Guangdong Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Guangdong Wang has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Gang Zhao
School of Materials Science & Engineering, Northeastern University, No. 3-11, Wenhua Road, Heping District, Shenyang 110819, China
4 shared publications - Kun Liu
Department of Applied Science, University of Quebec at Chicoutimi, Saguenay, QC G7H 2B1, Canada
4 shared publications - Liang Zuo
Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education), School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China
4 shared publications - Ni Tian
Northeastern Univ, Sch Mat Sci & Engn, Shenyang 110819, Peoples R China
4 shared publications - Yiran Zhou
School of Materials Science & Engineering, Northeastern University, No. 3-11, Wenhua Road, Heping District, Shenyang 110819, China
3 shared publications - Chuncheng Liu
Engineering Training Center, Northeastern University, No. 3-11, Wenhua Road, Heping District, Shenyang 110819, China
2 shared publications
Latest Publications
- 15 April 2024
- Published by Springer Nature in Journal of Materials Science
- Vol. 59 (17) , 7368-7386
Tensile properties and fracture behavior of Al–8Si alloy sheets with different Mg under natural aging
- 15 April 2024
- Published by Springer Nature in Journal of Materials Science
- Vol. 59 (17) , 7368-7386
Tensile properties and fracture behavior of Al–8Si alloy sheets with different Mg under natural aging
- Open Access
Phase Formation and Microstructure Evolution of Al-5Si-0.8Mg Alloys with Different Mn Concentrations
Mg-containing high-Si aluminum alloys are heat-treatable alloys that are widely used in industry. Substantial attention has been paid to increasing the performance of such alloys by adding a small amount of Mn, which is an effective and common alloying element in aluminum alloys. In the present work, the solidification process of Mn-free Al-5Si-0.8Mg alloy and Al-5Si-0.8Mg-(0.45–1.97)Mn alloys are analyzed by the experimental results combined with thermodynamic calculation. The results showed that α-Al, Si, Mg2Si and π (Al8Mg3FeSi6) are predominant phases in the Mn-free Al-5Si-0.8Mg alloy while the π (Al8Mg3FeSi6) phase are transformed to α-Al(FeMn)Si phase with the addition of 0.45% Mn. With increasing Mn addition to 0.72%, the L→α-Al was replaced by L→α-Al(FeMn)Si and a primary α-Al(FeMn)Si phase appeared. Further increasing the Mn to 1.97%, the solidification reactions remained unchanged. However, the size and number of the primary α-Al(FeMn)Si phase gradually increased, while the divorced eutectic phenomenon of quaternary eutectic structure gradually weakened. Meanwhile, the Mg2Si phase in the quaternary eutectic structure gradually transformed from blocky to fine eutectic lamellar, and the quaternary eutectic structure was significantly refined. Primary blocky α-Al(FeMn)Si began to form when the Mn content was higher than 0.75%.
Open AccessPhase Formation and Microstructure Evolution of Al-5Si-0.8Mg Alloys with Different Mn Concentrations
Mg-containing high-Si aluminum alloys are heat-treatable alloys that are widely used in industry. Substantial attention has been paid to increasing the performance of such alloys by adding a small amount of Mn, which is an effective and common alloying element in aluminum alloys. In the present work, the solidification process of Mn-free Al-5Si-0.8Mg alloy and Al-5Si-0.8Mg-(0.45–1.97)Mn alloys are analyzed by the experimental results combined with thermodynamic calculation. The results showed that α-Al, Si, Mg2Si and π (Al8Mg3FeSi6) are predominant phases in the Mn-free Al-5Si-0.8Mg alloy while the π (Al8Mg3FeSi6) phase are transformed to α-Al(FeMn)Si phase with the addition of 0.45% Mn. With increasing Mn addition to 0.72%, the L→α-Al was replaced by L→α-Al(FeMn)Si and a primary α-Al(FeMn)Si phase appeared. Further increasing the Mn to 1.97%, the solidification reactions remained unchanged. However, the size and number of the primary α-Al(FeMn)Si phase gradually increased, while the divorced eutectic phenomenon of quaternary eutectic structure gradually weakened. Meanwhile, the Mg2Si phase in the quaternary eutectic structure gradually transformed from blocky to fine eutectic lamellar, and the quaternary eutectic structure was significantly refined. Primary blocky α-Al(FeMn)Si began to form when the Mn content was higher than 0.75%.
- Open Access
Formation of Phases and Microstructures in Al-8Si Alloys with Different Mg Content
Mg-containing high-silicon aluminum alloy is a heat-treatable aluminum alloy that is now widely used in the aerospace and automotive industries because of its high specific strength, high wear resistance and corrosion resistance, low thermal expansion coefficient, and low cost. More attention has been paid to optimizing the microstructure to increase the performance of this type of aluminum alloy. In the present work, the solidification processes of Mg-free and Mg-containing (0.33–1.32%) Al-8Si alloys were analyzed by the experimental results combined with the thermodynamic calculation. The results showed that α-Al, Si, and Al5FeSi were in the Mg-free Al-8Si alloy ingots, while the Al5FeSi phases in alloys with Mg additions were transformed into π phases (Al8Mg3FeSi6) by the reaction L+Al5FeSi→α-Al+Si+Al8Mg3FeSi6. There was a binary eutectic reaction of L→α-Al+Al5FeSi when the Mg content exceeded 0.51% and the Fe content was higher than 0.17%. With the increase of Mg content, the volume of Mg2Si was gradually increased while the divorced eutectic phenomenon of the quaternary eutectic structure (α-Al+Si+Mg2Si+Al8Mg3FeSi6) was weakened and the eutectic structure was significantly refined.
Open AccessFormation of Phases and Microstructures in Al-8Si Alloys with Different Mg Content
Mg-containing high-silicon aluminum alloy is a heat-treatable aluminum alloy that is now widely used in the aerospace and automotive industries because of its high specific strength, high wear resistance and corrosion resistance, low thermal expansion coefficient, and low cost. More attention has been paid to optimizing the microstructure to increase the performance of this type of aluminum alloy. In the present work, the solidification processes of Mg-free and Mg-containing (0.33–1.32%) Al-8Si alloys were analyzed by the experimental results combined with the thermodynamic calculation. The results showed that α-Al, Si, and Al5FeSi were in the Mg-free Al-8Si alloy ingots, while the Al5FeSi phases in alloys with Mg additions were transformed into π phases (Al8Mg3FeSi6) by the reaction L+Al5FeSi→α-Al+Si+Al8Mg3FeSi6. There was a binary eutectic reaction of L→α-Al+Al5FeSi when the Mg content exceeded 0.51% and the Fe content was higher than 0.17%. With the increase of Mg content, the volume of Mg2Si was gradually increased while the divorced eutectic phenomenon of the quaternary eutectic structure (α-Al+Si+Mg2Si+Al8Mg3FeSi6) was weakened and the eutectic structure was significantly refined.
- Open Access
Prediction of the Work-Hardening Exponent for 3104 Aluminum Sheets with Different Grain Sizes
A practical approach to predict the yield strength and work-hardening exponent (n value) to evaluate the deep-drawing performance of annealed 3104 aluminum sheets is presented in the present work by only measuring and analyzing the grain size of the sheet. The various grain sizes were obtained through the different annealing treatment and then the evolution of the n value under different strains and the yield strength of annealed 3104 aluminum sheet were evaluated. Results showed that the n value and yield strength vary greatly with the grain size. A mathematical model relating grain size d, work-hardening exponent n, target strain ε, and yield strength Rp0.2 was developed in the present work. Within the studied grain size range d (12–29 μm), the n value generally increased with d in a strain-dependent manner, such that when the ε was less than 0.5%, but when the ε was greater than 2%. On the other hand, the n value was found to depend on the target strain ε as , where A1 varies with d and its value is in the range of 0.132–0.364. In addition, the relationship between Rp0.2 and d followed the Hall-Petch equation ( ).Open AccessPrediction of the Work-Hardening Exponent for 3104 Aluminum Sheets with Different Grain Sizes
A practical approach to predict the yield strength and work-hardening exponent (n value) to evaluate the deep-drawing performance of annealed 3104 aluminum sheets is presented in the present work by only measuring and analyzing the grain size of the sheet. The various grain sizes were obtained through the different annealing treatment and then the evolution of the n value under different strains and the yield strength of annealed 3104 aluminum sheet were evaluated. Results showed that the n value and yield strength vary greatly with the grain size. A mathematical model relating grain size d, work-hardening exponent n, target strain ε, and yield strength Rp0.2 was developed in the present work. Within the studied grain size range d (12–29 μm), the n value generally increased with d in a strain-dependent manner, such that when the ε was less than 0.5%, but when the ε was greater than 2%. On the other hand, the n value was found to depend on the target strain ε as , where A1 varies with d and its value is in the range of 0.132–0.364. In addition, the relationship between Rp0.2 and d followed the Hall-Petch equation ( ). - Open Access
Study of the Portevin-Le Chatelier (PLC) Characteristics of a 5083 Aluminum Alloy Sheet in Two Heat Treatment States
In the present work, the role of Mg atoms in the form of either Mg clusters or β phase on the moving dislocations in 5083 aluminum alloy sheet were investigated by comparing the plastic flow behavior and Portevin-Le Chatelier (PLC) character in annealed and quenched conditions. It is found that the tensile strength of quenched sheets at different strain rates is slightly higher than those under annealed condition while the yield strength at both conditions is similar. In annealed sheets, the yield plateau was clearly observed at all tested strain rates with a strain less than 0.012, and its width increased with the increasing strain rate. However, no yield plateau was observed in quenched sheets. On the other hand, the characters of PLC are greatly varied with applied conditions and strain rate. Generally, annealed sheets have a higher waiting time, but lower critical strain/stress at lower strain rate (~1 × 10−4 s−1), but they are similar at a higher strain rate (1 × 10−2 s−1). However, the falling time at both annealed and quenched conditions are almost the same at tested strain rates.
Open AccessStudy of the Portevin-Le Chatelier (PLC) Characteristics of a 5083 Aluminum Alloy Sheet in Two Heat Treatment States
In the present work, the role of Mg atoms in the form of either Mg clusters or β phase on the moving dislocations in 5083 aluminum alloy sheet were investigated by comparing the plastic flow behavior and Portevin-Le Chatelier (PLC) character in annealed and quenched conditions. It is found that the tensile strength of quenched sheets at different strain rates is slightly higher than those under annealed condition while the yield strength at both conditions is similar. In annealed sheets, the yield plateau was clearly observed at all tested strain rates with a strain less than 0.012, and its width increased with the increasing strain rate. However, no yield plateau was observed in quenched sheets. On the other hand, the characters of PLC are greatly varied with applied conditions and strain rate. Generally, annealed sheets have a higher waiting time, but lower critical strain/stress at lower strain rate (~1 × 10−4 s−1), but they are similar at a higher strain rate (1 × 10−2 s−1). However, the falling time at both annealed and quenched conditions are almost the same at tested strain rates.