Shun Myung Shin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Shun Myung Shin has a total of 40 co-authors. Here are the top co-authors by number of shared publications:
Dongseok Lee
Resources Recycling Research Center, Korea Institute of Geoscience and Mineral Resources (KIGAM), Daejeon, Republic of Korea
9 shared publicationsSung-Ho Joo
Resources Recovery Research Center, Korea Institute of Geoscience & Mineral Resources (KIGAM), 124 Gwahak-ro, Yuseong-gu, Daejeon 34132, Republic of Korea
8 shared publications- Dong Ju Shin
Resources Recycling Research Center, Resources Utilization Division Korea
7 shared publications Dong Ju Shin
Resources Recycling Research Center, Korea Institute of Geoscience and Mineral Resources (KIGAM), Daejeon, Republic of Korea
6 shared publications- Jei-Pil Wang
BB21 Plus Team, Department of Metallurgical Engineering, Pukyong National University, Busan 48513, Republic of Korea
6 shared publications - Sung-Ho Joo
Resources Recycling Research Center, Resources Utilization Division Korea
5 shared publications
Latest Publications
- 20 November 2023
- Published by Springer Nature in JOM
- Vol. 76 (3) , 1477-1484
Recovery of Lithium from Beta-Spodumene Through Serial Calcination and Water Leaching with CaO
- 20 November 2023
- Published by Springer Nature in JOM
- Vol. 76 (3) , 1477-1484
Recovery of Lithium from Beta-Spodumene Through Serial Calcination and Water Leaching with CaO
- Open Access
- 28 February 2023
- Published by The Korean Institute of Resources Recycling in Resources Recycling
- Vol. 32 (1) , 42-49
A Study on the Recovery of Lithium from Secondary Resources of Ceramic Glass Containing Li-Al-Si by Ca-based Salt Roasting and Water Leaching Process
The glass ceramic secondary resource containing Li-Al-Si is used in inductor, fireproof glass, and transparent cookware and accounts for 14% of the total consumption of Li, which is the second most widely used after Li-ion batteries. Therefore, new Li resources should be explored when the demand for Li is exploding, and extensive research on Li recovery is needed. Herein, we recovered Li from fireproof Li-Al-Si glass ceramic, which is a new secondary resource containing Li. The fireproof glass among all Li-Al-Si glass ceramics was used as raw material that contained 1.5% Li, 9.4% Al, and 28.9% Si. The process for recovering •
- 28 February 2023
- Published by The Korean Institute of Resources Recycling in Resources Recycling
- Vol. 32 (1) , 42-49
Open AccessA Study on the Recovery of Lithium from Secondary Resources of Ceramic Glass Containing Li-Al-Si by Ca-based Salt Roasting and Water Leaching Process
The glass ceramic secondary resource containing Li-Al-Si is used in inductor, fireproof glass, and transparent cookware and accounts for 14% of the total consumption of Li, which is the second most widely used after Li-ion batteries. Therefore, new Li resources should be explored when the demand for Li is exploding, and extensive research on Li recovery is needed. Herein, we recovered Li from fireproof Li-Al-Si glass ceramic, which is a new secondary resource containing Li. The fireproof glass among all Li-Al-Si glass ceramics was used as raw material that contained 1.5% Li, 9.4% Al, and 28.9% Si. The process for recovering •
- Open Access
- 28 February 2023
- Published by The Korean Institute of Resources Recycling in Resources Recycling
- Vol. 32 (1) , 33-41
Study for Manufacturing of Zinc Sulfate from Electric Arc Furnace Dust by Hydrometallrugical Process
Herein, we selectively recovered Zn and produced ZnSO 4 from electric arc furnace dust using a hydrometallurgical process. The analysis of the properties of the electric arc furnace dust revealed that the Fe content (9.9%) was relatively low while the Mn content (19%) was high as compared to the composition of general dust. Therefore, an appropriate hydrometallurgical process was designed based on the properties of the raw materials. In the leaching process involving the use of 1.6 M sulfuric acid and 20% solid-liquid ratio at 60℃ for 1 h, 85% of the Zn and Mn got dissolved while the Fe was not leached. To selectively recover Zn, a solvent extraction process using D2EHPA as the extractant was chosen, and 99% of the Zn was extracted using 0.8 M D2EHPA with 32% saponification and an O/A ratio of 2 using counter-current 3-stage extraction. Mn was entirely scrubbed with an aqueous sulfuric acid solution of pH 1.5. Finally, Zn was concentrated and stripped using 1.5 M sulfuric acid at an O/A ratio of 4 using counter-current 4-stage stripping. The stripping solution contained 40 g/L of Zn, and 99.9% of ZnSO 4 •H 2 O was obtained by vacuum distillation.
- 28 February 2023
- Published by The Korean Institute of Resources Recycling in Resources Recycling
- Vol. 32 (1) , 33-41
Open AccessStudy for Manufacturing of Zinc Sulfate from Electric Arc Furnace Dust by Hydrometallrugical Process
Herein, we selectively recovered Zn and produced ZnSO 4 from electric arc furnace dust using a hydrometallurgical process. The analysis of the properties of the electric arc furnace dust revealed that the Fe content (9.9%) was relatively low while the Mn content (19%) was high as compared to the composition of general dust. Therefore, an appropriate hydrometallurgical process was designed based on the properties of the raw materials. In the leaching process involving the use of 1.6 M sulfuric acid and 20% solid-liquid ratio at 60℃ for 1 h, 85% of the Zn and Mn got dissolved while the Fe was not leached. To selectively recover Zn, a solvent extraction process using D2EHPA as the extractant was chosen, and 99% of the Zn was extracted using 0.8 M D2EHPA with 32% saponification and an O/A ratio of 2 using counter-current 3-stage extraction. Mn was entirely scrubbed with an aqueous sulfuric acid solution of pH 1.5. Finally, Zn was concentrated and stripped using 1.5 M sulfuric acid at an O/A ratio of 4 using counter-current 4-stage stripping. The stripping solution contained 40 g/L of Zn, and 99.9% of ZnSO 4 •H 2 O was obtained by vacuum distillation.
- Open Access
- 28 February 2022
- Published by The Korean Institute of Resources Recycling in Resources Recycling
- Vol. 31 (1) , 65-77
Leaching Behavior of Vanadium and Possibility of Recovery of Valuable Metals from VTM Concentrate by Sulfuric Acid Leaching
- 28 February 2022
- Published by The Korean Institute of Resources Recycling in Resources Recycling
- Vol. 31 (1) , 65-77
Open AccessLeaching Behavior of Vanadium and Possibility of Recovery of Valuable Metals from VTM Concentrate by Sulfuric Acid Leaching
- Open Access
- 17 January 2022
- Published by Wiley in The Canadian Journal of Chemical Engineering
- Vol. 100 (12) , 3760-3767
Precipitation of lithium phosphate from lithium solution by using sodium phosphate
Lithium was studied to precipitate into Li3PO4 by adding Na3PO4 under various experimental conditions such as initial lithium concentration of the solution, initial pH of the solution, temperature, and the mol equivalent ratio of Na3PO4. The precipitation mechanism of Li3PO4 was investigated with the change of pH value of the solution over time. The precipitation efficiency of Li3PO4 was 95.4% in the condition of the mol equivalent ratio of Na3PO4 of 1, initial Li concentration of 7 g/L, initial pH of 9.5, and at 90°C. When Na3PO4 was added three times, divided in the mol equivalent ratio of 1 via the hydrolysis reaction of PO43−, which inhibits the Li3PO4 precipitation reaction, an excellent precipitation efficiency of 98.4% was obtained. Co‐precipitated Na2HPO4 with Li3PO4 was washed by distilled water in the condition of solid/liquid ratio of 10% and at 90°C. The purity of the final Li3PO4 product was found to be 99.1%.
- 17 January 2022
- Published by Wiley in The Canadian Journal of Chemical Engineering
- Vol. 100 (12) , 3760-3767
Open AccessPrecipitation of lithium phosphate from lithium solution by using sodium phosphate
Lithium was studied to precipitate into Li3PO4 by adding Na3PO4 under various experimental conditions such as initial lithium concentration of the solution, initial pH of the solution, temperature, and the mol equivalent ratio of Na3PO4. The precipitation mechanism of Li3PO4 was investigated with the change of pH value of the solution over time. The precipitation efficiency of Li3PO4 was 95.4% in the condition of the mol equivalent ratio of Na3PO4 of 1, initial Li concentration of 7 g/L, initial pH of 9.5, and at 90°C. When Na3PO4 was added three times, divided in the mol equivalent ratio of 1 via the hydrolysis reaction of PO43−, which inhibits the Li3PO4 precipitation reaction, an excellent precipitation efficiency of 98.4% was obtained. Co‐precipitated Na2HPO4 with Li3PO4 was washed by distilled water in the condition of solid/liquid ratio of 10% and at 90°C. The purity of the final Li3PO4 product was found to be 99.1%.
- 20 December 2021
- Published by Royal Society of Chemistry (RSC) in Green Chemistry
- Vol. 24 (2) , 790-799
Recovery of vanadium and cesium from spent sulfuric acid catalysts by a hydrometallurgical process
An environmentally friendly hydrometallurgical process was developed to recover vanadium and cesium selectively from spent sulfuric acid catalysts, and it has high recovery efficiency and economic advantages.
- 20 December 2021
- Published by Royal Society of Chemistry (RSC) in Green Chemistry
- Vol. 24 (2) , 790-799
Recovery of vanadium and cesium from spent sulfuric acid catalysts by a hydrometallurgical process
An environmentally friendly hydrometallurgical process was developed to recover vanadium and cesium selectively from spent sulfuric acid catalysts, and it has high recovery efficiency and economic advantages.
- Open Access
- 31 October 2021
- Published by The Korean Institute of Resources Recycling in Resources Recycling
- Vol. 30 (5) , 57-66
Study for Seperation Process of Copper from the Low-grade Copper Ore by Hydrometallrugical Process
- 31 October 2021
- Published by The Korean Institute of Resources Recycling in Resources Recycling
- Vol. 30 (5) , 57-66
Open AccessStudy for Seperation Process of Copper from the Low-grade Copper Ore by Hydrometallrugical Process
- 1 September 2021
- Published by Elsevier in Journal of Environmental Sciences
- Vol. 107, 98-110
Evaluation of leaching characteristic and kinetic study of lithium from lithium aluminum silicate glass-ceramics by NaOH
- 1 September 2021
- Published by Elsevier in Journal of Environmental Sciences
- Vol. 107, 98-110
Evaluation of leaching characteristic and kinetic study of lithium from lithium aluminum silicate glass-ceramics by NaOH
- Open Access
- 31 August 2021
- Published by The Korean Institute of Resources Recycling in Resources Recycling
- Vol. 30 (4) , 27-34
Vanadium Leaching Behavior from Domestic Vanadium Bearing Titanomagnetite Ore through CaO Roasting
- 31 August 2021
- Published by The Korean Institute of Resources Recycling in Resources Recycling
- Vol. 30 (4) , 27-34
Open AccessVanadium Leaching Behavior from Domestic Vanadium Bearing Titanomagnetite Ore through CaO Roasting
- Open Access
The Manufacture of Synthetic Rutile by Solvent Extraction of Tri-Alkyl Phosphine Oxide from HCl Leaching Solution of Soda-Roasted Ilmenite Ore
To manufacture TiO2, a high-purity synthetic rutile, the recovery of Ti was investigated using a hydro-metallurgical process. Using a feed solution containing 32050 mg/L Ti, 110 mg/L Si, 88 mg/L Nb, 2614 mg/L Fe, and 130 mg/L Zr, solvent-extraction experiments were conducted with alkyl phosphine oxide in conjunction with diluents such as kerosene and xylene. The results showed that the extraction mechanism of both diluents was very similar to slope analysis, which had a value of 1.9; however, the extraction equilibrium constant value of organic–metallic species in xylene as a diluent was lower than in kerosene as a diluent. This result affected the stripping efficiency of Ti in particular; therefore, xylene was selected as a diluent. To recover Ti ion from a leaching solution, a series of experiments was conducted, such as the McCabe–Thiele method and countercurrent simulation test for extraction and stripping of Ti. As a result, Ti and impurities such as Fe and Zr were extracted to 99.9% from Si and Nb under optimal conditions using countercurrent four-stage extraction, with 1 M Cyanex 923 at a ratio of organic phase/ aqueous phase=3. In the stripping test, Ti was selectively stripped to 90.1% from Fe and Zr in the organic phase by 1 M HCl. The obtained powder, which was hydrolyzed from an impurity-free solution, was analyzed to a purity of 99.9% by inductively coupled plasma. The TiO2, which has a spherical shape and a diameter of approximately 2 µm according to SEM, was evident by XRD.
Open AccessThe Manufacture of Synthetic Rutile by Solvent Extraction of Tri-Alkyl Phosphine Oxide from HCl Leaching Solution of Soda-Roasted Ilmenite Ore
To manufacture TiO2, a high-purity synthetic rutile, the recovery of Ti was investigated using a hydro-metallurgical process. Using a feed solution containing 32050 mg/L Ti, 110 mg/L Si, 88 mg/L Nb, 2614 mg/L Fe, and 130 mg/L Zr, solvent-extraction experiments were conducted with alkyl phosphine oxide in conjunction with diluents such as kerosene and xylene. The results showed that the extraction mechanism of both diluents was very similar to slope analysis, which had a value of 1.9; however, the extraction equilibrium constant value of organic–metallic species in xylene as a diluent was lower than in kerosene as a diluent. This result affected the stripping efficiency of Ti in particular; therefore, xylene was selected as a diluent. To recover Ti ion from a leaching solution, a series of experiments was conducted, such as the McCabe–Thiele method and countercurrent simulation test for extraction and stripping of Ti. As a result, Ti and impurities such as Fe and Zr were extracted to 99.9% from Si and Nb under optimal conditions using countercurrent four-stage extraction, with 1 M Cyanex 923 at a ratio of organic phase/ aqueous phase=3. In the stripping test, Ti was selectively stripped to 90.1% from Fe and Zr in the organic phase by 1 M HCl. The obtained powder, which was hydrolyzed from an impurity-free solution, was analyzed to a purity of 99.9% by inductively coupled plasma. The TiO2, which has a spherical shape and a diameter of approximately 2 µm according to SEM, was evident by XRD.