Dong-Woo Ryu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Dong-Woo Ryu has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Sang-Rak Sim
Department of Architectural Engineering, Daejin University, Pocheon-si 11159, Gyeonggi-do, Republic of Korea
5 shared publications - Euichul Hwang
Department of Architectural Engineering, Chungnam National University, 99 Daehak-ro, Yuseong-gu, Daejeon 34134, Korea
1 shared publication - Gyeong-Cheol Choe
Department of Architectural Engineering, Chungnam National University, 99 Daehak-ro, Yuseong-gu, Daejeon 34134, Korea
1 shared publication - Gyuyong Kim
Department of Architectural Engineering, Chungnam National University, Daejeon, Republic of Korea
1 shared publication - Jaesung Lee
Department of Electrical & Computer Engineering, College of Engineering & Computer Science University of Central Florida, Orlando, USA
1 shared publication - Jeongsoo Nam
Department of Architectural Engineering, Chungnam National University, 99 Daehak-ro, Yuseong-gu, Daejeon 34134, Republic of Korea
1 shared publication
Latest Publications
- Open Access
Experimental Study on Effects of CO2 Curing Conditions on Mechanical Properties of Cement Paste Containing CO2 Reactive Hardening Calcium Silicate Cement
Human survival is threatened by the rapid climate change due to global warming caused by the increase in CO2 emissions since the Second Industrial Revolution. This study developed a secondary cement product production technology by replacing cement, a conventional binder, with calcium silicate cement (CSC), i.e., CO2 reactive hardening cement, to reduce CO2 emissions and utilize CO2 from the cement industry, which emits CO2 in large quantities. Results showed that the carbonation depth, compressive strength increase rate, and CO2 sequestration rate increased as the CSC content increased, suggesting that CSC can be applied as a secondary cement product.
Open AccessExperimental Study on Effects of CO2 Curing Conditions on Mechanical Properties of Cement Paste Containing CO2 Reactive Hardening Calcium Silicate Cement
Human survival is threatened by the rapid climate change due to global warming caused by the increase in CO2 emissions since the Second Industrial Revolution. This study developed a secondary cement product production technology by replacing cement, a conventional binder, with calcium silicate cement (CSC), i.e., CO2 reactive hardening cement, to reduce CO2 emissions and utilize CO2 from the cement industry, which emits CO2 in large quantities. Results showed that the carbonation depth, compressive strength increase rate, and CO2 sequestration rate increased as the CSC content increased, suggesting that CSC can be applied as a secondary cement product.
- Open Access
Effect of the Concrete Slurry Waste Ratio on Supercritical CO2 Sequestration
To prevent drastic climate changes due to global warming, it is necessary to transition to a carbon-neutral society by reducing greenhouse gas emissions in all industrial sectors. This study aimed to develop carbon utilization sequestration technology that uses the concrete slurry water generated during the production of concrete as a new CO2 sink to reduce CO2 emissions from the cement industry. This was achieved by performing supercritical CO2 carbonation by varying the concrete slurry waste (CSW) ratio. The study’s results confirmed that, according to the CSW ratio (5 to 25%), complete carbonation occurred within only 10 min of the reaction at 40 °C and 100 bar.
Open AccessEffect of the Concrete Slurry Waste Ratio on Supercritical CO2 Sequestration
To prevent drastic climate changes due to global warming, it is necessary to transition to a carbon-neutral society by reducing greenhouse gas emissions in all industrial sectors. This study aimed to develop carbon utilization sequestration technology that uses the concrete slurry water generated during the production of concrete as a new CO2 sink to reduce CO2 emissions from the cement industry. This was achieved by performing supercritical CO2 carbonation by varying the concrete slurry waste (CSW) ratio. The study’s results confirmed that, according to the CSW ratio (5 to 25%), complete carbonation occurred within only 10 min of the reaction at 40 °C and 100 bar.
- Open Access
Supercritical CO2 Curing of Resource-Recycling Secondary Cement Products Containing Concrete Sludge Waste as Main Materials
This study aims to develop highly durable, mineral carbonation-based, resource-recycling, secondary cement products based on supercritical carbon dioxide (CO2) curing as part of carbon capture utilization technology that permanently fixes captured CO2. To investigate the basic characteristics of secondary cement products containing concrete sludge waste (CSW) as the main materials after supercritical CO2 curing, the compressive strengths of the paste and mortar (fabricated by using CSW as the main binder), ordinary Portland cement, blast furnace slag powder, and fly ash as admixtures were evaluated to derive the optimal mixture for secondary products. The carbonation curing method that can promote the surface densification (intensive CaCO3 formation) of the hardened body within a short period of time using supercritical CO2 curing was defined as “Lean Carbonation”. The optimal curing conditions were derived by evaluating the compressive strength and durability improvement effects of applying Lean Carbonation to secondary product specimens. As a result of the experiment, for specimens subjected to Lean Carbonation, compressive strength increased by up to 12%, and the carbonation penetration resistance also increased by more than 50%. The optimal conditions for Lean Carbonation used to improve compressive strength and durability were found to be 35 °C, 80 bar, and 1 min.
Open AccessSupercritical CO2 Curing of Resource-Recycling Secondary Cement Products Containing Concrete Sludge Waste as Main Materials
This study aims to develop highly durable, mineral carbonation-based, resource-recycling, secondary cement products based on supercritical carbon dioxide (CO2) curing as part of carbon capture utilization technology that permanently fixes captured CO2. To investigate the basic characteristics of secondary cement products containing concrete sludge waste (CSW) as the main materials after supercritical CO2 curing, the compressive strengths of the paste and mortar (fabricated by using CSW as the main binder), ordinary Portland cement, blast furnace slag powder, and fly ash as admixtures were evaluated to derive the optimal mixture for secondary products. The carbonation curing method that can promote the surface densification (intensive CaCO3 formation) of the hardened body within a short period of time using supercritical CO2 curing was defined as “Lean Carbonation”. The optimal curing conditions were derived by evaluating the compressive strength and durability improvement effects of applying Lean Carbonation to secondary product specimens. As a result of the experiment, for specimens subjected to Lean Carbonation, compressive strength increased by up to 12%, and the carbonation penetration resistance also increased by more than 50%. The optimal conditions for Lean Carbonation used to improve compressive strength and durability were found to be 35 °C, 80 bar, and 1 min.
- Open Access
Fundamental Studies on CO2 Sequestration of Concrete Slurry Water Using Supercritical CO2
To prevent drastic climate change due to global warming, it is necessary to transition to a carbon-neutral society by reducing greenhouse gas emissions in all industrial sectors. This study aims to prepare measures to reduce the greenhouse gas in the cement industry, which is a large source of greenhouse gas emissions. The research uses supercritical CO2 carbonation to develop a carbon utilization fixation technology that uses concrete slurry water generated via concrete production as a new CO2 fixation source. Experiments were conducted using this concrete slurry water and supernatant water under different conditions of temperature (40 and 80 °C), pressure (100 and 150 bar), and reaction time (10 and 30 min). The results showed that reaction for 10 min was sufficient for complete carbonation at a sludge solids content of 5%. However, reaction products of supernatant water could not be identified due to the presence of Ca(HCO3)2 as an aqueous solution, warranting further research.
Open AccessFundamental Studies on CO2 Sequestration of Concrete Slurry Water Using Supercritical CO2
To prevent drastic climate change due to global warming, it is necessary to transition to a carbon-neutral society by reducing greenhouse gas emissions in all industrial sectors. This study aims to prepare measures to reduce the greenhouse gas in the cement industry, which is a large source of greenhouse gas emissions. The research uses supercritical CO2 carbonation to develop a carbon utilization fixation technology that uses concrete slurry water generated via concrete production as a new CO2 fixation source. Experiments were conducted using this concrete slurry water and supernatant water under different conditions of temperature (40 and 80 °C), pressure (100 and 150 bar), and reaction time (10 and 30 min). The results showed that reaction for 10 min was sufficient for complete carbonation at a sludge solids content of 5%. However, reaction products of supernatant water could not be identified due to the presence of Ca(HCO3)2 as an aqueous solution, warranting further research.
- Open Access
Spalling Resistance of Fiber-Reinforced Ultra-High-Strength Concrete Subjected to the ISO-834 Standard Fire Curve: Effects of Thermal Strain and Water Vapor Pressure
The prevention and mitigation of spalling in high-strength concrete (HSC) rely on mixing polypropylene (PP) as an additive reinforcement. The dense internal structures of ultra-high-strength concrete (UHSC) result in risks associated with a high thermal stress and high water vapor pressure. Herein, the effects of pore formation and thermal strain on spalling are examined by subjecting fiber-laden UHSC to conditions similar to those under which the ISO-834 standard fire curve was obtained. Evaluation of the initial melting properties of the fibers based on thermogravimetric analysis (TGA) and differential thermal analysis (DTA) demon strated that although nylon fibers exhibit a higher melting point than polypropylene and polyethylene fibers, weight loss occurs below 200 °C. Nylon fibers were effective at reducing spalling in UHSC compared to polypropylene and polyethylene fibers as they rapidly melt, leading to pore formation. We anticipate that these results will serve as references for future studies on the prevention of spalling in fiber-reinforced UHSC.
Open AccessSpalling Resistance of Fiber-Reinforced Ultra-High-Strength Concrete Subjected to the ISO-834 Standard Fire Curve: Effects of Thermal Strain and Water Vapor Pressure
The prevention and mitigation of spalling in high-strength concrete (HSC) rely on mixing polypropylene (PP) as an additive reinforcement. The dense internal structures of ultra-high-strength concrete (UHSC) result in risks associated with a high thermal stress and high water vapor pressure. Herein, the effects of pore formation and thermal strain on spalling are examined by subjecting fiber-laden UHSC to conditions similar to those under which the ISO-834 standard fire curve was obtained. Evaluation of the initial melting properties of the fibers based on thermogravimetric analysis (TGA) and differential thermal analysis (DTA) demon strated that although nylon fibers exhibit a higher melting point than polypropylene and polyethylene fibers, weight loss occurs below 200 °C. Nylon fibers were effective at reducing spalling in UHSC compared to polypropylene and polyethylene fibers as they rapidly melt, leading to pore formation. We anticipate that these results will serve as references for future studies on the prevention of spalling in fiber-reinforced UHSC.
- Open Access
A Method for Instant Estimation of the Temperature Experienced by Fire-Damaged Reinforced Concrete Structures Using Titanium
When a concrete structure is exposed to fire, its structural safety is significantly compromised due to the spalling of members and scaling of concrete. In addition, its durability is substantially reduced due to certain chemical changes such as the dehydration of Ca(OH)2, the main hydration product of concrete, and the rehydration of CaO. Therefore, when fire damage occurs to a reinforced concrete (RC) building, rapid diagnosis and evaluation techniques are required for immediate repair and reinforcement, requiring a crucial step of quantitatively determining the heating temperature. This study aims to demonstrate a method of estimating the heating temperature experienced by fire damaged RC buildings. The experiments utilized two short RC column specimens with embedded titanium strips. The discoloration characteristics of titanium at high temperatures provided a quick, accurate, and simple mechanism for the estimation of the heating temperature by depth. Empirical equations were derived to estimate the heating temperature as a function of the discoloration characteristics of titanium. Thereafter, a comparison of this estimated temperature with the actual heating temperature measured using thermocouples revealed an average error of less than 20 °C, thereby demonstrating a significantly good correlation and an extremely high reliability of the proposed method.
Open AccessA Method for Instant Estimation of the Temperature Experienced by Fire-Damaged Reinforced Concrete Structures Using Titanium
When a concrete structure is exposed to fire, its structural safety is significantly compromised due to the spalling of members and scaling of concrete. In addition, its durability is substantially reduced due to certain chemical changes such as the dehydration of Ca(OH)2, the main hydration product of concrete, and the rehydration of CaO. Therefore, when fire damage occurs to a reinforced concrete (RC) building, rapid diagnosis and evaluation techniques are required for immediate repair and reinforcement, requiring a crucial step of quantitatively determining the heating temperature. This study aims to demonstrate a method of estimating the heating temperature experienced by fire damaged RC buildings. The experiments utilized two short RC column specimens with embedded titanium strips. The discoloration characteristics of titanium at high temperatures provided a quick, accurate, and simple mechanism for the estimation of the heating temperature by depth. Empirical equations were derived to estimate the heating temperature as a function of the discoloration characteristics of titanium. Thereafter, a comparison of this estimated temperature with the actual heating temperature measured using thermocouples revealed an average error of less than 20 °C, thereby demonstrating a significantly good correlation and an extremely high reliability of the proposed method.
- Open Access
- 30 September 2019
- Published by The Korean Movement Disorder Society in Journal of Movement Disorders
- Vol. 12 (3) , 172-176
The Impact of Impulsivity on Quality of Life in Early Drug-Naïve Parkinson’s Disease Patients
Impulse control disorders (ICDs) in Parkinson's disease (PD) are mostly related to dopamine replacement therapy (DRT); however, drug-naïve PD patients have also frequently experienced impulsivity. This phenomenon makes clinicians hesitate treating patients with DRT. In this study, we assessed the effect of impulsivity on quality of life (QOL) in drug-naïve PD patients. Two hundred three newly diagnosed, nonmedicated PD patients were enrolled, and they received structured clinical interviews, physical examinations and validated questionnaires to evaluate motor and nonmotor symptoms and QOL. Impulsivity was evaluated using the Questionnaire for Impulsive-Compulsive Disorders in Parkinson's Disease-Rating Scale (QUIP-RS). Thirty-eight patients (18.7%) had impulsivity with QUIP-RS scores ≥ 1 and 4 patients (2.0%) were diagnosed with combined ICDs. Motor and nonmotor symptoms were significantly correlated with the Parkinson's Disease Questionnaire-39 summary index. Female sex and QUIP-RS scores were also correlated with QOL in drug-naïve PD patients. The results of the present study showed that impulsivity negatively influences QOL in early drug-naïve PD patients. In addition, more severe motor and nonmotor symptoms were also associated with lower QOL. Such findings complicate treatment but provide valuable information for managing early PD.
- 30 September 2019
- Published by The Korean Movement Disorder Society in Journal of Movement Disorders
- Vol. 12 (3) , 172-176
Open AccessThe Impact of Impulsivity on Quality of Life in Early Drug-Naïve Parkinson’s Disease Patients
Impulse control disorders (ICDs) in Parkinson's disease (PD) are mostly related to dopamine replacement therapy (DRT); however, drug-naïve PD patients have also frequently experienced impulsivity. This phenomenon makes clinicians hesitate treating patients with DRT. In this study, we assessed the effect of impulsivity on quality of life (QOL) in drug-naïve PD patients. Two hundred three newly diagnosed, nonmedicated PD patients were enrolled, and they received structured clinical interviews, physical examinations and validated questionnaires to evaluate motor and nonmotor symptoms and QOL. Impulsivity was evaluated using the Questionnaire for Impulsive-Compulsive Disorders in Parkinson's Disease-Rating Scale (QUIP-RS). Thirty-eight patients (18.7%) had impulsivity with QUIP-RS scores ≥ 1 and 4 patients (2.0%) were diagnosed with combined ICDs. Motor and nonmotor symptoms were significantly correlated with the Parkinson's Disease Questionnaire-39 summary index. Female sex and QUIP-RS scores were also correlated with QOL in drug-naïve PD patients. The results of the present study showed that impulsivity negatively influences QOL in early drug-naïve PD patients. In addition, more severe motor and nonmotor symptoms were also associated with lower QOL. Such findings complicate treatment but provide valuable information for managing early PD.