Jian Sun
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Jian Sun has a total of 68 co-authors. Here are the top co-authors by number of shared publications:
Y. Li
Department of Materials Science and Engineering Hefei University of Technology HEFEI 230009 PEOPLE'S REPUBLIC OF CHINA
3 shared publicationsY.C. Wu
Department of Materials Science and Engineering Hefei University of Technology Hefei 230009 China
3 shared publications- Weiping Tong
Key Laboratory of Electromagnetic Processing of Materials, Northeastern University, Shenyang, 110819, China
2 shared publications X.C. Zhu
Department of Materials Science and Engineering Hefei University of Technology HEFEI 230009 PEOPLE'S REPUBLIC OF CHINA
2 shared publicationsX.D. Du
Department of Materials Science and Engineering Hefei University of Technology HEFEI 230009 PEOPLE'S REPUBLIC OF CHINA
2 shared publicationsZ. Chen
Department of Materials Science and Engineering Hefei University of Technology Hefei 230009 China
2 shared publications
Latest Publications
- 22 February 2025
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 54 (4) , 3097-3110
A novel W-Cu Thick Film Fabricated on High-Temperature Co-fired Ceramic Substrates Using W-CuO Raw Powder Materials
- 22 February 2025
- Published by Springer Nature in Journal of Electronic Materials
- Vol. 54 (4) , 3097-3110
A novel W-Cu Thick Film Fabricated on High-Temperature Co-fired Ceramic Substrates Using W-CuO Raw Powder Materials
- 1 June 2024
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 55 (6) , 851-863
Microstructure and properties of tungsten‐40 wt.–% copper composites fabricated by binder jet 3D printing
In this work, the tungsten‐copper composites were fabricated by binder jet 3D printing technology. The effects of different printing layer thicknesses (50 μm to 100 μm) on the green density and green strength were investigated. Then, under the optimal layer thickness, the effects of different sintering temperatures (1300 °C to 1600 °C) on the microstructure and densification of tungsten‐40 wt.–% copper composites were studied. The experimental results showed that when the printing layer thickness was set as a lower value (50 μm), the tungsten‐40 wt.–% copper green part had the best strength and its density reached a maximum value of 60.73 %. After sintering for green parts printed with 50 μm layer thickness, the relative density, thermal conductivity and electrical conductivity of sintered parts first increased and then decreased with increasing sintering temperature. In our experiments, the tungsten‐40 wt.–% copper sample fabricated by binder jet 3D printing with a printing layer thickness of 50 μm under a sintering temperature of 1500 °C displayed the best properties, in which the relative density, thermal conductivity and electrical conductivity were 97.04 %, 228 W⋅m−1⋅K−1 and 46.5 % IACS, respectively.
- 1 June 2024
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 55 (6) , 851-863
Microstructure and properties of tungsten‐40 wt.–% copper composites fabricated by binder jet 3D printing
In this work, the tungsten‐copper composites were fabricated by binder jet 3D printing technology. The effects of different printing layer thicknesses (50 μm to 100 μm) on the green density and green strength were investigated. Then, under the optimal layer thickness, the effects of different sintering temperatures (1300 °C to 1600 °C) on the microstructure and densification of tungsten‐40 wt.–% copper composites were studied. The experimental results showed that when the printing layer thickness was set as a lower value (50 μm), the tungsten‐40 wt.–% copper green part had the best strength and its density reached a maximum value of 60.73 %. After sintering for green parts printed with 50 μm layer thickness, the relative density, thermal conductivity and electrical conductivity of sintered parts first increased and then decreased with increasing sintering temperature. In our experiments, the tungsten‐40 wt.–% copper sample fabricated by binder jet 3D printing with a printing layer thickness of 50 μm under a sintering temperature of 1500 °C displayed the best properties, in which the relative density, thermal conductivity and electrical conductivity were 97.04 %, 228 W⋅m−1⋅K−1 and 46.5 % IACS, respectively.
- 16 December 2022
- Published by Wiley in Advanced Engineering Materials
- Vol. 25 (9)
Fabrication of Ti–N and Ti–Al–N Coatings on Mg–Li Alloy by Surface Mechanical Nanoalloying Treatment under Nitrogen Atmosphere at Room Temperature
Ti–N and Ti–Al–N coatings are fabricated on LZ91 Mg–Li alloy by surface mechanical nanoalloying treatment (SMNAT) in nitrogen atmosphere at room temperature. This method is proposed to improve the high cost and high treatment temperature of preparing nitride coatings on Mg–Li alloys. The microstructure, phase compositions, and hardness of coatings are investigated systematically. Results show that Ti–N coating containing α‐Ti, β‐Ti, TiN0.3 and TiN0.9 phases can be prepared by SMNAT with pure titanium powder at room temperature under nitrogen atmosphere. The structure of Ti–N coating is a mixture of nanocrystalline and amorphous. The surface microhardness of Ti–N coating is 566.8 HV, which is about 80 HV higher than that of Ti coating obtained in argon atmosphere. By adding of the aluminum powders, a Ti–Al–N composite coating composed of nitrides (Ti3Al2N2, Ti2AlN, TiN0.76, and AlN) and intermetallics (Al11Ti5 and Al2Ti) is formed. The surface microhardness of Ti–Al–N composite coating reaches 743.2 HV, which is about 165.4 HV higher than that of Ti–Al coating obtained in argon atmosphere. Additionally, the continuity and uniformity of Ti–Al–N composite coating is improved due to which the Al powders can be seen as the bonding agent during SMNAT.
- 16 December 2022
- Published by Wiley in Advanced Engineering Materials
- Vol. 25 (9)
Fabrication of Ti–N and Ti–Al–N Coatings on Mg–Li Alloy by Surface Mechanical Nanoalloying Treatment under Nitrogen Atmosphere at Room Temperature
Ti–N and Ti–Al–N coatings are fabricated on LZ91 Mg–Li alloy by surface mechanical nanoalloying treatment (SMNAT) in nitrogen atmosphere at room temperature. This method is proposed to improve the high cost and high treatment temperature of preparing nitride coatings on Mg–Li alloys. The microstructure, phase compositions, and hardness of coatings are investigated systematically. Results show that Ti–N coating containing α‐Ti, β‐Ti, TiN0.3 and TiN0.9 phases can be prepared by SMNAT with pure titanium powder at room temperature under nitrogen atmosphere. The structure of Ti–N coating is a mixture of nanocrystalline and amorphous. The surface microhardness of Ti–N coating is 566.8 HV, which is about 80 HV higher than that of Ti coating obtained in argon atmosphere. By adding of the aluminum powders, a Ti–Al–N composite coating composed of nitrides (Ti3Al2N2, Ti2AlN, TiN0.76, and AlN) and intermetallics (Al11Ti5 and Al2Ti) is formed. The surface microhardness of Ti–Al–N composite coating reaches 743.2 HV, which is about 165.4 HV higher than that of Ti–Al coating obtained in argon atmosphere. Additionally, the continuity and uniformity of Ti–Al–N composite coating is improved due to which the Al powders can be seen as the bonding agent during SMNAT.
- 1 November 2021
- Published by Walter de Gruyter GmbH in International Journal of Materials Research
- Vol. 112 (11) , 910-917
Improved in-vitro biocompatibility of LZ91 Mg–Li alloy by formation of nanostructured Ti coating through surface mechanical nano-alloying treatment
Surface mechanical nano-alloying treatment (SMNAT) was employed to fabricate a nanostructured Ti coating on LZ91 Mg–Li alloy. Microstructure, surface hardness and in-vitro biocompatibility of the Ti-coated sample were investigated in comparison with those of an untreated sample. Experimental results showed that a nanostructured Ti coating with a thickness of 35 to 60 μm was formed after SMNAT for 2 h. The average grain size in the top surface of the Ti coating was about 30 nm. The surface of the Ti coating is rougher than that of the untreated LZ91 sample, in which the values of Ra, Rq and Rz were 7.83, 9.57 and 14.85 μm, respectively. The hardness of the Ti coating top surface was about 483 HV. Cell proliferation and differentiation on Ti coated samples were enhanced relative to those on the untreated samples.
- 1 November 2021
- Published by Walter de Gruyter GmbH in International Journal of Materials Research
- Vol. 112 (11) , 910-917
Improved in-vitro biocompatibility of LZ91 Mg–Li alloy by formation of nanostructured Ti coating through surface mechanical nano-alloying treatment
Surface mechanical nano-alloying treatment (SMNAT) was employed to fabricate a nanostructured Ti coating on LZ91 Mg–Li alloy. Microstructure, surface hardness and in-vitro biocompatibility of the Ti-coated sample were investigated in comparison with those of an untreated sample. Experimental results showed that a nanostructured Ti coating with a thickness of 35 to 60 μm was formed after SMNAT for 2 h. The average grain size in the top surface of the Ti coating was about 30 nm. The surface of the Ti coating is rougher than that of the untreated LZ91 sample, in which the values of Ra, Rq and Rz were 7.83, 9.57 and 14.85 μm, respectively. The hardness of the Ti coating top surface was about 483 HV. Cell proliferation and differentiation on Ti coated samples were enhanced relative to those on the untreated samples.
- 14 May 2021
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 52 (5) , 503-510
Effects of process parameters on the microstructure of iron coating fabricated on pure aluminum by immersion plating
In this paper, an iron coating was designed to fabricate on the surface layer of pure aluminum. The effects of process parameters such as immersion plating method, durations and temperatures on the microstructure of iron coating were studied systematically. The experimental results showed that the quality of the iron coating fabricated on the sample by one‐step immersion plating is better than that obtained by two‐step immersion plating. The iron coating obtained by one‐step immersion plating for 1 min is continuous and without obvious gaps and cavities. With the immersion time increased to 3 min and 5 min, the coating is uneven and easy to fall off from the surface of sample. Additionally, due to that the higher temperature increases the efficiency of displacement reaction, the quality of the coating obtained at 40 °C is better than that obtained at 55 °C and 65 °C. Consequently, the optimal immersion plating parameters were one‐step immersion plating, 1 min, and 40 °C. This paper provides a novel method to prepare an iron coating as a pretreatment for electroplating of aluminum.
- 14 May 2021
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 52 (5) , 503-510
Effects of process parameters on the microstructure of iron coating fabricated on pure aluminum by immersion plating
In this paper, an iron coating was designed to fabricate on the surface layer of pure aluminum. The effects of process parameters such as immersion plating method, durations and temperatures on the microstructure of iron coating were studied systematically. The experimental results showed that the quality of the iron coating fabricated on the sample by one‐step immersion plating is better than that obtained by two‐step immersion plating. The iron coating obtained by one‐step immersion plating for 1 min is continuous and without obvious gaps and cavities. With the immersion time increased to 3 min and 5 min, the coating is uneven and easy to fall off from the surface of sample. Additionally, due to that the higher temperature increases the efficiency of displacement reaction, the quality of the coating obtained at 40 °C is better than that obtained at 55 °C and 65 °C. Consequently, the optimal immersion plating parameters were one‐step immersion plating, 1 min, and 40 °C. This paper provides a novel method to prepare an iron coating as a pretreatment for electroplating of aluminum.
- 10 November 2020
- Published by SAGE Publications in Surface Engineering
- Vol. 37 (9) , 1075-1083
Nitriding behaviour of Mg-Li alloy with surface mechanical nano-alloying pretreatment
The thick titanium nitrides coating was fabricated on LZ91 alloy by surface mechanical nano-alloying (SMNAT) combined with gas nitriding. Experimental results showed that a nanostructured titanium coating with thickness of 50–80 μm was formed on surface of LZ91 alloy by SMNAT with pure titanium powders for 30 min. By adding of the aluminium powders into titanium powders during the SMNAT, a thicker Ti-Al composite coating with improved continuity and uniformity was obtained. After nitriding at 450°C, the whole Ti and Ti-Al coating were successfully nitrided. The surface layer of nitrided Ti coated sample is mainly composed of TiN, Ti2N, TiN0.3, TiN0.61 and Ti4N2.33 phases and the surface layer of nitrided Ti-Al coated sample is composed of Ti2N, TiN0.9, TiN0.3, Ti4N2.33, AlN, Ti3Al2N2 and AlTi2N phases. The hardness measurements demonstrated that the surface hardness of nitrided Ti coated and nitrided Ti-Al coated samples reached to 634 and 734 HV, respectively.
- 10 November 2020
- Published by SAGE Publications in Surface Engineering
- Vol. 37 (9) , 1075-1083
Nitriding behaviour of Mg-Li alloy with surface mechanical nano-alloying pretreatment
The thick titanium nitrides coating was fabricated on LZ91 alloy by surface mechanical nano-alloying (SMNAT) combined with gas nitriding. Experimental results showed that a nanostructured titanium coating with thickness of 50–80 μm was formed on surface of LZ91 alloy by SMNAT with pure titanium powders for 30 min. By adding of the aluminium powders into titanium powders during the SMNAT, a thicker Ti-Al composite coating with improved continuity and uniformity was obtained. After nitriding at 450°C, the whole Ti and Ti-Al coating were successfully nitrided. The surface layer of nitrided Ti coated sample is mainly composed of TiN, Ti2N, TiN0.3, TiN0.61 and Ti4N2.33 phases and the surface layer of nitrided Ti-Al coated sample is composed of Ti2N, TiN0.9, TiN0.3, Ti4N2.33, AlN, Ti3Al2N2 and AlTi2N phases. The hardness measurements demonstrated that the surface hardness of nitrided Ti coated and nitrided Ti-Al coated samples reached to 634 and 734 HV, respectively.
- 20 July 2020
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 51 (7) , 938-947
Effects of aluminum content and mechanical nano‐alloying time on the preparation of titanium‐aluminum composite coatings on magnesium‐lithium alloy
A titanium‐aluminum composite coating was successfully fabricated on magnesium‐lithium alloy substrate by mechanical nano‐alloying treatment (SMNAT). The effects of aluminum content and mechanical nano‐alloying time on the microstructure and properties of titanium‐aluminum composite coatings were investigated. The experimental results showed that the ratio of titanium‐aluminum powder has a significant effect on the preparation of the coating. Low aluminum content and high aluminum content in the mixture powder resulted in the formation of the coatings with inhomogeneous thickness. The titanium‐aluminum ratio of 3 : 1 was considered to be optimal for fabricating the coating with homogeneous thickness under the selected milling parameters. The hardness of top surface layer on titanium‐ aluminum coatings decreased from 292.0 HV 0.01 to 121.4 HV 0.01 with the increase of aluminum content. Additionally, the prolongation of treatment time facilitated to increase the thickness and density of the coatings, resulting to enhance their hardness and corrosion resistance.
- 20 July 2020
- Published by Wiley in Materialwissenschaft und Werkstofftechnik
- Vol. 51 (7) , 938-947
Effects of aluminum content and mechanical nano‐alloying time on the preparation of titanium‐aluminum composite coatings on magnesium‐lithium alloy
A titanium‐aluminum composite coating was successfully fabricated on magnesium‐lithium alloy substrate by mechanical nano‐alloying treatment (SMNAT). The effects of aluminum content and mechanical nano‐alloying time on the microstructure and properties of titanium‐aluminum composite coatings were investigated. The experimental results showed that the ratio of titanium‐aluminum powder has a significant effect on the preparation of the coating. Low aluminum content and high aluminum content in the mixture powder resulted in the formation of the coatings with inhomogeneous thickness. The titanium‐aluminum ratio of 3 : 1 was considered to be optimal for fabricating the coating with homogeneous thickness under the selected milling parameters. The hardness of top surface layer on titanium‐ aluminum coatings decreased from 292.0 HV 0.01 to 121.4 HV 0.01 with the increase of aluminum content. Additionally, the prolongation of treatment time facilitated to increase the thickness and density of the coatings, resulting to enhance their hardness and corrosion resistance.
- 2 October 2019
- Published by Springer Nature
- p. 1298-1310
Design and Field Application of a Composite Microbial Flooding Process for a High-Water-Content Oilfield
- 2 October 2019
- Published by Springer Nature
- p. 1298-1310
Design and Field Application of a Composite Microbial Flooding Process for a High-Water-Content Oilfield
- 9 September 2019
- Published by Springer Nature in Journal of Materials Science
- Vol. 55 (2) , 688-700
Hierarchical NiCo2O4/MnO2 core–shell nanosheets arrays for flexible asymmetric supercapacitor
- 9 September 2019
- Published by Springer Nature in Journal of Materials Science
- Vol. 55 (2) , 688-700
Hierarchical NiCo2O4/MnO2 core–shell nanosheets arrays for flexible asymmetric supercapacitor
- 23 July 2019
- Published by Wiley in Advanced Engineering Materials
- Vol. 21 (10) , 1900359
Two‐Step Nitriding Behavior of Pure Iron with a Nanostructured Surface Layer
A two‐step gas nitriding treatment (280 °C for 2 h plus 550 °C for 6 h) is designed for pure iron with a nanostructured surface layer induced by surface mechanical attrition treatment (SMAT). The microstructure and surface properties of the SMAT sample after two‐step nitriding treatment are investigated in comparison with those of the SMAT sample after single‐step nitriding treatment (550 °C for 6 h). Experimental results show that a much thicker compound layer (up to 25 μm in thickness) is generated on the surface of the SMAT sample after two‐step nitriding treatment, in which the mean grain size of the Fe2‐3N phase is below 25 nm. The enhanced nitriding kinetic may be attributed to the formation of a large number of Fe(N) solid solutions and a small amount of dispersed Fe2‐3N particles on the SMAT sample after first low‐temperature nitriding, which enhances the thermal stability of nanostructured iron grains. Due to the enhanced nitriding kinetic and refined nitride structure, the SMAT sample after two‐step nitriding treatment displays higher surface hardness and improved wear resistance relative to its single‐step nitrided counterpart.
- 23 July 2019
- Published by Wiley in Advanced Engineering Materials
- Vol. 21 (10) , 1900359
Two‐Step Nitriding Behavior of Pure Iron with a Nanostructured Surface Layer
A two‐step gas nitriding treatment (280 °C for 2 h plus 550 °C for 6 h) is designed for pure iron with a nanostructured surface layer induced by surface mechanical attrition treatment (SMAT). The microstructure and surface properties of the SMAT sample after two‐step nitriding treatment are investigated in comparison with those of the SMAT sample after single‐step nitriding treatment (550 °C for 6 h). Experimental results show that a much thicker compound layer (up to 25 μm in thickness) is generated on the surface of the SMAT sample after two‐step nitriding treatment, in which the mean grain size of the Fe2‐3N phase is below 25 nm. The enhanced nitriding kinetic may be attributed to the formation of a large number of Fe(N) solid solutions and a small amount of dispersed Fe2‐3N particles on the SMAT sample after first low‐temperature nitriding, which enhances the thermal stability of nanostructured iron grains. Due to the enhanced nitriding kinetic and refined nitride structure, the SMAT sample after two‐step nitriding treatment displays higher surface hardness and improved wear resistance relative to its single‐step nitrided counterpart.