Lihui Yang

Lihui Yang

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article

Previous Organizations / Institutes

The organizations / institutes from the scholar's other articles in the past ten years


Lihui Yang has a total of 39 co-authors. Here are the top co-authors by number of shared publications:

  • Xiutong Wang

    Key Laboratory of Advanced Marine Materials, Key Laboratory of Marine Environmental Corrosion and Bio-Fouling, Institute of Oceanology, Chinese Academy of Sciences, Qingdao 266071, China

    5 shared publications
  • Yanliang Huang

    CAS Key Laboratory of Marine Environmental Corrosion and Bio-fouling, Institute of Oceanology, Chinese Academy of Sciences, Qingdao, China

    3 shared publications
  • Yantao Li

    Key Laboratory of Marine Environmental Corrosion and Bio-fouling, Institute of Oceanology, Chinese Academy of Sciences, Qingdao 266071, China

    3 shared publications
  • Cong Liu

    Southwest Technology and Engineering Research Institute, Chongqing 400039, China

    2 shared publications
  • Quantong Jiang

    Laboratory of Advanced Marine Materials, Institute of Oceanology, Chinese Academy of Sciences, No.7 Nanhai Road, Qingdao, China

    2 shared publications
  • Tianxing Chen

    School of Environment and Safety Engineering, Qingdao University of Science and Technology, Qingdao 266042, China

    2 shared publications

Latest Publications

  • Open Access

    Atmospheric Corrosion Behavior of Q235 Steel Exposed to the Subtropical Marine Environment in the East China Sea for Two Years

    by Tianxing Chen, Lihui Yang, Cong Liu, Tianlong Zhang, Shibo Chen, Xiaoyan Deng, Liang Sun

    The corrosion behavior and mechanism of Q235 steel during a two-year exposure to the subtropical marine atmospheric environment on an offshore platform in the East China Sea were investigated in this study. Methods including corrosion weight loss measurement, macro/micro-morphological observation (using a digital camera, SEM, and 3D-CLSM), composition analysis (XRD and XPS), and electrochemical tests (EIS and Tafel polarization curves) were employed to systematically examine corrosion kinetics, rust layer evolution, and electrochemical performance. The results indicated that the corrosion rate of Q235 steel initially increased and subsequently decreased with prolonged exposure, with the atmospheric corrosivity reaching CX level as defined (according to the ISO 9223 standard). The corrosion products transitioned from an early-stage rust layer predominantly consisting of γ-FeOOH to a later-stage layer primarily composed of α-FeOOH and Fe3O4. XPS analyses revealed that both the α*/γ* ratio and the Fe(II)/Fe(III) ratio increased over time, demonstrating a progressive improvement in the protective properties of the rust layer. The polarization resistance of the rust layer gradually rose, while the corrosion current density declined significantly, further confirming the enhanced stability and protective performance of the rust layer following long-term exposure. Chloride ions accumulated at defects within the rust layer, inducing local acidification, which played a key role in promoting the initiation and propagation of pitting corrosion. This study elucidated the corrosion behavior and mechanism of Q235 steel in the marine atmospheric environment of the East China Sea. Despite the increase in exposure time from 6 to 24 months, during which the electrochemical stability of the rust layer enhanced over time, it failed to prevent the initiation and propagation of severe localized corrosion—an issue of critical importance for load-bearing structures. The findings provide important theoretical and data support for service-life assessment and corrosion protection design of offshore photovoltaic steel structures.


  • Open Access

    Research on Comparative Marine Atmospheric Corrosion Behavior of AZ31 Magnesium Alloy in South China Sea

    by Tianlong Zhang, Shuai Wu, Hao Liu, Lihui Yang, Tianxing Chen, Xiutong Wang, Yantao Li

    In this study, the atmospheric corrosion behavior of AZ31 magnesium alloy exposed in Sanya and Nansha for one year was investigated. While existing studies have characterized marine corrosion of magnesium alloys, the synergistic corrosion mechanisms under extreme tropical marine conditions (simultaneous high Cl−, rainfall, and temperature fluctuations) remain poorly understood—particularly regarding dynamic corrosion–product evolution. The corrosion characteristics and behavior of AZ31 magnesium alloy exposed in Sanya and Nansha were evaluated using X-ray photoelectron spectroscopy, X-ray diffraction, electrochemical measurements, scanning electron microscopy, and weight loss tests. The results showed that the main components of corrosion products were MgCO3·xH2O(x = 3, 5), Mg5(CO3)4(OH)2·4H2O, Mg2Cl(OH)3·4H2O, and Mg(OH)2. The corrosion rate exposed in the Nansha was 26.5 μm·y−1, which was almost two times than that in Sanya. Localized corrosion is the typical corrosion characteristic of AZ31 magnesium alloy in this tropical marine atmosphere. This study exposes the dynamic crack–regeneration mechanism of corrosion products under high-Cl−-rainfall synergy. The corrosion types of AZ31 magnesium alloy in this tropical marine atmosphere were mainly represented by pitting corrosion and filamentous corrosion.


  • Open Access

    Recent Progress on Atmospheric Corrosion of Field-Exposed Magnesium Alloys

    by Mengqi Wang, Lihui Yang, Hao Liu, Xiutong Wang, Yantao Li, Yanliang Huang

    It is well known that the poor corrosion resistance of magnesium alloys is a key factor limiting their application. Field exposure is the most reliable means to evaluate the atmospheric corrosion performance of magnesium alloys. This article reviews the field exposure corrosion behavior of magnesium alloys in typical atmospheric environments (including the marine atmosphere, industrial atmosphere, etc.) in recent years. According to the literature review, it was found that there are significant regional differences in the atmospheric corrosion behavior of magnesium alloys, which is the result of the coupling of multiple factors in the atmospheric environment. By investigating the corrosion rate and corrosion products of different types of magnesium alloys in different environments, the corrosion mechanism of magnesium alloys in different environments was summarized. Specifically, environmental parameters such as atmospheric temperature, relative humidity, CO2, and chloride ion deposition rates in the marine atmospheric environment can affect the corrosion behavior of magnesium alloys. The corrosion of magnesium alloys in different industrial atmospheric environments is mainly affected by atmospheric temperature and relative humidity, as well as atmospheric pollutants (such as SO2, CO2, NO2) and dust. This review provides assistance to the development of new corrosion-resistant magnesium alloys.


  • Open Access

    Dynamic Marine Atmospheric Corrosion Behavior of AZ91 Mg Alloy Sailing from Yellow Sea to Western Pacific Ocean

    by Lihui Yang, Cong Liu, Ying Wang, Xiutong Wang, Haiping Gao

    In this work, the dynamic marine atmospheric corrosion behavior of AZ91 Mg alloy sailing from Yellow Sea to Western Pacific Ocean was studied. The corrosion rates were measured using the weight loss method. The microstructure, phase, and chemical composition of corroded samples were investigated by SEM, EDS, XRD, and XPS. The results show that the evolution of corrosion rates of AZ91 Mg alloy was divided into three stages: rapidly increasing during the first 3 months, then remaining stable for the next three months, and finally decreasing after 6 months. The annual corrosion rate of Mg alloy reached 32.50 μm/y after exposure for 12 months in a dynamic marine atmospheric environment, which was several times higher than that of the static field exposure tests. AZ91 magnesium alloy was mainly subjected to localized corrosion with more destructiveness to Mg parts, which is mainly due to the synergistic effect of high relative humidity, the high deposition rate of chloride ion, sulfur dioxide acidic gas produced by fuel combustion, and rapid temperature changes caused by the alternating changes in longitude and latitude during navigation. As the exposure time increased, the corrosion pits gradually increased and deepened. The maximum depth of the corrosion pit was 197 μm after 12 months of exposure, which is almost 6 times the average corrosion depth. This study provides scientific data support for the application of magnesium alloys in shipborne aircraft and electronic equipment. The results could provide guidance for the design of new magnesium alloys and development of anti-corrosion technologies.


  • Design of terahertz detector based on superconducting kinetic inductance

    by Shiling Yu, Ran Duan, Xiaohang Zhang, Lihui Yang, Di Li

    High time-frequency sampling in terahertz band has the potential to find significant discoveries, and superconducting kinetic inductance detector (KID) has the characteristics of fast response and low readout noise, which is a favorable reserve instrument for terahertz high-speed imaging detector. In this paper, we present our design of terahertz detector based on superconducting kinetic inductance effect, including six groups of comparative experiments.

  • Open Access

    Research on Dynamic Marine Atmospheric Corrosion Behavior of AZ31 Magnesium Alloy

    by Ying Wang, Weichen Xu, Xiutong Wang, Quantong Jiang, Yantao Li, Yanliang Huang, Lihui Yang

    The dynamic marine atmospheric corrosion behavior of AZ31 magnesium alloy was investigated in situ exposed on the deck of marine scientific research vessel for 1 year. The marine scientific research vessel carried out five voyages from the coast of China to the western Pacific Ocean, while the navigation track and environmental data were collected and analyzed. The corrosion rate and characteristics were evaluated by using weight loss tests, scanning electron microscopy (SEM), X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), and electrochemical measurements. The corrosion rate from weight loss values was 52.23 μm∙y−1 after exposure for 1 year, which was several times higher than that of the static field exposure test in marine atmospheric environment of other reported literature. The main corrosion products were Mg5(CO3)4(OH)2·4H2O, MgCO3·3H2O and Mg2(OH)3Cl·4H2O. The corrosion was initiated from pitting corrosion and evolved into general corrosion gradually. The serious corrosion maybe due to the harsh corrosive environment with alternating changes in temperature and relative humidity caused by multiple longitude and latitude changes, and particularly high deposition rate of chloride during voyage, which was nearly twenty times that on the coast of China. This study provides effective data for the application of magnesium alloy in shipboard aircraft and other equipment, and provides a reference for indoor simulation experiments.


  • Open Access

    Research on marine atmospheric corrosion behavior of AZ31 magnesium alloy based on scientific ocean voyage

    by Lihui Yang, Ying Wang, Weichen Xu, Xiutong Wang, Yantao Li, Yanliang Huang, Baorong Hou

    Corrosion behavior of AZ31 magnesium alloy based on marine scientific ocean voyage was investigated by using scanning electron microscope (SEM), X-Ray Diffraction (XRD), X-ray photoelectron spectroscopy (XPS) and electrochemical measurements. The results revealed that the AZ31 magnesium alloy suffered serious corrosion during exposure in marine atmosphere of ocean voyage. The corrosion rate was 52.23 μm∙y−1 and the maximum depth of corrosion pits was 105.84 μm after exposure for 1 year. The main corrosion products formed on AZ31 magnesium were Mg5(CO3)4(OH)2·4H2O, MgCO3·3H2O and Mg2(OH)3Cl·4H2O. Chloride ion plays an important role in the corrosion process of AZ31 magnesium alloy during ocean voyage. The corrosion of AZ31 magnesium alloy was initiated from pitting corrosion and evolved into general corrosion. This study will provide effective data for the application of magnesium alloy in marine equipment.


  • Open Access

    Evaluation of Hydrogen Permeation into High-Strength Steel during Corrosion in Different Marine Corrosion Zones

    by Yong Xu, Yanliang Huang, Fanfan Cai, Zhengquan Wang, Dongzhu Lu, Xiutong Wang, Lihui Yang

    Hydrogen permeation into high-strength steel during the corrosion process can deteriorate their mechanical properties, thus seriously threatening the safety of steel structures. However, the hydrogen permeation behavior of steels in corrosive marine environments is not well understood. In this study, the hydrogen permeation behavior and mechanism of AISI 4135 steel in different marine corrosion zones was investigated for the first time using an in situ hydrogen permeation monitoring system via outdoor and indoor tests. The three-month outdoor hydrogen permeation test showed that the diffusible hydrogen content of the steels exposed to the marine atmospheric, splash, tidal and immersion zone was 3.15 × 10−3, 7.00 × 10−2, 2.06 × 10−2 and 3.33 × 10−2 wt ppm, respectively. Meanwhile, results showed that the hydrogen permeation current density was positively correlated with the corrosion rate of the steel in the marine environments. This research is of great significance for guiding the safe application of high-strength steel in the marine environments.


  • Micron-scale ultrathin two-dimension zirconia nanosheets towards enhancing anticorrosion performance of epoxy coatings

    by Xin-Ding Lv, Hao-Tong Li, Xiao-Gang Dai, Xiang-Nan Sun, Hai-Yong Zhang, Yan-Zhen Zheng, Xia Tao, Li-Hui Yang


  • Open Access

    The Effect of Deep Cryogenic Treatment on the Corrosion Behavior of Mg-7Y-1.5Nd Magnesium Alloy

    by Quantong Jiang, Lihui Yang, Baorong Hou

    The effect of quenching on the corrosion resistance of Mg-7Y-1.5Nd alloy was investigated. The as-cast alloy was homogenized at 535 °C for 24 h, followed by quenching in air, water, and liquid nitrogen. Then, all of the samples were peak-aged at 225 °C for 14 h. The microstructures were studied by scanning electron microscopy, energy-dispersive spectrometry, and X-ray diffraction. Corrosion behavior was analyzed by using weight loss rate and gas collection. Electrochemical characterizations revealed that the T4-deep cryogenic sample displayed the strongest corrosion resistance among all of the samples. A new square phase was discovered in the microstructure of the T6-deep cryogenic sample; this phase was hugely responsible for the corrosion property. Cryogenic treatment significantly improved the corrosion resistance of Mg-7Y-1.5Nd alloy.