  • Open Access

    High-Temperature Creep Resistance of FeAlOY ODS Ferritic Alloy

    by Petr Dymáček, Milan Jarý, Denisa Bártková, Natália Luptáková, Štepán Gamanov, Petr Bořil, Vjaceslav Georgiev, Jiří Svoboda

    A significant effort in optimizing the chemical composition and powder metallurgical processing led to preparing new-generation ferritic coarse-grained ODS alloys with a high nano-oxide content. The optimization was aimed at high-temperature creep and oxidation resistance at temperatures in the range of 1100–1300 °C. An FeAlOY alloy, with the chemical composition Fe–10Al–4Cr–4Y2O3 (wt. %), seems as the most promising one. The consolidation of the alloy is preferably conducted by hot rolling in several steps, followed by static recrystallization for 1 h at 1200 °C, which provides a stable coarse-grain microstructure with homogeneous dispersion of nano-oxides. This represents the most cost-effective way of production. Another method of consolidation tested was hot rotary swaging, which also gave promising results. The compression creep testing of the alloy at 1100, 1200, and 1300 °C shows excellent creep performance, which is confirmed by the tensile creep tests at 1100 °C as well. The potential in such a temperature range is the target for possible applications of the FeAlOY for the pull rods of high-temperature testing machines, gas turbine blades, or furnace fan vanes. The key effort now focuses on expanding the production from laboratory samples to larger industrial pieces.


  • Open Access

    The Optimization of Mechanical Alloying Conditions of Powder for the Preparation of a Fe-10Al-4Cr-4Y2O3 ODS Nanocomposite

    by Jiří Svoboda, Štepán Gamanov, Denisa Bártková, Natália Luptáková, Petr Bořil, Milan Jarý, Bohuslav Mašek, Jakub Holzer, Petr Dymáček

    Mechanical alloying (MA) of powders represents the first processing step in the production of oxide dispersion-strengthened (ODS) alloys. MA is a time and energy-consuming process also in the production of Fe-10Al-4Cr-4Y2O3 creep and oxidation-resistant ODS nanocomposite, denoted as the FeAlOY, and it deserves to be optimized. MA is performed at two different temperatures at different times. The powder after MA, as well as the microstructure and high-temperature strength of the final FeAlOY, are characterized and the optimal MA conditions are evaluated. The obtained results show that the size distribution of the powder particles, as well as the dissolution and homogenization of the Y2O3, becomes saturated quite soon, while the homogenization of the metallic components, such as Al and Cr, takes significantly more time. The high-temperature tensile tests and grain microstructures of the secondary recrystallized FeAlOY, however, indicate that the homogenization of the metallic components during MA does not influence the quality of the FeAlOY, as the matrix of the FeAlOY is sufficiently homogenized during recrystallization. Thus, the conditions of MA correspond to sufficient dissolution and homogenization of Y2O3 and can be considered the optimal ones.


  • Open Access

    Substantial Improvement of High Temperature Strength of New-Generation Nano-Oxide-Strengthened Alloys by Addition of Metallic Yttrium

    by Jiří Svoboda, Petr Bořil, Jakub Holzer, Natália Luptáková, Milan Jarý, Bohuslav Mašek, Petr Dymáček

    Oxide-dispersion-strengthened (ODS) Fe-Al-Y2O3-based alloys (denoted as FeAlOY) containing 5 vol. % of nano-oxides have a potential to become top oxidation and creep-resistant alloys for applications at temperatures of 1100–1300 °C. Oxide dispersoids cause nearly perfect strengthening of grains; thus, grain boundaries with limited cohesive strength become the weak link in FeAlOY in this temperature range. One of the possibilities for significantly improving the strength of FeAlOY is alloying with appropriate elements and increasing the cohesive strength of grain boundaries. Nearly 20 metallic elements have been tested with the aim to increase cohesive strength in the frame of preliminary tests. A positive influence is revealed for Al, Cr, and Y, whereby the influence of Y is enormous (addition of 1% of metallic Y increases strength by a factor of 2), as it is presented in this paper.


  • Open Access

    Influence of Hot Consolidation Conditions and Cr-Alloying on Microstructure and Creep in New-Generation ODS Alloy at 1100 °C

    by Jiří Svoboda, Natália Luptáková, Milan Jarý, Petr Dymáček

    The coarse-grained new-generation Fe-Al-Y2O3-based oxide dispersion strengthened (ODS) alloys contain 5 vol.% homogeneously dispersed yttria nano-precipitates and exhibit very promising creep and oxidation resistance above 1000 °C. The alloy is prepared by the consolidation of mechanically alloyed powders via hot rolling followed by secondary recrystallization. The paper presents a systematic study of influence of rolling temperature on final microstructure and creep at 1100 °C for two grades (Fe-10Al-4Y2O3 and Fe-9Al-14Cr-4Y2O3 in wt%) of new-generation ODS alloys. The hot rolling temperatures exhibit a rather wide processing window and the influence of Cr-alloying on creep properties is evaluated as only slightly positive.


  • Open Access

    Tensile and Creep Testing of Sanicro 25 Using Miniature Specimens

    by Petr Dymáček, Milan Jarý, Ferdinand Dobeš, Luboš Kloc

    Tensile and creep properties of new austenitic steel Sanicro 25 at room temperature and operating temperature 700 °C were investigated by testing on miniature specimens. The results were correlated with testing on conventional specimens. Very good agreement of results was obtained, namely in yield and ultimate strength, as well as short-term creep properties. Although the creep rupture time was found to be systematically shorter and creep ductility lower in the miniature test, the minimum creep rates were comparable. The analysis of the fracture surfaces revealed similar ductile fracture morphology for both specimen geometries. One exception was found in a small area near the miniature specimen edge that was cut by electro discharge machining, where an influence of the steel fracture behavior at elevated temperature was identified.