Shuang Jun Nie
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Shuang Jun Nie has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Bingyang Gao
Key Laboratory of Solidification Control and Digital Preparation Technology (Liaoning Province), School of Materials Science and Engineering, Dalian University of Technology, Dalian 116024, China
1 shared publication - Enyu Guo
Key Laboratory of Solidification Control and Digital Preparation Technology (Liaoning Province), School of Materials Science and Engineering Dalian University of Technology Dalian China
1 shared publication - Guang Hui Yue
Center for Mobility and Rehabilitation Engineering Research, Kessler Foundation, West Orange, USA
1 shared publication Hao Geng
Xiamen University
1 shared publicationJun Bao Wang
Xiamen University
1 shared publicationLai Sen Wang
Xiamen University
1 shared publication
Latest Publications
- Open Access
The Influence of Holding Time on the Microstructure Evolution of Mg–10Zn–6.8Gd–4Y Alloy during Semi-Solid Isothermal Heat Treatment
A semi-solid microstructure of Mg–10Zn–6.8Gd–4Y alloys is acquired via an isothermal heat treatment process, and the effects of the holding time on the microstructure evolution of Mg–10Zn–6.8Gd–4Y alloys are investigated. The results show that the microstructure of the cast alloy is composed of primary α-Mg dendritic grains with a eutectic structure (W-phase and eutectic Mg) distributed at the grain boundaries. The primary α-Mg dendritic grains grow in size with increasing holding time, and they tend to grow into more globular structures in the initial stage; they then become a bit more dendritic, as small branches grow from the grain boundaries after holding the sample at 580 °C for 10 min. Meanwhile, the interdiffusion of magnesium atoms within the eutectic region, and between the primary α-Mg and eutectic structure, leads to the formation of fine and relatively globular eutectic Mg grains in the eutectic structure after holding for 10 min. The eutectic Mg grains begin to grow, coarsen, coalesce, or be swallowed by the surrounding primary grains, causing fluctuations of the general grain size. Over the whole isothermal heat treatment process, two mechanisms—coalescence and Ostwald ripening—dominate the grain coarsening.
Open AccessThe Influence of Holding Time on the Microstructure Evolution of Mg–10Zn–6.8Gd–4Y Alloy during Semi-Solid Isothermal Heat Treatment
A semi-solid microstructure of Mg–10Zn–6.8Gd–4Y alloys is acquired via an isothermal heat treatment process, and the effects of the holding time on the microstructure evolution of Mg–10Zn–6.8Gd–4Y alloys are investigated. The results show that the microstructure of the cast alloy is composed of primary α-Mg dendritic grains with a eutectic structure (W-phase and eutectic Mg) distributed at the grain boundaries. The primary α-Mg dendritic grains grow in size with increasing holding time, and they tend to grow into more globular structures in the initial stage; they then become a bit more dendritic, as small branches grow from the grain boundaries after holding the sample at 580 °C for 10 min. Meanwhile, the interdiffusion of magnesium atoms within the eutectic region, and between the primary α-Mg and eutectic structure, leads to the formation of fine and relatively globular eutectic Mg grains in the eutectic structure after holding for 10 min. The eutectic Mg grains begin to grow, coarsen, coalesce, or be swallowed by the surrounding primary grains, causing fluctuations of the general grain size. Over the whole isothermal heat treatment process, two mechanisms—coalescence and Ostwald ripening—dominate the grain coarsening.
- 1 May 2013
- Published by Trans Tech Publications, Ltd. in Advanced Materials Research
- Vol. 690-693, 1702-1706
The Structure and Magnetic Properties of NiZn-Ferrite Films Deposited by Magnetron Sputtering at Room Temperature
NiZn-ferrite thin films were deposited onto silicon and glass substrates by radio frequency magnetron sputtering at room temperature. The effects of the relative oxygen flow ratio on the structure and magnetic properties of the thin films were investigated. The study results reveal that the films deposited under higher relative oxygen flow ratio show a better crystallinity. Static magnetic measurement results indicated that the saturation magnetization of the films was greatly affected by the crystallinity, grain dimension, and cation distribution in the NiZn-ferrite films. The NiZn-ferrite thin films with a maximum saturation magnetization of 151 emucm-3, which is about 40% of the bulk NiZn ferrite, was obtained under relative oxygen flow ratio of 60%.
- 1 May 2013
- Published by Trans Tech Publications, Ltd. in Advanced Materials Research
- Vol. 690-693, 1702-1706
The Structure and Magnetic Properties of NiZn-Ferrite Films Deposited by Magnetron Sputtering at Room Temperature
NiZn-ferrite thin films were deposited onto silicon and glass substrates by radio frequency magnetron sputtering at room temperature. The effects of the relative oxygen flow ratio on the structure and magnetic properties of the thin films were investigated. The study results reveal that the films deposited under higher relative oxygen flow ratio show a better crystallinity. Static magnetic measurement results indicated that the saturation magnetization of the films was greatly affected by the crystallinity, grain dimension, and cation distribution in the NiZn-ferrite films. The NiZn-ferrite thin films with a maximum saturation magnetization of 151 emucm-3, which is about 40% of the bulk NiZn ferrite, was obtained under relative oxygen flow ratio of 60%.