Igor V. Blinkov
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Igor V. Blinkov has a total of 78 co-authors. Here are the top co-authors by number of shared publications:
A. O. Volkhonskii
National University of Science and Technology MISiS
15 shared publicationsD. S. Belov
National University of Science and Technology MISiS, Moscow, Russia
13 shared publicationsV. S. Sergevnin
Moscow Institute of Steel and Alloys (National University of Science and Technology), Moscow, Russia
9 shared publicationsA. V. Chernogor
National University of Science and Technology MISiS, Moscow, Russia
8 shared publicationsV. N. Anikin
National Research Technological University (MISiS)
6 shared publications- D. S. Belov
National University of Science and Technology “MISIS
5 shared publications
Latest Publications
- Open Access
Structure and Properties of Multicomponent Arc-PVD Ti–Cr–Mo–Ni–N Coatings Deposited on HG20, HS123 and HV420 Carbide Alloys and C80W1 Tool Steel
Although the arc-PVD Ti–Cr–Mo–Ni–N coatings deposited on HG20, HS123 and HV420 carbide alloys and C80W1 tool steel have approximately similar elemental and phase compositions, they differ in morphology, macrostructure, and macrostress level. The coating deposited on steel exhibits macrolayering, a wider coating–substrate transition zone and tensile structural macrostresses. In contrast, coatings deposited on carbide alloys develop compressive structural macrostresses. This behavior can be explained by the overheating during deposition caused by ion bombardment. Overheating is more pronounced for a coating on steel because the thermal diffusivity of steel is lower than that of hard alloys. The Ti–Cr–Mo–Ni–N coating on C80W1 steel exhibited a lower hardness (approximately 20.3 GPa) than the coatings on the carbide alloys (21.7–25.1 GPa). It also showed lower resistance to cohesive failure, with Lc3 ≈ 30 N, compared with ≈94 N for the coatings on the carbide alloys. Here, Lc3 denotes the critical load for cohesive cracking of the coating induced by plastic extrusion of the substrate material. The coating on steel also exhibited a higher specific wear rate at 20 °C and 500 °C. Its K20 and K500 values were 49.80 and 74.20, respectively. The corresponding values were 4.19 and 11.99 for HG20, 2.91 and 12.35 for HS123, and 6.33 and 14.71 for HV420, respectively, expressed in units of 10−6 mm3·N−1·m−1.
Open AccessStructure and Properties of Multicomponent Arc-PVD Ti–Cr–Mo–Ni–N Coatings Deposited on HG20, HS123 and HV420 Carbide Alloys and C80W1 Tool Steel
Although the arc-PVD Ti–Cr–Mo–Ni–N coatings deposited on HG20, HS123 and HV420 carbide alloys and C80W1 tool steel have approximately similar elemental and phase compositions, they differ in morphology, macrostructure, and macrostress level. The coating deposited on steel exhibits macrolayering, a wider coating–substrate transition zone and tensile structural macrostresses. In contrast, coatings deposited on carbide alloys develop compressive structural macrostresses. This behavior can be explained by the overheating during deposition caused by ion bombardment. Overheating is more pronounced for a coating on steel because the thermal diffusivity of steel is lower than that of hard alloys. The Ti–Cr–Mo–Ni–N coating on C80W1 steel exhibited a lower hardness (approximately 20.3 GPa) than the coatings on the carbide alloys (21.7–25.1 GPa). It also showed lower resistance to cohesive failure, with Lc3 ≈ 30 N, compared with ≈94 N for the coatings on the carbide alloys. Here, Lc3 denotes the critical load for cohesive cracking of the coating induced by plastic extrusion of the substrate material. The coating on steel also exhibited a higher specific wear rate at 20 °C and 500 °C. Its K20 and K500 values were 49.80 and 74.20, respectively. The corresponding values were 4.19 and 11.99 for HG20, 2.91 and 12.35 for HS123, and 6.33 and 14.71 for HV420, respectively, expressed in units of 10−6 mm3·N−1·m−1.
- Open Access
- 10 October 2026
- Published by MDPI AG in Preprints.org
Structure and Properties of Multicomponent Arc-PVD Ti–Cr–Mo–Ni–N Coatings on Carbide Alloys HG20, HS123, HV420 and Tool Steel C80W1
The arc-PVD Ti–Cr–Mo–Ni–N coatings on HG20, HS123, HV420 carbide alloys and C80W1 tool steel, while having approximately the same elemental and phase compositions, differ in morphology, macrostructure, and level of macrostresses. When deposited on steel, the coating exhibits macrolayering, a more extended coating–substrate transition zone, and develops tensile macrostresses, in contrast to the coatings on carbide alloys, which develop compressive macrostresses. The behaviour can be explained by the overheating of the coating during deposition, which results from ion bombardment and is more pronounced on steel due to its poorer thermal diffusivity relative to carbide alloys. The CLTE difference between steel and the coating is significantly larger than that between the carbides and the coating, further contributing to the effect. It was found that, considering these features, the Ti–Cr–Mo–Ni–N coating on steel exhibits lower hardness (~20.3GPa), lower adhesion strength to the substrate (Lc3≈30N, the indenter load at scratch testing corresponding to the onset of coating wear), and a higher wear intensity at room temperature and 500°C (49.80 and 74.20·10−6 mm3·N−1·m−1, respectively), as compared with the hardness values of 25.1–21.7GPa, Lc3≈100N, and wear intensity (corresponding to the absence of a visible wear crater) for the Ti–Cr–Mo–Ni–N coatings on the aforementioned carbide alloys.
- 10 October 2026
- Published by MDPI AG in Preprints.org
Open AccessStructure and Properties of Multicomponent Arc-PVD Ti–Cr–Mo–Ni–N Coatings on Carbide Alloys HG20, HS123, HV420 and Tool Steel C80W1
The arc-PVD Ti–Cr–Mo–Ni–N coatings on HG20, HS123, HV420 carbide alloys and C80W1 tool steel, while having approximately the same elemental and phase compositions, differ in morphology, macrostructure, and level of macrostresses. When deposited on steel, the coating exhibits macrolayering, a more extended coating–substrate transition zone, and develops tensile macrostresses, in contrast to the coatings on carbide alloys, which develop compressive macrostresses. The behaviour can be explained by the overheating of the coating during deposition, which results from ion bombardment and is more pronounced on steel due to its poorer thermal diffusivity relative to carbide alloys. The CLTE difference between steel and the coating is significantly larger than that between the carbides and the coating, further contributing to the effect. It was found that, considering these features, the Ti–Cr–Mo–Ni–N coating on steel exhibits lower hardness (~20.3GPa), lower adhesion strength to the substrate (Lc3≈30N, the indenter load at scratch testing corresponding to the onset of coating wear), and a higher wear intensity at room temperature and 500°C (49.80 and 74.20·10−6 mm3·N−1·m−1, respectively), as compared with the hardness values of 25.1–21.7GPa, Lc3≈100N, and wear intensity (corresponding to the absence of a visible wear crater) for the Ti–Cr–Mo–Ni–N coatings on the aforementioned carbide alloys.
- 3 June 2024
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 15 (3) , 752-759
Durability of Cutting Tools with Deposited Ceramic-Metal Coatings (Ti, Al)N–Cu and (Ti, Al)N–Ni during Turning and Milling of Steels
—Comparative durability tests of carbide cutting tools with (Ti, Al)N–Cu and (Ti, Al)N–Ni coatings applied to its working surfaces were carried out under conditions of continuous and interrupted cutting of steels 09G2S and EP302-Sh, respectively. Under milling conditions of EP302-Sh steel, using VK6NST inserts with (Ti, Al)N–Cu and (Ti,Al)N–Ni coatings, the tool life increases by 3.1 and 1.7 times, respectively. When turning the 09G2S steel using VK6NST inserts coated with (Ti, Al)N–Cu and (Ti, Al)N–Ni, the tool life increases by 7.6 and 10.8 times, respectively, and the cutting forces Fz, Fx, and Fy are reduced by ~20%. It is shown that this effect is determined by the presence of a nanostructure in the formed coatings and the presence of a highly consistent ceramic component and ductile metal, which determine their hardness (more than 35 GPa) and fracture toughness (relative work of plastic deformation during indentation over ~60%) and increased tribological characteristics (friction coefficient of ~0.5 compared to uncoated carbide of ~0.7).
- 3 June 2024
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 15 (3) , 752-759
Durability of Cutting Tools with Deposited Ceramic-Metal Coatings (Ti, Al)N–Cu and (Ti, Al)N–Ni during Turning and Milling of Steels
—Comparative durability tests of carbide cutting tools with (Ti, Al)N–Cu and (Ti, Al)N–Ni coatings applied to its working surfaces were carried out under conditions of continuous and interrupted cutting of steels 09G2S and EP302-Sh, respectively. Under milling conditions of EP302-Sh steel, using VK6NST inserts with (Ti, Al)N–Cu and (Ti,Al)N–Ni coatings, the tool life increases by 3.1 and 1.7 times, respectively. When turning the 09G2S steel using VK6NST inserts coated with (Ti, Al)N–Cu and (Ti, Al)N–Ni, the tool life increases by 7.6 and 10.8 times, respectively, and the cutting forces Fz, Fx, and Fy are reduced by ~20%. It is shown that this effect is determined by the presence of a nanostructure in the formed coatings and the presence of a highly consistent ceramic component and ductile metal, which determine their hardness (more than 35 GPa) and fracture toughness (relative work of plastic deformation during indentation over ~60%) and increased tribological characteristics (friction coefficient of ~0.5 compared to uncoated carbide of ~0.7).
- 3 June 2024
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 15 (3) , 728-736
Tribological Characteristics of Ti–Al– N, Ti–Al– Ni–N, Ti–Cr–Ni–N, and Ti–Cr–Ni–Mo–N Strengthening Coatings on Steel 20Kh13 in a Friction Pair with Carbon Fiber and Their Corrosion Resistance
—The possibility of using Ti–Al–N, Ti–Al–Ni–N, Ti–Cr–Ni–N, and Ti–Cr–Ni–Mo–N coatings deposited by ion-plasma vacuum-arc deposition as protective on products made of steel 20Kh13, working in a friction pair with carbon fiber plastic of the UGET grade in contact with seawater, has been investigated. An improvement in the resistance properties of a steel surface is shown when using coatings of the Ti–Al–Ni–N, Ti–Cr–Ni—N, and Ti–Cr–Ni–Mo–N systems. And the products without or with Ti–Al–N coating showed high friction wear rates (109.21 × 10–5 and 19.24 × 10–5 mm3/(N m), respectively), as well as active oxidation during electrochemical tests under conditions of interaction with a medium simulating seawater (3% NaCl solution). Specimens with Ti–Al–Ni–N, Ti–Cr–Ni–N, and Ti–Cr–Ni–Mo–N coatings did not demonstrate significant wear during friction when paired with carbon fiber. Electrochemical tests of the coatings showed that they were self-passivated and there was no pitting on the surface of the coated specimens. On the basis of the analysis of the data obtained, a conclusion was made about the high efficiency of the studied coatings as protective for work in contact with seawater.
- 3 June 2024
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 15 (3) , 728-736
Tribological Characteristics of Ti–Al– N, Ti–Al– Ni–N, Ti–Cr–Ni–N, and Ti–Cr–Ni–Mo–N Strengthening Coatings on Steel 20Kh13 in a Friction Pair with Carbon Fiber and Their Corrosion Resistance
—The possibility of using Ti–Al–N, Ti–Al–Ni–N, Ti–Cr–Ni–N, and Ti–Cr–Ni–Mo–N coatings deposited by ion-plasma vacuum-arc deposition as protective on products made of steel 20Kh13, working in a friction pair with carbon fiber plastic of the UGET grade in contact with seawater, has been investigated. An improvement in the resistance properties of a steel surface is shown when using coatings of the Ti–Al–Ni–N, Ti–Cr–Ni—N, and Ti–Cr–Ni–Mo–N systems. And the products without or with Ti–Al–N coating showed high friction wear rates (109.21 × 10–5 and 19.24 × 10–5 mm3/(N m), respectively), as well as active oxidation during electrochemical tests under conditions of interaction with a medium simulating seawater (3% NaCl solution). Specimens with Ti–Al–Ni–N, Ti–Cr–Ni–N, and Ti–Cr–Ni–Mo–N coatings did not demonstrate significant wear during friction when paired with carbon fiber. Electrochemical tests of the coatings showed that they were self-passivated and there was no pitting on the surface of the coated specimens. On the basis of the analysis of the data obtained, a conclusion was made about the high efficiency of the studied coatings as protective for work in contact with seawater.
- 1 October 2022
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 58 (10) , 1017-1027
Structure, Mechanical Properties, Thermal Stability, and Chemical Stability of Metastable Ti1 – xAlxN (x = 0.03–0.05) Solid Solutions Prepared as Arc PVD Coatings on WC–Co Alloys
We report a comparative study of the chemical and thermal stability and mechanical properties of arc PVD TiN and Ti0.97Al0.03N coatings. Heating the coatings in vacuum to 600 and 700°C has been shown to cause an increase in crystallite size and a decrease in biaxial macrostress, lattice parameter, and lattice strain. These effects are due to thermally activated structure restoration processes associated with annihilation of defects generated during the growth of the coatings. The stress relaxation rate in the Ti0.97Al0.03N coating is higher because it contains a higher defect density. At 700°C, the Ti0.97Al0.03N solid solution undergoes spinodal decomposition into TiN and AlN (FCC). Unlike those of the TiN coating, the hardness and the parameters H3/E2 and H/E of the Ti0.97Al0.03N coating remain essentially unchanged as the annealing temperature is raised to 700°C, which is due to dispersion hardening as a result of the spinodal decomposition. The coatings exhibit similar behavior in acidic and alkaline media, but Ti0.97Al0.03N has a somewhat higher oxidation resistance in air at 550°C.
- 1 October 2022
- Published by Pleiades Publishing Ltd in Inorganic Materials
- Vol. 58 (10) , 1017-1027
Structure, Mechanical Properties, Thermal Stability, and Chemical Stability of Metastable Ti1 – xAlxN (x = 0.03–0.05) Solid Solutions Prepared as Arc PVD Coatings on WC–Co Alloys
We report a comparative study of the chemical and thermal stability and mechanical properties of arc PVD TiN and Ti0.97Al0.03N coatings. Heating the coatings in vacuum to 600 and 700°C has been shown to cause an increase in crystallite size and a decrease in biaxial macrostress, lattice parameter, and lattice strain. These effects are due to thermally activated structure restoration processes associated with annihilation of defects generated during the growth of the coatings. The stress relaxation rate in the Ti0.97Al0.03N coating is higher because it contains a higher defect density. At 700°C, the Ti0.97Al0.03N solid solution undergoes spinodal decomposition into TiN and AlN (FCC). Unlike those of the TiN coating, the hardness and the parameters H3/E2 and H/E of the Ti0.97Al0.03N coating remain essentially unchanged as the annealing temperature is raised to 700°C, which is due to dispersion hardening as a result of the spinodal decomposition. The coatings exhibit similar behavior in acidic and alkaline media, but Ti0.97Al0.03N has a somewhat higher oxidation resistance in air at 550°C.
- Open Access
- 23 September 2021
- Published by National University of Science and Technology MISiS in Powder Metallurgy аnd Functional Coatings
- No. 2,p. 49-59
Production of α-Fe 2O 3 powder material with multilevel gradient porosity
Исследованы способы получения материала с градиентной разноуровневой пористостью путем спекания послойно распределенных нано- и субмикропорошков α-Fe2O3. Нанопорошки со средним размером частиц 12 нм были получены методом соосаждения, а субмикропорошки, представляющие собой полые сферы, – спрей-пиролизом. Консолидация порошков осуществлялась спеканием в муфельной печи, горячим прессованием и искровым плазменным спеканием (SPS) при различных температурах, нагрузках и времени выдержки. Показано, что методы спекания в муфельной печи и горячим прессом не позволяют получить компактный образец достаточной прочности по причине различной активности нано- и субмикропорошков. Методом искрового плазменного спекания были получены порошковые материалы при температурах выдержки 700, 750, 800 и 900 °С в течение 3 мин. Установлено, что серия образцов, полученных методом SPS при температуре 750 °С, обладает достаточной прочностью и открытой пористостью 20 % при общей пористости 37 %. Увеличение температуры при использовании метода SPS приводит к увеличению размера частиц в объеме нанопорошков до микронного размера и частичному разрушению полых субмикросфер. При исследовании фазового состава полученных образцов выявлено, что он идентичен фазовому составу исходных порошков. Однако для серий образцов, изготовленных методами горячего прессования и SPS, в объеме нанопорошков наблюдается направленный рост кристаллов в направлении наибольшей электро- и теплопроводности [001] по оси пуансонов. Это связано с температурным градиентом между объемом порошка и пуансонами и наименьшим значением поверхностной энергии плоскости (110), включающей в себя направление [001].
- 23 September 2021
- Published by National University of Science and Technology MISiS in Powder Metallurgy аnd Functional Coatings
- No. 2,p. 49-59
Open AccessProduction of α-Fe 2O 3 powder material with multilevel gradient porosity
Исследованы способы получения материала с градиентной разноуровневой пористостью путем спекания послойно распределенных нано- и субмикропорошков α-Fe2O3. Нанопорошки со средним размером частиц 12 нм были получены методом соосаждения, а субмикропорошки, представляющие собой полые сферы, – спрей-пиролизом. Консолидация порошков осуществлялась спеканием в муфельной печи, горячим прессованием и искровым плазменным спеканием (SPS) при различных температурах, нагрузках и времени выдержки. Показано, что методы спекания в муфельной печи и горячим прессом не позволяют получить компактный образец достаточной прочности по причине различной активности нано- и субмикропорошков. Методом искрового плазменного спекания были получены порошковые материалы при температурах выдержки 700, 750, 800 и 900 °С в течение 3 мин. Установлено, что серия образцов, полученных методом SPS при температуре 750 °С, обладает достаточной прочностью и открытой пористостью 20 % при общей пористости 37 %. Увеличение температуры при использовании метода SPS приводит к увеличению размера частиц в объеме нанопорошков до микронного размера и частичному разрушению полых субмикросфер. При исследовании фазового состава полученных образцов выявлено, что он идентичен фазовому составу исходных порошков. Однако для серий образцов, изготовленных методами горячего прессования и SPS, в объеме нанопорошков наблюдается направленный рост кристаллов в направлении наибольшей электро- и теплопроводности [001] по оси пуансонов. Это связано с температурным градиентом между объемом порошка и пуансонами и наименьшим значением поверхностной энергии плоскости (110), включающей в себя направление [001].
- 1 September 2021
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 62 (5) , 602-610
Production of Powdered α-Fe2O3 with Multilevel Gradient Porosity
This article discusses methods for producing a material with gradient multilevel porosity by sintering layer-by-layer distributed α-Fe2O3 nanopowders
- 1 September 2021
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 62 (5) , 602-610
Production of Powdered α-Fe2O3 with Multilevel Gradient Porosity
This article discusses methods for producing a material with gradient multilevel porosity by sintering layer-by-layer distributed α-Fe2O3 nanopowders
- Open Access
- 1 February 2021
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1799 (1) , 012002
Cathodic arc-PVD Zr-B-Si-C-Ti-(N) coatings
Arc-PVD coatings Zr-B-Si-C-Ti-N and Zr-B-Si-C-Ti were obtained using combined evaporated ZrB2-SiC-Ti cathodes in a residual atmosphere of N2 and Ar. Their structure and composition were investigated. The Zr-B-Si-C-Ti-N coating has a predominantly amorphous structure, formed mainly on the basis of nitride, carbide, boride phases and complex compounds Zr, Si, Ti. The Zr-B-Si-C-Ti coating is characterized by an amorphous-nanocrystalline structure. The amorphous component of this coating is formed mainly by phases based on Zr and Si. The nanocrystalline structure is formed by a complex carbide (Zr, Ti) C.
- 1 February 2021
- Published by IOP Publishing in Journal of Physics: Conference Series
- Vol. 1799 (1) , 012002
Open AccessCathodic arc-PVD Zr-B-Si-C-Ti-(N) coatings
Arc-PVD coatings Zr-B-Si-C-Ti-N and Zr-B-Si-C-Ti were obtained using combined evaporated ZrB2-SiC-Ti cathodes in a residual atmosphere of N2 and Ar. Their structure and composition were investigated. The Zr-B-Si-C-Ti-N coating has a predominantly amorphous structure, formed mainly on the basis of nitride, carbide, boride phases and complex compounds Zr, Si, Ti. The Zr-B-Si-C-Ti coating is characterized by an amorphous-nanocrystalline structure. The amorphous component of this coating is formed mainly by phases based on Zr and Si. The nanocrystalline structure is formed by a complex carbide (Zr, Ti) C.
- Open Access
The Effect of the Metal Phase on the Compressive and Tensile Stresses Reduction in the Superhard Nitride Coatings
The influence of the compressive and tensile stresses forming in the nanostructured Ti–Al–N coatings during deposition on their physical-mechanical properties was studied. The modifying influence of metal components (Ni and Cu) introduction into Ti–Al–N coatings, which do not interact with nitrogen and have limited solubility with the nitride phase, was also under research. Coatings were deposited on WC–(6 wt.%)Co carbide cutting inserts with an arc-PVD method using a cathodic vacuum arc evaporation apparatus. The introduction of Ni and Cu to the composition leads to the reduction of nitride phases grain size in both investigated coatings from 120 to 10–12 nm for Ti–Al–Cu–N and to 15–18 nm for Ti–Al–Ni–N. Thus, the hardness increases from 29 to 43 and 51 GPa for the mentioned above coatings, respectively. Meanwhile, Ti–Al–Cu–N and Ti–Al–Ni–N coatings are characterized by tensile stresses about 0.12–0.32 MPa against the much higher value of compressive stresses in Ti–Al–N coatings (4.29–5.31 GPa). The modification of Ti–Al–N coatings also leads to the changing of their destruction mechanism during the scratch-test. The critical loads characterizing the emergence of the first cracks in the coatings and complete abrasion of the coating (Lc1 and Lc3) were determined. They had the value of 20; 22 N (Lc1) and 64; 57 N (Lc3) for Ti–Al–Ni–N; Ti–Al–Cu–N coatings, respectively. The Lc1 parameter for Ti–Al–N coatings was much lower and was equal to 11 N. Along with those, Ti–Al–N coatings destructed according to the adhesion mechanism when the critical load was 35 N. In addition, the decreasing level of compressive stresses in Ti–Al–Cu–N and Ti–Al–Ni–N coatings as compared to that in the Ti–Al–N coating, their crack resistance during multi-cycle shock-dynamic impact test was significantly higher. The results can indicate that high hardness and crack resistance of the coatings is to a greater extent determined by coatings nanostructuring, not the stresses value. In addition, it confirms the possibility to obtain coatings with low stresses value while maintaining their superhardness.
Open AccessThe Effect of the Metal Phase on the Compressive and Tensile Stresses Reduction in the Superhard Nitride Coatings
The influence of the compressive and tensile stresses forming in the nanostructured Ti–Al–N coatings during deposition on their physical-mechanical properties was studied. The modifying influence of metal components (Ni and Cu) introduction into Ti–Al–N coatings, which do not interact with nitrogen and have limited solubility with the nitride phase, was also under research. Coatings were deposited on WC–(6 wt.%)Co carbide cutting inserts with an arc-PVD method using a cathodic vacuum arc evaporation apparatus. The introduction of Ni and Cu to the composition leads to the reduction of nitride phases grain size in both investigated coatings from 120 to 10–12 nm for Ti–Al–Cu–N and to 15–18 nm for Ti–Al–Ni–N. Thus, the hardness increases from 29 to 43 and 51 GPa for the mentioned above coatings, respectively. Meanwhile, Ti–Al–Cu–N and Ti–Al–Ni–N coatings are characterized by tensile stresses about 0.12–0.32 MPa against the much higher value of compressive stresses in Ti–Al–N coatings (4.29–5.31 GPa). The modification of Ti–Al–N coatings also leads to the changing of their destruction mechanism during the scratch-test. The critical loads characterizing the emergence of the first cracks in the coatings and complete abrasion of the coating (Lc1 and Lc3) were determined. They had the value of 20; 22 N (Lc1) and 64; 57 N (Lc3) for Ti–Al–Ni–N; Ti–Al–Cu–N coatings, respectively. The Lc1 parameter for Ti–Al–N coatings was much lower and was equal to 11 N. Along with those, Ti–Al–N coatings destructed according to the adhesion mechanism when the critical load was 35 N. In addition, the decreasing level of compressive stresses in Ti–Al–Cu–N and Ti–Al–Ni–N coatings as compared to that in the Ti–Al–N coating, their crack resistance during multi-cycle shock-dynamic impact test was significantly higher. The results can indicate that high hardness and crack resistance of the coatings is to a greater extent determined by coatings nanostructuring, not the stresses value. In addition, it confirms the possibility to obtain coatings with low stresses value while maintaining their superhardness.
- 1 July 2020
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 61 (4) , 466-474
Nickel Effect on the Structure and Properties of Adaptive Wear-Resistant Arc-PVD Ti–Al–Mo–N Coatings
Comparative investigations of the structural characteristics and functional properties of Ti–Al–Mo–N and Ti–Al–Mo–Ni
- 1 July 2020
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 61 (4) , 466-474
Nickel Effect on the Structure and Properties of Adaptive Wear-Resistant Arc-PVD Ti–Al–Mo–N Coatings
Comparative investigations of the structural characteristics and functional properties of Ti–Al–Mo–N and Ti–Al–Mo–Ni