A. V. Larionov
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
A. V. Larionov has a total of 50 co-authors. Here are the top co-authors by number of shared publications:
V. M. Chumarev
7 shared publications- L. Yu. Udoeva
Institute of Metallurgy, Ural Branch, Russian Academy of Sciences, Yekaterinburg, Russia
6 shared publications A. N. Rylov
Uralredmet JSC, Verkhnyaya Pyshma, Russia
4 shared publications- E. N. Selivanov
Russian Academy of Sciences
4 shared publications M. V. Trubachev
Uralredmet JSC, Verkhnyaya Pyshma, Russia
4 shared publicationsN. I. Sel’MEnskikh
Siberian Academy of Sciences
4 shared publications
Latest Publications
- 1 October 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (5-6) , 1458-1464
Results on Testing New Process to Make Nitrogen- and Carbon-Containing Precursor Based on Vanadium and Aluminum to Smelt V–Al–N–C Master Alloy
A new process to make complex nitrogen- and carbon-containing precursor materials V(51–43)–Al(30–36)–N(13.4–16.4)–C(2.7–6.0) is developed involving nitriding mixtures of powder of industrial alloys V(65–50)–Al with graphite using self-propagating high-temperature synthesis. The results of pilot tests are encouraging. The ratio of nitrogen to carbon can vary in precursors over a wide range: N/C = 5.5–2.2. X‑ray diffraction analysis confirms that in these materials nitrogen has the form of AlN and VN nitrides, and carbon has the form of double V2C and VC and triple V2Al0.96C1.1 carbides. It is proved experimentally that graphite can be replaced by alternative precursor V(51)–Al(30)–N(15)–C(2.7) in the charge of ladle aluminothermic smelting master alloy V–Al–N–C. The comparison is made between phase composition and distribution of nitride and carbide inclusions in master alloy V–Al–N–C ingots and in those of master alloys smelted using other carbon-containing materials. The comparison involves X-ray diffraction analysis, electron microscopy, and X-ray spectral microanalysis. Matching results are obtained. The nitrogen, carbon, and oxygen content in the ingot meets the requirements set forth in the technical specifications for the master alloys of grade V–Al–N–C.
- 1 October 2023
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 14 (5-6) , 1458-1464
Results on Testing New Process to Make Nitrogen- and Carbon-Containing Precursor Based on Vanadium and Aluminum to Smelt V–Al–N–C Master Alloy
A new process to make complex nitrogen- and carbon-containing precursor materials V(51–43)–Al(30–36)–N(13.4–16.4)–C(2.7–6.0) is developed involving nitriding mixtures of powder of industrial alloys V(65–50)–Al with graphite using self-propagating high-temperature synthesis. The results of pilot tests are encouraging. The ratio of nitrogen to carbon can vary in precursors over a wide range: N/C = 5.5–2.2. X‑ray diffraction analysis confirms that in these materials nitrogen has the form of AlN and VN nitrides, and carbon has the form of double V2C and VC and triple V2Al0.96C1.1 carbides. It is proved experimentally that graphite can be replaced by alternative precursor V(51)–Al(30)–N(15)–C(2.7) in the charge of ladle aluminothermic smelting master alloy V–Al–N–C. The comparison is made between phase composition and distribution of nitride and carbide inclusions in master alloy V–Al–N–C ingots and in those of master alloys smelted using other carbon-containing materials. The comparison involves X-ray diffraction analysis, electron microscopy, and X-ray spectral microanalysis. Matching results are obtained. The nitrogen, carbon, and oxygen content in the ingot meets the requirements set forth in the technical specifications for the master alloys of grade V–Al–N–C.
- 1 March 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 12 (2) , 280-287
Effect of Yttrium on the Structural-Phase State of the In Situ Mo–15.3 V–10.5 Si Composite
By means of X-ray phase analysis and energy-dispersive X-ray analysis, the effect of yttrium on the structural-phase state of the hypoeutectic Mo–15.3 V–10.5 Si alloy is investigated. It is established that the main phases of the Мо–(15.4–14.3) V–(10.6–9.8) Si–(0.3–5.3) Y alloys obtained under the conditions of nonequilibrium solidification are the (Mo1 – xVx)ss metal solid solution (matrix), (Mo1 – xVx)3Si silicide solid solution, and Y5Si3 silicide. In alloys doped with yttrium up to 1.0 at %, the space between dendrites of the (Mo1 – xVx)ss metal phase is filled with the (Mo1 – xVx)3Si solid solution, and at the boundaries of the metal solid solution, Y5Si3 is located. At the yttrium concentration of alloys higher than 3.0 at %, space between the (Mo1 – xVx)ss dendrites is filled with Y5Si3 silicide, inside which (Mo1 – xVx)3Si grains are formed. No ternary and quaternary yttrium-containing compounds are detected. The elemental composition of phases of the Мо–(15.4–14.3) V–(10.6–9.8) Si–(0.3–5.3) Y alloys is almost identical and is characterized by silicon nonstoichiometry. The silicon content of the (Mo1 – xVx)ss and (Mo1 – xVx)3Si phases lies within the accepted limits of the homogeneity region, and the silicon concentration of Y5Si3 (≈35.4 at %) goes beyond the defined limits. Doping the Мо–15.3 V–10.5 Si alloy with yttrium increases the degree of dispersion of the structure. Particles of the main structural constituents become close in size. At the same time, the volumetric ratio of the metal phase to the silicide phase increases as the yttrium content of the alloys is raised. The density of the alloys varies within 8.7 and 9.0 g/cm3.
- 1 March 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 12 (2) , 280-287
Effect of Yttrium on the Structural-Phase State of the In Situ Mo–15.3 V–10.5 Si Composite
By means of X-ray phase analysis and energy-dispersive X-ray analysis, the effect of yttrium on the structural-phase state of the hypoeutectic Mo–15.3 V–10.5 Si alloy is investigated. It is established that the main phases of the Мо–(15.4–14.3) V–(10.6–9.8) Si–(0.3–5.3) Y alloys obtained under the conditions of nonequilibrium solidification are the (Mo1 – xVx)ss metal solid solution (matrix), (Mo1 – xVx)3Si silicide solid solution, and Y5Si3 silicide. In alloys doped with yttrium up to 1.0 at %, the space between dendrites of the (Mo1 – xVx)ss metal phase is filled with the (Mo1 – xVx)3Si solid solution, and at the boundaries of the metal solid solution, Y5Si3 is located. At the yttrium concentration of alloys higher than 3.0 at %, space between the (Mo1 – xVx)ss dendrites is filled with Y5Si3 silicide, inside which (Mo1 – xVx)3Si grains are formed. No ternary and quaternary yttrium-containing compounds are detected. The elemental composition of phases of the Мо–(15.4–14.3) V–(10.6–9.8) Si–(0.3–5.3) Y alloys is almost identical and is characterized by silicon nonstoichiometry. The silicon content of the (Mo1 – xVx)ss and (Mo1 – xVx)3Si phases lies within the accepted limits of the homogeneity region, and the silicon concentration of Y5Si3 (≈35.4 at %) goes beyond the defined limits. Doping the Мо–15.3 V–10.5 Si alloy with yttrium increases the degree of dispersion of the structure. Particles of the main structural constituents become close in size. At the same time, the volumetric ratio of the metal phase to the silicide phase increases as the yttrium content of the alloys is raised. The density of the alloys varies within 8.7 and 9.0 g/cm3.
- 1 March 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 12 (2) , 296-306
Microstructure and Corrosion Resistance of the Alloys of Mo–15 at % Si–REE (Sc, Nd) in Air and in Air-Vapor Medium
The influence of REEs, for example, Sc and Nd, on the structural phase state and behavior at oxidation in a dry and humid atmosphere of hypoeutectic high-temperature composite Mo–Si, crystallization of which from melt proceeds with formation of a two-phase in situ composite, was investigated. Samples of the model alloys with different concentration of REE were formed by vacuum arc melting of the charge material consisting of the binary alloy Mo–15 Si (at %) and additions of the doping elements. According to the data of X-ray diffraction and electron microscopy, the phase composition was determined, the peculiarities of the microstructure and pattern of distribution of alloying constituents in metal silicide composites Mo–Mo3Si containing from 0.5 to 3.0 at % Sc or Nd were revealed. The corrosion resistance of alloys Mo–15 at % Si–REE (Sc, Nd) at continuous heating to 700 and 850°C in air and in an air-vapor medium was estimated by the methods of thermal analysis (differential scanning calorimetry (DSC) and differential thermal analysis (DTA)). It was demonstrated that microalloying of the Mo–15 at % Si alloy with scandium or neodymium within the limits of 0.5 at % results in decrease of the oxidation rate at heating in air to 850°C. Increase in the concentration of doping elements to 3.0 at % REE at oxidation in air adversely affects the corrosion resistance of the samples; at the same time, oxidation of the alloys with neodymium proceeds at a higher rate than that with scandium. In an air-vapor medium, at nonisothermal heating, the alloy doped with scandium is oxidized more slowly than the binary alloy, while the sample with neodymium, on the contrary, is oxidized at a much greater rate in comparison with dry air.
- 1 March 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 12 (2) , 296-306
Microstructure and Corrosion Resistance of the Alloys of Mo–15 at % Si–REE (Sc, Nd) in Air and in Air-Vapor Medium
The influence of REEs, for example, Sc and Nd, on the structural phase state and behavior at oxidation in a dry and humid atmosphere of hypoeutectic high-temperature composite Mo–Si, crystallization of which from melt proceeds with formation of a two-phase in situ composite, was investigated. Samples of the model alloys with different concentration of REE were formed by vacuum arc melting of the charge material consisting of the binary alloy Mo–15 Si (at %) and additions of the doping elements. According to the data of X-ray diffraction and electron microscopy, the phase composition was determined, the peculiarities of the microstructure and pattern of distribution of alloying constituents in metal silicide composites Mo–Mo3Si containing from 0.5 to 3.0 at % Sc or Nd were revealed. The corrosion resistance of alloys Mo–15 at % Si–REE (Sc, Nd) at continuous heating to 700 and 850°C in air and in an air-vapor medium was estimated by the methods of thermal analysis (differential scanning calorimetry (DSC) and differential thermal analysis (DTA)). It was demonstrated that microalloying of the Mo–15 at % Si alloy with scandium or neodymium within the limits of 0.5 at % results in decrease of the oxidation rate at heating in air to 850°C. Increase in the concentration of doping elements to 3.0 at % REE at oxidation in air adversely affects the corrosion resistance of the samples; at the same time, oxidation of the alloys with neodymium proceeds at a higher rate than that with scandium. In an air-vapor medium, at nonisothermal heating, the alloy doped with scandium is oxidized more slowly than the binary alloy, while the sample with neodymium, on the contrary, is oxidized at a much greater rate in comparison with dry air.
- 12 November 2020
- Published by Springer Nature in Metallurgist
- Vol. 64 (7-8) , 822-829
Effect of Preliminary Firing on Oxidation of Mo–Mo3Si Alloyed with Sc or Nd
- 12 November 2020
- Published by Springer Nature in Metallurgist
- Vol. 64 (7-8) , 822-829
Effect of Preliminary Firing on Oxidation of Mo–Mo3Si Alloyed with Sc or Nd
- 17 March 2019
- Published by Knowledge E DMCC in KnE Materials Science
- Vol. 5 (1) , 108-117
Phase Composition of Mo-Si-V Hypoeutectic Alloys
Phase Composition of Mo-Si-V Hypoeutectic Alloys
- 17 March 2019
- Published by Knowledge E DMCC in KnE Materials Science
- Vol. 5 (1) , 108-117
Phase Composition of Mo-Si-V Hypoeutectic Alloys
Phase Composition of Mo-Si-V Hypoeutectic Alloys
- 17 March 2019
- Published by Knowledge E DMCC in KnE Materials Science
- Vol. 5 (1) , 118-125
Structure and Phase Composition of V-Al-N-C Master Alloy
Structure and Phase Composition of V-Al-N-C Master Alloy
- 17 March 2019
- Published by Knowledge E DMCC in KnE Materials Science
- Vol. 5 (1) , 118-125
Structure and Phase Composition of V-Al-N-C Master Alloy
Structure and Phase Composition of V-Al-N-C Master Alloy
- Open Access
- 17 March 2019
- Published by Knowledge E DMCC in KnE Materials Science
- Vol. 5 (1) , 254-262
Research on the Process of Al–Mo–Ti Master Alloy Dissolution in Titanium
Research on the Process of Al–Mo–Ti Master Alloy Dissolution in Titanium
- 17 March 2019
- Published by Knowledge E DMCC in KnE Materials Science
- Vol. 5 (1) , 254-262
Open AccessResearch on the Process of Al–Mo–Ti Master Alloy Dissolution in Titanium
Research on the Process of Al–Mo–Ti Master Alloy Dissolution in Titanium
- 1 March 2018
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 9 (2) , 257-263
Influence of Rare Earth Elements on the Structural-Phase State of Mo–Si–X (X = Sc, Y, Nd) in situ Composites
The microstructure and phase composition of the Mo-Si alloy doped with Sc, Y or Nd were investigated. The methods of X-ray diffraction analysis (XRD), electron microscopy, and electron probe...
- 1 March 2018
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 9 (2) , 257-263
Influence of Rare Earth Elements on the Structural-Phase State of Mo–Si–X (X = Sc, Y, Nd) in situ Composites
The microstructure and phase composition of the Mo-Si alloy doped with Sc, Y or Nd were investigated. The methods of X-ray diffraction analysis (XRD), electron microscopy, and electron probe...
- 30 November 2017
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 60-64
Phase composition and thermal properties of ladle smelting slags of AVTU, AKhMK and ATsMO foundry alloys
Our article shows the results of X-ray phase and differential-thermal analysis of phase composition and thermal properties of rapidly cooled high-aluminous slags, formed during the aluminothermic smelting of AVTU (Al – V – Ti – C), AKhMK (Al – Cr – Mo – Si) and ATsMO (Al – Zr – Mo – Sn) foundry alloys in copper moulds. The AVTU and AKhMK slags have the following basic phases: Al2O3, CaAl12O19 (CA6) and CaOAl4O6 (CA2). According to the chemical analysis data, CaF2 was found in all slag samples, and a small amount of KCl was found in the AVTU foundry alloy smelting slag. This KCl was entered as halite into the foundry alloy smelting charge. The ATsMO foundry alloy smelting slag revealed the aluminate СaAl2O4 (CA) of orthorhombic and monoclinic crystal systems, clacium zirconates CaZrO3, CaZr4O9 and free aluminium oxide α-Al2O3.Two modifications of aluminate CaAl2O4 in slag are explained by metastability. The X-ray phase analysis showed that a high velocity of slag cooling and presence of small amounts of calcium fluoride and rare metal oxides in this slag have no significant effect on phase formation. The diffractometry data made a conclusion that the main phases of rapidly-cooled slags of ladle aluminothermic smelting of foundry alloys (based on rare refractory metals) are identical to the ones, formed in the equilibrium solidification of foundry alloys based on Al2O3 – CaO melts. The amorphism of the investigated slag samples is insignificant. Thermal analysis of the samples of AVTU, AKhMK and ATsMO slags defined the effects of devitrification and “cold” crystallization, confirming the presence of amorphous phases in slags, and endoeffects related to the smelting of their phase terms. The heating thermograms showed that the complete dissolutions of smelting slag of AVTU, AKhMK and ATsMO foundry alloys are in the temperatures of 1879 oC, 1881 oC and 1773 oC, respectively. In comparison with the AVTU and AKhMK slags, lower temperatures of ATsMO slag crystallization are connected with its lesser content of aluminium oxide.Our research work was carnied out with the financial support of the Program of the Ural Branch of RAS, project No. 15-6-3-30.
- 30 November 2017
- Published by Ore and Metals Publishing House in Tsvetnye Metally
- p. 60-64
Phase composition and thermal properties of ladle smelting slags of AVTU, AKhMK and ATsMO foundry alloys
Our article shows the results of X-ray phase and differential-thermal analysis of phase composition and thermal properties of rapidly cooled high-aluminous slags, formed during the aluminothermic smelting of AVTU (Al – V – Ti – C), AKhMK (Al – Cr – Mo – Si) and ATsMO (Al – Zr – Mo – Sn) foundry alloys in copper moulds. The AVTU and AKhMK slags have the following basic phases: Al2O3, CaAl12O19 (CA6) and CaOAl4O6 (CA2). According to the chemical analysis data, CaF2 was found in all slag samples, and a small amount of KCl was found in the AVTU foundry alloy smelting slag. This KCl was entered as halite into the foundry alloy smelting charge. The ATsMO foundry alloy smelting slag revealed the aluminate СaAl2O4 (CA) of orthorhombic and monoclinic crystal systems, clacium zirconates CaZrO3, CaZr4O9 and free aluminium oxide α-Al2O3.Two modifications of aluminate CaAl2O4 in slag are explained by metastability. The X-ray phase analysis showed that a high velocity of slag cooling and presence of small amounts of calcium fluoride and rare metal oxides in this slag have no significant effect on phase formation. The diffractometry data made a conclusion that the main phases of rapidly-cooled slags of ladle aluminothermic smelting of foundry alloys (based on rare refractory metals) are identical to the ones, formed in the equilibrium solidification of foundry alloys based on Al2O3 – CaO melts. The amorphism of the investigated slag samples is insignificant. Thermal analysis of the samples of AVTU, AKhMK and ATsMO slags defined the effects of devitrification and “cold” crystallization, confirming the presence of amorphous phases in slags, and endoeffects related to the smelting of their phase terms. The heating thermograms showed that the complete dissolutions of smelting slag of AVTU, AKhMK and ATsMO foundry alloys are in the temperatures of 1879 oC, 1881 oC and 1773 oC, respectively. In comparison with the AVTU and AKhMK slags, lower temperatures of ATsMO slag crystallization are connected with its lesser content of aluminium oxide.Our research work was carnied out with the financial support of the Program of the Ural Branch of RAS, project No. 15-6-3-30.