Peng Chai
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Peng Chai has a total of 7 co-authors. Here are the top co-authors by number of shared publications:
- Shujuan Li
School of Mechanical and Precision Instrument Engineering, Xi’an University of Technology, Xi’an 710048, China
4 shared publications - Yan Li
Xi’an University of Technology
3 shared publications - Xincheng Yin
School of Mechanical and Electrical Engineering, Lanzhou University of Technology, Lanzhou 730050, People’s Republic of China
2 shared publications - Kehao Lan
School of Mechanical and Precision Instrument Engineering, Xi’an University of Technology, Xi’an 710048, China
1 shared publication - Lie Liang
School of Mechanical and Precision Instrument Engineering, Xi’an University of Technology, Xi’an 710048, China
1 shared publication - Lie Liang
School of Mechanical and Precision Instrument Engineering, Xi’an University of Technology, Xi’an 710048, China
1 shared publication
Latest Publications
- Open Access
Molecular Dynamics Simulation of Single-Crystal 4H-SiC Nano Scratching with Different Scratching Directions of the Tool
4H-SiC (silicon carbide) is widely used in semiconductor devices due to its superior characteristics. However, processing techniques such as cutting, grinding, and polishing generally have problems such as low processing efficiency, high cost, difficulties guaranteeing processing quality, and serious material waste. The in-depth research on the mechanical behavior, material removal, and damage mechanism of SiC single crystals at the micro/nano scale is the foundation for solving these problems. This paper establishes a molecular dynamics simulation model for 4H-SiC single-crystal nano scratches, using three different directions of a Berkovich indenter to scratch the surface of the workpiece, studying the surface morphology, scratching force, and material removal during the scratching process. The results indicate that scratching directions of the tool varies, and the surface morphology also varies. After the scratching depth exceeds 1.6 nm, complete dislocations with a Burges vector of 1/3 appear on the crystal subsurface, leading to the plastic removal of the material. During the process of material removal, a smaller tool rake angle removes a larger amount of material chips. By analyzing the damage layer of the workpiece, the difference in the damage layer is smaller when the scratching direction is different, but the damage layer generated by the smaller rake angle of the scratching tool is thinner. It shows that the scratching force and workpiece temperature are relatively small when the rake angle of the scratching tool is small. Therefore, when scratching 4H-SiC single crystals, choosing a tool with a smaller rake angle is more beneficial for the process.
Open AccessMolecular Dynamics Simulation of Single-Crystal 4H-SiC Nano Scratching with Different Scratching Directions of the Tool
4H-SiC (silicon carbide) is widely used in semiconductor devices due to its superior characteristics. However, processing techniques such as cutting, grinding, and polishing generally have problems such as low processing efficiency, high cost, difficulties guaranteeing processing quality, and serious material waste. The in-depth research on the mechanical behavior, material removal, and damage mechanism of SiC single crystals at the micro/nano scale is the foundation for solving these problems. This paper establishes a molecular dynamics simulation model for 4H-SiC single-crystal nano scratches, using three different directions of a Berkovich indenter to scratch the surface of the workpiece, studying the surface morphology, scratching force, and material removal during the scratching process. The results indicate that scratching directions of the tool varies, and the surface morphology also varies. After the scratching depth exceeds 1.6 nm, complete dislocations with a Burges vector of 1/3 appear on the crystal subsurface, leading to the plastic removal of the material. During the process of material removal, a smaller tool rake angle removes a larger amount of material chips. By analyzing the damage layer of the workpiece, the difference in the damage layer is smaller when the scratching direction is different, but the damage layer generated by the smaller rake angle of the scratching tool is thinner. It shows that the scratching force and workpiece temperature are relatively small when the rake angle of the scratching tool is small. Therefore, when scratching 4H-SiC single crystals, choosing a tool with a smaller rake angle is more beneficial for the process.
- Open Access
- 27 August 2020
- Published by MDPI AG in Applied Sciences
- Vol. 10 (17) , 5944
Study on Damage of 4H-SiC Single Crystal through Indentation and Scratch Testing in Micro–Nano Scales
In this paper, a series of indentation tests in which the maximum normal force ranged from 0.4 to 3.3 N were carried out to determine the fracture toughness of 4H-SiC single crystals. The results indicated that an appropriate ratio of the distance from the indentation center to the radial crack tip to the distance from the indentation center to the indentation corner is significant to calculate fracture toughness of 4H-SiC single crystals. The critical condition with no cracks on the edge of the indentation was obtained through a fitting method. The surface morphologies of the groove were analyzed by scanning electron microscopy (SEM). Plastic deformation was observed and characterized by the smooth groove without cracks and ductile chips on the edge of the groove in the initial stages of scratch. With increased normal force, median cracks, radial cracks, and microcracks appeared in turn, followed by the crack system no longer being able to stably extend, causing the brittle fracture to dominate the material removal. The size of the edge damages were measured through SEM and the experimental data highly agreed with the predicted curve. A modified calculation model considering elastic recovery of the sample by the indenter during the scratching process was suggested. These results prove that elastic recovery of 4H-SiC single crystals cannot be ignored during ultra-precision machining.
- 27 August 2020
- Published by MDPI AG in Applied Sciences
- Vol. 10 (17) , 5944
Open AccessStudy on Damage of 4H-SiC Single Crystal through Indentation and Scratch Testing in Micro–Nano Scales
In this paper, a series of indentation tests in which the maximum normal force ranged from 0.4 to 3.3 N were carried out to determine the fracture toughness of 4H-SiC single crystals. The results indicated that an appropriate ratio of the distance from the indentation center to the radial crack tip to the distance from the indentation center to the indentation corner is significant to calculate fracture toughness of 4H-SiC single crystals. The critical condition with no cracks on the edge of the indentation was obtained through a fitting method. The surface morphologies of the groove were analyzed by scanning electron microscopy (SEM). Plastic deformation was observed and characterized by the smooth groove without cracks and ductile chips on the edge of the groove in the initial stages of scratch. With increased normal force, median cracks, radial cracks, and microcracks appeared in turn, followed by the crack system no longer being able to stably extend, causing the brittle fracture to dominate the material removal. The size of the edge damages were measured through SEM and the experimental data highly agreed with the predicted curve. A modified calculation model considering elastic recovery of the sample by the indenter during the scratching process was suggested. These results prove that elastic recovery of 4H-SiC single crystals cannot be ignored during ultra-precision machining.
- Open Access
- 17 January 2020
- Published by MDPI AG in Micromachines
- Vol. 11 (1) , 102
Mechanical Behavior Investigation of 4H-SiC Single Crystal at the Micro–Nano Scale
In this paper, theoretical models of the critical indentation depth and critical force on brittle materials using cleavage strength and contact theory are proposed. A Berkovich indenter is adopted for nanoindentation tests on a 4H-SiC single crystal sample to evaluate its mechanical behaviors. The stages of brittle material deformation (elastic, plastic, and brittle) can be characterized by the load versus indentation depth curves through the nanoindentation test. The curve of the elastic deformation stage follows the Hertz contact theory, and plastic deformation occurs at an indentation depth of up to 10 nm. The mechanism of 4H-SiC single crystal cracking is discussed, and the critical indentation depth and critical force for the plastic–brittle transition are obtained through the occurrence of the pop-in point. This shows that the theoretical results have good coherence with the test results. Both the values of the elastic modulus and hardness decrease as the crack length increases. In order to obtain more accurate mechanical property values in the nanoindentation test for brittle materials such as SiC, GaN, and sapphire, an appropriate load that avoids surface cracks should be adopted.
- 17 January 2020
- Published by MDPI AG in Micromachines
- Vol. 11 (1) , 102
Open AccessMechanical Behavior Investigation of 4H-SiC Single Crystal at the Micro–Nano Scale
In this paper, theoretical models of the critical indentation depth and critical force on brittle materials using cleavage strength and contact theory are proposed. A Berkovich indenter is adopted for nanoindentation tests on a 4H-SiC single crystal sample to evaluate its mechanical behaviors. The stages of brittle material deformation (elastic, plastic, and brittle) can be characterized by the load versus indentation depth curves through the nanoindentation test. The curve of the elastic deformation stage follows the Hertz contact theory, and plastic deformation occurs at an indentation depth of up to 10 nm. The mechanism of 4H-SiC single crystal cracking is discussed, and the critical indentation depth and critical force for the plastic–brittle transition are obtained through the occurrence of the pop-in point. This shows that the theoretical results have good coherence with the test results. Both the values of the elastic modulus and hardness decrease as the crack length increases. In order to obtain more accurate mechanical property values in the nanoindentation test for brittle materials such as SiC, GaN, and sapphire, an appropriate load that avoids surface cracks should be adopted.
- Open Access
- 7 June 2019
- Published by MDPI AG in Micromachines
- Vol. 10 (6) , 382
Modeling and Experiment of the Critical Depth of Cut at the Ductile–Brittle Transition for a 4H-SiC Single Crystal
In this paper, a theoretical model of the critical depth of cut of nanoscratching on a 4H-SiC single crystal with a Berkovich indenter is proposed, and a series of scratch tests in a nanomechanical test system was performed. Through nanoindentation experimentation on fused quartz, the Berkovich indenter nose radius was indirectly confirmed using least squares. The range of critical depths of cut at the ductile–brittle transition was obtained by SEM observation, and the size of cracks was amplified with increasing scratching depth. The theoretical result of the critical depth of cut at the ductile–brittle transition for a 4H-SiC single crystal is 91.7 nm, which is close to the first obvious pop-in point of the relation curve between tangential force and lateral displacement. Repeated experimental results show good consistency and good agreement with other references.
- 7 June 2019
- Published by MDPI AG in Micromachines
- Vol. 10 (6) , 382
Open AccessModeling and Experiment of the Critical Depth of Cut at the Ductile–Brittle Transition for a 4H-SiC Single Crystal
In this paper, a theoretical model of the critical depth of cut of nanoscratching on a 4H-SiC single crystal with a Berkovich indenter is proposed, and a series of scratch tests in a nanomechanical test system was performed. Through nanoindentation experimentation on fused quartz, the Berkovich indenter nose radius was indirectly confirmed using least squares. The range of critical depths of cut at the ductile–brittle transition was obtained by SEM observation, and the size of cracks was amplified with increasing scratching depth. The theoretical result of the critical depth of cut at the ductile–brittle transition for a 4H-SiC single crystal is 91.7 nm, which is close to the first obvious pop-in point of the relation curve between tangential force and lateral displacement. Repeated experimental results show good consistency and good agreement with other references.