Benjamin D. Gould
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Benjamin D. Gould has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
- Karen Swider-Lyons
U.S. Naval Research Laboratory
8 shared publications - Yannick Garsany
Excet Inc
7 shared publications - Robert Atkinson Iii
Excet Inc./ US Naval Research Laboratory
5 shared publications Joseph A. Rodgers
4 shared publications- Keith Bethune
University of Hawaii - Manoa
4 shared publications Matthew W. Hazard
2 shared publications
Latest Publications
- 23 November 2020
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2020-02 (34) , 2212
Operation of PEMFC Anodes in Dead-Ended Vs. Flow-through Modes
Low system complexity and high hydrogen utilization are important attributes for effective proton exchange membrane fuel cells (PEMFCs). Operating a PEMFC with a dead-ended anode (DEA) mode configuration is a simple and effective way to solve these two challenges1, 2. In comparison with the hydrogen flow-through and recirculation mode, in DEA mode the hydrogen supplied to the anode compartment is controlled by pressure regulation instead of a mass flow controller, where a pressure regulator is installed at the anode inlet and a normally closed solenoid valve blocks the outlet. Over time, accumulated water and nitrogen diffused from the cathode are removed by forced gas convection through intermittent opening of the solenoid valve. The anode and cathode gas diffusion media (GDM) play a role in PEMFC water management and have a significant impact on PEMFC performance. We compare an asymmetric GDM pairing with Freudenberg GDM (H24C3 at anode, H23C2 at cathode) to a symmetric GDM pairing frequently used in the open literature containing SGL 29BC at both the anode and cathode, to highlight the impact of the GDM water management on fuel cell operation in flow-through mode and DEA mode. We have previously shown in open-cathode fuel cells that an asymmetric GDM pairing featuring higher porosity in the anode GDM than the cathode significantly improves hydration and power production3, 4. The results at 25% relative humidity (RH) are shown in Figure 1. Consistent with our prior results5, in regular flow-through mode, Figure 1A shows the PEMFC with an asymmetric Freudenberg GDM pairing has significantly higher current densities vs. the PEMFC with symmetric SGL 29BC GDM at an operating cell voltage ≤ 0.60 V. The advantage of using asymmetric GDM observed in flow-through mode is maintained when the PEMFCs are operated in DEA mode (i.e. open symbols). There is only a marginal decrease in cell voltages during operation in DEA mode compared to flow-through mode probably due to the use of dry hydrogen on the anode side during testing in DEA mode. Figure 1B shows that the cell voltage decay is significantly different for a PEMFC containing the symmetric SGL 29BC GDM compared one with asymmetric Freudenberg GDM when tested in DEA mode configuration. The time between purge events is much greater for the asymmetric Freudenberg GDM pairing. The anode is purged with 99.999% H2 when the cell voltage drops by 100 mV. The PEMFC tested with the asymmetric Freudenberg GDM pairing dwells longer at steady-state prior to voltage decay, and its periods of voltage decay are more gradual. The PEMFC containing the symmetric SGL 29BC pairing has a mean purge interval of about 2min 33s and a total of fourteen purge events are necessary over 80 minutes operation, compared to a mean purge interval of about 18min 29s and a total of four purge events are necessary for the PEMFC containing the asymmetric Freudenberg pairing. A longer purge duration is desirable in a fuel cell system because it increases H2 utilization and reduces valve wear. The results show that the asymmetric GDM pairing improves water management in PEMFCs and improves both power density and system level performance. Acknowledgements: The authors are grateful to the Office of Naval Research for support of this research. References I.-S. Han, J. Jeong and H. K. Shin, Int. J. Hydrogen Energy, 38, 11996 (2013). K. Nikiforow, H. Karimäki, T. M. Keränen and J. Ihonen, J. Power Sources, 238, 336 (2013). R. W. Atkinson, M. W. Hazard, J. A. Rodgers, R. O. Stroman and B. D. Gould, J. Electrochem. Soc., 166, F926 (2019). R. W. Atkinson, J. A. Rodgers, M. W. Hazard, R. O. Stroman and B. D. Gould, J. Electrochem. Soc., 165, F1002 (2018). R. W. Atkinson, Y. Garsany, B. D. Gould, K. E. Swider-Lyons and I. V. Zenyuk, ACS Appl. Energy Mater., 1, 191 (2018) Figure 1. (A) Comparison of I-V polarization curves measured for a PEMFC containing a typical symmetric SGL 29BC GDM pairing on the anode and cathode side and a PEMFC containing an asymmetric Freudenberg GDM pairing . Polarization curves are measured in DEA mode and flow-through mode at 25 % RHinlet cathode. In all cases the cell temperature is 65 °C, in H2|air, with air supplied to the cathode a stoichiometric ratio of 2 at atmospheric pressure. During DEA mode, dry H2 is supplied to the anode at 2 psi. (B) Time evolution of the cell voltage obtained at a current density of 1200 mA cm-2 for an H2 inlet pressure of 2 psi and 25 % RHinlet cathode. Figure 1
- 23 November 2020
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2020-02 (34) , 2212
Operation of PEMFC Anodes in Dead-Ended Vs. Flow-through Modes
Low system complexity and high hydrogen utilization are important attributes for effective proton exchange membrane fuel cells (PEMFCs). Operating a PEMFC with a dead-ended anode (DEA) mode configuration is a simple and effective way to solve these two challenges1, 2. In comparison with the hydrogen flow-through and recirculation mode, in DEA mode the hydrogen supplied to the anode compartment is controlled by pressure regulation instead of a mass flow controller, where a pressure regulator is installed at the anode inlet and a normally closed solenoid valve blocks the outlet. Over time, accumulated water and nitrogen diffused from the cathode are removed by forced gas convection through intermittent opening of the solenoid valve. The anode and cathode gas diffusion media (GDM) play a role in PEMFC water management and have a significant impact on PEMFC performance. We compare an asymmetric GDM pairing with Freudenberg GDM (H24C3 at anode, H23C2 at cathode) to a symmetric GDM pairing frequently used in the open literature containing SGL 29BC at both the anode and cathode, to highlight the impact of the GDM water management on fuel cell operation in flow-through mode and DEA mode. We have previously shown in open-cathode fuel cells that an asymmetric GDM pairing featuring higher porosity in the anode GDM than the cathode significantly improves hydration and power production3, 4. The results at 25% relative humidity (RH) are shown in Figure 1. Consistent with our prior results5, in regular flow-through mode, Figure 1A shows the PEMFC with an asymmetric Freudenberg GDM pairing has significantly higher current densities vs. the PEMFC with symmetric SGL 29BC GDM at an operating cell voltage ≤ 0.60 V. The advantage of using asymmetric GDM observed in flow-through mode is maintained when the PEMFCs are operated in DEA mode (i.e. open symbols). There is only a marginal decrease in cell voltages during operation in DEA mode compared to flow-through mode probably due to the use of dry hydrogen on the anode side during testing in DEA mode. Figure 1B shows that the cell voltage decay is significantly different for a PEMFC containing the symmetric SGL 29BC GDM compared one with asymmetric Freudenberg GDM when tested in DEA mode configuration. The time between purge events is much greater for the asymmetric Freudenberg GDM pairing. The anode is purged with 99.999% H2 when the cell voltage drops by 100 mV. The PEMFC tested with the asymmetric Freudenberg GDM pairing dwells longer at steady-state prior to voltage decay, and its periods of voltage decay are more gradual. The PEMFC containing the symmetric SGL 29BC pairing has a mean purge interval of about 2min 33s and a total of fourteen purge events are necessary over 80 minutes operation, compared to a mean purge interval of about 18min 29s and a total of four purge events are necessary for the PEMFC containing the asymmetric Freudenberg pairing. A longer purge duration is desirable in a fuel cell system because it increases H2 utilization and reduces valve wear. The results show that the asymmetric GDM pairing improves water management in PEMFCs and improves both power density and system level performance. Acknowledgements: The authors are grateful to the Office of Naval Research for support of this research. References I.-S. Han, J. Jeong and H. K. Shin, Int. J. Hydrogen Energy, 38, 11996 (2013). K. Nikiforow, H. Karimäki, T. M. Keränen and J. Ihonen, J. Power Sources, 238, 336 (2013). R. W. Atkinson, M. W. Hazard, J. A. Rodgers, R. O. Stroman and B. D. Gould, J. Electrochem. Soc., 166, F926 (2019). R. W. Atkinson, J. A. Rodgers, M. W. Hazard, R. O. Stroman and B. D. Gould, J. Electrochem. Soc., 165, F1002 (2018). R. W. Atkinson, Y. Garsany, B. D. Gould, K. E. Swider-Lyons and I. V. Zenyuk, ACS Appl. Energy Mater., 1, 191 (2018) Figure 1. (A) Comparison of I-V polarization curves measured for a PEMFC containing a typical symmetric SGL 29BC GDM pairing on the anode and cathode side and a PEMFC containing an asymmetric Freudenberg GDM pairing . Polarization curves are measured in DEA mode and flow-through mode at 25 % RHinlet cathode. In all cases the cell temperature is 65 °C, in H2|air, with air supplied to the cathode a stoichiometric ratio of 2 at atmospheric pressure. During DEA mode, dry H2 is supplied to the anode at 2 psi. (B) Time evolution of the cell voltage obtained at a current density of 1200 mA cm-2 for an H2 inlet pressure of 2 psi and 25 % RHinlet cathode. Figure 1
- 1 September 2019
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2019-02 (32) , 1423
Cathode Catalyst Layer Design with Graded Porous Structure for Proton Exchange Membrane Fuel Cells
Cathode catalyst layer (CL) design is important for improved performance, durability and stability of proton exchange membrane fuel cells (PEMFCs). An effective cathode CL must serve multiple functions simultaneously: electron and H+ conduction, O2 or H2 supply, and effective water management. The reaction in the CL requires three-phase boundaries (or interfaces) among ionomer (for proton transfer), platinum (for catalysis), and carbon (for electron transfer), as well as voids (reactant diffusion); an optimized cathode CL structure should have micropores and mesopores to balance water egress and O2 diffusion. Our previous research showed that increasing microporosity in the cathode CL increases the power production of the PEMFCs [1]. Modeling indicates that high CL microporosity enhances water evaporation, which reduces mass transport resistances to enable higher power production [2]. Meanwhile, low microporosity encourages liquid water retention. It is known that catalyst support type has a profound effect on electrode porosity, influencing both micro- and mesoporosity [3, 4]. By constructing electrodes with layers of different carbon supported catalyst types, we demonstrate that we can create porosity gradients in the CLs that vary the electrode water management properties and the power of the PEMFC. Two different types of commercial platinum/carbon electrocatalysts are used in dual cathode CLs – 40 wt. % Pt on Vulcan carbon (Pt/VC) having low micropores and low porosity and 40 wt. % Pt on Ketjen black (Pt/KB) having large micropores and high porosity. CLs are created with both homogeneous porosity in the Z direction (Figure 1a), and compared to ones with non-uniform porosity across the Z-direction (Figure 1b). The microstructure of these cathode CLs is characterized using N2-sorption porosimetry. The CLs are assembled into PEMFCs and probed with polarization curves (at 100, 50 and 25% RH), cyclic voltammetry, O2 gain, electrochemical impedance spectroscopy, and limiting current measurements to quantify the sources of mass transport resistance. The results indicate that the regions with low microporosity encourage liquid water retention, while high microporosity encourages water evaporation. These countering actions are balanced for high CL hydration and gas diffusion, and better PEMFC performance. References [1] Y. Garsany, R.W. Atkinson, M.B. Sassin, R.M.E. Hjelm, B.D. Gould, K.E. Swider-Lyons, J. Electrochem. Soc., 165 (2018) F381-F391. [2] M. Eikerling, J. Electrochem. Soc., 153 (2006) E58-E70. [3] T. Soboleva, K. Malek, Z. Xie, T. Navessin, S. Holdcroft, ACS Appl. Mater. Interfaces, 3 (2011) 1827-1837. [4] Y.-C. Park, H. Tokiwa, K. Kakinuma, M. Watanabe, M. Uchida, Journal of Power Sources, 315 (2016) 179-191. Figure 1
- 1 September 2019
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2019-02 (32) , 1423
Cathode Catalyst Layer Design with Graded Porous Structure for Proton Exchange Membrane Fuel Cells
Cathode catalyst layer (CL) design is important for improved performance, durability and stability of proton exchange membrane fuel cells (PEMFCs). An effective cathode CL must serve multiple functions simultaneously: electron and H+ conduction, O2 or H2 supply, and effective water management. The reaction in the CL requires three-phase boundaries (or interfaces) among ionomer (for proton transfer), platinum (for catalysis), and carbon (for electron transfer), as well as voids (reactant diffusion); an optimized cathode CL structure should have micropores and mesopores to balance water egress and O2 diffusion. Our previous research showed that increasing microporosity in the cathode CL increases the power production of the PEMFCs [1]. Modeling indicates that high CL microporosity enhances water evaporation, which reduces mass transport resistances to enable higher power production [2]. Meanwhile, low microporosity encourages liquid water retention. It is known that catalyst support type has a profound effect on electrode porosity, influencing both micro- and mesoporosity [3, 4]. By constructing electrodes with layers of different carbon supported catalyst types, we demonstrate that we can create porosity gradients in the CLs that vary the electrode water management properties and the power of the PEMFC. Two different types of commercial platinum/carbon electrocatalysts are used in dual cathode CLs – 40 wt. % Pt on Vulcan carbon (Pt/VC) having low micropores and low porosity and 40 wt. % Pt on Ketjen black (Pt/KB) having large micropores and high porosity. CLs are created with both homogeneous porosity in the Z direction (Figure 1a), and compared to ones with non-uniform porosity across the Z-direction (Figure 1b). The microstructure of these cathode CLs is characterized using N2-sorption porosimetry. The CLs are assembled into PEMFCs and probed with polarization curves (at 100, 50 and 25% RH), cyclic voltammetry, O2 gain, electrochemical impedance spectroscopy, and limiting current measurements to quantify the sources of mass transport resistance. The results indicate that the regions with low microporosity encourage liquid water retention, while high microporosity encourages water evaporation. These countering actions are balanced for high CL hydration and gas diffusion, and better PEMFC performance. References [1] Y. Garsany, R.W. Atkinson, M.B. Sassin, R.M.E. Hjelm, B.D. Gould, K.E. Swider-Lyons, J. Electrochem. Soc., 165 (2018) F381-F391. [2] M. Eikerling, J. Electrochem. Soc., 153 (2006) E58-E70. [3] T. Soboleva, K. Malek, Z. Xie, T. Navessin, S. Holdcroft, ACS Appl. Mater. Interfaces, 3 (2011) 1827-1837. [4] Y.-C. Park, H. Tokiwa, K. Kakinuma, M. Watanabe, M. Uchida, Journal of Power Sources, 315 (2016) 179-191. Figure 1
- 12 August 2019
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 166 (13) , F926-F934
Influence of Gas Diffusion Media Compression on Open-Cathode Fuel Cells
- 12 August 2019
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 166 (13) , F926-F934
Influence of Gas Diffusion Media Compression on Open-Cathode Fuel Cells
- 8 September 2018
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 165 (11) , F1002-F1011
Influence of Cathode Gas Diffusion Media Porosity on Open-Cathode Fuel Cells
We investigate the effect of gas diffusion media (GDM) porosity on open-cathode fuel cell operation in challenging ambient air conditions known to exacerbate either cell dehydration or liquid water saturation. A less porous cathode GDM improves cell contact that decreases interfacial contact resistances. We relate structural properties of the cathode GDM to heat rejection, oxygen transport, and water management in the open-cathode fuel cell using polarization behavior and electrochemical impedance spectroscopy. Less porous cathode GDM reduce the measured cell temperature at the cathode surface and decrease ohmic resistance by >33% at 0.6 V, increasing current density from 0.197 to 0.299 mA cm−2. Small decreases in cathode GDM porosity considerably improve thermal management, cell hydration, cathode charge transfer, and decrease ohmic resistance, increasing current density and power production despite concomitant increases in mass transport resistance.
- 8 September 2018
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 165 (11) , F1002-F1011
Influence of Cathode Gas Diffusion Media Porosity on Open-Cathode Fuel Cells
We investigate the effect of gas diffusion media (GDM) porosity on open-cathode fuel cell operation in challenging ambient air conditions known to exacerbate either cell dehydration or liquid water saturation. A less porous cathode GDM improves cell contact that decreases interfacial contact resistances. We relate structural properties of the cathode GDM to heat rejection, oxygen transport, and water management in the open-cathode fuel cell using polarization behavior and electrochemical impedance spectroscopy. Less porous cathode GDM reduce the measured cell temperature at the cathode surface and decrease ohmic resistance by >33% at 0.6 V, increasing current density from 0.197 to 0.299 mA cm−2. Small decreases in cathode GDM porosity considerably improve thermal management, cell hydration, cathode charge transfer, and decrease ohmic resistance, increasing current density and power production despite concomitant increases in mass transport resistance.
- Open Access
- 15 March 2018
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 165 (5) , F381-F391
Improving PEMFC Performance Using Short-Side-Chain Low-Equivalent-Weight PFSA Ionomer in the Cathode Catalyst Layer
Incorporation of short-side chain (SSC) ionomers in the catalyst layers (CL) of proton exchange membrane fuel cells (PEMFCs) can improve performance, particularly at low relative humidities. We attempt to understand this effect by comparing PEMFCs with cathode CLs containing Pt on carbon-black (CB) and either SSC Aquivion ionomer or a standard long-side-chain (LSC) Nafion ionomer at 50% and 100% RH. The CL microstructures are characterized for their micro- and mesoporosity. The CLs are formed into PEMFCs and probed with polarization curves, cyclic voltammetry, O2 gain, limiting current measurements, and electrochemical impedance spectroscopy. PEMFCs containing the SSC ionomer in the cathode CL have superior polarization curves compared to those containing the LSC ionomer in the mass transport region under all conditions. We find that the SSC ionomer imparts lower proton transport resistances, lower charge transfer resistance to the cathode near 0.60 V, and lower mass transport resistance at 0.40 V. We attribute some of the performance improvements to the superior proton conductivity of the SSC ionomer, and the remainder to the higher micropore volume in the SSC-containing CLs which can more effectively evaporate water to the gas phase, improving both the availability of catalyst sites for charge transfer and mesopores for gas transport.
- 15 March 2018
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 165 (5) , F381-F391
Open AccessImproving PEMFC Performance Using Short-Side-Chain Low-Equivalent-Weight PFSA Ionomer in the Cathode Catalyst Layer
Incorporation of short-side chain (SSC) ionomers in the catalyst layers (CL) of proton exchange membrane fuel cells (PEMFCs) can improve performance, particularly at low relative humidities. We attempt to understand this effect by comparing PEMFCs with cathode CLs containing Pt on carbon-black (CB) and either SSC Aquivion ionomer or a standard long-side-chain (LSC) Nafion ionomer at 50% and 100% RH. The CL microstructures are characterized for their micro- and mesoporosity. The CLs are formed into PEMFCs and probed with polarization curves, cyclic voltammetry, O2 gain, limiting current measurements, and electrochemical impedance spectroscopy. PEMFCs containing the SSC ionomer in the cathode CL have superior polarization curves compared to those containing the LSC ionomer in the mass transport region under all conditions. We find that the SSC ionomer imparts lower proton transport resistances, lower charge transfer resistance to the cathode near 0.60 V, and lower mass transport resistance at 0.40 V. We attribute some of the performance improvements to the superior proton conductivity of the SSC ionomer, and the remainder to the higher micropore volume in the SSC-containing CLs which can more effectively evaporate water to the gas phase, improving both the availability of catalyst sites for charge transfer and mesopores for gas transport.
- 1 September 2016
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2016-02 (38) , 2565
Laboratory-Scale Method for Fabricating High Performance Catalyst-Coated Membranes and Membrane Electrode Assemblies
Laboratory-made membrane electrode assemblies (MEAs) for proton exchange membrane fuel cells typically perform poorly compared to commercial ones. A key issue is the difficulty with making a high performance catalyst coated membranes (CCMs) at the laboratory scale by unautomated processes that often leads to irreproducible results due to lack of control of important parameters in the catalyst layer (CL). We have developed a method to fabricate reproducible CCMs with high activity using direct ultrasonic spray deposition of electrocatalysts onto a heated commercial perfluorosulfonic membrane. The CCMs are optimized by varying the number of catalyst layers sprayed, the height of spay nozzle from the membrane, and the pressure used for hot pressing on CLs after spraying. Nitrogen adsorption and scanning electron microscopy (SEM) are used to investigate the effects of ionomer/carbon ratio (I/C) on the surface area, pore structure and morphology of the CLs. How the CCMs are assembled into MEAs is another key issue in the fuel cell performance, particularly the compression, which governs the porosity of the CL and gas diffusion media and resistance. The resulting MEAs are analyzed by I-V polarization, cyclic voltammetry and electrochemical impedance spectroscopy. A comparative study is also made with CCMs prepared with low equivalent weight Nafion ionomer in the CLs. Operating the cell at 80°C and 50 % RH, a cell voltage of 0.6 V a current density of 971 ± 41mA cm-2 is achieved in Air/H2 at a stoichiometric ratio of 2/2 at ambient pressure and increased to 1432 ± 131 mA cm-2 at a back pressure of 150 KPa. These tools can be used to guide the laboratory development and understanding of new catalyst layer structures and catalyst compositions.
- 1 September 2016
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2016-02 (38) , 2565
Laboratory-Scale Method for Fabricating High Performance Catalyst-Coated Membranes and Membrane Electrode Assemblies
Laboratory-made membrane electrode assemblies (MEAs) for proton exchange membrane fuel cells typically perform poorly compared to commercial ones. A key issue is the difficulty with making a high performance catalyst coated membranes (CCMs) at the laboratory scale by unautomated processes that often leads to irreproducible results due to lack of control of important parameters in the catalyst layer (CL). We have developed a method to fabricate reproducible CCMs with high activity using direct ultrasonic spray deposition of electrocatalysts onto a heated commercial perfluorosulfonic membrane. The CCMs are optimized by varying the number of catalyst layers sprayed, the height of spay nozzle from the membrane, and the pressure used for hot pressing on CLs after spraying. Nitrogen adsorption and scanning electron microscopy (SEM) are used to investigate the effects of ionomer/carbon ratio (I/C) on the surface area, pore structure and morphology of the CLs. How the CCMs are assembled into MEAs is another key issue in the fuel cell performance, particularly the compression, which governs the porosity of the CL and gas diffusion media and resistance. The resulting MEAs are analyzed by I-V polarization, cyclic voltammetry and electrochemical impedance spectroscopy. A comparative study is also made with CCMs prepared with low equivalent weight Nafion ionomer in the CLs. Operating the cell at 80°C and 50 % RH, a cell voltage of 0.6 V a current density of 971 ± 41mA cm-2 is achieved in Air/H2 at a stoichiometric ratio of 2/2 at ambient pressure and increased to 1432 ± 131 mA cm-2 at a back pressure of 150 KPa. These tools can be used to guide the laboratory development and understanding of new catalyst layer structures and catalyst compositions.
- 18 August 2014
- Published by The Electrochemical Society in ECS Transactions
- Vol. 64 (3) , 935-944
Performance of 3D-Printed Fuel Cells and Stacks
Additive manufacturing (AM) is being touted as a possible tool for rapid prototyping fuel cell bipolar plate (BPP) designs. We use the AM method of direct metal laser sintering (DMLS) to make 21 cm2 titanium-alloy BPPs with embedded flow channels. The surface of the BPPs is then polished to the appropriate roughness and coated with a conductive corrosion barrier. The coated BPPs are assembled with the appropriate seals, catalyst coated membranes and gas diffusion layers into a 40-cell stack and tested. The resulting 400 W fuel cell stack power is 20% less than expected because of inadequate flatness of several of the DMLS BPPs as determined by white light profilometry, leading to high contact resistance. While DMLS clearly shows the benefit of being able to make complex flow fields and hollow parts with no welds, more work is needed toward reducing the weight and increasing the flatness of BPPs made by AM.
- 18 August 2014
- Published by The Electrochemical Society in ECS Transactions
- Vol. 64 (3) , 935-944
Performance of 3D-Printed Fuel Cells and Stacks
Additive manufacturing (AM) is being touted as a possible tool for rapid prototyping fuel cell bipolar plate (BPP) designs. We use the AM method of direct metal laser sintering (DMLS) to make 21 cm2 titanium-alloy BPPs with embedded flow channels. The surface of the BPPs is then polished to the appropriate roughness and coated with a conductive corrosion barrier. The coated BPPs are assembled with the appropriate seals, catalyst coated membranes and gas diffusion layers into a 40-cell stack and tested. The resulting 400 W fuel cell stack power is 20% less than expected because of inadequate flatness of several of the DMLS BPPs as determined by white light profilometry, leading to high contact resistance. While DMLS clearly shows the benefit of being able to make complex flow fields and hollow parts with no welds, more work is needed toward reducing the weight and increasing the flatness of BPPs made by AM.
- 18 August 2014
- Published by The Electrochemical Society in ECS Transactions
- Vol. 64 (3) , 793-804
Deactivation and Recovery of Pt/C with Commercial Glycol-Based Coolants in Rotating Disk Electrodes and Membrane Electrode Assemblies
The performance of proton exchange membrane fuel cells (PEMFCs) can degrade when exposed to glycol-based coolants through leaks in seals or cracks in carbon bipolar plates. We study the poisoning of Pt/Carbon electrocatalysts by a glycol (1, 3 propanediol)-based coolant containing an ethoxylated nonylphenol surfactant, and azole- or polyol-based non-ionic corrosion inhibitors both by rotating disk electrode (RDE) voltammetry and in a membrane electrode assembly (MEA) in a fuel cell. There is good agreement between RDE and MEA experiments. The RDE results show that the azole corrosion inhibitor irreversibly deactivates the Pt/Vulcan carbon electrocatalyst, while exposure to all of the other coolant components is reversible. The MEA measurements also show a permanent 30% loss in mass activity after exposure to the azole-containing coolants, and provide the additional insight that repeated coolant exposure causes Pt surface area loss, and thereby permanent performance degradation.
- 18 August 2014
- Published by The Electrochemical Society in ECS Transactions
- Vol. 64 (3) , 793-804
Deactivation and Recovery of Pt/C with Commercial Glycol-Based Coolants in Rotating Disk Electrodes and Membrane Electrode Assemblies
The performance of proton exchange membrane fuel cells (PEMFCs) can degrade when exposed to glycol-based coolants through leaks in seals or cracks in carbon bipolar plates. We study the poisoning of Pt/Carbon electrocatalysts by a glycol (1, 3 propanediol)-based coolant containing an ethoxylated nonylphenol surfactant, and azole- or polyol-based non-ionic corrosion inhibitors both by rotating disk electrode (RDE) voltammetry and in a membrane electrode assembly (MEA) in a fuel cell. There is good agreement between RDE and MEA experiments. The RDE results show that the azole corrosion inhibitor irreversibly deactivates the Pt/Vulcan carbon electrocatalyst, while exposure to all of the other coolant components is reversible. The MEA measurements also show a permanent 30% loss in mass activity after exposure to the azole-containing coolants, and provide the additional insight that repeated coolant exposure causes Pt surface area loss, and thereby permanent performance degradation.
- 5 August 2014
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2014-02 (21) , 1103
Performance of 3D-Printed Fuel Cells and Stacks
3D-printing, a.k.a. additive manufacturing (AM), has become a popular topic in the general public and in industry [1]. There is recent interest in using AM to fabricate fuel cell components because of AMs ability to build metal parts with complex geometries with relatively short lead times [2]. Fuel cell bipolar plates (BPPs) require complex internal passageways for coolant flow fields making them a good candidate for AM. By building one piece BPPs the number of parts, the number of seals and the complexity of assembly can be decreased. We present the performance characteristics of a 400W fuel cell system made with BPPs made of Ti-alloy (Ti-6Al-4V) and built by 3D-printing. The BPPs are made by direct metal laser sintering (DMLS) and are coated by Treadstone Inc. with Au-microdots and a TiO2layer to decrease contact resistance and protect against corrosion. Titanium alloy is examined because of its high strength-to-weight ratio which makes it an ideal material for aerospace applications. This work extends our previous work regarding the contact resistance of 3D-printed metal BPPs to include functional fuel cell stacks [3]. The performance characteristics of single cells and stacks will be discussed in the context of surface finish, flatness, feature tolerance, weight, cell-to-cell variability, scaling and contact resistance. Overall DMLS is an exciting new technique with great promise for future rapid prototyping of BPP designs and many other fuel cell components. However, greater advances in surface finish, feature thinness and flatness are needed before BPPs built by 3D-printing will compete with the traditional machined or formed BPPs. References [1] http://techland.time.com/tag/3d-printing/ (2014) [2] http://energy.gov/eere/articles/doe-announces-webinars-natural-gas-biomass-technologies-additive-manufacturing-fuel. (2014) [3] C. J. Netwall, B. D. Gould, J. A. Rodger, N. J. Nasello, K. E. Swider-Lyons, J. Power Sources, 227, 137 (2013).
- 5 August 2014
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2014-02 (21) , 1103
Performance of 3D-Printed Fuel Cells and Stacks
3D-printing, a.k.a. additive manufacturing (AM), has become a popular topic in the general public and in industry [1]. There is recent interest in using AM to fabricate fuel cell components because of AMs ability to build metal parts with complex geometries with relatively short lead times [2]. Fuel cell bipolar plates (BPPs) require complex internal passageways for coolant flow fields making them a good candidate for AM. By building one piece BPPs the number of parts, the number of seals and the complexity of assembly can be decreased. We present the performance characteristics of a 400W fuel cell system made with BPPs made of Ti-alloy (Ti-6Al-4V) and built by 3D-printing. The BPPs are made by direct metal laser sintering (DMLS) and are coated by Treadstone Inc. with Au-microdots and a TiO2layer to decrease contact resistance and protect against corrosion. Titanium alloy is examined because of its high strength-to-weight ratio which makes it an ideal material for aerospace applications. This work extends our previous work regarding the contact resistance of 3D-printed metal BPPs to include functional fuel cell stacks [3]. The performance characteristics of single cells and stacks will be discussed in the context of surface finish, flatness, feature tolerance, weight, cell-to-cell variability, scaling and contact resistance. Overall DMLS is an exciting new technique with great promise for future rapid prototyping of BPP designs and many other fuel cell components. However, greater advances in surface finish, feature thinness and flatness are needed before BPPs built by 3D-printing will compete with the traditional machined or formed BPPs. References [1] http://techland.time.com/tag/3d-printing/ (2014) [2] http://energy.gov/eere/articles/doe-announces-webinars-natural-gas-biomass-technologies-additive-manufacturing-fuel. (2014) [3] C. J. Netwall, B. D. Gould, J. A. Rodger, N. J. Nasello, K. E. Swider-Lyons, J. Power Sources, 227, 137 (2013).
- 5 August 2014
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2014-02 (21) , 1270
Deactivation and Recovery of Pt/C with Commercial Glycol-Based Coolants in Rotating Disk Electrodes and Membrane Electrode Assemblies
Numerous power applications utilize a coolant loop and radiator to exhaust excess heat to the environment. In a multi-cell stack, coolant is typically circulated through the separating plates of each cell to maintain a uniform temperature distribution across the stack and keep the coolant isolated from the electrocatalyst. If glycol-based coolants contact the catalyst layer in the electrodes, deactivation of Pt active sites is possible leading to the loss of fuel cell performance. Coolant can contact the fuel cell catalyst through faulty sealing, porous materials or improper use. In principle, glycols should not pose a risk to fuel cell electrocatalysts because organic alcohols are easily oxidized from the surface during operation. However, the additives in commercial coolants can be highly active catalyst poisons with varying degrees of reversibility. We present the extent to which coolant materials deactivate commercial carbon–supported Pt nanoparticles (Pt/C) in membrane electrode assemblies (MEAs) in the context of polarization behavior, cyclic voltammetry and rotating disk electrode (RDE) experiments. We have previously developed these methodologies to investigate Pt/C deactivation by SO2 [1,2] and recently applied them to study coolants [3]. The role of different coolant components such as corrosion inhibitors and surfactants will be identified and compared to the base glycol/water coolant. In prior work, RDE showed that azole additives are highly poisonous to the Pt surface, while polyols can be removed from the Pt surface. However, deactivation of RDEs by coolant occurs in excess liquid electrolyte, while in a fuel cell deactivation occurs in an air-coolant mixed phase exposure. The objective of this paper is to compare RDE results to those in a single cell fuel cell. Recovery methods and strategies will be discussed along with the difference between deactivation in the RDE environment versus the fuel cell environment. Figure 1a compares the activity of a pristine MEA to one exposed to a glycol-based coolant with an azole corrosion inhibitor before and after cycling the electrode between 0.07 and 1.2 V in H2/N2, anode/cathode to clean the surface. Figure 1b compares the activity of the pristine MEA compared to one exposed to a glycol-based coolant with a polyol corrosion inhibitor and the activity after cycling the electrode between 0.07 and 1.2 V in H2/N2, anode/cathode. Figure 1a clearly shows that glycol-based coolants with azole corrosion inhibitors are particularly damaging to fuel cell catalytic activity. Even after aggressive recovery procedures the mass activity is 35% less than the pristine material. The azole caused a permanent loss of Pt surface area when examined with cyclic voltammetry. In comparison polyol corrosion inhibitors are not nearly as potent a catalyst poison and can be fully recovered with mild recovery procedures after the 1st exposure. The difference in behavior can be rationalized by the strong coordination between nitrogen and sulfur containing aromatic rings in the azole with the d-bands of the Pt atoms on the surface of the nanoparticles. In contrast, the polyols tend to oxidize off the surface. This work is significant because it confirms that the deleterious coolant components identified by RDE experiments match the results of single cell measurements. This agreement verifies that RDE results for coolant deactivation are scalable to practical fuel cells. Interestingly, coolant exposure to MEAs is more deleterious than for RDEs and can cause greater loss of electrochemical surface area by Pt corrosion, even with benign coolants. References [1] Y. Garsany, O. A. Baturina and K. E. Swider-Lyons, J. Electrochem. Soc., 154, B670 (2007). [2] B. D. Gould, O. A. Baturina and K. E. Swider-Lyons, J. Power Sources, 188, 89 (2009). [3] Y. Garsany, S. Dutta and K. E. Swider-Lyons, J. Power Sources, 216, 515 (2012).
- 5 August 2014
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2014-02 (21) , 1270
Deactivation and Recovery of Pt/C with Commercial Glycol-Based Coolants in Rotating Disk Electrodes and Membrane Electrode Assemblies
Numerous power applications utilize a coolant loop and radiator to exhaust excess heat to the environment. In a multi-cell stack, coolant is typically circulated through the separating plates of each cell to maintain a uniform temperature distribution across the stack and keep the coolant isolated from the electrocatalyst. If glycol-based coolants contact the catalyst layer in the electrodes, deactivation of Pt active sites is possible leading to the loss of fuel cell performance. Coolant can contact the fuel cell catalyst through faulty sealing, porous materials or improper use. In principle, glycols should not pose a risk to fuel cell electrocatalysts because organic alcohols are easily oxidized from the surface during operation. However, the additives in commercial coolants can be highly active catalyst poisons with varying degrees of reversibility. We present the extent to which coolant materials deactivate commercial carbon–supported Pt nanoparticles (Pt/C) in membrane electrode assemblies (MEAs) in the context of polarization behavior, cyclic voltammetry and rotating disk electrode (RDE) experiments. We have previously developed these methodologies to investigate Pt/C deactivation by SO2 [1,2] and recently applied them to study coolants [3]. The role of different coolant components such as corrosion inhibitors and surfactants will be identified and compared to the base glycol/water coolant. In prior work, RDE showed that azole additives are highly poisonous to the Pt surface, while polyols can be removed from the Pt surface. However, deactivation of RDEs by coolant occurs in excess liquid electrolyte, while in a fuel cell deactivation occurs in an air-coolant mixed phase exposure. The objective of this paper is to compare RDE results to those in a single cell fuel cell. Recovery methods and strategies will be discussed along with the difference between deactivation in the RDE environment versus the fuel cell environment. Figure 1a compares the activity of a pristine MEA to one exposed to a glycol-based coolant with an azole corrosion inhibitor before and after cycling the electrode between 0.07 and 1.2 V in H2/N2, anode/cathode to clean the surface. Figure 1b compares the activity of the pristine MEA compared to one exposed to a glycol-based coolant with a polyol corrosion inhibitor and the activity after cycling the electrode between 0.07 and 1.2 V in H2/N2, anode/cathode. Figure 1a clearly shows that glycol-based coolants with azole corrosion inhibitors are particularly damaging to fuel cell catalytic activity. Even after aggressive recovery procedures the mass activity is 35% less than the pristine material. The azole caused a permanent loss of Pt surface area when examined with cyclic voltammetry. In comparison polyol corrosion inhibitors are not nearly as potent a catalyst poison and can be fully recovered with mild recovery procedures after the 1st exposure. The difference in behavior can be rationalized by the strong coordination between nitrogen and sulfur containing aromatic rings in the azole with the d-bands of the Pt atoms on the surface of the nanoparticles. In contrast, the polyols tend to oxidize off the surface. This work is significant because it confirms that the deleterious coolant components identified by RDE experiments match the results of single cell measurements. This agreement verifies that RDE results for coolant deactivation are scalable to practical fuel cells. Interestingly, coolant exposure to MEAs is more deleterious than for RDEs and can cause greater loss of electrochemical surface area by Pt corrosion, even with benign coolants. References [1] Y. Garsany, O. A. Baturina and K. E. Swider-Lyons, J. Electrochem. Soc., 154, B670 (2007). [2] B. D. Gould, O. A. Baturina and K. E. Swider-Lyons, J. Power Sources, 188, 89 (2009). [3] Y. Garsany, S. Dutta and K. E. Swider-Lyons, J. Power Sources, 216, 515 (2012).