Eric K. Lin
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Eric K. Lin has a total of 31 co-authors. Here are the top co-authors by number of shared publications:
- Wen-Li Wu
National Institute of Standards and Technology
4 shared publications Marie Angelopoulos
IBM T. J. Watson Research Center, Yorktown Heights, New York 10598
3 shared publications- Christopher L. Soles
Material Measurement Laboratory National Institute of Standards and Technology Gaithersburg Maryland USA
2 shared publications Dario L. Goldfarb
IBM T. J. Watson Research Center, Yorktown Heights, New York 10598
2 shared publications- Ronald L. Jones
National Institute of Standards and Technology
2 shared publications - Vivek M. Prabhu
NIST Polymers & Complex Fluids Group, 100 Bureau Dr, Gaithersburg, MD 20899, USA
2 shared publications
Latest Publications
- 1 January 2019
- Published by Elsevier in Proceedings of the Combustion Institute
- Vol. 37 (2) , 1791-1798
Dynamics and burning limits of near-limit hot, warm, and cool diffusion flames of dimethyl ether at elevated pressures
- 1 January 2019
- Published by Elsevier in Proceedings of the Combustion Institute
- Vol. 37 (2) , 1791-1798
Dynamics and burning limits of near-limit hot, warm, and cool diffusion flames of dimethyl ether at elevated pressures
- 16 March 2007
- Published by SPIE-Intl Soc Optical Eng
- Vol. 6519, 651910-651910-12
Direct measurement of the in-situ developed latent image: the residual swelling fraction
The spatial distribution of polymer photoresist and deuterium labeled developer highlights a fraction of material at a model line edge that swells, but does not dissolve. This residual swelling fraction remains swollen during both the in situ development and rinse steps uncovering that the final lithographic feature is resolved by a collapse mechanism during the drying step. We demonstrate that contrast variant neutron reflectivity provides a general method to probe the nanometer resolved in situ development and rinse process step.
- 16 March 2007
- Published by SPIE-Intl Soc Optical Eng
- Vol. 6519, 651910-651910-12
Direct measurement of the in-situ developed latent image: the residual swelling fraction
The spatial distribution of polymer photoresist and deuterium labeled developer highlights a fraction of material at a model line edge that swells, but does not dissolve. This residual swelling fraction remains swollen during both the in situ development and rinse steps uncovering that the final lithographic feature is resolved by a collapse mechanism during the drying step. We demonstrate that contrast variant neutron reflectivity provides a general method to probe the nanometer resolved in situ development and rinse process step.
- 1 November 2003
- Published by American Vacuum Society in Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena
- Vol. 21 (6) , 3162-3165
Near edge x-ray absorption fine structure measurements of surface segregation in 157 nm photoresist blends
The surface and bulk chemistry of photoresist blends for use at the 157 nm node were analyzed using near edge x-ray absorption fine structure spectroscopy to quantify component segregation and identify surface phenomena that may impact pattern formation. Spectral combinations of the constituent polymers are used to fit the spectra of the blend films. Significant segregation of one component to the surface of the photoresist film was found, in excess of the composition of that component in the blend. The bulk data were consistent with initial blend compositions. As expected, the more hydrophobic or lower surface tension component wets the film surface even under typical photoresist processing conditions.
- 1 November 2003
- Published by American Vacuum Society in Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena
- Vol. 21 (6) , 3162-3165
Near edge x-ray absorption fine structure measurements of surface segregation in 157 nm photoresist blends
The surface and bulk chemistry of photoresist blends for use at the 157 nm node were analyzed using near edge x-ray absorption fine structure spectroscopy to quantify component segregation and identify surface phenomena that may impact pattern formation. Spectral combinations of the constituent polymers are used to fit the spectra of the blend films. Significant segregation of one component to the surface of the photoresist film was found, in excess of the composition of that component in the blend. The bulk data were consistent with initial blend compositions. As expected, the more hydrophobic or lower surface tension component wets the film surface even under typical photoresist processing conditions.
- 15 July 2002
- Published by SPIE-Intl Soc Optical Eng
- Vol. 4690, 342-350
Chain conformation in ultrathin polymer films
Using Small Angle Neutron Scattering (SANS), we present the first quantitative measurements of the 3-dimensional conformation of macromolecules in thin polymer films of D < RG,Bulk, where D is the film thickness and RG,Bulk is the bulk radius of gyration. For D approximately equals 0.5 RG,Bulk, the molecular size along the film normal is less than 0.5 RG,Bulk, while relatively small changes are observed parallel to the surface. The observed changes in molecular size agree with predictions of molecular dynamics simulations of polymers confined in thin films, resulting from increased molecular orientation rather than chain distortion. Segregation of molecular centers of mass to the film center facilitates molecular packing while minimizing chain distortion. Estimates of length scales relating to the onset of chain distortion and chain orientation in thin film resists are D approximately equals 0.1 RG,Bulk and D approximately equals N(sigma ) respectively, where D is the film thickness, N is the number of chain segments, and (sigma) is the persistence length.
- 15 July 2002
- Published by SPIE-Intl Soc Optical Eng
- Vol. 4690, 342-350
Chain conformation in ultrathin polymer films
Using Small Angle Neutron Scattering (SANS), we present the first quantitative measurements of the 3-dimensional conformation of macromolecules in thin polymer films of D < RG,Bulk, where D is the film thickness and RG,Bulk is the bulk radius of gyration. For D approximately equals 0.5 RG,Bulk, the molecular size along the film normal is less than 0.5 RG,Bulk, while relatively small changes are observed parallel to the surface. The observed changes in molecular size agree with predictions of molecular dynamics simulations of polymers confined in thin films, resulting from increased molecular orientation rather than chain distortion. Segregation of molecular centers of mass to the film center facilitates molecular packing while minimizing chain distortion. Estimates of length scales relating to the onset of chain distortion and chain orientation in thin film resists are D approximately equals 0.1 RG,Bulk and D approximately equals N(sigma ) respectively, where D is the film thickness, N is the number of chain segments, and (sigma) is the persistence length.
- 1 March 2002
- Published by American Vacuum Society in Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena
- Vol. 20 (2) , 704-709
Combinatorial methodologies offer potential for rapid research of photoresist materials and formulations
A combinatorial research methodology is outlined with the potential to investigate material factors in photoresist formulations more rapidly than with traditional experimental design. The approach involves generating a gradient of processing variables in the photoresist film and using a set of analysis tools to “map” the photoresist properties as a function of the gradient variables. While high-throughput strategies have proven useful for empirical optimization of photoresist processing conditions, they have not been fully exploited to probe the complex array of material issues in projection lithography. Of primary importance in combinatorial methodologies is the generation of variable gradients. The focus of this article is to illustrate techniques to generate a gradient in bake temperature and bake time in the polymer films, and to illustrate that these gradient techniques can be used to probe fundamental properties of lithographic materials, such as deprotection kinetics. These gradient techniques were...
- 1 March 2002
- Published by American Vacuum Society in Journal of Vacuum Science & Technology B: Microelectronics and Nanometer Structures Processing, Measurement, and Phenomena
- Vol. 20 (2) , 704-709
Combinatorial methodologies offer potential for rapid research of photoresist materials and formulations
A combinatorial research methodology is outlined with the potential to investigate material factors in photoresist formulations more rapidly than with traditional experimental design. The approach involves generating a gradient of processing variables in the photoresist film and using a set of analysis tools to “map” the photoresist properties as a function of the gradient variables. While high-throughput strategies have proven useful for empirical optimization of photoresist processing conditions, they have not been fully exploited to probe the complex array of material issues in projection lithography. Of primary importance in combinatorial methodologies is the generation of variable gradients. The focus of this article is to illustrate techniques to generate a gradient in bake temperature and bake time in the polymer films, and to illustrate that these gradient techniques can be used to probe fundamental properties of lithographic materials, such as deprotection kinetics. These gradient techniques were...
- 1 January 2001
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 148 (10) , F195-F199
X-Ray Reflectivity and FTIR Measurements of N[sub 2] Plasma Effects on the Density Profile of Hydrogen Silsesquioxane Thin Films
The density depth profile and chemical bond structure of hydrogen silsesquioxane (HSQ) thin films treated with an N2N2 plasma with varying power and exposure time were measured using specular X-ray reflectivity (SXR) and Fourier transform infrared (FTIR) spectroscopy. The SXR data indicated that the density profile of an untreated HSQ film is not uniform. At least four layers with different electron densities were required to fit the SXR data. For HSQ films treated with either increasing plasma power or plasma exposure time, the film roughness increased and a densified layer was observed at the film/air interface. The thickness of the densified layer increased with both plasma power and plasma exposure time. In the FTIR spectra of the plasma-treated films, the intensities of the Si-O peaks due to the network structure and the Si-OH peak due to water absorption increased and the intensities of the Si-H peaks decreased. The FTIR data show that the plasma converts the HSQ structure into a SiO2SiO2 -like structure and are consistent with the densification observed in the SXR measurements. In general, the HSQ film is more sensitive to increasing plasma power than to increasing plasma exposure time. © 2001 The Electrochemical Society. All rights reserved.
- 1 January 2001
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 148 (10) , F195-F199
X-Ray Reflectivity and FTIR Measurements of N[sub 2] Plasma Effects on the Density Profile of Hydrogen Silsesquioxane Thin Films
The density depth profile and chemical bond structure of hydrogen silsesquioxane (HSQ) thin films treated with an N2N2 plasma with varying power and exposure time were measured using specular X-ray reflectivity (SXR) and Fourier transform infrared (FTIR) spectroscopy. The SXR data indicated that the density profile of an untreated HSQ film is not uniform. At least four layers with different electron densities were required to fit the SXR data. For HSQ films treated with either increasing plasma power or plasma exposure time, the film roughness increased and a densified layer was observed at the film/air interface. The thickness of the densified layer increased with both plasma power and plasma exposure time. In the FTIR spectra of the plasma-treated films, the intensities of the Si-O peaks due to the network structure and the Si-OH peak due to water absorption increased and the intensities of the Si-H peaks decreased. The FTIR data show that the plasma converts the HSQ structure into a SiO2SiO2 -like structure and are consistent with the densification observed in the SXR measurements. In general, the HSQ film is more sensitive to increasing plasma power than to increasing plasma exposure time. © 2001 The Electrochemical Society. All rights reserved.
- 15 December 2000
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 88 (12) , 7298-7303
Small angle neutron scattering measurements of nanoscale lithographic features
State-of-the-art lithographic techniques are able to fabricatestructures for the semiconductor and other nanofabrication industries with dimensions below 150 nm. The relentless drive to further miniaturize semiconductor devices has placed increasingly stringent demands on current microscopy-based techniques for precisely measuring the size and the quality (line-edge roughness) of lithographically produced features. Using newly developed neutron optics, we demonstrate the first application of small-angle neutron scattering to nondestructively and quantitatively measure both the dimension and the quality of 150 nm lines fabricated on single crystal silicon wafers.
- 15 December 2000
- Published by AIP Publishing in Journal of Applied Physics
- Vol. 88 (12) , 7298-7303
Small angle neutron scattering measurements of nanoscale lithographic features
State-of-the-art lithographic techniques are able to fabricatestructures for the semiconductor and other nanofabrication industries with dimensions below 150 nm. The relentless drive to further miniaturize semiconductor devices has placed increasingly stringent demands on current microscopy-based techniques for precisely measuring the size and the quality (line-edge roughness) of lithographically produced features. Using newly developed neutron optics, we demonstrate the first application of small-angle neutron scattering to nondestructively and quantitatively measure both the dimension and the quality of 150 nm lines fabricated on single crystal silicon wafers.