bend composite laminates. Carbon veils with areal densities of 15, 20, and 30 g/m2 , and glass veils with 25 and 30 g/m2 were used as interleaving materials. The L-bend laminates, both interleaved and non-interleaved, were fabricated using the compression moulding technique. A four-point bending test was employed to evaluate the influence of veil interleaving and areal density on CBS and ILRS. The experimental results demonstrated that interleaving with carbon and glass non-woven veils significantly affects the performance of curved laminates. Notably, the CBS of the glass/epoxy laminate improved by 88% and 17% for specimens interleaved with 15 g/m2 carbon and 30 g/m2 glass veils, respectively. Furthermore, the ILRS of carbon veil-interleaved laminates showed a strong dependence on the veil’s areal density. In contrast, interleaving with glass veils did not exhibit a significant effect on ILRS. Finally, the fracture surfaces of the tested laminates were examined using scanning electron microscopy (SEM) to identify the various failure modes in the curved region and to understand the underlying fracture mechanisms.
- 23 July 2025
- Published by Wiley in Polymer Composites
- Vol. 47 (1) , 887-897
Coupled Effects of In‐Plane Fiber Waviness and Circular Cutout on Axial Buckling Behavior of Glass‐Epoxy Composites
Coupled effects of in‐plane fiber waviness and the presence of circular cutouts in glass fiber‐reinforced laminates (GFRLs) were investigated under the action of buckling load. The research evaluates the wave severity, structural integrity, and failure processes of composites by combining cutting‐edge image processing methods with experimental testing. Composites were fabricated using a novel manufacturing technique to induce in‐plane fiber waviness. Image processing techniques, using the OpenCV library in Python, were applied to measure the waviness ratio (WR) in the composites. These measurements were validated by comparison with instrumental results to ensure accuracy. Circular cutouts were drilled in the waviness region to investigate the coupled effects of WR and cutouts. These composites were then subjected to actual tests to assess their buckling behavior. The findings of the study reveal that the composite without waviness and without a circular cut exhibited the highest critical buckling load. Further, composites exhibiting a WR of 0.032, 0.042, 0.052, 0.062, and 0.072 showed about 19%, 22%, 24%, 26%, and 28% decrease in load‐bearing capacity, respectively. Moreover, a significant coupled impact was seen when these composites included a circular cutout of 4 mm diameter, which resulted in 25%, 28%, 32%, 35%, and 38% reduction in their load‐bearing capacity, respectively. Additionally, finite element (FE) simulations reliably assess GFRL by capturing buckling behavior with the variation of 3.15%–7.79% with respect to experimental results. Finally, tested composites were examined through a scanning electron microscope (SEM) to explore the modes of failure and to understand their failure mechanism.
- 23 July 2025
- Published by Wiley in Polymer Composites
- Vol. 47 (1) , 887-897
Coupled Effects of In‐Plane Fiber Waviness and Circular Cutout on Axial Buckling Behavior of Glass‐Epoxy Composites
Coupled effects of in‐plane fiber waviness and the presence of circular cutouts in glass fiber‐reinforced laminates (GFRLs) were investigated under the action of buckling load. The research evaluates the wave severity, structural integrity, and failure processes of composites by combining cutting‐edge image processing methods with experimental testing. Composites were fabricated using a novel manufacturing technique to induce in‐plane fiber waviness. Image processing techniques, using the OpenCV library in Python, were applied to measure the waviness ratio (WR) in the composites. These measurements were validated by comparison with instrumental results to ensure accuracy. Circular cutouts were drilled in the waviness region to investigate the coupled effects of WR and cutouts. These composites were then subjected to actual tests to assess their buckling behavior. The findings of the study reveal that the composite without waviness and without a circular cut exhibited the highest critical buckling load. Further, composites exhibiting a WR of 0.032, 0.042, 0.052, 0.062, and 0.072 showed about 19%, 22%, 24%, 26%, and 28% decrease in load‐bearing capacity, respectively. Moreover, a significant coupled impact was seen when these composites included a circular cutout of 4 mm diameter, which resulted in 25%, 28%, 32%, 35%, and 38% reduction in their load‐bearing capacity, respectively. Additionally, finite element (FE) simulations reliably assess GFRL by capturing buckling behavior with the variation of 3.15%–7.79% with respect to experimental results. Finally, tested composites were examined through a scanning electron microscope (SEM) to explore the modes of failure and to understand their failure mechanism.
- 27 June 2025
- Published by Wiley in Polymer Composites
- Vol. 46 (18) , 16877-16885
Dual Microcapsules Self‐Healing Performance in Glass Epoxy Composite Under Flexural Load
This study examines the impact of dual‐microcapsule reinforcement in glass epoxy composites on self‐healing performance under flexural loading. Epoxy and hardener microcapsules encapsulated in a polymethylmethacrylate (PMMA) shell were synthesized using an oil‐in‐water emulsion solvent evaporation technique. Scanning electronic microscopy (SEM) analysis was conducted to assess the morphology, size variation, and distribution of the microcapsules. Glass epoxy laminate was fabricated using a manual layup technique by incorporating dual microcapsules with 5, 10, and 15 wt%. The effect of dual‐microcapsule reinforcement on flexural strength and healing efficiency was evaluated through three‐point bending tests. These results demonstrated a notable improvement in flexural strength with a maximum increase of approximately 27% observed in composites reinforced with 10 wt% microcapsules compared to the unreinforced composite. Furthermore, all the microcapsule‐reinforced composites exhibited significant healing efficiencies of 42%, 63%, and 50% for 5, 10, and 15 wt% microcapsule‐filled composites, respectively. The SEM analysis of the fractured composites revealed insights into fracture mechanisms, including microcapsule rupture, crack deviation, and the formation of a rough matrix surface, indicating successful polymerization and effective mitigation of microcrack propagation.
- 27 June 2025
- Published by Wiley in Polymer Composites
- Vol. 46 (18) , 16877-16885
Dual Microcapsules Self‐Healing Performance in Glass Epoxy Composite Under Flexural Load
This study examines the impact of dual‐microcapsule reinforcement in glass epoxy composites on self‐healing performance under flexural loading. Epoxy and hardener microcapsules encapsulated in a polymethylmethacrylate (PMMA) shell were synthesized using an oil‐in‐water emulsion solvent evaporation technique. Scanning electronic microscopy (SEM) analysis was conducted to assess the morphology, size variation, and distribution of the microcapsules. Glass epoxy laminate was fabricated using a manual layup technique by incorporating dual microcapsules with 5, 10, and 15 wt%. The effect of dual‐microcapsule reinforcement on flexural strength and healing efficiency was evaluated through three‐point bending tests. These results demonstrated a notable improvement in flexural strength with a maximum increase of approximately 27% observed in composites reinforced with 10 wt% microcapsules compared to the unreinforced composite. Furthermore, all the microcapsule‐reinforced composites exhibited significant healing efficiencies of 42%, 63%, and 50% for 5, 10, and 15 wt% microcapsule‐filled composites, respectively. The SEM analysis of the fractured composites revealed insights into fracture mechanisms, including microcapsule rupture, crack deviation, and the formation of a rough matrix surface, indicating successful polymerization and effective mitigation of microcrack propagation.
- 26 June 2025
- Published by Wiley in Polymer Composites
- Vol. 46 (15) , 13804-13821
Role of Mesoscale Wire Mesh in Abaca–Pineapple–Epoxy Composites for Improved Mechanical Properties—An Experimental Study With ANN Prediction
This study examines how microscaled wire mesh reinforcement affects the mechanical performance of abaca–pineapple–epoxy composites. The composite structure incorporates four types of microsized wire meshes: stainless steel (SSWM), mild steel (MSWM), aluminium (AWM), and plastic (PWM). These were evaluated for their influence on tensile, flexural, impact, interlaminar shear, and fracture properties. Composites were fabricated using the hand layup method followed by hot pressing. Notably, the composites reinforced with MSWM demonstrated significantly better mechanical performance compared to the unreinforced abaca‐pineapple (PA) composite, with improvements of 34% in tensile strength, 38% in flexural strength, and 46% in interlaminar shear strength (ILSS). Furthermore, the fracture toughness increased by 78%, the impact strength rose by 72%, and hardness increased by 42%, underscoring the effectiveness of mild steel reinforcement.A machine learning‐based artificial neural network (ANN) model was developed to predict tensile strength and elastic modulus, achieving accuracy rates of 85% and 93%, respectively, for the MSWM composite. The ANN model demonstrated strong alignment between predicted and experimental results, affirming its capability to model complex behavior in hybrid composites. From the SEM analysis, it was observed that there is strong adhesion between MSWM and the matrix. These findings indicate that MSWM‐reinforced NF composites offer promising potential for structural applications in automotive, packaging, and construction industries.
- 26 June 2025
- Published by Wiley in Polymer Composites
- Vol. 46 (15) , 13804-13821
Role of Mesoscale Wire Mesh in Abaca–Pineapple–Epoxy Composites for Improved Mechanical Properties—An Experimental Study With ANN Prediction
This study examines how microscaled wire mesh reinforcement affects the mechanical performance of abaca–pineapple–epoxy composites. The composite structure incorporates four types of microsized wire meshes: stainless steel (SSWM), mild steel (MSWM), aluminium (AWM), and plastic (PWM). These were evaluated for their influence on tensile, flexural, impact, interlaminar shear, and fracture properties. Composites were fabricated using the hand layup method followed by hot pressing. Notably, the composites reinforced with MSWM demonstrated significantly better mechanical performance compared to the unreinforced abaca‐pineapple (PA) composite, with improvements of 34% in tensile strength, 38% in flexural strength, and 46% in interlaminar shear strength (ILSS). Furthermore, the fracture toughness increased by 78%, the impact strength rose by 72%, and hardness increased by 42%, underscoring the effectiveness of mild steel reinforcement.A machine learning‐based artificial neural network (ANN) model was developed to predict tensile strength and elastic modulus, achieving accuracy rates of 85% and 93%, respectively, for the MSWM composite. The ANN model demonstrated strong alignment between predicted and experimental results, affirming its capability to model complex behavior in hybrid composites. From the SEM analysis, it was observed that there is strong adhesion between MSWM and the matrix. These findings indicate that MSWM‐reinforced NF composites offer promising potential for structural applications in automotive, packaging, and construction industries.
- 28 May 2025
- Published by IOP Publishing in Engineering Research Express
- Vol. 7 (2) , 025551
Mechanical response of glass fibre tufted composites for structural applications
In the present work, Tufting of glass fibre laminas (GFL) was done using E Glass fibre yarn. Epoxy grade matrix is reinforced with constant volume fraction of Carbon Nanotubes (CNTs) and Tufted laminas/plies are fabricated. Mechanical properties such as Tensile, Flexural and Impact were investigated on the prepared composites. Tufting of GFL are done with three different configurations, [2 × 2], [3 × 3], [4 × 4], and plain laminates without tufting are also tested for comparison. Results reveal that tufting of plies in composites has positive effect in variations of mechanical properties. Tufting of composites have led to enhanced bending and tensile strengths. Due to enriched fibers packing near Tufting region than far locations exhibited improved properties. The tensile strength, flexural strength and impact resistance of tufted laminates were 5.34% to 34.85%, 19.79% to 58.43% and 7.43% to 12.53% greater than plain laminates respectively. Fiber pull-out, inadequate matrix diffusion, and stress accumulation along the z-direction tufting were identified by SEM analysis as contributing factors to failure processes. Because of through-thickness reinforcement a decreases delamination and thereby increases damage tolerance. Hence this supports the idea of greater tufting density by improving mechanical performance of tufted composites. The most efficient tufting pattern was the [2 × 2] pattern, which showed excellent mechanical qualities. According to these results, tufting is a practical way of reinforcing method for structural composite applications.
- 28 May 2025
- Published by IOP Publishing in Engineering Research Express
- Vol. 7 (2) , 025551
Mechanical response of glass fibre tufted composites for structural applications
In the present work, Tufting of glass fibre laminas (GFL) was done using E Glass fibre yarn. Epoxy grade matrix is reinforced with constant volume fraction of Carbon Nanotubes (CNTs) and Tufted laminas/plies are fabricated. Mechanical properties such as Tensile, Flexural and Impact were investigated on the prepared composites. Tufting of GFL are done with three different configurations, [2 × 2], [3 × 3], [4 × 4], and plain laminates without tufting are also tested for comparison. Results reveal that tufting of plies in composites has positive effect in variations of mechanical properties. Tufting of composites have led to enhanced bending and tensile strengths. Due to enriched fibers packing near Tufting region than far locations exhibited improved properties. The tensile strength, flexural strength and impact resistance of tufted laminates were 5.34% to 34.85%, 19.79% to 58.43% and 7.43% to 12.53% greater than plain laminates respectively. Fiber pull-out, inadequate matrix diffusion, and stress accumulation along the z-direction tufting were identified by SEM analysis as contributing factors to failure processes. Because of through-thickness reinforcement a decreases delamination and thereby increases damage tolerance. Hence this supports the idea of greater tufting density by improving mechanical performance of tufted composites. The most efficient tufting pattern was the [2 × 2] pattern, which showed excellent mechanical qualities. According to these results, tufting is a practical way of reinforcing method for structural composite applications.
- Open Access
- 1 January 2025
- Published by Materials Research Forum, LLC in Materials Research Proceedings
- Vol. 55, 7-11
Effect of heat treatment on mechanical and wear properties of aluminum tin (Pb free) bearing material
Aluminum tin is a lead-free bearing material and is widely used in automobile industries because of its anti-frictional, self-lubricating property. The present study focused on assessing the mechanical and wear properties of custom-made binary Al¬15Sn subjected to heat treatment at 250°C for 1 hour and then cooled in different mediums (furnace, air, and oil). Air-cooled samples showed slightly higher hardness properties, 40% more impact energy, and reduced weight loss (0.2 gms) than furnace (0.32 gms) and oil-cooled (0.52 gms) samples.
- 1 January 2025
- Published by Materials Research Forum, LLC in Materials Research Proceedings
- Vol. 55, 7-11
Open AccessEffect of heat treatment on mechanical and wear properties of aluminum tin (Pb free) bearing material
Aluminum tin is a lead-free bearing material and is widely used in automobile industries because of its anti-frictional, self-lubricating property. The present study focused on assessing the mechanical and wear properties of custom-made binary Al¬15Sn subjected to heat treatment at 250°C for 1 hour and then cooled in different mediums (furnace, air, and oil). Air-cooled samples showed slightly higher hardness properties, 40% more impact energy, and reduced weight loss (0.2 gms) than furnace (0.32 gms) and oil-cooled (0.52 gms) samples.
- 12 October 2024
- Published by Wiley in Polymer Composites
- Vol. 46 (3) , 2803-2814
Performance of glass epoxy composites under combined effect of in‐plane fiber waviness with circular cutout through tensile test, and image processing technique
Present study comprehensively explores the phenomenon of in‐plane fiber waviness in glass/epoxy fiber reinforced polymer (GFRP) composites. Utilizing a pioneering technique that employs a semi‐circular bar to induce controlled fiber waviness, coupled with image processing using OpenCV library in Python coding for precise measurement and analysis of in‐plane fiber waviness. This defect is commonly found in components fabricated with fiber‐reinforced composites. During the process of manufacturing fibers may deviate from their intended orientation due to process variables or resin flow dynamics. Understanding in‐plane fiber waviness is crucial due to its impact on mechanical properties of composites. It is essential for optimizing manufacturing processes and ensuring enhanced structural performance in diverse engineering applications through analysis of strength and failure mechanism. A novel study was conducted by introducing a circular cutout within the fiber waviness region to investigate the combined effect of multiple defects. The experimental tensile test reveals that as waviness ratio (WR) increases a significant decrease in its tensile strength and vice versa. The study incorporates scanning electron microscopy (SEM) image analysis to examine composite failure. By advancing the understanding of in‐plane fiber waviness and its implications, this research significantly contributes to ongoing efforts in composite design and optimization.Highlights: Adopting a cutting‐edge method to create controlled fiber waviness that makes use of a semi‐circular bar. Image processing with Python code that makes use of the OpenCV package to precisely measure and analyze in‐plane fiber waviness. A new investigation was carried out to examine the combined effect of multiple flaws by creating a circular cutout within the fiber waviness zone.
- 12 October 2024
- Published by Wiley in Polymer Composites
- Vol. 46 (3) , 2803-2814
Performance of glass epoxy composites under combined effect of in‐plane fiber waviness with circular cutout through tensile test, and image processing technique
Present study comprehensively explores the phenomenon of in‐plane fiber waviness in glass/epoxy fiber reinforced polymer (GFRP) composites. Utilizing a pioneering technique that employs a semi‐circular bar to induce controlled fiber waviness, coupled with image processing using OpenCV library in Python coding for precise measurement and analysis of in‐plane fiber waviness. This defect is commonly found in components fabricated with fiber‐reinforced composites. During the process of manufacturing fibers may deviate from their intended orientation due to process variables or resin flow dynamics. Understanding in‐plane fiber waviness is crucial due to its impact on mechanical properties of composites. It is essential for optimizing manufacturing processes and ensuring enhanced structural performance in diverse engineering applications through analysis of strength and failure mechanism. A novel study was conducted by introducing a circular cutout within the fiber waviness region to investigate the combined effect of multiple defects. The experimental tensile test reveals that as waviness ratio (WR) increases a significant decrease in its tensile strength and vice versa. The study incorporates scanning electron microscopy (SEM) image analysis to examine composite failure. By advancing the understanding of in‐plane fiber waviness and its implications, this research significantly contributes to ongoing efforts in composite design and optimization.Highlights: Adopting a cutting‐edge method to create controlled fiber waviness that makes use of a semi‐circular bar. Image processing with Python code that makes use of the OpenCV package to precisely measure and analyze in‐plane fiber waviness. A new investigation was carried out to examine the combined effect of multiple flaws by creating a circular cutout within the fiber waviness zone.
- Open Access
- 1 August 2024
- Published by IOP Publishing in Materials Research Express
- Vol. 11 (8) , 085309
The impact of ecological aging on the mechanical performance of jute-banana fibre phenol-formaldehyde hybrid composites
Natural fiber composites provide an environmentally favorable and sustainable alternative to traditional materials, greatly reducing environmental impact. Aging tests are required to evaluate the long-term mechanical performance and durability of these composites under varied situations, ensuring their dependability and safety over time. This study investigates the effects of ecological aging on jute-banana fiber reinforced phenol-formaldehyde (JBP-F) composites. The experiment involved fabricating JBP-F composites using jute and banana fibers with varying weight ratios (60:40, 50:50, 40:60, 30:70) and subjecting them to various aging tests like long-time water resistance, accelerated water resistance, thermal aging, hydrothermal aging, soil burial test, and accelerated weathering test. The result showed that the composite with a 50:50 jute-banana fiber to resin ratio (JBP-F50) outperformed the other compositions examined in terms of aging resistance. This balanced ratio likely optimized fiber-matrix interaction, leading to superior strength and water resistance. Higher fiber content composites (like JBP-F60) absorbed more water due to weaker bonding, while lower fiber content (JBP-F30) suffered more in high temperatures. All composites experienced strength loss during thermal and hydrothermal aging due to heat and moisture cycles. JBP-F50 again showed the least degradation, possibly due to the resin’s ability to recover. In soil burial tests, biodegradation impacted strength, with higher fiber content composites (JBP-F60) degrading more. Finally, weathering tests revealed some surface deterioration due to UV radiation. However, the resin offered protection, with JBP-F30 (higher resin content) experiencing the most weight loss.JBP-F50, with its balanced fiber-resin ratio, demonstrated the best resistance to various environmental stresses, making it a promising option for sustainable composite applications.
- 1 August 2024
- Published by IOP Publishing in Materials Research Express
- Vol. 11 (8) , 085309
Open AccessThe impact of ecological aging on the mechanical performance of jute-banana fibre phenol-formaldehyde hybrid composites
Natural fiber composites provide an environmentally favorable and sustainable alternative to traditional materials, greatly reducing environmental impact. Aging tests are required to evaluate the long-term mechanical performance and durability of these composites under varied situations, ensuring their dependability and safety over time. This study investigates the effects of ecological aging on jute-banana fiber reinforced phenol-formaldehyde (JBP-F) composites. The experiment involved fabricating JBP-F composites using jute and banana fibers with varying weight ratios (60:40, 50:50, 40:60, 30:70) and subjecting them to various aging tests like long-time water resistance, accelerated water resistance, thermal aging, hydrothermal aging, soil burial test, and accelerated weathering test. The result showed that the composite with a 50:50 jute-banana fiber to resin ratio (JBP-F50) outperformed the other compositions examined in terms of aging resistance. This balanced ratio likely optimized fiber-matrix interaction, leading to superior strength and water resistance. Higher fiber content composites (like JBP-F60) absorbed more water due to weaker bonding, while lower fiber content (JBP-F30) suffered more in high temperatures. All composites experienced strength loss during thermal and hydrothermal aging due to heat and moisture cycles. JBP-F50 again showed the least degradation, possibly due to the resin’s ability to recover. In soil burial tests, biodegradation impacted strength, with higher fiber content composites (JBP-F60) degrading more. Finally, weathering tests revealed some surface deterioration due to UV radiation. However, the resin offered protection, with JBP-F30 (higher resin content) experiencing the most weight loss.JBP-F50, with its balanced fiber-resin ratio, demonstrated the best resistance to various environmental stresses, making it a promising option for sustainable composite applications.
- Open Access
- 1 June 2024
- Published by IOP Publishing in Engineering Research Express
- Vol. 6 (2) , 022505
Techniques of creating in-plane fiber waviness in composites and its mechanical performance – a review
In-plane fiber waviness is a common manufacturing flaw in composites, which can be observed during the production of items such as wind turbine blades, industrial components, aircraft structures, and automobile parts, etc. When manufacturing large composite structures, the traditional hand lay-up with fabric is labor-intensive and comes with several other issues, leading to various defects. One major but often overlooked defect is in-plane fiber waviness. The current investigation provides an overview of creating several techniques of in-plane fiber waviness faults in composites. Previously, numerous techniques were reported by researchers, employed to induce in-plane fiber waviness with specific parameters for their investigations. An effort has been made to highlight the various non-destructive techniques used for characterizing in-plane fiber waviness. Additionally, this paper presents a compilation of data on the impact of in-plane fiber waviness on the mechanical performance of composites. The paper concludes by proposing scope for additional research in the area of in-plane fiber waviness. Further, a novel method was proposed for creating in-plane fiber waviness which can reduce the possible fiber rotation using semi-circular wooden bars along with clamping arrangements instead of circular bars in the earlier investigations. Consequently, this could be a significant approach which resembles with realistic in-plane waviness generated while producing fiber reinforced polymer (FRP) composite components.
- 1 June 2024
- Published by IOP Publishing in Engineering Research Express
- Vol. 6 (2) , 022505
Open AccessTechniques of creating in-plane fiber waviness in composites and its mechanical performance – a review
In-plane fiber waviness is a common manufacturing flaw in composites, which can be observed during the production of items such as wind turbine blades, industrial components, aircraft structures, and automobile parts, etc. When manufacturing large composite structures, the traditional hand lay-up with fabric is labor-intensive and comes with several other issues, leading to various defects. One major but often overlooked defect is in-plane fiber waviness. The current investigation provides an overview of creating several techniques of in-plane fiber waviness faults in composites. Previously, numerous techniques were reported by researchers, employed to induce in-plane fiber waviness with specific parameters for their investigations. An effort has been made to highlight the various non-destructive techniques used for characterizing in-plane fiber waviness. Additionally, this paper presents a compilation of data on the impact of in-plane fiber waviness on the mechanical performance of composites. The paper concludes by proposing scope for additional research in the area of in-plane fiber waviness. Further, a novel method was proposed for creating in-plane fiber waviness which can reduce the possible fiber rotation using semi-circular wooden bars along with clamping arrangements instead of circular bars in the earlier investigations. Consequently, this could be a significant approach which resembles with realistic in-plane waviness generated while producing fiber reinforced polymer (FRP) composite components.
- 6 May 2024
- Published by Wiley in Polymer Composites
- Vol. 45 (12) , 10654-10665
Interleaving carbon‐glass veils in glass epoxy composite for enhanced fracture toughness and interlaminar shear strength—A hybrid approach
The present study investigates the mode‐II fracture resistance and interlaminar shear strength (ILSS) in glass epoxy laminates with the aid of glass‐carbon veils hybrid interleaving technique. Hybrid interleaves were prepared using various areal densities of non‐woven carbon and glass veils. Two methods, specifically inter‐ply and inter‐weaved ply interleaved glass epoxy composite laminates were manufactured by hand layup technique. End notch flexural and short beam test specimens were tested to estimate the mode‐II fracture resistance and ILSS. Test results indicated that the interleaved with inter‐weaved veil composite exhibited ~58% to ~82% and ~13% to ~61% enhancement for inter‐ply veil composite laminates when compared to plain samples. In context with the short beam test, a significant enhancement of approximately 23% in ILSS was noticed for the plain inter‐weaved veil constructed with a lower areal density of the carbon veil. Finally, the plain inter‐weaved interleaving technique has a prominent role in enhancing the resistance to fracture and shear strength in Glass epoxy laminates. Further, the fracture mechanisms of non‐interleaved and hybrid ply interleaved composite laminates were observed by scanning electron microscopic images.Highlights: Interleaving non‐woven microfiber veil is the most promising and cost‐effective strategy to enhance the Interlayer toughness and strength. Interleaving techniques used in this investigation have a significant effect on interlaminar fracture toughness (IFT) and interlaminar shear strength (ILSS). The areal density of high‐modulus carbon veil showed a different phenomenal influence on IFT and ILSS.
- 6 May 2024
- Published by Wiley in Polymer Composites
- Vol. 45 (12) , 10654-10665
Interleaving carbon‐glass veils in glass epoxy composite for enhanced fracture toughness and interlaminar shear strength—A hybrid approach
The present study investigates the mode‐II fracture resistance and interlaminar shear strength (ILSS) in glass epoxy laminates with the aid of glass‐carbon veils hybrid interleaving technique. Hybrid interleaves were prepared using various areal densities of non‐woven carbon and glass veils. Two methods, specifically inter‐ply and inter‐weaved ply interleaved glass epoxy composite laminates were manufactured by hand layup technique. End notch flexural and short beam test specimens were tested to estimate the mode‐II fracture resistance and ILSS. Test results indicated that the interleaved with inter‐weaved veil composite exhibited ~58% to ~82% and ~13% to ~61% enhancement for inter‐ply veil composite laminates when compared to plain samples. In context with the short beam test, a significant enhancement of approximately 23% in ILSS was noticed for the plain inter‐weaved veil constructed with a lower areal density of the carbon veil. Finally, the plain inter‐weaved interleaving technique has a prominent role in enhancing the resistance to fracture and shear strength in Glass epoxy laminates. Further, the fracture mechanisms of non‐interleaved and hybrid ply interleaved composite laminates were observed by scanning electron microscopic images.Highlights: Interleaving non‐woven microfiber veil is the most promising and cost‐effective strategy to enhance the Interlayer toughness and strength. Interleaving techniques used in this investigation have a significant effect on interlaminar fracture toughness (IFT) and interlaminar shear strength (ILSS). The areal density of high‐modulus carbon veil showed a different phenomenal influence on IFT and ILSS.