Takahiro Suzuki
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Takahiro Suzuki has a total of 108 co-authors. Here are the top co-authors by number of shared publications:
Shohji Tsushima
55 shared publications- Patcharawat Charoen-Amornkitt
Electrochemical Energy Storage and Conversion Laboratory, Department of Mechanical Engineering, Faculty of Engineering, King Mongkut’s University of Technology Thonburi, 126 Pracha Uthit Rd., Bang Mod, Thung Khru, Bangkok 10140, Thailand
19 shared publications - Mehrzad Alizadeh
Department of Mechanical Engineering, Graduate School of Engineering, Osaka University, Suita, Osaka 565-0871, JAPAN
10 shared publications - Makoto Uchida
University of Yamanashi
8 shared publications Akihiro Iiyama
University of Yamanashi
7 shared publications- Shohji Tsushima
The University of Osaka
6 shared publications
Latest Publications
- Open Access
- 18 July 2026
- Published by Elsevier in International Journal of Heat and Mass Transfer
- Vol. 271
Thermodynamic origin of root-like architectures in topology-optimized porous electrodes
- 18 July 2026
- Published by Elsevier in International Journal of Heat and Mass Transfer
- Vol. 271
Open AccessThermodynamic origin of root-like architectures in topology-optimized porous electrodes
- Open Access
- 21 May 2026
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 173 (11)
Agglomeration and Peculiar Rheological Hysteresis Behavior of Electrode Slurries Containing Platinum-Supported Carbon and Ionomer
This study examined the correlation between particle agglomeration and the rheological properties of electrode slurries composed of porous electrode materials for polymer electrolyte fuel cells, and presented two different agglomeration mechanisms in the electrode slurries. Electrode slurries are used to fabricate the porous electrodes. The state of the electrode slurries is influenced by the materials, dispersion medium, and dispersion conditions, and is believed to affect the resulting porous electrode structure. However, the dispersion state of the materials within the electrode slurries remains inadequately understood. This study identified the peculiar rheological behavior in the rheological measurement of electrode slurries, which arises depending on the composition ratio of the materials and the dispersion conditions. The formation of two distinct particle agglomerate structures that differed in scale and formation mechanisms within the electrode slurries and their correlation with the rheological properties were revealed based on experimental approaches, including centrifugal classification, X-ray radiography, and rheo-small-angle X-ray scattering (rheo-SAXS).
- 21 May 2026
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 173 (11)
Open AccessAgglomeration and Peculiar Rheological Hysteresis Behavior of Electrode Slurries Containing Platinum-Supported Carbon and Ionomer
This study examined the correlation between particle agglomeration and the rheological properties of electrode slurries composed of porous electrode materials for polymer electrolyte fuel cells, and presented two different agglomeration mechanisms in the electrode slurries. Electrode slurries are used to fabricate the porous electrodes. The state of the electrode slurries is influenced by the materials, dispersion medium, and dispersion conditions, and is believed to affect the resulting porous electrode structure. However, the dispersion state of the materials within the electrode slurries remains inadequately understood. This study identified the peculiar rheological behavior in the rheological measurement of electrode slurries, which arises depending on the composition ratio of the materials and the dispersion conditions. The formation of two distinct particle agglomerate structures that differed in scale and formation mechanisms within the electrode slurries and their correlation with the rheological properties were revealed based on experimental approaches, including centrifugal classification, X-ray radiography, and rheo-small-angle X-ray scattering (rheo-SAXS).
- 27 December 2025
- Published by Elsevier in Journal of Power Sources
- Vol. 666
Engineered flow fields for enhanced vanadium redox flow battery performance using topology optimization
- 27 December 2025
- Published by Elsevier in Journal of Power Sources
- Vol. 666
Engineered flow fields for enhanced vanadium redox flow battery performance using topology optimization
- Open Access
- 1 September 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (9) , 090543
Investigation of Kinetic and Mass Transport Behaviors of VO2+ and VO2 + Ions by Using Symmetric Vanadium Redox Flow Battery Configuration
Improving electrode performance through heat treatment is an effective way to lower overpotentials of vanadium redox flow batteries (VRFBs). However, the effect of heat treatment on VO2+/VO2 + still needs to be further clarified. This study systematically investigated how electrode heat treatment affects the kinetic and mass transport behaviors of the VO2+/VO2 + couple in a symmetric VRFB. Total overpotential was separated into ohmic, activation, and mass transport contributions using electrochemical impedance spectroscopy, with additional analysis of precipitation-induced polarization. Results showed that heat treatment significantly increased the electrochemically active surface area (ECSA), improving wettability and electrolyte transport, thus markedly reducing activation and mass transport overpotentials despite a moderate decrease in the reaction rate constant. Notably, the electrode without heat treatment resulted in precipitation at moderate current densities (100–125 mA cm−2) for the reduction reaction, substantially increasing both activation and mass transport overpotentials due to pore blockage and ECSA loss. These findings clarify the effects of heat treatment in the VO2+/VO2 + reaction, emphasizing the importance of heat treating the VO2 + reduction electrode to prevent precipitation-induced performance deterioration. This study provides case-specific insights for SGL 39AA under 500 °C air treatment, which may inform electrode design under comparable conditions.
- 1 September 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (9) , 090543
Open AccessInvestigation of Kinetic and Mass Transport Behaviors of VO2+ and VO2 + Ions by Using Symmetric Vanadium Redox Flow Battery Configuration
Improving electrode performance through heat treatment is an effective way to lower overpotentials of vanadium redox flow batteries (VRFBs). However, the effect of heat treatment on VO2+/VO2 + still needs to be further clarified. This study systematically investigated how electrode heat treatment affects the kinetic and mass transport behaviors of the VO2+/VO2 + couple in a symmetric VRFB. Total overpotential was separated into ohmic, activation, and mass transport contributions using electrochemical impedance spectroscopy, with additional analysis of precipitation-induced polarization. Results showed that heat treatment significantly increased the electrochemically active surface area (ECSA), improving wettability and electrolyte transport, thus markedly reducing activation and mass transport overpotentials despite a moderate decrease in the reaction rate constant. Notably, the electrode without heat treatment resulted in precipitation at moderate current densities (100–125 mA cm−2) for the reduction reaction, substantially increasing both activation and mass transport overpotentials due to pore blockage and ECSA loss. These findings clarify the effects of heat treatment in the VO2+/VO2 + reaction, emphasizing the importance of heat treating the VO2 + reduction electrode to prevent precipitation-induced performance deterioration. This study provides case-specific insights for SGL 39AA under 500 °C air treatment, which may inform electrode design under comparable conditions.
- Open Access
- 1 July 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (7) , 070504
Sinusoidal Potential Scans for Unified Capacitance Measurement in Double-Layer and Redox-Active Electrolyte Systems
This study addresses challenges in capacitance measurement stemming from significant variations in results obtained through different analytical methods, which complicate the comparison of energy storage performance. It proposes sinusoidal potential scans as a unified and consistent approach for capacitance measurement across various analytical methods. The investigation begins with cyclic voltammetry (CV) measurements using triangular potential scans, highlighting discrepancies in capacitance values when analyzed with conventional methods. Numerical simulations were conducted to replicate these responses, distinguishing between Faradaic and non-Faradaic contributions, and revealing that discrepancies persist regardless of current type. Extended to CV with sinusoidal potential scans, commonly visualized as Lissajous plots in electrochemical impedance spectroscopy, the concept is validated through experimental results which demonstrate that capacitance values obtained using both differential and integral approaches are consistent across all analyses. The model was employed to investigate the effects of key parameters such as redox-active surface area, reaction rate constant, and constant phase element parameters, confirming that sinusoidal scans unify capacitance measurements, providing consistent values even when these parameters are varied. In summary, this study highlights the reliability and robustness of sinusoidal potential scans for capacitance evaluation, particularly in systems with mixed Faradaic and non-Faradaic contributions.
- 1 July 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (7) , 070504
Open AccessSinusoidal Potential Scans for Unified Capacitance Measurement in Double-Layer and Redox-Active Electrolyte Systems
This study addresses challenges in capacitance measurement stemming from significant variations in results obtained through different analytical methods, which complicate the comparison of energy storage performance. It proposes sinusoidal potential scans as a unified and consistent approach for capacitance measurement across various analytical methods. The investigation begins with cyclic voltammetry (CV) measurements using triangular potential scans, highlighting discrepancies in capacitance values when analyzed with conventional methods. Numerical simulations were conducted to replicate these responses, distinguishing between Faradaic and non-Faradaic contributions, and revealing that discrepancies persist regardless of current type. Extended to CV with sinusoidal potential scans, commonly visualized as Lissajous plots in electrochemical impedance spectroscopy, the concept is validated through experimental results which demonstrate that capacitance values obtained using both differential and integral approaches are consistent across all analyses. The model was employed to investigate the effects of key parameters such as redox-active surface area, reaction rate constant, and constant phase element parameters, confirming that sinusoidal scans unify capacitance measurements, providing consistent values even when these parameters are varied. In summary, this study highlights the reliability and robustness of sinusoidal potential scans for capacitance evaluation, particularly in systems with mixed Faradaic and non-Faradaic contributions.
- Open Access
- 1 May 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (5) , 050520
Investigation of Kinetic and Mass Transport Behaviors of V2+ and V3+ Ions Using Symmetric Vanadium Redox Flow Battery Configuration
Vanadium redox flow batteries (VRFBs) have attracted attention for their long lifespan, high safety, and flexible design. In the overall cell reaction, the V2+/V3+ redox couple on the negative side is considered performance-limiting due to its high overpotential, underscoring the need to enhance negative electrode performance. Heat treatment, an effective electrode modification method, improves the structural and interfacial properties of carbon electrodes, significantly impacting the reaction kinetics and mass transport of V2+ and V3+. This study employed a symmetric cell configuration with or without heat-treated electrodes to investigate the kinetic and mass transport processes of V2+ and V3+. Electrochemical impedance spectroscopy and polarization curve analysis separated impedance contributions and calculated overpotentials. The results indicated that V2+ has a higher reaction rate constant, while V3+ exhibits a larger diffusion coefficient, reflecting distinct kinetic and mass transport properties despite belonging to the same redox couple. Heat treatment enhanced porosity, wettability, and reaction kinetics, particularly improving V3+ reduction. However, single-side heat treatment caused electrode performance mismatches, limiting the overall enhancement. These findings emphasize the importance of considering the distinct behaviors of V2+ and V3+ rather than treating them as a single redox couple, providing valuable insights for improving VRFB performance.
- 1 May 2025
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 172 (5) , 050520
Open AccessInvestigation of Kinetic and Mass Transport Behaviors of V2+ and V3+ Ions Using Symmetric Vanadium Redox Flow Battery Configuration
Vanadium redox flow batteries (VRFBs) have attracted attention for their long lifespan, high safety, and flexible design. In the overall cell reaction, the V2+/V3+ redox couple on the negative side is considered performance-limiting due to its high overpotential, underscoring the need to enhance negative electrode performance. Heat treatment, an effective electrode modification method, improves the structural and interfacial properties of carbon electrodes, significantly impacting the reaction kinetics and mass transport of V2+ and V3+. This study employed a symmetric cell configuration with or without heat-treated electrodes to investigate the kinetic and mass transport processes of V2+ and V3+. Electrochemical impedance spectroscopy and polarization curve analysis separated impedance contributions and calculated overpotentials. The results indicated that V2+ has a higher reaction rate constant, while V3+ exhibits a larger diffusion coefficient, reflecting distinct kinetic and mass transport properties despite belonging to the same redox couple. Heat treatment enhanced porosity, wettability, and reaction kinetics, particularly improving V3+ reduction. However, single-side heat treatment caused electrode performance mismatches, limiting the overall enhancement. These findings emphasize the importance of considering the distinct behaviors of V2+ and V3+ rather than treating them as a single redox couple, providing valuable insights for improving VRFB performance.
- 22 November 2024
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2024-02 (44) , 3055
Effect of GDL Structure and Operating Conditions on PEMFC Performance and Liquid Water Removal
Proton exchange membrane fuel cells (PEMFCs) are a highly efficient and environmentally friendly energy device that has potential for fuel cell vehicles and other applications due to its low operating temperature and compact size. The PEMFC is assembled by placing a membrane electrode assembly (MEA), which consists of a polymer electrolyte membrane with a catalyst layer and a gas diffusion layer on both sides, between separators. The GDL is responsible for diffusion of the reaction gas into the catalyst layers, current collection and removal of produced water. Excessive accumulation of produced liquid water within the GDL, known as flooding, inhibits reaction gas feed and causes concentration overpotential. Therefore, clarification of oxygen transport and produced water removal characteristics is essential to improve cell performance. The objective of this study is to clarify the effects of different GDL structures and operating conditions, such as cell composition, gas flow rate, and humidification conditions, on the liquid water production and removal characteristics and power generation. In this study, the cells with two types of GDLs were prepared and the liquid-water behavior in the MEA and the power generation performance during fuel cell operation under various conditions were investigated using X-ray radiography. Since the effect of GDL structure depends on the cell composition and operating conditions, the GDLs were characterized under the power generation tests of the cell. PEMFCs with a catalyst layer reaction area and a GDL area of 5×8 mm2 were constructed. Two types of GDL structures were used in the cathode. One was a conventional GDL (SIGRACET®GDL28BC, SGL) and the other was a novel GDL developed by Enomoto Co., Ltd [1-4]. On the other hand, the same GDL (28BC) was used in the anode. The PEMFC was observed with an X-ray imaging system consisting of an X-ray source (TX-9000D, Mars Tohken Solution) and a detector (C15926-01, Hamamatsu Photonics). Hydrogen and air were supplied to the anode and cathode, respectively. The relative humidity of the anode and cathode was 90%. In-situ observation of the liquid water behavior in the PEMFC was performed by taking images in the MEA cross-sectional direction simultaneously with power generation. Figure 1 shows an X-ray visualization image of liquid water after 800 seconds of power generation at a current density of 0.5 A/cm2 under highly humidified conditions. In this condition, excessive water was produced, causing some of the channels to become plugged with liquid water. The average liquid water thickness of the GDLs under the unblocked channel, indicated by the yellow frame in the figure, was 1.33 mm for the Enomoto GDL and 2.75 mm for the SGL GDL. The result suggests that the liquid water removal property under the operating condition is different depending on the types of GDLs. Acknowledgments This work was partially supported by NEDO of Japan through the ECCEED_GDL project. References [1] M. Watanabe et al., J. Electrochem. Soc., 166, F3210 (2019). [2] M. Nasu et al., J. Power Sources, 530, 231251 (2022). [3] T. Inoue et al., J. Electrochem. Soc., 169, 114504 (2022). [4] T. Inoue et al., J. Power Sources, 585, 233623 (2023). Figure 1
- 22 November 2024
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2024-02 (44) , 3055
Effect of GDL Structure and Operating Conditions on PEMFC Performance and Liquid Water Removal
Proton exchange membrane fuel cells (PEMFCs) are a highly efficient and environmentally friendly energy device that has potential for fuel cell vehicles and other applications due to its low operating temperature and compact size. The PEMFC is assembled by placing a membrane electrode assembly (MEA), which consists of a polymer electrolyte membrane with a catalyst layer and a gas diffusion layer on both sides, between separators. The GDL is responsible for diffusion of the reaction gas into the catalyst layers, current collection and removal of produced water. Excessive accumulation of produced liquid water within the GDL, known as flooding, inhibits reaction gas feed and causes concentration overpotential. Therefore, clarification of oxygen transport and produced water removal characteristics is essential to improve cell performance. The objective of this study is to clarify the effects of different GDL structures and operating conditions, such as cell composition, gas flow rate, and humidification conditions, on the liquid water production and removal characteristics and power generation. In this study, the cells with two types of GDLs were prepared and the liquid-water behavior in the MEA and the power generation performance during fuel cell operation under various conditions were investigated using X-ray radiography. Since the effect of GDL structure depends on the cell composition and operating conditions, the GDLs were characterized under the power generation tests of the cell. PEMFCs with a catalyst layer reaction area and a GDL area of 5×8 mm2 were constructed. Two types of GDL structures were used in the cathode. One was a conventional GDL (SIGRACET®GDL28BC, SGL) and the other was a novel GDL developed by Enomoto Co., Ltd [1-4]. On the other hand, the same GDL (28BC) was used in the anode. The PEMFC was observed with an X-ray imaging system consisting of an X-ray source (TX-9000D, Mars Tohken Solution) and a detector (C15926-01, Hamamatsu Photonics). Hydrogen and air were supplied to the anode and cathode, respectively. The relative humidity of the anode and cathode was 90%. In-situ observation of the liquid water behavior in the PEMFC was performed by taking images in the MEA cross-sectional direction simultaneously with power generation. Figure 1 shows an X-ray visualization image of liquid water after 800 seconds of power generation at a current density of 0.5 A/cm2 under highly humidified conditions. In this condition, excessive water was produced, causing some of the channels to become plugged with liquid water. The average liquid water thickness of the GDLs under the unblocked channel, indicated by the yellow frame in the figure, was 1.33 mm for the Enomoto GDL and 2.75 mm for the SGL GDL. The result suggests that the liquid water removal property under the operating condition is different depending on the types of GDLs. Acknowledgments This work was partially supported by NEDO of Japan through the ECCEED_GDL project. References [1] M. Watanabe et al., J. Electrochem. Soc., 166, F3210 (2019). [2] M. Nasu et al., J. Power Sources, 530, 231251 (2022). [3] T. Inoue et al., J. Electrochem. Soc., 169, 114504 (2022). [4] T. Inoue et al., J. Power Sources, 585, 233623 (2023). Figure 1