Takalani Madzivhandila
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Takalani Madzivhandila has a total of 20 co-authors. Here are the top co-authors by number of shared publications:
- Festus Ben
Federal Polytechnic Ede
3 shared publications - Maje Phasha
Advanced Materials Division, Mintek, 200 Malibongwe Drive, Randburg 2125, South Africa
3 shared publications - Willie Nheta
Mineral Processing and Technology Research Centre, University of Johannesburg, P.O. Box 17011, Doornfontein, Johannesburg 2028, South Africa
3 shared publications - Mbulelo Ngqase
Faculty of Engineering and Built Environment, University of Johannesburg, P.O. Box 524, Auckland Park, Johannesburg 2006, South Africa
2 shared publications - Peter Apata Olubambi
University of Johannesburg
2 shared publications - Adebayo Felix Owa
Department of Materials and Metallurgical Engineering, Federal University Oye-Ekiti, 371101 Oye-Ekiti, Nigeria
1 shared publication
Latest Publications
- Open Access
- 12 June 2026
- Published by IOP Publishing in Materials Research Express
- Vol. 13 (11) , 112001
Caesalpinia pulcherrima ash as a sustainable reinforcement in metallic biomaterials for biomedical applications: a review on mechanisms, compatibility, and prospects
Agro-waste-derived oxides are increasingly investigated as sustainable reinforcement phases in metal-matrix composites. However, their translation into biomedical metallic systems remains underexplored. Caesalpinia pulcherrima (Pride of Barbados) ash represents an oxide-bearing biomass derivative with a reported silica-rich composition. Yet, its suitability as a reinforcement in biomedical metal matrix composites (MMC) has not been systematically evaluated. This review assesses whether Caesalpinia pulcherrima ash (CPA) satisfies the chemical, mechanical, electrochemical, and biological criteria required of reinforcements in biomedical metals (316L stainless steel, Ti-6Al-4V, Cr–Co–Mn alloys, magnesium systems). It develops a transferable reinforcement-selection framework for agro-waste residues. Available evidence indicates that CPA exhibits silica-rich oxide (91%) composition and predominantly amorphous phase characteristics consistent with oxide-based reinforcement behaviour. Comparative matrix compatibility screening indicates conditional plausibility in passive-film-forming metals such as stainless steel and titanium, whereas galvanic and electrochemical uncertainties persist for magnesium systems. However, key performance metrics, including mechanical strengthening, corrosion durability in simulated body fluids, ion-release control, and cytocompatibility, have not yet been experimentally validated for biomedical MMC applications. Accordingly, the principal translational gap lies in the absence of performance-qualified validation studies. The reinforcement-selection framework proposed in this work provides a systematic pathway for screening oxide-rich agro-waste ashes based on chemical stability, matrix compatibility, strengthening mechanisms, corrosion behaviour, and biological thresholds. Future research should prioritise interface characterisation, electrochemical durability testing, mechanical qualification, and biocompatibility assessment to advance sustainable oxide reinforcements toward biomedical deployment.
- 12 June 2026
- Published by IOP Publishing in Materials Research Express
- Vol. 13 (11) , 112001
Open AccessCaesalpinia pulcherrima ash as a sustainable reinforcement in metallic biomaterials for biomedical applications: a review on mechanisms, compatibility, and prospects
Agro-waste-derived oxides are increasingly investigated as sustainable reinforcement phases in metal-matrix composites. However, their translation into biomedical metallic systems remains underexplored. Caesalpinia pulcherrima (Pride of Barbados) ash represents an oxide-bearing biomass derivative with a reported silica-rich composition. Yet, its suitability as a reinforcement in biomedical metal matrix composites (MMC) has not been systematically evaluated. This review assesses whether Caesalpinia pulcherrima ash (CPA) satisfies the chemical, mechanical, electrochemical, and biological criteria required of reinforcements in biomedical metals (316L stainless steel, Ti-6Al-4V, Cr–Co–Mn alloys, magnesium systems). It develops a transferable reinforcement-selection framework for agro-waste residues. Available evidence indicates that CPA exhibits silica-rich oxide (91%) composition and predominantly amorphous phase characteristics consistent with oxide-based reinforcement behaviour. Comparative matrix compatibility screening indicates conditional plausibility in passive-film-forming metals such as stainless steel and titanium, whereas galvanic and electrochemical uncertainties persist for magnesium systems. However, key performance metrics, including mechanical strengthening, corrosion durability in simulated body fluids, ion-release control, and cytocompatibility, have not yet been experimentally validated for biomedical MMC applications. Accordingly, the principal translational gap lies in the absence of performance-qualified validation studies. The reinforcement-selection framework proposed in this work provides a systematic pathway for screening oxide-rich agro-waste ashes based on chemical stability, matrix compatibility, strengthening mechanisms, corrosion behaviour, and biological thresholds. Future research should prioritise interface characterisation, electrochemical durability testing, mechanical qualification, and biocompatibility assessment to advance sustainable oxide reinforcements toward biomedical deployment.
- Open Access
- 5 June 2026
- Published by MDPI AG in Engineering Proceedings
- Vol. 140 (1) , 50
Risk-Based Inspection Applied to Cost Savings in Pumped Energy Storage Scheme Pressure Vessels
Pumped Energy Storage Schemes play a critical role in electricity grid stability and energy security by storing excess electricity for later use. Pressure vessels in these systems are subject to rigorous inspection regimes because of their potential risks to safety and performance. Traditional Time-Based Inspection, while effective, can be costly and inefficient. This paper investigates the application of Risk-Based Inspection methodologies to optimise inspection planning, reduce costs, and maintain safety in Pumped Energy Storage Scheme pressure vessels. The study presents a structured framework for implementing Risk-Based Inspection, demonstrates the potential for cost savings through comparative analysis, and highlights its alignment with regulatory requirements in South Africa.
- 5 June 2026
- Published by MDPI AG in Engineering Proceedings
- Vol. 140 (1) , 50
Open AccessRisk-Based Inspection Applied to Cost Savings in Pumped Energy Storage Scheme Pressure Vessels
Pumped Energy Storage Schemes play a critical role in electricity grid stability and energy security by storing excess electricity for later use. Pressure vessels in these systems are subject to rigorous inspection regimes because of their potential risks to safety and performance. Traditional Time-Based Inspection, while effective, can be costly and inefficient. This paper investigates the application of Risk-Based Inspection methodologies to optimise inspection planning, reduce costs, and maintain safety in Pumped Energy Storage Scheme pressure vessels. The study presents a structured framework for implementing Risk-Based Inspection, demonstrates the potential for cost savings through comparative analysis, and highlights its alignment with regulatory requirements in South Africa.
- Open Access
Effect of Casting Shakeout Temperature on Residual Stresses of Hypoeutectic High-Chromium Iron Alloys Using the Hole-Drilling Method
In this investigation, optical emission spectrometers, a Brinell hardness tester, optical light and scanning microscopes, and X-ray diffraction were used for general metallurgical characterization of the experimental irons in as-cast states. The hole-drilling method was used to assess residual stress distributions under gross and net casting weight conditions. To create experimental irons using the casting process, raw materials were transformed from a solid to a liquid state using an industrial furnace and ladle to melt and cast, respectively. The casting shakeout temperatures for samples A and B were recorded at 60 °C and 180 °C, respectively, after a characteristic stress lattice casting component was allowed to cool for about 1645 min and 1295 min. Chemical analysis verified the experimental hypoeutectic irons of ASTM A532, Type A, Class III, 25%Cr, i.e., high chromium white cast iron alloys. Additionally, it was discovered that micrographs were made of an austenitic-martensitic matrix that contained eutectic M7C3 and secondary M23C6-type carbides. The residual stress distributions were found to be influenced by various carbide and metallic volume fraction proportions, casting section thickness, and casting shakeout duration and temperature. Optimal hardness values, however, were shown to be associated with higher residual stress distributions and an increase in major alloying elements in experimental irons. Consequently, different residual stress distributions are produced by casting shakeout temperatures at lower and higher values under gross and net casting weight conditions.
Open AccessEffect of Casting Shakeout Temperature on Residual Stresses of Hypoeutectic High-Chromium Iron Alloys Using the Hole-Drilling Method
In this investigation, optical emission spectrometers, a Brinell hardness tester, optical light and scanning microscopes, and X-ray diffraction were used for general metallurgical characterization of the experimental irons in as-cast states. The hole-drilling method was used to assess residual stress distributions under gross and net casting weight conditions. To create experimental irons using the casting process, raw materials were transformed from a solid to a liquid state using an industrial furnace and ladle to melt and cast, respectively. The casting shakeout temperatures for samples A and B were recorded at 60 °C and 180 °C, respectively, after a characteristic stress lattice casting component was allowed to cool for about 1645 min and 1295 min. Chemical analysis verified the experimental hypoeutectic irons of ASTM A532, Type A, Class III, 25%Cr, i.e., high chromium white cast iron alloys. Additionally, it was discovered that micrographs were made of an austenitic-martensitic matrix that contained eutectic M7C3 and secondary M23C6-type carbides. The residual stress distributions were found to be influenced by various carbide and metallic volume fraction proportions, casting section thickness, and casting shakeout duration and temperature. Optimal hardness values, however, were shown to be associated with higher residual stress distributions and an increase in major alloying elements in experimental irons. Consequently, different residual stress distributions are produced by casting shakeout temperatures at lower and higher values under gross and net casting weight conditions.
- Open Access
- 8 May 2026
- Published by Elsevier in Results in Engineering
- Vol. 30
Closing the loop: A circular economy approach to magnetite synthesis through acid mine drainage valorization and its applications
- 8 May 2026
- Published by Elsevier in Results in Engineering
- Vol. 30
Open AccessClosing the loop: A circular economy approach to magnetite synthesis through acid mine drainage valorization and its applications
- Open Access
- 13 April 2026
- Published by Elsevier in Materials & Design
- Vol. 265
Structure-property optimization in natural fiber-reinforced aluminum composites for enhanced mechanical performance: Effect of coconut husk ash and Al2O3 particulates
- 13 April 2026
- Published by Elsevier in Materials & Design
- Vol. 265
Open AccessStructure-property optimization in natural fiber-reinforced aluminum composites for enhanced mechanical performance: Effect of coconut husk ash and Al2O3 particulates
- Open Access
- 1 January 2026
- Published by Wiley in Advances in Materials Science and Engineering
- Vol. 2026 (1)
Influence of the Addition of Strontium on Eutectic Aluminium Alloys
This paper studies the effect of strontium on eutectic aluminium alloy (LM6) and its mechanical properties, with the aim of impacting high strength and ductility. Four alloy samples of LM6 with varying amounts (0%–0.1%) of strontium were cast. Universal tensile and Micro Vickers hardness testing machines were used to determine the alloy’s mechanical properties (tensile strength and percentage elongation) and hardness. An optical microscope was used to analyse the alloy’s microstructure. The results showed a reduction in hardness and an improvement in tensile strength and percentage elongation. The alloy with 0.05 wt% of strontium recorded the best results in tensile strength (232.24 ± 12 MPa), and this represents an improvement of 17.4% compared with the neat alloy (197.89 ± 10 MPa), and the same trend was observed for its percentage elongation, with an improvement of 3.52% compared with the neat alloy. ImageJ software statistical analysis showed that the mean average grain size of the detected phases ranges between 31.298 and 33.063 μm, while optical microscopic analysis showed that the addition of strontium to eutectic Al–Si alloy changes the Al–Si eutectic structure which resulted in the alloy’s mechanical properties enhancement, and the alloy is a suitable candidate for stress applications within 200–232 MPa.
- 1 January 2026
- Published by Wiley in Advances in Materials Science and Engineering
- Vol. 2026 (1)
Open AccessInfluence of the Addition of Strontium on Eutectic Aluminium Alloys
This paper studies the effect of strontium on eutectic aluminium alloy (LM6) and its mechanical properties, with the aim of impacting high strength and ductility. Four alloy samples of LM6 with varying amounts (0%–0.1%) of strontium were cast. Universal tensile and Micro Vickers hardness testing machines were used to determine the alloy’s mechanical properties (tensile strength and percentage elongation) and hardness. An optical microscope was used to analyse the alloy’s microstructure. The results showed a reduction in hardness and an improvement in tensile strength and percentage elongation. The alloy with 0.05 wt% of strontium recorded the best results in tensile strength (232.24 ± 12 MPa), and this represents an improvement of 17.4% compared with the neat alloy (197.89 ± 10 MPa), and the same trend was observed for its percentage elongation, with an improvement of 3.52% compared with the neat alloy. ImageJ software statistical analysis showed that the mean average grain size of the detected phases ranges between 31.298 and 33.063 μm, while optical microscopic analysis showed that the addition of strontium to eutectic Al–Si alloy changes the Al–Si eutectic structure which resulted in the alloy’s mechanical properties enhancement, and the alloy is a suitable candidate for stress applications within 200–232 MPa.
- Open Access
- 24 July 2025
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 38, 212-225
Mechanistic performance of Al–Mg–Si alloy reinforced agro-waste residue for structural applications
- 24 July 2025
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 38, 212-225
Open AccessMechanistic performance of Al–Mg–Si alloy reinforced agro-waste residue for structural applications
- Open Access
- 27 June 2025
- Published by MDPI AG in Preprints.org
Effect of Casting Shakeout Temperature on Residual Stresses of Hypoeutectic High Chromium Iron Alloys Using Hole-Drilling Method
Attention on residual stress development, magnitude, and distribution on abrasive wear materials, such as high chromium iron alloys, has been minimal, even though these materials are prone to tearing or inferior mechanical properties because of distortion during manufacturing processes, such as casting and heat treatment, leading to premature failure of cast components. Identification of the source and succeeding management of residual stress provides an opportune possibility to enhance product quality. In the current study, the as-cast hypoeutectic irons of ASTM A532, Type A, Class III, 25% Cr, i.e., sample A and sample B, were cast at 1384 and 1390 degrees Celsius and allowed to solidify and cool for approximately 1645 and 1295 minutes, respectively. Thus, the shakeout temperatures of sample A and sample B products were established to be approximately 60 and 180°C, respectively. Resultant residual stress and macrohardness were determined at ambient temperatures using the hole-drilling method and Brinell hardness tester machines, respectively. Higher hardness values of 600 BHN were established on sample B compared to 526 BHN for sample A. In addition, casting shakeout at higher temperatures, i.e., 180°C on sample B, yielded higher magnitudes of residual stress distribution compared to 60°C shakeout for sample A.
- 27 June 2025
- Published by MDPI AG in Preprints.org
Open AccessEffect of Casting Shakeout Temperature on Residual Stresses of Hypoeutectic High Chromium Iron Alloys Using Hole-Drilling Method
Attention on residual stress development, magnitude, and distribution on abrasive wear materials, such as high chromium iron alloys, has been minimal, even though these materials are prone to tearing or inferior mechanical properties because of distortion during manufacturing processes, such as casting and heat treatment, leading to premature failure of cast components. Identification of the source and succeeding management of residual stress provides an opportune possibility to enhance product quality. In the current study, the as-cast hypoeutectic irons of ASTM A532, Type A, Class III, 25% Cr, i.e., sample A and sample B, were cast at 1384 and 1390 degrees Celsius and allowed to solidify and cool for approximately 1645 and 1295 minutes, respectively. Thus, the shakeout temperatures of sample A and sample B products were established to be approximately 60 and 180°C, respectively. Resultant residual stress and macrohardness were determined at ambient temperatures using the hole-drilling method and Brinell hardness tester machines, respectively. Higher hardness values of 600 BHN were established on sample B compared to 526 BHN for sample A. In addition, casting shakeout at higher temperatures, i.e., 180°C on sample B, yielded higher magnitudes of residual stress distribution compared to 60°C shakeout for sample A.
- Open Access
- 13 May 2025
- Published by MDPI AG in Preprints.org
Effect of Casting Shakeout Temperature on Residual Stresses of Hypoeutectic High Chromium Iron Alloys Using Hole-Drilling Method
Attention on residual stress (RS) development, magnitude, and distribution on abrasive wear materials, i.e., high chromium (Cr) iron alloys, has been minimal, even though these materials are prone to tearing or inferior mechanical properties because of distortion during manufacturing processes, such as casting and heat treatment, leading to premature failure of cast components. Identification of the source and succeeding management of RS provides an opportune possibility to enhance the product quality. In the current study, the as-cast hypoeutectic irons of ASTM A532, Type A, Class III, 25% Cr, i.e., sample A (S/A) and sample B (S/B), were cast at 1384 and 1390 degrees Celsius (oC) and allowed to solidify and cool for approximately 1645 and 1295 minutes (mins), respectively. Thus, the shakeout temperatures of S/A and S/B cast products were established to be approximately 60 and 180oC respectively. Resultant RS and macrohardness were determined at ambient temperatures using the hole-drilling method (HDM) and Brinell hardness (BH) tester machines, respectively. Higher hardness values of 600BHN were established on S/B compared to 526BHN for S/A. In addition, casting shakeout at higher temperatures, i.e., 180oC on S/B, yielded higher magnitudes of RS distribution compared to 60oC shakeout for S/A.
- 13 May 2025
- Published by MDPI AG in Preprints.org
Open AccessEffect of Casting Shakeout Temperature on Residual Stresses of Hypoeutectic High Chromium Iron Alloys Using Hole-Drilling Method
Attention on residual stress (RS) development, magnitude, and distribution on abrasive wear materials, i.e., high chromium (Cr) iron alloys, has been minimal, even though these materials are prone to tearing or inferior mechanical properties because of distortion during manufacturing processes, such as casting and heat treatment, leading to premature failure of cast components. Identification of the source and succeeding management of RS provides an opportune possibility to enhance the product quality. In the current study, the as-cast hypoeutectic irons of ASTM A532, Type A, Class III, 25% Cr, i.e., sample A (S/A) and sample B (S/B), were cast at 1384 and 1390 degrees Celsius (oC) and allowed to solidify and cool for approximately 1645 and 1295 minutes (mins), respectively. Thus, the shakeout temperatures of S/A and S/B cast products were established to be approximately 60 and 180oC respectively. Resultant RS and macrohardness were determined at ambient temperatures using the hole-drilling method (HDM) and Brinell hardness (BH) tester machines, respectively. Higher hardness values of 600BHN were established on S/B compared to 526BHN for S/A. In addition, casting shakeout at higher temperatures, i.e., 180oC on S/B, yielded higher magnitudes of RS distribution compared to 60oC shakeout for S/A.
- Open Access
- 28 March 2023
- Published by Springer Nature in Research Square
Optimization of Sand Parameters to Improve the Quality of Cast Iron Using Taguchi
The main aim of the foundry industries is to produce quality castings with no rejection. In addition, in the present era of global competition, manufacturing industries has bound to take the challenge that is demand for high quality product with reduced lead–time. However, with the diversity of greensand casting parameters, it results in varying effects on the quality. With sand being one of the most frequent cause of quality reject/rework, it is essential to understand the effect it has on the casting outcome. Taguchi’s approach in quality states that the quality of a product is dependent on the input, he figured that the perfect time to eliminate differences in products is during the designing and manufacturing of products, he developed a strategy for quality that can be used in process. Therefore, it is important to understand the inputs in sand mould preparation. The focus of the research is on greensand moulding process. The casting defect is the most contributing factor to quality reject in most foundries. The sand moulding process is the most contributing factor to the formation scrap. The target in foundries is to achieve low casting defects at minimum cost. It is essential to select significant parameters that cause variation of quality characteristic of castings .data should be collected dictated by the chosen orthogonal array (OA) and parameter levels. With the collected at the analysis of variance (ANOVA) can be generated to determine the statistical importance of parameter and response graphs are plotted to determine the optimum setting of control parameter
- 28 March 2023
- Published by Springer Nature in Research Square
Open AccessOptimization of Sand Parameters to Improve the Quality of Cast Iron Using Taguchi
The main aim of the foundry industries is to produce quality castings with no rejection. In addition, in the present era of global competition, manufacturing industries has bound to take the challenge that is demand for high quality product with reduced lead–time. However, with the diversity of greensand casting parameters, it results in varying effects on the quality. With sand being one of the most frequent cause of quality reject/rework, it is essential to understand the effect it has on the casting outcome. Taguchi’s approach in quality states that the quality of a product is dependent on the input, he figured that the perfect time to eliminate differences in products is during the designing and manufacturing of products, he developed a strategy for quality that can be used in process. Therefore, it is important to understand the inputs in sand mould preparation. The focus of the research is on greensand moulding process. The casting defect is the most contributing factor to quality reject in most foundries. The sand moulding process is the most contributing factor to the formation scrap. The target in foundries is to achieve low casting defects at minimum cost. It is essential to select significant parameters that cause variation of quality characteristic of castings .data should be collected dictated by the chosen orthogonal array (OA) and parameter levels. With the collected at the analysis of variance (ANOVA) can be generated to determine the statistical importance of parameter and response graphs are plotted to determine the optimum setting of control parameter