Sukangkana Talangkun
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Sukangkana Talangkun has a total of 34 co-authors. Here are the top co-authors by number of shared publications:
- Apichart Boonma
Khon Kaen Univ, Fac Engn, Dept Ind Engn, Khon Kaen 40002, Thailand
2 shared publications Autsadawooth Kummoo
Mae Fah Luang University
2 shared publicationsDhammasook Mingmuang
Khon Kaen University
2 shared publications- Kowit Ponhan
Department of Industrial Engineering, Faculty of Engineering, Khon Kaen University, Khon Kaen, Thailand
2 shared publications Onthida Kosasang
Mae Fah Luang University
2 shared publicationsPhuriphut Saenpong
Khon Kaen University
2 shared publications
Latest Publications
- Open Access
- 9 February 2026
- Published by Engineering, Technology & Applied Science Research in Engineering, Technology & Applied Science Research
- Vol. 16 (1) , 32739-32746
Multi-Criteria Evaluation of Brake Disc Materials Using BWM-TOPSIS Linear Programming
The selection of the best all-around material for brake discs remains a challenging engineering problem due to the conflicting requirements for wear resistance, thermal stability, mechanical strength, and manufacturability. To address this multi-criteria challenge, this study proposes an integrated decision-making framework combining the index of Item-Objective Congruence (IOC), the Best-Worst Method (BWM), and the Technique for Order Preference by Similarity to Ideal Solution Linear Programming (TOPSIS-LP) approach. The IOC was employed to validate the relevance of six evaluation criteria based on input from five domain experts, while BWM derived weights for these criteria. TOPSIS-LP was then used to rank five material alternatives, including gray cast iron, steel alloy, Aluminum Metal Matrix Composite (Al-MMC), Carbon-Carbon/Carbon-Silicon Carbide Composite (C-C/SiC), and Ceramic-Based Composites (CMC), through linear optimization of the weighted decision matrix. The results indicated that the CMC achieved the highest performance with a relative closeness coefficient CCi of 0.7629, followed by C-C/SiC and Al-MMC, while a four-scenario sensitivity analysis confirmed perfect rank stability (Spearman's rank correlation: ρs = 1.00) under ±20% weight variations. Overall, the findings indicate that advanced ceramic and composite materials outperform conventional metals in tribological and thermal performance, while the proposed IOC-BWM-TOPSIS-LP framework demonstrates strong robustness, interpretability, and applicability to complex engineering material selection problems.
- 9 February 2026
- Published by Engineering, Technology & Applied Science Research in Engineering, Technology & Applied Science Research
- Vol. 16 (1) , 32739-32746
Open AccessMulti-Criteria Evaluation of Brake Disc Materials Using BWM-TOPSIS Linear Programming
The selection of the best all-around material for brake discs remains a challenging engineering problem due to the conflicting requirements for wear resistance, thermal stability, mechanical strength, and manufacturability. To address this multi-criteria challenge, this study proposes an integrated decision-making framework combining the index of Item-Objective Congruence (IOC), the Best-Worst Method (BWM), and the Technique for Order Preference by Similarity to Ideal Solution Linear Programming (TOPSIS-LP) approach. The IOC was employed to validate the relevance of six evaluation criteria based on input from five domain experts, while BWM derived weights for these criteria. TOPSIS-LP was then used to rank five material alternatives, including gray cast iron, steel alloy, Aluminum Metal Matrix Composite (Al-MMC), Carbon-Carbon/Carbon-Silicon Carbide Composite (C-C/SiC), and Ceramic-Based Composites (CMC), through linear optimization of the weighted decision matrix. The results indicated that the CMC achieved the highest performance with a relative closeness coefficient CCi of 0.7629, followed by C-C/SiC and Al-MMC, while a four-scenario sensitivity analysis confirmed perfect rank stability (Spearman's rank correlation: ρs = 1.00) under ±20% weight variations. Overall, the findings indicate that advanced ceramic and composite materials outperform conventional metals in tribological and thermal performance, while the proposed IOC-BWM-TOPSIS-LP framework demonstrates strong robustness, interpretability, and applicability to complex engineering material selection problems.
- Open Access
- 1 January 2025
- Published by IOP Publishing in Materials Research Express
- Vol. 12 (1) , 016509
Improvement of microstructure and mechanical properties for Al7075 aluminium reinforced with hybrid graphite and SiC particles via a combination of mechanical alloying and stir casting
This research focuses on the fabrication of Al7075 composites reinforced with varying amounts of nano-sized SiC particles (1.0, 1.5, and 2.0 wt%) combined with 0.5 wt% graphite (Gr), employing a hybrid process of mechanical alloying and semi-solid stir casting. The study investigates the influence of SiC content, nanoparticle feeding method, and the role of Gr on the microstructures, mechanical characteristics, and machinability of the composites. Microstructural analysis revealed that integrating milled powders into the molten Al7075 alloy produced a uniform dispersion of nanoscale SiC particles within the α-Al matrix, avoiding the particle agglomeration observed with the conventional method. Higher SiC content resulted in finer grains and improved mechanical performance. The Al7075-0.5Gr-2.0SiC composite exhibited a 16% increase in hardness relative to the unreinforced Al7075 alloy. The inclusion of nanoscale SiC particles notably enhanced tensile strength, while the presence of Gr acted as a lubricant, improving surface roughness.
- 1 January 2025
- Published by IOP Publishing in Materials Research Express
- Vol. 12 (1) , 016509
Open AccessImprovement of microstructure and mechanical properties for Al7075 aluminium reinforced with hybrid graphite and SiC particles via a combination of mechanical alloying and stir casting
This research focuses on the fabrication of Al7075 composites reinforced with varying amounts of nano-sized SiC particles (1.0, 1.5, and 2.0 wt%) combined with 0.5 wt% graphite (Gr), employing a hybrid process of mechanical alloying and semi-solid stir casting. The study investigates the influence of SiC content, nanoparticle feeding method, and the role of Gr on the microstructures, mechanical characteristics, and machinability of the composites. Microstructural analysis revealed that integrating milled powders into the molten Al7075 alloy produced a uniform dispersion of nanoscale SiC particles within the α-Al matrix, avoiding the particle agglomeration observed with the conventional method. Higher SiC content resulted in finer grains and improved mechanical performance. The Al7075-0.5Gr-2.0SiC composite exhibited a 16% increase in hardness relative to the unreinforced Al7075 alloy. The inclusion of nanoscale SiC particles notably enhanced tensile strength, while the presence of Gr acted as a lubricant, improving surface roughness.
- Open Access
- 1 February 2024
- Published by IOP Publishing in Materials Research Express
- Vol. 11 (2) , 026506
Effect of heat treatment on microstructural characteristics and mechanical properties of hypereutectic B390 aluminium alloys modified by phosphorus and bismuth
This study investigated the effects of solution treatment and aging processes on microstructural characteristics and mechanical properties of hypereutectic B390 Al-Si Alloy modified by phosphorus (P) and bismuth (Bi). The morphology evolution of primary Si, eutectic Si, intermetallic compounds, and secondary dendrite arm spacing (SDAS) of both initial and modified alloys were investigated in as-cast and heat-treated conditions. It was found that the combination of 0.1 wt%P and 0.5 wt%Bi in B390 alloy resulted in a remarkable modification and refinement of primary Si, eutectic Si, and SDAS compared to initial specimens in the as-cast condition. After heat treating, the fine lamellar eutectic Si and intermetallic compounds underwent a higher degree of fragmentation and coarsening, appearing as small round particles, leading to a more pronounced formation of a supersaturated solid solution. Additionally, the peak aging time of the B390-P-Bi alloy was only 7 h, 2 h less than the initial specimen. After T6 treatment and addition of both 0.1 wt%P and 0.5 wt%Bi, the B390-P-Bi alloy exhibited a smaller rounded Mg3Bi2 phase at peak aging with a 62.07% size reduction compared to the B390-Bi alloy. The results show that adding P with Bi enhanced hardness, ultimate tensile strength (UTS) and elongation because of refinement of the SDAS, primary Si and eutectic Si. These refinements played a crucial role in increasing tensile strength by more effective strengthening through precipitation and grain size reduction. The B390-P-Bi alloy is a promising choice for applications requiring a balance between strength and ductility.
- 1 February 2024
- Published by IOP Publishing in Materials Research Express
- Vol. 11 (2) , 026506
Open AccessEffect of heat treatment on microstructural characteristics and mechanical properties of hypereutectic B390 aluminium alloys modified by phosphorus and bismuth
This study investigated the effects of solution treatment and aging processes on microstructural characteristics and mechanical properties of hypereutectic B390 Al-Si Alloy modified by phosphorus (P) and bismuth (Bi). The morphology evolution of primary Si, eutectic Si, intermetallic compounds, and secondary dendrite arm spacing (SDAS) of both initial and modified alloys were investigated in as-cast and heat-treated conditions. It was found that the combination of 0.1 wt%P and 0.5 wt%Bi in B390 alloy resulted in a remarkable modification and refinement of primary Si, eutectic Si, and SDAS compared to initial specimens in the as-cast condition. After heat treating, the fine lamellar eutectic Si and intermetallic compounds underwent a higher degree of fragmentation and coarsening, appearing as small round particles, leading to a more pronounced formation of a supersaturated solid solution. Additionally, the peak aging time of the B390-P-Bi alloy was only 7 h, 2 h less than the initial specimen. After T6 treatment and addition of both 0.1 wt%P and 0.5 wt%Bi, the B390-P-Bi alloy exhibited a smaller rounded Mg3Bi2 phase at peak aging with a 62.07% size reduction compared to the B390-Bi alloy. The results show that adding P with Bi enhanced hardness, ultimate tensile strength (UTS) and elongation because of refinement of the SDAS, primary Si and eutectic Si. These refinements played a crucial role in increasing tensile strength by more effective strengthening through precipitation and grain size reduction. The B390-P-Bi alloy is a promising choice for applications requiring a balance between strength and ductility.
- Open Access
- 6 June 2023
- Published by Springer Nature in SN Applied Sciences
- Vol. 5 (7) , 1-11
Design of the semi-closed die for shaping the thick coin-like carbon steel parts in a single operation
The current study strives to improve the precision and accuracy of a die and reduce unnecessary production steps. Upset cold forging for thick coin-like carbon steel parts were studied and redesigned for a single operation. The slug used in this experiment was an annealed AISI 1020 carbon steel bar sheared into cylinders having a height to diameter ratio (h0/d0) of 2.07. The design problem is to prevent an inclined slug surface due to surface roughness when it is loaded in the die cavity. The redesigned die is semi-closed with a fixed support at a position 0.25 of the initial height of the slug. Six springs were employed to set the start-to-finish position during forging. The results showed that slugs with rough and uneven surfaces, with an h0/d0ratio of 2.07, could successfully undergo a single forging. Furthermore, the upset forged coin was designed to have a straight 2.4 mm outer edge, providing area for a set of mechanical fingers to grasp the workpiece during transfer to subsequent steps in the work process of a vertical and/or horizontal forging die set.
- 6 June 2023
- Published by Springer Nature in SN Applied Sciences
- Vol. 5 (7) , 1-11
Open AccessDesign of the semi-closed die for shaping the thick coin-like carbon steel parts in a single operation
The current study strives to improve the precision and accuracy of a die and reduce unnecessary production steps. Upset cold forging for thick coin-like carbon steel parts were studied and redesigned for a single operation. The slug used in this experiment was an annealed AISI 1020 carbon steel bar sheared into cylinders having a height to diameter ratio (h0/d0) of 2.07. The design problem is to prevent an inclined slug surface due to surface roughness when it is loaded in the die cavity. The redesigned die is semi-closed with a fixed support at a position 0.25 of the initial height of the slug. Six springs were employed to set the start-to-finish position during forging. The results showed that slugs with rough and uneven surfaces, with an h0/d0ratio of 2.07, could successfully undergo a single forging. Furthermore, the upset forged coin was designed to have a straight 2.4 mm outer edge, providing area for a set of mechanical fingers to grasp the workpiece during transfer to subsequent steps in the work process of a vertical and/or horizontal forging die set.
- Open Access
Microstructural Modification Hardness and Surface Roughness of Hypereutectic Al-Si Alloys by a Combination of Bismuth and Phosphorus
This research aimed to investigate the effects of bismuth (Bi) and phosphorus (P) addition on the microstructure and roughness of a B390 hypereutectic Al-Si alloy. Microstructural variation of as-cast alloys showed that P is an effective refiner of primary Si and its distribution, while Bi has the opposite effect. The liquidus temperature increased with greater amounts of P, resulting in a wider solidification range. The solidus temperature increased with Bi content, resulting in a shortened solidification range. The benefit of Bi on eutectic silicon was through changing its morphology from fibrous to lamellar structures. It was observed that both primary Si and eutectic Si were modified when both P and Bi were added to the alloys. For effective refinement, the size of primary Si can be reduced by 50.6% and, the P content should not be less than 0.1 wt% with a Bi content of 0.5–1.0 wt%. Furthermore, an intermetallic phase size reduction also occurs. P addition results in a significant (5.85%) increase in hardness. Adding Bi (up to 1.0 wt%) together with P (up to 0.1 wt%) did not reduce the effect of P on the hardness of the modified alloys. The most effective reduction in roughness achieved during cutting at both low and high speeds was 26.5% and 57.7%, respectively, from modifying the B390 alloy using 0.1 wt%P with 1.0 wt%Bi.
Open AccessMicrostructural Modification Hardness and Surface Roughness of Hypereutectic Al-Si Alloys by a Combination of Bismuth and Phosphorus
This research aimed to investigate the effects of bismuth (Bi) and phosphorus (P) addition on the microstructure and roughness of a B390 hypereutectic Al-Si alloy. Microstructural variation of as-cast alloys showed that P is an effective refiner of primary Si and its distribution, while Bi has the opposite effect. The liquidus temperature increased with greater amounts of P, resulting in a wider solidification range. The solidus temperature increased with Bi content, resulting in a shortened solidification range. The benefit of Bi on eutectic silicon was through changing its morphology from fibrous to lamellar structures. It was observed that both primary Si and eutectic Si were modified when both P and Bi were added to the alloys. For effective refinement, the size of primary Si can be reduced by 50.6% and, the P content should not be less than 0.1 wt% with a Bi content of 0.5–1.0 wt%. Furthermore, an intermetallic phase size reduction also occurs. P addition results in a significant (5.85%) increase in hardness. Adding Bi (up to 1.0 wt%) together with P (up to 0.1 wt%) did not reduce the effect of P on the hardness of the modified alloys. The most effective reduction in roughness achieved during cutting at both low and high speeds was 26.5% and 57.7%, respectively, from modifying the B390 alloy using 0.1 wt%P with 1.0 wt%Bi.
- 19 May 2020
- Published by Trans Tech Publications, Ltd. in Solid State Phenomena
- Vol. 304, 3-8
Impact Resistance and Fracture Surface of Al6061 Hybrid Composites Reinforced by Fly Ash and Calcium Oxide
Phase formation, impact resistance, and fracture surface were investigated in unreinforced Al6061, Al6061-5wt% fly ash and Al6061 hybrid composites containing 5wt% fly ash and 1,3 wt% CaO. The Al6061 composites were fabricated the stir casting process. The XRD patterns reveal the formation of second phases (MgAl2O4, CaAl4O7 and MgSiO3), which were found in the Al6061 hybrid composites. The average grain size of Al6061 hybrid composite are much smaller than that of unreinforced Al6061.The impact resistance was enhanced by approximately 67% in Al6061 hybrid composite as compared to unreinforced Al6061 alloy. Brittle fracture indicting brittle fracture was observed in unreinforced Al6061 alloy while evidence of a mixture of brittle and ductile fracture was found in the Al6061 hybrid composites.
- 19 May 2020
- Published by Trans Tech Publications, Ltd. in Solid State Phenomena
- Vol. 304, 3-8
Impact Resistance and Fracture Surface of Al6061 Hybrid Composites Reinforced by Fly Ash and Calcium Oxide
Phase formation, impact resistance, and fracture surface were investigated in unreinforced Al6061, Al6061-5wt% fly ash and Al6061 hybrid composites containing 5wt% fly ash and 1,3 wt% CaO. The Al6061 composites were fabricated the stir casting process. The XRD patterns reveal the formation of second phases (MgAl2O4, CaAl4O7 and MgSiO3), which were found in the Al6061 hybrid composites. The average grain size of Al6061 hybrid composite are much smaller than that of unreinforced Al6061.The impact resistance was enhanced by approximately 67% in Al6061 hybrid composite as compared to unreinforced Al6061 alloy. Brittle fracture indicting brittle fracture was observed in unreinforced Al6061 alloy while evidence of a mixture of brittle and ductile fracture was found in the Al6061 hybrid composites.
- Open Access
Thixoforming and Rheo-Die-Casting of A356/SiC Composite
This research investigated the rheo-die-casting process and the production of an A356/silicon carbide (SiC) composite by a thixoforming. The composite contained 15 percent by weight SiC particles of around 15–37 µm in size as the reinforcing phase. The composite feedstock was produced by semi-solid stir-casting, where pretreated SiC powder was gradually added into the A356 alloy melt to form a continuously stirred slurry composite melt, which was then cast in a steel mold. For thixoforming, the feedstock was reheated to 583 °C (approximately 0.4 fraction liquid), and its viscosity was reduced with shear rate, implying that A356/SiC exhibits shear thinning or non-Newtonian behavior. This is caused by the characteristic billet structure obtained having relatively globular grains that accommodate the flow of the semisolid composite. In the rheo-die-casting process, the A356/SiC feedstock was re-melted at 610–615 °C (approximately 0.8–0.9 fraction liquid) prior to die-casting and the resulting slurry was injected into a die with injection speeds of 3 and 4 m/s and pressures of 11 and 12 MPa, respectively. Two work-pieces of 16 × 15.6 × 205 mm3 were produced in one shot, and the resulting samples were subjected to T6 solution treatment at 540 °C for 1 h, quenched, and aged at 135 °C for 12 h. The results show that both low speed and low pressure rheo-die-cast samples exhibit uneven filling at the end of the part, whilst both high pressure and high speed promote more uniform distribution of SiC particles throughout the part length. In the as-rheo-die-cast condition, the most uniform of microstructures and hardness obtained from a sample fabricated at 4 m/s speed and 12 MPa pressure.
Open AccessThixoforming and Rheo-Die-Casting of A356/SiC Composite
This research investigated the rheo-die-casting process and the production of an A356/silicon carbide (SiC) composite by a thixoforming. The composite contained 15 percent by weight SiC particles of around 15–37 µm in size as the reinforcing phase. The composite feedstock was produced by semi-solid stir-casting, where pretreated SiC powder was gradually added into the A356 alloy melt to form a continuously stirred slurry composite melt, which was then cast in a steel mold. For thixoforming, the feedstock was reheated to 583 °C (approximately 0.4 fraction liquid), and its viscosity was reduced with shear rate, implying that A356/SiC exhibits shear thinning or non-Newtonian behavior. This is caused by the characteristic billet structure obtained having relatively globular grains that accommodate the flow of the semisolid composite. In the rheo-die-casting process, the A356/SiC feedstock was re-melted at 610–615 °C (approximately 0.8–0.9 fraction liquid) prior to die-casting and the resulting slurry was injected into a die with injection speeds of 3 and 4 m/s and pressures of 11 and 12 MPa, respectively. Two work-pieces of 16 × 15.6 × 205 mm3 were produced in one shot, and the resulting samples were subjected to T6 solution treatment at 540 °C for 1 h, quenched, and aged at 135 °C for 12 h. The results show that both low speed and low pressure rheo-die-cast samples exhibit uneven filling at the end of the part, whilst both high pressure and high speed promote more uniform distribution of SiC particles throughout the part length. In the as-rheo-die-cast condition, the most uniform of microstructures and hardness obtained from a sample fabricated at 4 m/s speed and 12 MPa pressure.
- 16 January 2020
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 975, 176-181
Effect of Heat Treatment Process on the Hardness of Aluminium356/Silicon Carbide Particulate Composites
This research is aimed to study effect of holding time and temperature in solution treatment and ageing on the hardness of the Aluminum A356 reinforced with silicon carbide particles. Alumimium matrix coposite was particulated with 15 microns-SiC with the content of 15 percent by weight. A356/SiC composites was prepared by the stirr casting. The stirrer was continuously stired at a speed of 300 rpm during acooling temperature to semi-solid state of 610 °C. During stirring the SiC powder was slowly added into the melt and continuously stirred for another 10 min. Then poured into the mold at the pouring temperature of 680°C. A356/SiC composites then subjected to a solid solution treatment with temperature of 540 °C for 1 hr. quenched with water and age hardening temperature of 120 and 135 °C for 3, 6, 12 and 18 hr. The result showed that, in as cast conditions, the composite with 15 microns silicon carbide, the 15 wt%SiC specimen exhibited the average hardness of 64.33 HB. After solution treated, the hardness of samples decreased. the specimen exhibited the average hardness of 53.83 HB. After ageing, the hardness of samples increased. the specimen ageing 120 °C 6 hr. exhibited the lowest average hardness of 51.45 HB while the specimen ageing 135 °C 18 hr. exhibited the highest average hardness of 73.54 HB.
- 16 January 2020
- Published by Trans Tech Publications, Ltd. in Materials Science Forum
- Vol. 975, 176-181
Effect of Heat Treatment Process on the Hardness of Aluminium356/Silicon Carbide Particulate Composites
This research is aimed to study effect of holding time and temperature in solution treatment and ageing on the hardness of the Aluminum A356 reinforced with silicon carbide particles. Alumimium matrix coposite was particulated with 15 microns-SiC with the content of 15 percent by weight. A356/SiC composites was prepared by the stirr casting. The stirrer was continuously stired at a speed of 300 rpm during acooling temperature to semi-solid state of 610 °C. During stirring the SiC powder was slowly added into the melt and continuously stirred for another 10 min. Then poured into the mold at the pouring temperature of 680°C. A356/SiC composites then subjected to a solid solution treatment with temperature of 540 °C for 1 hr. quenched with water and age hardening temperature of 120 and 135 °C for 3, 6, 12 and 18 hr. The result showed that, in as cast conditions, the composite with 15 microns silicon carbide, the 15 wt%SiC specimen exhibited the average hardness of 64.33 HB. After solution treated, the hardness of samples decreased. the specimen exhibited the average hardness of 53.83 HB. After ageing, the hardness of samples increased. the specimen ageing 120 °C 6 hr. exhibited the lowest average hardness of 51.45 HB while the specimen ageing 135 °C 18 hr. exhibited the highest average hardness of 73.54 HB.
- 1 October 2019
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 824, 260-266
Corrosion Investigation and Microstructure of High Calcium Fly Ash Reinforced Al6061
In this study, the effect of high Ca fly ash on the corrosion behavior and microstructure of Al6061 alloy matrix composite was investigated. The Al6061 matrix composites containing 5, 7, and 10 wt% of fly ash particles were prepared by the stir casting process. The corrosion behavior was investigated using potentiodynamic polarization measurement using 5 wt% NaCl. The results revealed that the Icorr increased from 2.44 µA/cm2 to 8.60 µA/cm2 as the fly ash concentration increased from 5 wt% to 10 wt%. This increase of Icorr indicates an increase of the corrosion rate. The corrosion mainly occurs at the interface between fly ash particles and Al 6061 matrix.
- 1 October 2019
- Published by Trans Tech Publications, Ltd. in Key Engineering Materials
- Vol. 824, 260-266
Corrosion Investigation and Microstructure of High Calcium Fly Ash Reinforced Al6061
In this study, the effect of high Ca fly ash on the corrosion behavior and microstructure of Al6061 alloy matrix composite was investigated. The Al6061 matrix composites containing 5, 7, and 10 wt% of fly ash particles were prepared by the stir casting process. The corrosion behavior was investigated using potentiodynamic polarization measurement using 5 wt% NaCl. The results revealed that the Icorr increased from 2.44 µA/cm2 to 8.60 µA/cm2 as the fly ash concentration increased from 5 wt% to 10 wt%. This increase of Icorr indicates an increase of the corrosion rate. The corrosion mainly occurs at the interface between fly ash particles and Al 6061 matrix.