Raja Annamalai Arunjunai Rajan
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Raja Annamalai Arunjunai Rajan has a total of 128 co-authors. Here are the top co-authors by number of shared publications:
- Chun-Ping Jen
Department of Mechanical Engineering and Advanced Institute of Manufacturing for High-Tech Innovations, National Chung Cheng University, Chiayi 62102, Taiwan
17 shared publications A. Muthuchamy
Department of Metallurgical and Materials Engineering, National Institute of Technology, Tiruchirappalli 620015, India
13 shared publications- Ayyapparaj Muthuchamy
Department of Metallurgical and Materials Engineering, National Institute of Technology, Trichy, Trichy, India
11 shared publications - Gopalan Venkatachalam
Centre for Advanced Materials and Innovative Technologies, Vellore Institute of Technology, Chennai, India
9 shared publications - Muthe Srikanth
School of Mechanical Engineering, VIT, Vellore 632014, India
9 shared publications Dinesh K. Agrawal
7 shared publications
Latest Publications
- Open Access
- 19 June 2026
- Published by AccScience Publishing in Materials Science in Additive Manufacturing
- Vol. 5  (3) , 026080014
Additive manufacturing of Inconel 939: A review of microstructure, defects, and mechanical properties
Additive manufacturing (AM) has created new possibilities to eliminate secondary processes such as machining. By reducing material waste and shortening lead times, AM is regarded as a key enabling technology for Industry 4.0 in the global market. Among nickel-based superalloys, Inconel 939 (IN939), a precipitation-hardened alloy, is widely explored for high-temperature components operating at service temperatures of ~850 °C in demanding aerospace applications such as gas turbine blades. The pronounced cracking susceptibility of IN939 introduces processing challenges in the AM environment. Fabricating dense components requires optimized processing parameters (laser power, scan speed, hatch spacing, and layer thickness). This review addresses the influence of AM routesâspecifically powder bed fusion, directed energy deposition, and electron beam meltingâon the microstructure and tensile properties of IN939. The mechanical performance of IN939 is primarily determined by the alloying element composition, with microstructural studies focusing on the formation of precipitate types. Mechanistic insights are provided that correlate the thermodynamic factors (solidification pathway and driving force for precipitation) and kinetic factors (cooling rate, diffusion) governing microstructural evolution with their influence on the strength-ductility trade-off. The compiled literature sheds light on the effects of heat treatment, the formation of various defect types, and fatigue and creep behavior of IN939.
- 19 June 2026
- Published by AccScience Publishing in Materials Science in Additive Manufacturing
- Vol. 5  (3) , 026080014
Open AccessAdditive manufacturing of Inconel 939: A review of microstructure, defects, and mechanical properties
Additive manufacturing (AM) has created new possibilities to eliminate secondary processes such as machining. By reducing material waste and shortening lead times, AM is regarded as a key enabling technology for Industry 4.0 in the global market. Among nickel-based superalloys, Inconel 939 (IN939), a precipitation-hardened alloy, is widely explored for high-temperature components operating at service temperatures of ~850 °C in demanding aerospace applications such as gas turbine blades. The pronounced cracking susceptibility of IN939 introduces processing challenges in the AM environment. Fabricating dense components requires optimized processing parameters (laser power, scan speed, hatch spacing, and layer thickness). This review addresses the influence of AM routesâspecifically powder bed fusion, directed energy deposition, and electron beam meltingâon the microstructure and tensile properties of IN939. The mechanical performance of IN939 is primarily determined by the alloying element composition, with microstructural studies focusing on the formation of precipitate types. Mechanistic insights are provided that correlate the thermodynamic factors (solidification pathway and driving force for precipitation) and kinetic factors (cooling rate, diffusion) governing microstructural evolution with their influence on the strength-ductility trade-off. The compiled literature sheds light on the effects of heat treatment, the formation of various defect types, and fatigue and creep behavior of IN939.
- Open Access
- 17 June 2026
- Published by MDPI AG in Corrosion and Materials Degradation
- Vol. 7  (2) , 38
Effect of Sintering Temperature on Protective Oxide Formation and Corrosion Resistance of Ti-6Al-4V in Na2SO4âNaCl Salt Mixtures
This study investigates the effect of sintering temperature on the hot-corrosion behavior of Ti-6Al-4V alloy in a molten salt environment. Samples were sintered at 800 °C, 900 °C, 1000 °C and 1100 °C, then exposed to the Na2SO4â25%NaCl for 300 h at 650 °C. The corrosion kinetics were evaluated by measuring the mass change in the specimens, and the results were correlated with their corresponding corrosion rates. The results show that the sintering temperature drives corrosion kinetics by influencing the sample density and grain size. The sample sintered at 900 °C shows a low corrosion rate due to its refined microstructure. This refined microstructure provides a high grain boundary density, which serves as a diffusion path and enables the formation of a dense, protective Al2O3âTiO2 layer, as confirmed by XPS. In contrast, the sample sintered at 800 °C exhibits high porosity, resulting in an initial weight loss due to molten-salt penetration and evaporation of volatile metal chlorides. The samples sintered at 1000 °C and 1100 °C exhibit coarsened grains, leading to a thicker, brittle oxide layer and severe delamination, which in turn result in high corrosion rates. The results show that optimizing the sintering temperature to around 900 °C would enhance hot-corrosion resistance in salt-contaminated environments.
- 17 June 2026
- Published by MDPI AG in Corrosion and Materials Degradation
- Vol. 7  (2) , 38
Open AccessEffect of Sintering Temperature on Protective Oxide Formation and Corrosion Resistance of Ti-6Al-4V in Na2SO4âNaCl Salt Mixtures
This study investigates the effect of sintering temperature on the hot-corrosion behavior of Ti-6Al-4V alloy in a molten salt environment. Samples were sintered at 800 °C, 900 °C, 1000 °C and 1100 °C, then exposed to the Na2SO4â25%NaCl for 300 h at 650 °C. The corrosion kinetics were evaluated by measuring the mass change in the specimens, and the results were correlated with their corresponding corrosion rates. The results show that the sintering temperature drives corrosion kinetics by influencing the sample density and grain size. The sample sintered at 900 °C shows a low corrosion rate due to its refined microstructure. This refined microstructure provides a high grain boundary density, which serves as a diffusion path and enables the formation of a dense, protective Al2O3âTiO2 layer, as confirmed by XPS. In contrast, the sample sintered at 800 °C exhibits high porosity, resulting in an initial weight loss due to molten-salt penetration and evaporation of volatile metal chlorides. The samples sintered at 1000 °C and 1100 °C exhibit coarsened grains, leading to a thicker, brittle oxide layer and severe delamination, which in turn result in high corrosion rates. The results show that optimizing the sintering temperature to around 900 °C would enhance hot-corrosion resistance in salt-contaminated environments.
- Open Access
- 25 May 2026
- Published by AccScience Publishing in Materials Science in Additive Manufacturing
- Vol. 5  (2) , 026040007
Build orientation-dependent evolution of residual stress, crystallographic texture, and mechanical anisotropy in laser powder bed-fused IN625
The mechanical anisotropy of laser powder bed-fused IN625 necessitates consideration of build orientation, as inherent directional solidification during additive manufacturing induces mechanical anisotropy and affects grain morphology, texture evolution, and mechanical behavior, thereby requiring an orientation-specific evaluation to optimize structural integrity. This paper presents the structureâproperty relationships of as-built specimens fabricated in three distinct build orientations. To assess orientation-dependent effects, tensile specimens were printed in three build orientations: 0°, 45°, and 90°. Grain morphology, grain size distribution, and microstructural variation were investigated using electron backscatter diffraction. The statistical distribution of grain orientation and pole figure analysis revealed significant textural variation and directional dependence, consistent with anisotropic behavior. The findings demonstrate that build orientation significantly influences the structural integrity of laser powder bed-fused IN625 components. Among the examined orientations, the 0° condition exhibits a pronounced texture aligned with the build direction. Pole figure and orientation distribution function analyses confirm a dominant cube texture at 0°, which transitions to a cubeâgoss texture at 45°. Mechanical testing corroborates the electron backscatter diffraction results, with the 0° orientation exhibiting the highest yield strength (727 MPa) and ultimate tensile strength (963 MPa), attributed to a favorable alignment of load-bearing grains. Residual stress-assisted characterization indicates that nominal in-plane compressive stresses predominate in the 0° orientation.
- 25 May 2026
- Published by AccScience Publishing in Materials Science in Additive Manufacturing
- Vol. 5  (2) , 026040007
Open AccessBuild orientation-dependent evolution of residual stress, crystallographic texture, and mechanical anisotropy in laser powder bed-fused IN625
The mechanical anisotropy of laser powder bed-fused IN625 necessitates consideration of build orientation, as inherent directional solidification during additive manufacturing induces mechanical anisotropy and affects grain morphology, texture evolution, and mechanical behavior, thereby requiring an orientation-specific evaluation to optimize structural integrity. This paper presents the structureâproperty relationships of as-built specimens fabricated in three distinct build orientations. To assess orientation-dependent effects, tensile specimens were printed in three build orientations: 0°, 45°, and 90°. Grain morphology, grain size distribution, and microstructural variation were investigated using electron backscatter diffraction. The statistical distribution of grain orientation and pole figure analysis revealed significant textural variation and directional dependence, consistent with anisotropic behavior. The findings demonstrate that build orientation significantly influences the structural integrity of laser powder bed-fused IN625 components. Among the examined orientations, the 0° condition exhibits a pronounced texture aligned with the build direction. Pole figure and orientation distribution function analyses confirm a dominant cube texture at 0°, which transitions to a cubeâgoss texture at 45°. Mechanical testing corroborates the electron backscatter diffraction results, with the 0° orientation exhibiting the highest yield strength (727 MPa) and ultimate tensile strength (963 MPa), attributed to a favorable alignment of load-bearing grains. Residual stress-assisted characterization indicates that nominal in-plane compressive stresses predominate in the 0° orientation.
- Open Access
- 12 May 2026
- Published by Springer Nature in Discover Materials
- Vol. 6  (1)
Review of Ti-6Al-4 V alloy processing, microstructure, and mechanical properties from powder metallurgy to additive manufacturing for engineering applications
- 12 May 2026
- Published by Springer Nature in Discover Materials
- Vol. 6  (1)
Open AccessReview of Ti-6Al-4 V alloy processing, microstructure, and mechanical properties from powder metallurgy to additive manufacturing for engineering applications
- 30 March 2026
- Published by Springer Nature in Journal of the Brazilian Society of Mechanical Sciences and Engineering
- Vol. 48  (5) , 314
Parameteric optimization of dry milling process on stir-cast and heat-treated AZ63 magnesium alloy using TOPSIS method
- 30 March 2026
- Published by Springer Nature in Journal of the Brazilian Society of Mechanical Sciences and Engineering
- Vol. 48  (5) , 314
Parameteric optimization of dry milling process on stir-cast and heat-treated AZ63 magnesium alloy using TOPSIS method
- Open Access
- 10 February 2026
- Published by Springer Nature in Discover Materials
- Vol. 6  (1)
Influence of post-processing heat treatment on nanoscale mechanical properties of laser powder bed fused Inconel 625
- 10 February 2026
- Published by Springer Nature in Discover Materials
- Vol. 6  (1)
Open AccessInfluence of post-processing heat treatment on nanoscale mechanical properties of laser powder bed fused Inconel 625
- 18 October 2025
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 20  (4) , 2816-2830
Effects of Thermal Aging on Mechanical Properties and Microstructure Characteristics of Mg E675 Alloy
- 18 October 2025
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 20  (4) , 2816-2830
Effects of Thermal Aging on Mechanical Properties and Microstructure Characteristics of Mg E675 Alloy
- Open Access
- 5 September 2025
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 9  (9) , 304
Effect of Heat Treatment on High-Temperature Tribological Behavior of WE54 Alloy: An Experimental Study
This study examines the high-temperature tribological behavior of WE54 Mg alloy under various conditions: as-cast, solution-treated (T4), age-hardened (T6), and secondary aged (S.A). Wear tests were performed using a pin-on-disc setup, applying a normal load of 10 N, with a sliding velocity of 1 m/s, a sliding distance of 1000 m, and temperatures from 25 °C to 150 °C. Responses such as the coefficient of friction and volumetric wear rate were recorded. The results indicate that heat treatment significantly influences the wear behavior of the WE54 alloy. The lowest volumetric wear rate (8.16 ¹ 1.47 mm3) and wear coefficient (0.112 ¹ 0.02) occurred in the as-cast sample at 100 °C, while the highest volumetric wear rate (14.68 ¹ 1.59 mm3) and wear coefficient (0.171 ¹ 0.02) were found in the S.A. sample at 150 °C. Surface characterization of worn samples was conducted using field emission scanning electron microscopy (FESEM) and X-ray diffraction (XRD). The wear mechanisms identified include abrasive wear, oxidative wear, and delamination across all conditions, regardless of temperature. The elevated volumetric wear rate at 150 °C, irrespective of the sample condition, is attributed to oxidation and thermal softening of the material.
- 5 September 2025
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 9  (9) , 304
Open AccessEffect of Heat Treatment on High-Temperature Tribological Behavior of WE54 Alloy: An Experimental Study
This study examines the high-temperature tribological behavior of WE54 Mg alloy under various conditions: as-cast, solution-treated (T4), age-hardened (T6), and secondary aged (S.A). Wear tests were performed using a pin-on-disc setup, applying a normal load of 10 N, with a sliding velocity of 1 m/s, a sliding distance of 1000 m, and temperatures from 25 °C to 150 °C. Responses such as the coefficient of friction and volumetric wear rate were recorded. The results indicate that heat treatment significantly influences the wear behavior of the WE54 alloy. The lowest volumetric wear rate (8.16 ¹ 1.47 mm3) and wear coefficient (0.112 ¹ 0.02) occurred in the as-cast sample at 100 °C, while the highest volumetric wear rate (14.68 ¹ 1.59 mm3) and wear coefficient (0.171 ¹ 0.02) were found in the S.A. sample at 150 °C. Surface characterization of worn samples was conducted using field emission scanning electron microscopy (FESEM) and X-ray diffraction (XRD). The wear mechanisms identified include abrasive wear, oxidative wear, and delamination across all conditions, regardless of temperature. The elevated volumetric wear rate at 150 °C, irrespective of the sample condition, is attributed to oxidation and thermal softening of the material.
- Open Access
- 2 September 2025
- Published by Elsevier in Results in Engineering
- Vol. 28
Low-cycle fatigue behavior of as-cast and heat-treated Haynes 25 superalloy under varying strain amplitudes
- 2 September 2025
- Published by Elsevier in Results in Engineering
- Vol. 28
Open AccessLow-cycle fatigue behavior of as-cast and heat-treated Haynes 25 superalloy under varying strain amplitudes
- 15 July 2025
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
Experimental investigation of the turning performance of high-pressure die-cast WE54 magnesium alloys under dry and minimum quantity lubrication conditions
The increasing demand for lightweight materials in the automotive and aerospace industries has driven interest in magnesium alloys, such as WE54, due to their high strength-to-weight ratio and potential for improved fuel efficiency. However, machining magnesium alloys presents challenges regarding surface quality, tool wear, and process optimization. This study addresses these issues by evaluating the turning performance of WE54 alloy under dry and minimum quantity lubrication (MQL) conditions. This study focuses on the cutting parameters: speed, feed, and depth of cut. The primary response variables optimized using the multi-objective optimization technique are surface roughness, cutting force, and material removal rate. A Taguchi L18 orthogonal array design and the statistical method analysis of variance (ANOVA) were used to understand the effect of the parameters on the response variables. Under MQL, a better surface roughness value of 0.53 Îźm was achieved compared to 0.70 Îźm under dry conditions. The Techniques for Order Preferences by Similarity to Ideal Solution analysis finds that S = 100, f = 0.2, and d = 0.75 under MQL machining are the optimum parameters with maximum closeness coefficient value (0.7581), a combined measure of the response variables. According to the ANOVA results, the machining condition is the most influential factor on the closeness coefficient, contributing 34.80%, followed by feed and cutting speed. In addition, artificial neural networks (ANNs) have been used to predict the closeness coefficient value based on the input parameters. The ANN model showed good prediction accuracy with an R-squared value of 0.92017. Overall, utilization of the MQL has shown positive effects in reducing cutting force and surface roughness. This research exceeds previous studies by integrating experimental work, statistical analysis, and neural networks to better understand and improve the machining of WE54 using eco-friendly lubrication methods.
- 15 July 2025
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
Experimental investigation of the turning performance of high-pressure die-cast WE54 magnesium alloys under dry and minimum quantity lubrication conditions
The increasing demand for lightweight materials in the automotive and aerospace industries has driven interest in magnesium alloys, such as WE54, due to their high strength-to-weight ratio and potential for improved fuel efficiency. However, machining magnesium alloys presents challenges regarding surface quality, tool wear, and process optimization. This study addresses these issues by evaluating the turning performance of WE54 alloy under dry and minimum quantity lubrication (MQL) conditions. This study focuses on the cutting parameters: speed, feed, and depth of cut. The primary response variables optimized using the multi-objective optimization technique are surface roughness, cutting force, and material removal rate. A Taguchi L18 orthogonal array design and the statistical method analysis of variance (ANOVA) were used to understand the effect of the parameters on the response variables. Under MQL, a better surface roughness value of 0.53 Îźm was achieved compared to 0.70 Îźm under dry conditions. The Techniques for Order Preferences by Similarity to Ideal Solution analysis finds that S = 100, f = 0.2, and d = 0.75 under MQL machining are the optimum parameters with maximum closeness coefficient value (0.7581), a combined measure of the response variables. According to the ANOVA results, the machining condition is the most influential factor on the closeness coefficient, contributing 34.80%, followed by feed and cutting speed. In addition, artificial neural networks (ANNs) have been used to predict the closeness coefficient value based on the input parameters. The ANN model showed good prediction accuracy with an R-squared value of 0.92017. Overall, utilization of the MQL has shown positive effects in reducing cutting force and surface roughness. This research exceeds previous studies by integrating experimental work, statistical analysis, and neural networks to better understand and improve the machining of WE54 using eco-friendly lubrication methods.