Shusen Wu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Shusen Wu has a total of 78 co-authors. Here are the top co-authors by number of shared publications:
Shulin Lü
9 shared publications- Shulin Lü
State Key Lab of Materials Processing and Die & Mould Technology, School of Materials Science and Engineering, Huazhong University of Science and Technology, Wuhan 430074, China
7 shared publications - Wei Guo
State Key Lab of Materials Processing and Die & Mould Technology, School of Materials Science and Engineering, Huazhong University of Science and Technology, Wuhan 430074, China
7 shared publications - Jianyu Li
State Key Laboratory of Advanced Design and Manufacturing Technology for Vehicle, College of Mechanical and Vehicle Engineering, Hunan University, Changsha 410082, China
5 shared publications Ping An
Huazhong University of Science and Technology
5 shared publicationsShu-Lin Lü
State Key Lab of Materials Processing and Die & Mould Technology, School of Materials Science and Engineering, Huazhong University of Science and Technology, Wuhan, China
5 shared publications
Latest Publications
- Open Access
- 23 September 2025
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 39, 1977-1990
Breaking the strength-ductility trade-off in nano-TiB2/Al–2Li–2Cu-0.2Sc metal-matrix composites
- 23 September 2025
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 39, 1977-1990
Open AccessBreaking the strength-ductility trade-off in nano-TiB2/Al–2Li–2Cu-0.2Sc metal-matrix composites
- 30 June 2025
- Published by Springer Nature in China Foundry
- Vol. 23 (1) , 101-107
On AlNP/Mg-Zn-Cu cast composites with low expansion and high thermal conductivity
- 30 June 2025
- Published by Springer Nature in China Foundry
- Vol. 23 (1) , 101-107
On AlNP/Mg-Zn-Cu cast composites with low expansion and high thermal conductivity
- Open Access
Enhancement of Strength–Ductility Synergy of Al-Li Cast Alloy via New Forming Processes and Sc Addition
In this study, concurrent enhancements in both strength and ductility of the Al-2Li-2Cu-0.5Mg-0.2Zr cast alloy (hereafter referred to as Al-Li) were achieved through an optimized forming process comprising ultrasonic treatment followed by squeeze casting, coupled with the incorporation of Sc. Initially, the variations in the microstructure and mechanical properties of the Sc-free Al-Li cast alloy (i.e., alloy A) during various forming processes were investigated. The results revealed that the grain size in the UT+SC (ultrasonic treatment + squeeze casting) alloy was reduced by 76.3% and 57.7%, respectively, compared to those of the GC (gravity casting) or SC alloys. Additionally, significant improvements were observed in its compositional segregation and porosity reduction. After UT+SC, the ultimate tensile strength (UTS), yield strength (YS), and elongation reached 235 MPa, 135 MPa, and 15%, respectively, which were 113.6%, 28.6%, and 1150% higher than those of the GC alloy. Subsequently, the Al-Li cast alloy containing 0.2 wt.% Sc (referred to as alloy B) exhibited even finer grains under the UT+SC process, resulting in simultaneous enhancements in its UTS, YS, and elongation. Interestingly, the product of ultimate tensile strength and elongation (i.e., UTS × EL) for both alloys reached 36 GPa•% and 42 GPa•%, respectively, which is much higher than that of other Al-Li cast alloys reported in the available literature.
Open AccessEnhancement of Strength–Ductility Synergy of Al-Li Cast Alloy via New Forming Processes and Sc Addition
In this study, concurrent enhancements in both strength and ductility of the Al-2Li-2Cu-0.5Mg-0.2Zr cast alloy (hereafter referred to as Al-Li) were achieved through an optimized forming process comprising ultrasonic treatment followed by squeeze casting, coupled with the incorporation of Sc. Initially, the variations in the microstructure and mechanical properties of the Sc-free Al-Li cast alloy (i.e., alloy A) during various forming processes were investigated. The results revealed that the grain size in the UT+SC (ultrasonic treatment + squeeze casting) alloy was reduced by 76.3% and 57.7%, respectively, compared to those of the GC (gravity casting) or SC alloys. Additionally, significant improvements were observed in its compositional segregation and porosity reduction. After UT+SC, the ultimate tensile strength (UTS), yield strength (YS), and elongation reached 235 MPa, 135 MPa, and 15%, respectively, which were 113.6%, 28.6%, and 1150% higher than those of the GC alloy. Subsequently, the Al-Li cast alloy containing 0.2 wt.% Sc (referred to as alloy B) exhibited even finer grains under the UT+SC process, resulting in simultaneous enhancements in its UTS, YS, and elongation. Interestingly, the product of ultimate tensile strength and elongation (i.e., UTS × EL) for both alloys reached 36 GPa•% and 42 GPa•%, respectively, which is much higher than that of other Al-Li cast alloys reported in the available literature.
- Open Access
Effects of Low Nickel Content on Microstructure and High-Temperature Mechanical Properties of Al-7Si-1.5Cu-0.4Mg Aluminum Alloy
In this paper, the effects of Ni content on the room and elevated temperature (250 °C) tensile strength of Al-7Si-1.5Cu-0.4Mg-0.3Mn-0.1RE-xNi (x = 0, 0.3, 0.6, 0.9 wt.%) alloys were investigated, along with microstructure characterization and tensile testing. In the as-cast state, the dominant Ni-rich phases were primarily the γ-Al7Cu4Ni and δ-Al3CuNi phases. Following the solution heat treatment, a significant reduction in the γ-Al7Cu4Ni phase was noted, accompanied by the emergence of numerous small ε-Al3Ni phases. Both room temperature strength and high temperature strength at 250 °C exhibited a consistent increase with rising Ni content, reaching 405 MPa and 261 MPa, respectively, at 0.9 Ni content, which were increased by 6.4% and 16.8%, respectively, compared with 0 Ni content. The elongation exhibited an oscillating increase within the Ni content range of 0 to 0.6, reaching peak values of 2.6% in room temperature and 4.3% in high temperature at 0.6 Ni, followed by a rapid decline. At 0.6 Ni content, the alloy demonstrated a well-balanced combination of mechanical properties, featuring commendable strength and plasticity.
Open AccessEffects of Low Nickel Content on Microstructure and High-Temperature Mechanical Properties of Al-7Si-1.5Cu-0.4Mg Aluminum Alloy
In this paper, the effects of Ni content on the room and elevated temperature (250 °C) tensile strength of Al-7Si-1.5Cu-0.4Mg-0.3Mn-0.1RE-xNi (x = 0, 0.3, 0.6, 0.9 wt.%) alloys were investigated, along with microstructure characterization and tensile testing. In the as-cast state, the dominant Ni-rich phases were primarily the γ-Al7Cu4Ni and δ-Al3CuNi phases. Following the solution heat treatment, a significant reduction in the γ-Al7Cu4Ni phase was noted, accompanied by the emergence of numerous small ε-Al3Ni phases. Both room temperature strength and high temperature strength at 250 °C exhibited a consistent increase with rising Ni content, reaching 405 MPa and 261 MPa, respectively, at 0.9 Ni content, which were increased by 6.4% and 16.8%, respectively, compared with 0 Ni content. The elongation exhibited an oscillating increase within the Ni content range of 0 to 0.6, reaching peak values of 2.6% in room temperature and 4.3% in high temperature at 0.6 Ni, followed by a rapid decline. At 0.6 Ni content, the alloy demonstrated a well-balanced combination of mechanical properties, featuring commendable strength and plasticity.
- Open Access
- 5 February 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 29, 2750-2757
Rejuvenation behavior of Cu–Zr metallic glass under different holding times during deep cryogenic cycling treatment: Experiments and simulation
- 5 February 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 29, 2750-2757
Open AccessRejuvenation behavior of Cu–Zr metallic glass under different holding times during deep cryogenic cycling treatment: Experiments and simulation
- Open Access
- 16 January 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 29, 40-49
Synergistic effects of ultrasonic vibration and isothermal treatment on the peritectic transformation and microstructure evolution of Cu–Sn alloy
- 16 January 2024
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 29, 40-49
Open AccessSynergistic effects of ultrasonic vibration and isothermal treatment on the peritectic transformation and microstructure evolution of Cu–Sn alloy
- 1 August 2023
- Published by Springer Nature in China Foundry
- Vol. 21 (1) , 1-10
Progress in preparation of AlN-reinforced magnesium matrix composites: A review
- 1 August 2023
- Published by Springer Nature in China Foundry
- Vol. 21 (1) , 1-10
Progress in preparation of AlN-reinforced magnesium matrix composites: A review
- Open Access
- 6 June 2023
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 25, 1334-1343
Precipitates strengthening mechanism of a new squeeze-cast Al–Cu–Li–Mn alloy with high strength and ductility
- 6 June 2023
- Published by Elsevier in Journal of Materials Research and Technology
- Vol. 25, 1334-1343
Open AccessPrecipitates strengthening mechanism of a new squeeze-cast Al–Cu–Li–Mn alloy with high strength and ductility
- Open Access
From Mo–Si–B to Mo–Ti–Si–B Alloys: A Short Review
Mo–Si–B alloys have attracted considerable research interest during the last several decades due to their high melting points, excellent high-temperature strength and relatively good oxidation resistance. However, insufficient room-temperature fracture toughness and high-temperature oxidation resistance restrain their further application. Generally, a sufficient volume fraction of BCC-Mo solid-solution phase, providing the ductility, and a high Si content, responsible for the formation of passive oxide scales, is difficult to achieve simultaneously in this ternary system. Recently, macroalloying of Ti has been proposed to establish a novel phase equilibrium with a combination of enough BCC phase and intermetallic compounds that contain a large amount of Si. In this article, the development history from the ternary Mo–Si–B to the quaternary Mo–Ti–Si–B system was reviewed. It was found that the constitution phases could be easily tailored by changing the Ti content. In this regard, better performance of mechanical properties and oxidation resistance can be obtained through proper alloy design. In-depth understanding of the advantages of the quaternary alloys over their ternary ancestors may contribute to bringing about a new concept in designing novel ultra-high-temperature structural materials.
Open AccessFrom Mo–Si–B to Mo–Ti–Si–B Alloys: A Short Review
Mo–Si–B alloys have attracted considerable research interest during the last several decades due to their high melting points, excellent high-temperature strength and relatively good oxidation resistance. However, insufficient room-temperature fracture toughness and high-temperature oxidation resistance restrain their further application. Generally, a sufficient volume fraction of BCC-Mo solid-solution phase, providing the ductility, and a high Si content, responsible for the formation of passive oxide scales, is difficult to achieve simultaneously in this ternary system. Recently, macroalloying of Ti has been proposed to establish a novel phase equilibrium with a combination of enough BCC phase and intermetallic compounds that contain a large amount of Si. In this article, the development history from the ternary Mo–Si–B to the quaternary Mo–Ti–Si–B system was reviewed. It was found that the constitution phases could be easily tailored by changing the Ti content. In this regard, better performance of mechanical properties and oxidation resistance can be obtained through proper alloy design. In-depth understanding of the advantages of the quaternary alloys over their ternary ancestors may contribute to bringing about a new concept in designing novel ultra-high-temperature structural materials.
- Open Access
Effects of Al-Ti-C Refiner and Forming Processes on the Microstructure and Properties of Al-Zn-Mg-Cu Alloys
In this paper, the refinement effect of Al-5Ti-0.2C refiner on Al-Zn-Mg-Cu alloys was first investigated, and then the effects of three forming processes, i.e., Gravity Casting (GC), Squeeze Casting (SC), and Squeeze Casting after Ultrasonic Treatment (UT-SC), on microstructure and properties of Al-Zn-Mg-Cu alloys were studied. The results show that the refining effect of Al-5Ti-0.2C refiner is obvious; first, the average grain size of the alloy decreases and then increases with the increase in Ti content from 0.15 wt.% to 0.3 wt.%. The optimal amount of added Al-5Ti-0.2C is 0.2 wt.% Ti content. The good refining effect is attributed to the formation of TiC particles and Al3Ti compounds by the refiner, which can all be the nucleus of solidification. The poor refining effect when the Ti content was more than 0.2 wt.% is due to the formation of coarse Al3Ti particles. The results of three forming processes that cast Al-Zn-Mg-Cu alloys under the addition of Al-5Ti-0.2C with 0.2 wt.% Ti content show that the mechanical properties under the UT-SC process are the best; the tensile strength in the as-cast state reaches 367 MPa, and the elongation is 3.84%. The effect of tiny TiC particles in the refiner on the microstructure and properties of Al-Zn-Mg-Cu alloys is also discussed.
Open AccessEffects of Al-Ti-C Refiner and Forming Processes on the Microstructure and Properties of Al-Zn-Mg-Cu Alloys
In this paper, the refinement effect of Al-5Ti-0.2C refiner on Al-Zn-Mg-Cu alloys was first investigated, and then the effects of three forming processes, i.e., Gravity Casting (GC), Squeeze Casting (SC), and Squeeze Casting after Ultrasonic Treatment (UT-SC), on microstructure and properties of Al-Zn-Mg-Cu alloys were studied. The results show that the refining effect of Al-5Ti-0.2C refiner is obvious; first, the average grain size of the alloy decreases and then increases with the increase in Ti content from 0.15 wt.% to 0.3 wt.%. The optimal amount of added Al-5Ti-0.2C is 0.2 wt.% Ti content. The good refining effect is attributed to the formation of TiC particles and Al3Ti compounds by the refiner, which can all be the nucleus of solidification. The poor refining effect when the Ti content was more than 0.2 wt.% is due to the formation of coarse Al3Ti particles. The results of three forming processes that cast Al-Zn-Mg-Cu alloys under the addition of Al-5Ti-0.2C with 0.2 wt.% Ti content show that the mechanical properties under the UT-SC process are the best; the tensile strength in the as-cast state reaches 367 MPa, and the elongation is 3.84%. The effect of tiny TiC particles in the refiner on the microstructure and properties of Al-Zn-Mg-Cu alloys is also discussed.