AMAnna Malmros

Anna Malmros

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Anna Malmros has a total of 23 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Characterization of Drain-Induced Barrier Lowering in GaN HEMTs Using a Drain Current Injection Technique

    by Björn Hult, Johan Bergsten, Ragnar Ferrand-Drake Del Castillo, Vanya Darakchieva, Anna Malmros, Hans Hjelmgren, Mattias Thorsell, Niklas Rorsman

    Assessing short channel effects (SCEs) is crucial in the high-frequency optimization of downscaled field-effect transistors (FETs) such as GaN high electron mobility transistors (HEMTs). Drain-induced barrier lowering (DIBL) is commonly used for quantifying the ability of the gate to modulate the drain–source current at high drain voltages. DIBL is traditionally extracted from the relative shift of the threshold voltage at different drain–source voltages. In this article, we propose a new method based on a drain current injection technique (DCIT) to assess DIBL. This method facilitates a direct measure of the threshold voltage over a wide range of drain–source voltages in a single measurement. The method is demonstrated and compared to the conventional method using AlGaN/GaN and InAlGaN HEMTs with a Fe-doped buffer and a $\textit{C}$ -doped AlGaN back-barrier, respectively. Furthermore, the impact of different gate lengths and GaN channel layer thicknesses is presented. The measurements are analyzed and discussed with supporting technology computer-aided design (TCAD) simulations. The proposed method facilitates a more general and detailed measurement of the DIBL for HEMTs.


  • Microwave Performance of ‘Buffer-Free’ GaN-on-SiC High Electron Mobility Transistors

    by Ding-Yuan Chen, Anna Malmros, Mattias Thorsell, Hans Hjelmgren, Olof Kordina, Jr-Tai Chen, Niklas Rorsman

    High performance microwave GaN-on-SiC HEMTs are demonstrated on a heterostructure without a conventional thick doped buffer. The HEMT is fabricated on a high-quality 0.25 μm unintentional doped GaN layer grown directly on a transmorphic epitaxially grown AlN nucleation layer. This approach allows the AlN-nucleation layer to act as a back-barrier, limiting short channel effects and removing buffer leakage. The devices with the ‘buffer-free’ heterostructure show competitive DC and RF characteristics, as benchmarked against the devices made on a commercial Fe-doped epi-wafer. Peak transconductances of 500 mS/mm and a maximum saturated drain current of ~1 A/mm are obtained. An extrinsic fT of 70 GHz and fmax of 130 GHz are achieved for transistors with a gate length of 100 nm. Pulsed-IV measurements reveal a lower current slump and a smaller knee walkout. The dynamic IV performance translates to an output power of 4.1 W/mm, as measured with active load-pull at 3 GHz. These devices suggest that the ‘bufferfree’ concept may offer an alternative route for high frequency GaN HEMTs with less electron trapping effects.


  • Enhanced Mobility in InAlN/AlN/GaN HEMTs Using a GaN Interlayer

    by Anna Malmros, Jr-Tai Chen, Hans Hjelmgren, Jun Lu, Lars Hultman, Olof Kordina, Einar O. Sveinbjornsson, Herbert Zirath, Niklas Rorsman

    An enhancement of the electron mobility (μ) in InAlN/AlN/GaN heterostructures is demonstrated by the incorporation of a thin GaN interlayer (IL) between the InAlN and AlN. The introduction of a GaN IL increases μ at room temperature (RT) from 1600 to 1930 cm²/Vs. The effect is further enhanced at cryogenic temperature (5 K), where the GaN IL sample exhibits a μ of 16,000 cm²/Vs, compared to 6900 cm²/Vs without IL. The results indicate the reduction of one or more scattering mechanisms normally present in InAlN/AlN/GaN heterostructures. We propose that the improvement in μ is either due to the suppression of fluctuations in the quantum well subband energies or to reduced Coulomb scattering, both related to compositional variations in the InAlN. HEMTs fabricated on the GaN IL sample demonstrate larger improvement in dc- and high-frequency performance at 5 K; fmax increases by 25 GHz to 153 GHz, compared to an increase of 6 GHz to 133 GHz without IL. The difference in improvement was associated mainly with the drop in the access resistances.


  • Impact of Channel Thickness on the Large-Signal Performance in InAlGaN/AlN/GaN HEMTs With an AlGaN Back Barrier

    by Anna Malmros, Piero Gamarra, Mattias Thorsell, Hans Hjelmgren, Cedric Lacam, Sylvain Laurent Delage, Herbert Zirath, Niklas Rorsman

    The impact of varying the GaN channel layer thickness (t ch ) in InAlGaN/AlN/GaN HEMTs with C-doped AlGaN back barriers is investigated. t ch was 50, 100, and 150 nm, and the gate length of the fabricated HEMTs ranged from 50 to 200 nm. It is found that short-channel effects (SCEs) are significantly mitigated with a small t ch . For HEMTs with a gate length of 50 nm, the drain-induced barrier lowering changes from 40 to 93 mV/V as t ch is increased from 50 to 150 nm. On the other hand, it is shown that dispersive effects are more severe for a smaller t ch , as demonstrated by a sixfold increase in the dynamic ON-resistance for t ch = 50 nm compared to t ch = 150 nm. The tradeoff between dispersion and SCEs is reflected in large-signal measurements at 30 GHz. The 50-nm channel, mainly limited by dispersion, exhibits an output power of 3.5 W/mm. The thicker channels reach a maximum of around 5 W/mm, but for different gate lengths due to the difference in severity of the SCEs. This paper elucidates the interplay between SCEs and dispersion related to t ch , its consequences for the large-signal performance and for the limitation in downscaling of the gate length.


  • Evaluation of Thermal Versus Plasma-Assisted ALD Al2O3 as Passivation for InAlN/AlN/GaN HEMTs

    by Anna Malmros, Piero Gamarra, Marie-Antoinette Di Forte-Poisson, Hans Hjelmgren, Cedric Lacam, Mattias Thorsell, Maurice Tordjman, Raphael Aubry, Niklas Rorsman

    Al 2 O 3 films deposited by thermal and plasma-assisted atomic layer deposition (ALD) were evaluated as passivation layers for InAlN/AlN/GaN HEMTs. As a reference, a comparison was made with the more conventional plasma enhanced chemical vapor deposition deposited SiN x passivation. The difference in sheet charge density, threshold voltage, f T and f max was moderate for the three samples. The gate leakage current differed by several orders of magnitude, in favor of Al 2 O 3 passivation, regardless of the deposition method. Severe current slump was measured for the HEMT passivated by thermal ALD, whereas near-dispersion free operation was observed for the HEMT passivated by plasma-assisted ALD. This had a direct impact on the microwave output power. Large-signal measurements at 3 GHz revealed that HEMTs with Al 2 O 3 passivation exhibited 77% higher output power using plasma-assisted ALD compared with thermal ALD.


  • Evaluation of an InAlN/AlN/GaN HEMT with Ta‐based ohmic contacts and PECVD SiN passivation

    by Anna Malmros, Piero Gamarra, Mattias Thorsell, Marie‐Antoinette di Forte‐Poisson, Cedric Lacam, Maurice Tordjman, Raphaël Aubry, Herbert Zirath, Niklas Rorsman

    An InAlN/AlN/GaN HEMT with Au‐free Ta‐based ohmic contacts and a high‐quality PECVD SiN pas‐sivation is reported. The ohmic contacts were annealed at 550 °C, resulting in a contact resistance of 0.64 Ωmm. The gate length was 50 nm. The device performance and the process were evaluated by performing DC‐, pulsed IV‐, RF‐, and load‐pull measurements. It was observed that current slump was effectively mitigated by the passivation layer. The DC channel current density increased by 71 % to 1170 mA/mm at the knee of the IV curve, and the transconductance increased from 382 to 477 mS/mm after passivation. At the same time the gate leakage increased, and the extrinsic fmax decreased from 207 to 140 GHz. Output powers of 4.1 and 3.5 W/mm were measured after passivation at 31 and 40 GHz, respectively.