Zhifu Huang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Zhifu Huang has a total of 36 co-authors. Here are the top co-authors by number of shared publications:
- Yongxin Jian
School of Mechanical Engineering, Xi’an Jiaotong University, Xi’an 710049, China
6 shared publications - Lei Zhang
State Key Laboratory for Mechanical Behavior of Materials, Xi’an Jiaotong University, Xi’an 710049, China
3 shared publications - Yupeng Shen
State Key Laboratory for Mechanical Behavior of Materials, Xi’an Jiaotong University, Xi’an 710049, China
3 shared publications - Zhen Cao
State Key Laboratory for Mechanical Behavior of Materials, Xi’an Jiaotong University, Xi’an 710049, China
3 shared publications - Kemin Li
Xi'an Jiaotong University, Xi'an, 710049, China
2 shared publications Qiaoling Zheng
Xi'an Jiaotong University, Xi'an, Shaanxi, China
2 shared publications
Latest Publications
- Open Access
Effect of Mo Content on In-Situ Anisometric Grains Growth and Mechanical Properties of Mo2FeB2-Based Cermets
Mo2FeB2-based cermets have wide applications in fields of wear resistance, corrosion resistance and heat resistance due to their simple preparation process, low-cost raw materials, and prominent mechanical properties. Herein, Mo2FeB2-based cermets with xMo (x = 43.5, 45.5, 47.5, 49.5, wt.%) were prepared by means of the vacuum liquid phase sintering technique. Investigations on the microstructure and mechanical properties of Mo2FeB2-based cermets with Mo addition were performed. Experimental results show that, with Mo content increasing, the average particle size decreases gradually, revealing that the grain coarsening of Mo2FeB2-based cermets is controlled by interface reaction. In addition, Mo2FeB2 grains gradually transform from an elongated shape to a nearly equiaxed shape. The improvement of Mo2FeB2 hard phase on the morphology is mainly due to the inhibition of solution–precipitation reaction by increasing Mo. Furthermore, the relative density of cermets decreases due to the reduced Fe content. When Mo content is 47.5 wt.%, a relatively small grain size of Mo2FeB2 is obtained (about 2.03 μm). Moreover, with the increase in Mo content, hardness and transverse rupture strength (TRS) of Mo2FeB2-based cermets increase firstly and then decrease. Whereas, with increasing Mo content, the fracture toughness deteriorates gradually. When Mo content is 47.5 wt.%, the comprehensive mechanical properties of cermets are the best. The optimal raw material ratio for the preparation of Mo2FeB2-based cermets in this study is determined to be 47.5 wt.% Mo–6.0 wt.% B-Fe.
Open AccessEffect of Mo Content on In-Situ Anisometric Grains Growth and Mechanical Properties of Mo2FeB2-Based Cermets
Mo2FeB2-based cermets have wide applications in fields of wear resistance, corrosion resistance and heat resistance due to their simple preparation process, low-cost raw materials, and prominent mechanical properties. Herein, Mo2FeB2-based cermets with xMo (x = 43.5, 45.5, 47.5, 49.5, wt.%) were prepared by means of the vacuum liquid phase sintering technique. Investigations on the microstructure and mechanical properties of Mo2FeB2-based cermets with Mo addition were performed. Experimental results show that, with Mo content increasing, the average particle size decreases gradually, revealing that the grain coarsening of Mo2FeB2-based cermets is controlled by interface reaction. In addition, Mo2FeB2 grains gradually transform from an elongated shape to a nearly equiaxed shape. The improvement of Mo2FeB2 hard phase on the morphology is mainly due to the inhibition of solution–precipitation reaction by increasing Mo. Furthermore, the relative density of cermets decreases due to the reduced Fe content. When Mo content is 47.5 wt.%, a relatively small grain size of Mo2FeB2 is obtained (about 2.03 μm). Moreover, with the increase in Mo content, hardness and transverse rupture strength (TRS) of Mo2FeB2-based cermets increase firstly and then decrease. Whereas, with increasing Mo content, the fracture toughness deteriorates gradually. When Mo content is 47.5 wt.%, the comprehensive mechanical properties of cermets are the best. The optimal raw material ratio for the preparation of Mo2FeB2-based cermets in this study is determined to be 47.5 wt.% Mo–6.0 wt.% B-Fe.
- Open Access
Sintering Mechanism, Microstructure Evolution, and Mechanical Properties of Ti-Added Mo2FeB2-Based Cermets
Four series of Mo2FeB2-based cermets with Ti contents between 0 wt.% and 1.5 wt.% in 0.5 wt.% increments were prepared by in situ reaction and liquid phase sintering technology. Influences of Ti on microstructure and mechanical properties of cermets were studied. It was found that Ti addition increases formation temperatures of liquid phases in liquid-phase stage. Ti atoms replace a fraction of Mo atoms in Mo2FeB2 and the solution of Ti atoms causes the Mo2FeB2 crystal to be equiaxed. In addition, the cermets with 1.0 wt.% Ti content exhibit the smallest particle size. The solution of Ti atoms in Mo2FeB2 promotes the transformation of Mo2FeB2 particles from elongated shape to equiaxed shape. With Ti content increasing from 0 wt.% to 1.5 wt.%, the hardness and transverse rupture strength (TRS) first increase and then decrease. The maximum hardness and TRS occur with 1.0 wt.% Ti content. However, the fracture toughness decreases as Ti content increases. The cermets with 1.0 wt.% Ti content show excellent comprehensive mechanical properties, and the hardness, fracture toughness, and TRS are HRA 89.5, 12.9 MPa∙m1/2, and 1612.6 MPa, respectively.
Open AccessSintering Mechanism, Microstructure Evolution, and Mechanical Properties of Ti-Added Mo2FeB2-Based Cermets
Four series of Mo2FeB2-based cermets with Ti contents between 0 wt.% and 1.5 wt.% in 0.5 wt.% increments were prepared by in situ reaction and liquid phase sintering technology. Influences of Ti on microstructure and mechanical properties of cermets were studied. It was found that Ti addition increases formation temperatures of liquid phases in liquid-phase stage. Ti atoms replace a fraction of Mo atoms in Mo2FeB2 and the solution of Ti atoms causes the Mo2FeB2 crystal to be equiaxed. In addition, the cermets with 1.0 wt.% Ti content exhibit the smallest particle size. The solution of Ti atoms in Mo2FeB2 promotes the transformation of Mo2FeB2 particles from elongated shape to equiaxed shape. With Ti content increasing from 0 wt.% to 1.5 wt.%, the hardness and transverse rupture strength (TRS) first increase and then decrease. The maximum hardness and TRS occur with 1.0 wt.% Ti content. However, the fracture toughness decreases as Ti content increases. The cermets with 1.0 wt.% Ti content show excellent comprehensive mechanical properties, and the hardness, fracture toughness, and TRS are HRA 89.5, 12.9 MPa∙m1/2, and 1612.6 MPa, respectively.
- 25 July 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (10) , 106506
Effect of oxidation time on the short time oxidation behavior and tribological performance of bulk Fe2B
The effects of oxidation time on the short time oxidation behavior and tribological performance of bulk Fe2B have been investigated in this present study. The results reveal that oxidation weight gain, average roughness of oxidation surface and oxidation layer thickness increase with oxidation time increases. Micro-bulges appear and grow up gradually on the oxidation surface as the increasing of oxidation time. The oxidation produces consisting of ɑ-Fe, Fe2O3, Fe3O4, FeBO3,Fe2OBO3, B2O3 and H3BO3 are generated on the surface. At a relative speed of 0.075 m/s under a normal load of 8 N, the values of friction coefficient and wear rate go down first, later go up, and then go down again. The lowest friction coefficient and wear rate can be obtained for the sample with a 9 min oxidation treatment before friction.
- 25 July 2019
- Published by IOP Publishing in Materials Research Express
- Vol. 6 (10) , 106506
Effect of oxidation time on the short time oxidation behavior and tribological performance of bulk Fe2B
The effects of oxidation time on the short time oxidation behavior and tribological performance of bulk Fe2B have been investigated in this present study. The results reveal that oxidation weight gain, average roughness of oxidation surface and oxidation layer thickness increase with oxidation time increases. Micro-bulges appear and grow up gradually on the oxidation surface as the increasing of oxidation time. The oxidation produces consisting of ɑ-Fe, Fe2O3, Fe3O4, FeBO3,Fe2OBO3, B2O3 and H3BO3 are generated on the surface. At a relative speed of 0.075 m/s under a normal load of 8 N, the values of friction coefficient and wear rate go down first, later go up, and then go down again. The lowest friction coefficient and wear rate can be obtained for the sample with a 9 min oxidation treatment before friction.
- Open Access
Effects of Mechanical Ball Milling Time on the Microstructure and Mechanical Properties of Mo2NiB2-Ni Cermets
Mo2NiB2-Ni cermets have been extensively investigated due to their outstanding properties. However, studies have not systematically examined the effect of the powder milling process on the cermets. In this study, Mo, Ni, and B raw powders were subjected to mechanical ball milling from 1 h to 15 h. XRD patterns of the milled powders confirmed that a new phase was not observed at milling times of 1 h to 15 h. With the increase in the mechanical ball milling time from 1 h to 11 h, raw powders were crushed to small fragments, in addition to a more uniform distribution, and with the increase in the mechanical ball milling time to greater than 11 h, milled powders changed slightly. Mo2NiB2-Ni cermets were fabricated by reaction boronizing sintering using the milled powders at different ball milling times. The milling time significantly affected the microstructure and mechanical properties of Mo2NiB2-Ni cermets. Moreover, the Mo2NiB2 cermet powder subjected to a milling time of 11 h exhibited the finest crystal size and the maximum volume fraction of the Mo2NiB2 hard phase. Furthermore, the cermets with a milling time of 11 h exhibited a maximum hardness and bending strength of 87.6 HRA and 1367.3 MPa, respectively.
Open AccessEffects of Mechanical Ball Milling Time on the Microstructure and Mechanical Properties of Mo2NiB2-Ni Cermets
Mo2NiB2-Ni cermets have been extensively investigated due to their outstanding properties. However, studies have not systematically examined the effect of the powder milling process on the cermets. In this study, Mo, Ni, and B raw powders were subjected to mechanical ball milling from 1 h to 15 h. XRD patterns of the milled powders confirmed that a new phase was not observed at milling times of 1 h to 15 h. With the increase in the mechanical ball milling time from 1 h to 11 h, raw powders were crushed to small fragments, in addition to a more uniform distribution, and with the increase in the mechanical ball milling time to greater than 11 h, milled powders changed slightly. Mo2NiB2-Ni cermets were fabricated by reaction boronizing sintering using the milled powders at different ball milling times. The milling time significantly affected the microstructure and mechanical properties of Mo2NiB2-Ni cermets. Moreover, the Mo2NiB2 cermet powder subjected to a milling time of 11 h exhibited the finest crystal size and the maximum volume fraction of the Mo2NiB2 hard phase. Furthermore, the cermets with a milling time of 11 h exhibited a maximum hardness and bending strength of 87.6 HRA and 1367.3 MPa, respectively.
- 25 June 2018
- Published by IOP Publishing in Materials Research Express
- Vol. 5 (7) , 076506
Influence of Cr addition on tribological properties of bulk Fe2B under dry friction and water lubrication
In the present study, friction and wear properties of bulk Fe2B with different Cr additions were examined under dry friction and water lubrication conditions. The morphology, structure, mechanical properties and tribological properties were investigated by OM, SEM, XRD and XPS. The results show that there is no obvious new phase generated and the crystal structure has no changes with Cr addition. Cr element solubilizes in Fe2B gains without any segregation, only bits of (Fe, Cr)2B crystals formed. With the increasing of Cr addition, the fracture toughness increases first then decreases, and 2Cr sample has the highest toughness. Under dry friction condition, the friction coefficient and wear loss are all decrease first and then increase. 2Cr sample has the highest friction coefficient and wear loss. The tribochemical products form a lubricating film to reduce the friction coefficient and wear loss. And the wear mechanism is mainly brittle fracture. Under water lubrication condition, the friction coefficient drops remarkably, then slightly rises up. In contrast, the wear loss increases first and then decreases. 2Cr sample has the lowest friction coefficient, but the highest wear loss. The wear mechanism is mainly tribo-chemical wear in water. A comparison of the results under dry friction and water lubrication conditions, for the same sample, the friction coefficient is lower, but the wear loss is higher in water.
- 25 June 2018
- Published by IOP Publishing in Materials Research Express
- Vol. 5 (7) , 076506
Influence of Cr addition on tribological properties of bulk Fe2B under dry friction and water lubrication
In the present study, friction and wear properties of bulk Fe2B with different Cr additions were examined under dry friction and water lubrication conditions. The morphology, structure, mechanical properties and tribological properties were investigated by OM, SEM, XRD and XPS. The results show that there is no obvious new phase generated and the crystal structure has no changes with Cr addition. Cr element solubilizes in Fe2B gains without any segregation, only bits of (Fe, Cr)2B crystals formed. With the increasing of Cr addition, the fracture toughness increases first then decreases, and 2Cr sample has the highest toughness. Under dry friction condition, the friction coefficient and wear loss are all decrease first and then increase. 2Cr sample has the highest friction coefficient and wear loss. The tribochemical products form a lubricating film to reduce the friction coefficient and wear loss. And the wear mechanism is mainly brittle fracture. Under water lubrication condition, the friction coefficient drops remarkably, then slightly rises up. In contrast, the wear loss increases first and then decreases. 2Cr sample has the lowest friction coefficient, but the highest wear loss. The wear mechanism is mainly tribo-chemical wear in water. A comparison of the results under dry friction and water lubrication conditions, for the same sample, the friction coefficient is lower, but the wear loss is higher in water.
- 2 January 2018
- Published by Springer Nature in Journal of Materials Science
- Vol. 53 (7) , 5329-5338
Effects of chromium on the morphology and mechanical properties of Fe2B intermetallic in Fe-3.0B alloy
- 2 January 2018
- Published by Springer Nature in Journal of Materials Science
- Vol. 53 (7) , 5329-5338
Effects of chromium on the morphology and mechanical properties of Fe2B intermetallic in Fe-3.0B alloy
- 12 December 2017
- Published by Taylor & Francis in Tribology Transactions
- Vol. 61 (3) , 513-521
Friction and Wear Behavior of Single-Phase Fe2B Bulk under Dry Sliding Condition
The effects of normal load and velocity on the friction and wear behavior of single-phase Fe2B bulk have been investigated by optical microscopy, X-ray diffraction, scanning electron microscopy, and X-ray photoelectron spectroscopy. Results indicate that the friction coefficient and wear rate both decrease at first and then increase with increasing load and velocity, respectively. Attributed to the formation of a lamellar film on the Fe2B surface, the lowest friction coefficient and wear rate are obtained at a velocity of 0.2 m/s under a load of 12 N. The dynamic friction coefficients under loads of 4 and 12 N are around 0.8 in the initial steady stage and then decrease to about 0.6, whereas the friction coefficient at 20 N shows no obvious change and remains around 0.82. The lubricating film consisting of Fe2O3, B2O3, SiO2, and H3BO3 reduces the friction coefficient at 0.2 m/s under a load of 12 N.
- 12 December 2017
- Published by Taylor & Francis in Tribology Transactions
- Vol. 61 (3) , 513-521
Friction and Wear Behavior of Single-Phase Fe2B Bulk under Dry Sliding Condition
The effects of normal load and velocity on the friction and wear behavior of single-phase Fe2B bulk have been investigated by optical microscopy, X-ray diffraction, scanning electron microscopy, and X-ray photoelectron spectroscopy. Results indicate that the friction coefficient and wear rate both decrease at first and then increase with increasing load and velocity, respectively. Attributed to the formation of a lamellar film on the Fe2B surface, the lowest friction coefficient and wear rate are obtained at a velocity of 0.2 m/s under a load of 12 N. The dynamic friction coefficients under loads of 4 and 12 N are around 0.8 in the initial steady stage and then decrease to about 0.6, whereas the friction coefficient at 20 N shows no obvious change and remains around 0.82. The lubricating film consisting of Fe2O3, B2O3, SiO2, and H3BO3 reduces the friction coefficient at 0.2 m/s under a load of 12 N.
- 1 August 2017
- Published by IOP Publishing in Materials Research Express
- Vol. 4 (8) , 086504
Synthesis of single-phase Cr7C3 bulk with phenolic resin addition by hot pressing and its mechanical properties
By optimizing the addition of phenolic resin to mixed powders of Cr and C, the single-phase Cr7C3 bulk was synthesized by hot pressing at 1673 K, and the effects of duration times on the relative densities and mechanical properties were also investigated. The results indicate that, with a phenolic resin of 2.0 wt.% in the mixed powders, the single-phase Cr7C3 bulk can be synthesized. At a duration time of less than 90 min, the relative density plays a dominant role in the mechanical properties of Cr7C3 bulk; at durations exceeding 90 min, the grain size plays a dominant role. Compared with the bending strength and fracture toughness values of Cr7C3 bulks reported elsewhere, the mechanical properties of Cr7C3 synthesized by hot pressing can achieve the maximal values: bending strength of 689 MPa, fracture toughness of 8.6 MPa m−1/2 and hardness of 1843 Hv.
- 1 August 2017
- Published by IOP Publishing in Materials Research Express
- Vol. 4 (8) , 086504
Synthesis of single-phase Cr7C3 bulk with phenolic resin addition by hot pressing and its mechanical properties
By optimizing the addition of phenolic resin to mixed powders of Cr and C, the single-phase Cr7C3 bulk was synthesized by hot pressing at 1673 K, and the effects of duration times on the relative densities and mechanical properties were also investigated. The results indicate that, with a phenolic resin of 2.0 wt.% in the mixed powders, the single-phase Cr7C3 bulk can be synthesized. At a duration time of less than 90 min, the relative density plays a dominant role in the mechanical properties of Cr7C3 bulk; at durations exceeding 90 min, the grain size plays a dominant role. Compared with the bending strength and fracture toughness values of Cr7C3 bulks reported elsewhere, the mechanical properties of Cr7C3 synthesized by hot pressing can achieve the maximal values: bending strength of 689 MPa, fracture toughness of 8.6 MPa m−1/2 and hardness of 1843 Hv.