Latest Publications

  • Open Access

    Surface Grain Refinement of 304L Stainless Steel by Combined Severe Shot Peening and Reversion Annealing Treatment

    by Xuanpei Wu, Zeyou Qi, Zhiling Zhou, Hongcheng Zhang, Weijie Wu, Yanfei Wang

    The present study proposes a novel method, i.e., combined severe shot peening (SP) and reversion annealing treatment, to grain-refine the surface layers of 304L austenitic stainless steel. Steel specimens were shot-peened at 0.7 MPa for 30 min, introducing 40% vol. α′ martensite, and then were annealed at 700 or 800 °C for different durations (30 s). As annealing reversed α′ martensite to austenite, the obtained surface layers consist of fully austenitic ultrafine grains. The smallest grain size obtained is about 500 nm at the top surface. SP elevates the microhardness to more than 500 HV. Although the grain-refined surface layers produced by the combined method are not as hard as that treated by only SP, they are harder (e.g., the specimen annealed at 700 °C for 30 s using a heating rate of 50 °C/s exhibited a peak microhardness of 400 HV) than the untreated surface layer (225 HV) due to grain refinement. Moreover, due to the absence of α′ martensite, they have higher corrosion resistance in H2SO4 solution than that treated by only SP.


  • Open Access

    Effect of α′ Martensite Content Induced by Tensile Plastic Prestrain on Hydrogen Transport and Hydrogen Embrittlement of 304L Austenitic Stainless Steel

    by Yanfei Wang, Xuanpei Wu, Weijie Wu

    Effects of microstructural changes induced by prestraining on hydrogen transport and hydrogen embrittlement (HE) of austenitic stainless steels were studied by hydrogen precharging and tensile testing. Prestrains higher than 20% at 20 °C significantly enhance the HE of 304L steel, as they induce severe α′ martensite transformation, accelerating hydrogen transport and hydrogen entry during subsequent hydrogen exposure. In contrast, 304L steel prestrained at 50 and 80 °C and 316L steel prestrained at 20 °C exhibit less HE, due to less α′ after prestraining. The increase of dislocations after prestraining has a negligible influence on apparent hydrogen diffusivity compared with pre-existing α′. The deformation twins in heavily prestrained 304L steel can modify HE mechanism by assisting intergranular (IG) fracture. Regardless of temperature and prestrain level, HE and apparent diffusivity ( D app ) increase monotonously with α′ volume fraction ( f α ′ ). D app can be described as log D app = log ( D α ′ s α ′ / s γ ) + log [ f α ′ / ( 1 − f α ′ ) ] for 10 % < f α ′ < 90 % , with D α ′ is diffusivity in α′, s α ′ and s γ are solubility in α′ and austenite, respectively. The two equations can also be applied to these more typical duplex materials containing both BCC and FCC phases.


  • Open Access

    Warm Pre-Strain: Strengthening the Metastable 304L Austenitic Stainless Steel without Compromising Its Hydrogen Embrittlement Resistance

    by Yanfei Wang, Zhiling Zhou, Weijie Wu, Jianming Gong

    Plastic pre-strains were applied to the metastable 304L austenitic stainless steel at both room temperature (20 °C) and higher temperatures (i.e., 50, 80 and 100 °C), and then the hydrogen embrittlement (HE) susceptibility of the steel was evaluated by cathodically hydrogen-charging and tensile testing. The 20 °C pre-strain greatly strengthened the steel, but simultaneously significantly increased the HE susceptibility of the steel, since α′ martensite was induced by the pre-strain, causing the pre-existence of α′ martensite, which provided “highways” for hydrogen to transport deep into the steel during the hydrogen-charging. Although the warm pre-strains did not strengthen the steel as significantly as the 20 °C pre-strain, they retained the HE resistance of the steel. This is because the higher temperatures, particularly 80 and 100 °C, suppressed the α′ martensite transformation during the pre-straining. Pre-strain at a temperature slightly higher than room temperature has a potential to strengthen the metastable 304L austenitic stainless steel without compromising its initial HE resistance.