Yuxin Chai
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Yuxin Chai has a total of 3 co-authors. Here are the top co-authors by number of shared publications:
Huayu Zhang
Harbin Institute of Technology, Shenzhen Graduate School, Shenzhen Key Laboratory for Advanced Materials and Department of Material Science and Engineering, University Town, Shenzhen, Guangdong 518055, China
2 shared publicationsXingui Zhou
National University of Defense Technology, Science and Technology on Advanced Ceramic Fibres and Composites Laboratory, Changsha, Hunan 410073, China
2 shared publicationsYumin Zhang
Harbin Institute of Technology, Center for Composite Materials, Harbin, Heilongjiang 150001, China
1 shared publication
Latest Publications
- 6 November 2018
- Published by Taylor & Francis in Fusion Science and Technology
- Vol. 75 (2) , 112-119
The Effect of Heat Treatment on the Properties of SiCf/SiC Composites Prepared with Different SiC Fibers
Silicon carbide (SiC) fiber–reinforced SiC matrix (SiCf/SiC) composites, employing two SiC fibers, KD-I and KD-II, respectively, were fabricated by the precursor infiltration and pyrolysis process. A pyrocarbon coating was used as the fiber-matrix interface. In addition, the effects of heat treatment on the properties of the SiC fibers and SiCf/SiC composites were investigated. Results revealed marginal performance degradation of the KD-I and KD-II SiC fibers after heat treatment at 1100°C for 1 h. However, heat treatment at 1400°C for 1 h led to the decrease in the single-filament tensile strength of the KD-I and KD-II SiC fibers by 50.2% and 10.1%, respectively. In addition, the flexural strength of the SiCf/SiC composites, which were fabricated using the KD-I and KD-II SiC fibers, decreased by 49.6% and 15.9%, respectively. The difference in the composition of the KD-I and KD-II SiC fibers demonstrated that the SiC fibers and SiCf/SiC composites decreased by varying degrees.
- 6 November 2018
- Published by Taylor & Francis in Fusion Science and Technology
- Vol. 75 (2) , 112-119
The Effect of Heat Treatment on the Properties of SiCf/SiC Composites Prepared with Different SiC Fibers
Silicon carbide (SiC) fiber–reinforced SiC matrix (SiCf/SiC) composites, employing two SiC fibers, KD-I and KD-II, respectively, were fabricated by the precursor infiltration and pyrolysis process. A pyrocarbon coating was used as the fiber-matrix interface. In addition, the effects of heat treatment on the properties of the SiC fibers and SiCf/SiC composites were investigated. Results revealed marginal performance degradation of the KD-I and KD-II SiC fibers after heat treatment at 1100°C for 1 h. However, heat treatment at 1400°C for 1 h led to the decrease in the single-filament tensile strength of the KD-I and KD-II SiC fibers by 50.2% and 10.1%, respectively. In addition, the flexural strength of the SiCf/SiC composites, which were fabricated using the KD-I and KD-II SiC fibers, decreased by 49.6% and 15.9%, respectively. The difference in the composition of the KD-I and KD-II SiC fibers demonstrated that the SiC fibers and SiCf/SiC composites decreased by varying degrees.
- 24 June 2017
- Published by SAGE Publications in Advances in Applied Ceramics: Structural, Functional and Bioceramics
- Vol. 116 (7) , 392-399
Mechanical properties of SiC f /SiC composites with alternating PyC/BN multilayer interfaces
Alternating pyrolytic carbon/boron nitride (PyC/BN)n multilayer coatings were applied to the KD–II silicon carbide (SiC) fibres by chemical vapour deposition technique to fabricate continuous SiC fibre-reinforced SiC matrix (SiCf/SiC) composites with improved flexural strength and fracture toughness. Three-dimensional SiCf/SiC composites with different interfaces were fabricated by polymer infiltration and pyrolysis process. The microstructure of the coating was characterised by scanning electron microscopy, X–photoelectron spectroscopy and transmission electron microscopy. The interfacial shear strength was determined by the single-fibre push-out test. Single-edge notched beam (SENB) test and three-point bending test were used to evaluate the influence of multilayer interfaces on the mechanical properties of SiCf/SiC composites. The results indicated that the (PyC/BN)n multilayer interface led to optimum flexural strength and fracture toughness of 566.0 MPa and 21.5 MPa m1/2, respectively, thus the fracture toughness of the composites was significantly improved.
- 24 June 2017
- Published by SAGE Publications in Advances in Applied Ceramics: Structural, Functional and Bioceramics
- Vol. 116 (7) , 392-399
Mechanical properties of SiC f /SiC composites with alternating PyC/BN multilayer interfaces
Alternating pyrolytic carbon/boron nitride (PyC/BN)n multilayer coatings were applied to the KD–II silicon carbide (SiC) fibres by chemical vapour deposition technique to fabricate continuous SiC fibre-reinforced SiC matrix (SiCf/SiC) composites with improved flexural strength and fracture toughness. Three-dimensional SiCf/SiC composites with different interfaces were fabricated by polymer infiltration and pyrolysis process. The microstructure of the coating was characterised by scanning electron microscopy, X–photoelectron spectroscopy and transmission electron microscopy. The interfacial shear strength was determined by the single-fibre push-out test. Single-edge notched beam (SENB) test and three-point bending test were used to evaluate the influence of multilayer interfaces on the mechanical properties of SiCf/SiC composites. The results indicated that the (PyC/BN)n multilayer interface led to optimum flexural strength and fracture toughness of 566.0 MPa and 21.5 MPa m1/2, respectively, thus the fracture toughness of the composites was significantly improved.