Shuai Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Shuai Wang has a total of 31 co-authors. Here are the top co-authors by number of shared publications:
Pengfei Xing
Department of New Energy Science and Engineering School of Metallurgy Northeastern University Shenyang P. R. China
6 shared publications- Yanxin Zhuang
Key Laboratory of Electromagnetic Processing of Materials (Ministry of Education), Northeastern University, Shenyang, China
3 shared publications Haojie Wei
School of Metallurgy Northeastern University Shenyang Liaoning Province P. R. China
2 shared publications- Pengfei Xing
School of Metallurgy, Northeastern University, Shenyang, China
2 shared publications - Shuaibo Gao
School of Resource and Environmental Science, Wuhan University, 299 Bayi Road, Wuchang District, Wuhan 430072, P. R. China
2 shared publications Yanxin Zhuang
Key Laboratory of Electromagnetic Processing of Materials (Ministry of Education), Northeastern University, Shenyang, 110819, China; School of Material Science and Engineering, Northeastern University, Shenyang, 110819, China
2 shared publications
Latest Publications
- Open Access
Effects of Cerium on the Mechanical Properties of Al–20Si Alloy
The chemical modification of Al–20Si alloy in the case of incorporation of rare earth cerium (Ce) is investigated in this study, focusing on the resulting microstructure evolution and changes in mechanical properties and hardness before and after cerium modification. The microstructure of the cerium-modified alloy is composed of the aluminum matrix, eutectic silicon, and primary silicon phases, as well as the Al2Si2Ce phase, a cerium-containing solid solution, and the α-Al11Ce3 phase. It is worth noting that this study reports for the first time an unusual phenomenon in which the addition of cerium raises tensile strength of the alloy while concurrently decreasing its surface hardness. The increase in tensile strength is mainly ascribed to the refinement of primary silicon. On the contrary, the reduction of hardness is explained by the competition between Ce-induced toughening and solid solution strengthening, as well as the generation of the relatively soft α-Al11Ce3 phase. Mechanical properties at room temperature show that the greatest tensile strength of 153 ± 7 MPa is reached at a cerium concentration of 0.7 wt.%, while the corresponding elongation of the mechanical specimen is 1.36 ± 0.287. The fracture mechanism changes from cleavage fracture in the unmodified alloy to ductile fracture after Ce addition.
Open AccessEffects of Cerium on the Mechanical Properties of Al–20Si Alloy
The chemical modification of Al–20Si alloy in the case of incorporation of rare earth cerium (Ce) is investigated in this study, focusing on the resulting microstructure evolution and changes in mechanical properties and hardness before and after cerium modification. The microstructure of the cerium-modified alloy is composed of the aluminum matrix, eutectic silicon, and primary silicon phases, as well as the Al2Si2Ce phase, a cerium-containing solid solution, and the α-Al11Ce3 phase. It is worth noting that this study reports for the first time an unusual phenomenon in which the addition of cerium raises tensile strength of the alloy while concurrently decreasing its surface hardness. The increase in tensile strength is mainly ascribed to the refinement of primary silicon. On the contrary, the reduction of hardness is explained by the competition between Ce-induced toughening and solid solution strengthening, as well as the generation of the relatively soft α-Al11Ce3 phase. Mechanical properties at room temperature show that the greatest tensile strength of 153 ± 7 MPa is reached at a cerium concentration of 0.7 wt.%, while the corresponding elongation of the mechanical specimen is 1.36 ± 0.287. The fracture mechanism changes from cleavage fracture in the unmodified alloy to ductile fracture after Ce addition.
- 14 March 2025
- Published by Royal Society of Chemistry (RSC) in Reaction Chemistry & Engineering
- Vol. 10 (6) , 1378-1385
Is it reliable to determine the stoichiometry of extraction complexes using the classic slope analysis model in acidic extraction systems?
The applicability and reliability of the classic slope analysis model for determining the stoichiometry of extraction complexes in acidic extraction systems need to be re-reviewed.
- 14 March 2025
- Published by Royal Society of Chemistry (RSC) in Reaction Chemistry & Engineering
- Vol. 10 (6) , 1378-1385
Is it reliable to determine the stoichiometry of extraction complexes using the classic slope analysis model in acidic extraction systems?
The applicability and reliability of the classic slope analysis model for determining the stoichiometry of extraction complexes in acidic extraction systems need to be re-reviewed.
- 26 December 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (3)
Recycling boron carbide dust waste for preparing high‐performance ceramics by hot‐pressed sintering
B 4 C dust waste causes environmental pollution and is difficult to be recycled. This paper proposes a method of recycling B 4 C dust waste to fabricate high‐performance ceramics via the processes of raw material treatment and hot pressing. The characteristics of B 4 C dust waste are analyzed and the existing states of the impurities are detected. Dust wastes, removed different impurities via different processes, are simultaneously hot pressed at 2050°C for 15 min under 20 MPa pressure, and the microstructure and mechanical property of the fabricated ceramics are detected and compared. Results indicate that the particle size of dust waste is fine (2.7 µm), and the impurities B 2 O 3 /H 3 BO 3 , Fe, and BN exist in dust waste. The mechanical properties of the ceramics fabricated with dust wastes treated via different methods are similar or even superior to those of the commercial ceramics, and among them, the ceramics fabricated with the dust waste removed oxygen with ethanol show the excellent comprehensive performance, of which the hardness, flexural strength, and fractural toughness reach 30.78 GPa, 410 MPa, 4.3 MPa m 1/2 , respectively. Removing oxygen of dust waste can effectively enhance the densification, and the impurity Fe can also improve the densification owing to the formed low‐melting‐point FeB from the reaction between Fe and boron carbide in the dust waste. The pullout of FeB, BN particles, and the loosening area induced by residual stress of FeB contributes to the promotion of fracture toughness. This paper proves the feasibility of preparing high‐performance ceramics with B 4 C dust waste and lays a theoretical and practical foundation for the recycling and value‐added reuse of B 4 C dust waste, and for the low‐cost preparing of high‐performance B 4 C ceramics.
- 26 December 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (3)
Recycling boron carbide dust waste for preparing high‐performance ceramics by hot‐pressed sintering
B 4 C dust waste causes environmental pollution and is difficult to be recycled. This paper proposes a method of recycling B 4 C dust waste to fabricate high‐performance ceramics via the processes of raw material treatment and hot pressing. The characteristics of B 4 C dust waste are analyzed and the existing states of the impurities are detected. Dust wastes, removed different impurities via different processes, are simultaneously hot pressed at 2050°C for 15 min under 20 MPa pressure, and the microstructure and mechanical property of the fabricated ceramics are detected and compared. Results indicate that the particle size of dust waste is fine (2.7 µm), and the impurities B 2 O 3 /H 3 BO 3 , Fe, and BN exist in dust waste. The mechanical properties of the ceramics fabricated with dust wastes treated via different methods are similar or even superior to those of the commercial ceramics, and among them, the ceramics fabricated with the dust waste removed oxygen with ethanol show the excellent comprehensive performance, of which the hardness, flexural strength, and fractural toughness reach 30.78 GPa, 410 MPa, 4.3 MPa m 1/2 , respectively. Removing oxygen of dust waste can effectively enhance the densification, and the impurity Fe can also improve the densification owing to the formed low‐melting‐point FeB from the reaction between Fe and boron carbide in the dust waste. The pullout of FeB, BN particles, and the loosening area induced by residual stress of FeB contributes to the promotion of fracture toughness. This paper proves the feasibility of preparing high‐performance ceramics with B 4 C dust waste and lays a theoretical and practical foundation for the recycling and value‐added reuse of B 4 C dust waste, and for the low‐cost preparing of high‐performance B 4 C ceramics.
- 26 December 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (3)
Synergistically reinforced boron carbide ceramics by introduction of Fe and BN
Boron carbide (B 4 C)‐FeB ceramics and B 4 C‐FeB‐BN ceramics are prepared via hot pressing with B 4 C plus different contents of iron (Fe) and B 4 C plus 5 wt% Fe and different contents of boron nitride (BN), respectively. The phase composition, microstructure, and mechanical properties of the prepared ceramics are studied in detail. The synergistic effect of Fe and BN on hot‐pressed B 4 C ceramics is discussed. Results indicate that Fe can react with B 4 C to form FeB, and enhance the densification and mechanical property of B 4 C ceramics. 5 wt% Fe is the optimal addition amount. Fe and BN can synergistically reinforce B 4 C ceramics. The ceramics fabricated with B 4 C‐5 wt% Fe‐4 wt% BN have the optimal comprehensive performance, of which the relative density, hardness, flexural strength, and fracture toughness reach 98.5%, 32.74 GPa, 668.92 MPa, and 4.09 MPa·m 1/2 , respectively, higher than those of the ceramics fabricated with B 4 C or with B 4 C plus Fe. The liquid formed by Fe during sintering enhances the dispersion of BN, which is beneficial to realizing the function of pinning grain boundary and pulling out. The toughening phenomena include intergranular and transgranular fracture, particle pulling out, and bridging.
- 26 December 2024
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 22 (3)
Synergistically reinforced boron carbide ceramics by introduction of Fe and BN
Boron carbide (B 4 C)‐FeB ceramics and B 4 C‐FeB‐BN ceramics are prepared via hot pressing with B 4 C plus different contents of iron (Fe) and B 4 C plus 5 wt% Fe and different contents of boron nitride (BN), respectively. The phase composition, microstructure, and mechanical properties of the prepared ceramics are studied in detail. The synergistic effect of Fe and BN on hot‐pressed B 4 C ceramics is discussed. Results indicate that Fe can react with B 4 C to form FeB, and enhance the densification and mechanical property of B 4 C ceramics. 5 wt% Fe is the optimal addition amount. Fe and BN can synergistically reinforce B 4 C ceramics. The ceramics fabricated with B 4 C‐5 wt% Fe‐4 wt% BN have the optimal comprehensive performance, of which the relative density, hardness, flexural strength, and fracture toughness reach 98.5%, 32.74 GPa, 668.92 MPa, and 4.09 MPa·m 1/2 , respectively, higher than those of the ceramics fabricated with B 4 C or with B 4 C plus Fe. The liquid formed by Fe during sintering enhances the dispersion of BN, which is beneficial to realizing the function of pinning grain boundary and pulling out. The toughening phenomena include intergranular and transgranular fracture, particle pulling out, and bridging.
- 4 November 2024
- Published by Elsevier in Journal of Environmental Management
- Vol. 371, 123230
Recycling B4C grinding waste to fabricate high-performance ceramics by modification treatments and hot pressing
- 4 November 2024
- Published by Elsevier in Journal of Environmental Management
- Vol. 371, 123230
Recycling B4C grinding waste to fabricate high-performance ceramics by modification treatments and hot pressing
- 22 May 2023
- Published by Springer Nature in Journal of the Australian Ceramic Society
- Vol. 59 (4) , 1065-1077
Influence of dispersant on the microstructure and performance of the hot-pressed B4C-YB4 ceramics
- 22 May 2023
- Published by Springer Nature in Journal of the Australian Ceramic Society
- Vol. 59 (4) , 1065-1077
Influence of dispersant on the microstructure and performance of the hot-pressed B4C-YB4 ceramics
- 8 May 2023
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 20 (5) , 2955-2973
Microstructure evolution and performance of B 4 C–NdB 6 composites fabricated by in situ hot pressing
B 4 C–NdB 6 composites were fabricated by in situ hot pressing at different temperatures (1950–2150°C) with B 4 C and Nd 2 O 3 (2–4 wt%) as raw materials. The microstructure evolution of the composites with sintering temperature and Nd 2 O 3 content was studied in detail, and the influence of pressure on the sintering of B 4 C with different contents of Nd 2 O 3 was also investigated. The performance of the fabricated composites was researched and the toughening mechanism was discussed. The results indicate that Nd 2 O 3 can react with B 4 C to form the thin‐sheet intermediate products (Nd(BO 2 ) 3 , Nd 2 CO 5 ) first, which then transform to band‐shaped NdB 6 . Pressure can reduce the distance of B 4 C and Nd 2 O 3 , accelerating the mass transfer and contributing to the formation of NdB 6 . NdB 6 and intermediate products are first in agglomerate structure at 1950°C, and then the agglomerates are broken to form dispersive micron and submicron NdB 6 at 2000°C by the synergistic function of pressure, diffusion at high temperature, and liquid phase sintering. NdB 6 can enhance the densification owing to the bonding function. Excessive Nd 2 O 3 content leads to residual pores, and excessive temperature (2150°C) results in the coarsening of phases. The coexistence of transgranular and intergranular fracture of NdB 6 promote the fracture toughness.
- 8 May 2023
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 20 (5) , 2955-2973
Microstructure evolution and performance of B 4 C–NdB 6 composites fabricated by in situ hot pressing
B 4 C–NdB 6 composites were fabricated by in situ hot pressing at different temperatures (1950–2150°C) with B 4 C and Nd 2 O 3 (2–4 wt%) as raw materials. The microstructure evolution of the composites with sintering temperature and Nd 2 O 3 content was studied in detail, and the influence of pressure on the sintering of B 4 C with different contents of Nd 2 O 3 was also investigated. The performance of the fabricated composites was researched and the toughening mechanism was discussed. The results indicate that Nd 2 O 3 can react with B 4 C to form the thin‐sheet intermediate products (Nd(BO 2 ) 3 , Nd 2 CO 5 ) first, which then transform to band‐shaped NdB 6 . Pressure can reduce the distance of B 4 C and Nd 2 O 3 , accelerating the mass transfer and contributing to the formation of NdB 6 . NdB 6 and intermediate products are first in agglomerate structure at 1950°C, and then the agglomerates are broken to form dispersive micron and submicron NdB 6 at 2000°C by the synergistic function of pressure, diffusion at high temperature, and liquid phase sintering. NdB 6 can enhance the densification owing to the bonding function. Excessive Nd 2 O 3 content leads to residual pores, and excessive temperature (2150°C) results in the coarsening of phases. The coexistence of transgranular and intergranular fracture of NdB 6 promote the fracture toughness.
- 18 April 2022
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 19 (4) , 1991-2003
Performance of B 4 C/CeB 6 composites fabricated via hot pressing under different processes
In this work, CeO 2 sintering additive reinforced B 4 C ceramic composites were prepared by hot‐pressing reaction sintering under different processes of low temperature–long holding time (1980°C, 30 MPa, 3 h, 4 wt% CeO 2 ) and high temperature–short holding time (2050°C, 30 MPa, .5 h, 4 wt% and 6 wt% CeO 2 ). The effect of sintering process and CeO 2 content on the microstructure and mechanical properties of B 4 C‐CeB 6 composites were investigated. The existed impurities in the obtained composites were also analyzed. Results show that CeO 2 is an active sintering additive. CeB 6 is formed by the reaction between CeO 2 , B 4 C and C in sintering process. The densification of B 4 C ceramics is enhanced, and the grains can be refined by the formed CeB 6 , which promotes the strength. The thermal expansion coefficient mismatch, crack deflection, and fracture mode change caused by the in situ formed CeB 6 improve the toughness. The process of low temperature–long holding time is more suitable for playing the role of CeO 2 additive in sintering of B 4 C, under which condition the relative density, flexural strength, fracture toughness, and hardness reach 99%, 417 MPa, 5.32 MPa·m 1/2 , and 30.66 GPa, respectively. The impurities in the composites are the kinds of Ti‐contained, C‐O‐Mg‐Ca‐contained, C‐O‐Ca‐S‐contained, and Si‐contained impurities.
- 18 April 2022
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 19 (4) , 1991-2003
Performance of B 4 C/CeB 6 composites fabricated via hot pressing under different processes
In this work, CeO 2 sintering additive reinforced B 4 C ceramic composites were prepared by hot‐pressing reaction sintering under different processes of low temperature–long holding time (1980°C, 30 MPa, 3 h, 4 wt% CeO 2 ) and high temperature–short holding time (2050°C, 30 MPa, .5 h, 4 wt% and 6 wt% CeO 2 ). The effect of sintering process and CeO 2 content on the microstructure and mechanical properties of B 4 C‐CeB 6 composites were investigated. The existed impurities in the obtained composites were also analyzed. Results show that CeO 2 is an active sintering additive. CeB 6 is formed by the reaction between CeO 2 , B 4 C and C in sintering process. The densification of B 4 C ceramics is enhanced, and the grains can be refined by the formed CeB 6 , which promotes the strength. The thermal expansion coefficient mismatch, crack deflection, and fracture mode change caused by the in situ formed CeB 6 improve the toughness. The process of low temperature–long holding time is more suitable for playing the role of CeO 2 additive in sintering of B 4 C, under which condition the relative density, flexural strength, fracture toughness, and hardness reach 99%, 417 MPa, 5.32 MPa·m 1/2 , and 30.66 GPa, respectively. The impurities in the composites are the kinds of Ti‐contained, C‐O‐Mg‐Ca‐contained, C‐O‐Ca‐S‐contained, and Si‐contained impurities.
- 6 August 2020
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 17 (6) , 2569-2579
Microstructure and mechanical property of (TiB2‐SiC) agglomerate‐toughened B4C‐TiB2‐SiC composites
B4C‐TiB2‐SiC composites toughened by (TiB2‐SiC) agglomerates were prepared via reactive hot pressing with B4C and TiSi2 as raw materials. Phase composition, microstructure, and mechanical properties of the fabricated composites were investigated. The function of (TiB2‐SiC) agglomerates was analyzed, and the strengthening and toughening mechanism were also discussed. Results indicated that some of the in situ formed TiB2 and SiC were interlocked to form special (TiB2‐SiC) agglomerates in the matrix. The good comprehensive performances of 510 MPa flexural strength, 5.84 MPa·m1/2 fracture toughness, and 31.93 GPa hardness were obtained in the composites fabricated with 30 wt% TiSi2. The in situ introduced fine TiB2 and SiC grains refined the grains of B4C due to the pinning effect, which enhanced the strength. The special (TiB2‐SiC) agglomerates and the existing toughening phenomena such as crack deflection, branching, and microcrack regions induced by the mismatch of thermal expansion coefficients, had cumulative effects on improving the fracture toughness.
- 6 August 2020
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 17 (6) , 2569-2579
Microstructure and mechanical property of (TiB2‐SiC) agglomerate‐toughened B4C‐TiB2‐SiC composites
B4C‐TiB2‐SiC composites toughened by (TiB2‐SiC) agglomerates were prepared via reactive hot pressing with B4C and TiSi2 as raw materials. Phase composition, microstructure, and mechanical properties of the fabricated composites were investigated. The function of (TiB2‐SiC) agglomerates was analyzed, and the strengthening and toughening mechanism were also discussed. Results indicated that some of the in situ formed TiB2 and SiC were interlocked to form special (TiB2‐SiC) agglomerates in the matrix. The good comprehensive performances of 510 MPa flexural strength, 5.84 MPa·m1/2 fracture toughness, and 31.93 GPa hardness were obtained in the composites fabricated with 30 wt% TiSi2. The in situ introduced fine TiB2 and SiC grains refined the grains of B4C due to the pinning effect, which enhanced the strength. The special (TiB2‐SiC) agglomerates and the existing toughening phenomena such as crack deflection, branching, and microcrack regions induced by the mismatch of thermal expansion coefficients, had cumulative effects on improving the fracture toughness.
- 11 October 2019
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 17 (2) , 509-518
Preparation of B 4 C composites toughened by MoB 2 /Mo 2 B 5 ‐SiC interlocking structure via reactive hot pressing
B 4 C composites toughened by MoB 2 /Mo 2 B 5 ‐SiC interlocking structure were prepared via reactive hot pressing with B 4 C and MoSi 2 as raw materials. The phase composition, microstructure, and mechanical properties of the fabricated B 4 C composites were studied. The crack propagation and fracture surface were observed, and the toughening mechanism was analyzed. The results indicate that the interlocking structure of MoB 2 /Mo 2 B 5 ‐SiC is formed in the obtained B 4 C composites. The relative density, flexural strength, and fracture toughness of the B 4 C composites reach 99.3%, 480 MPa, and 5.2 MPa·m 1/2 , respectively, when the MoSi 2 content is 30 wt%. The hardness is 33 GPa when the MoSi 2 content is 20 wt%. The special laminar fracture of the interlocking structure of MoB 2 /Mo 2 B 5 ‐SiC elongates the crack extending path and thus consumes more energy of crack extension. The phenomena of crack bridging and branching and the special laminar fracture of the interlocking structure have a synergistic effect on promoting the overall fracture toughness.
- 11 October 2019
- Published by Wiley in International Journal of Applied Ceramic Technology
- Vol. 17 (2) , 509-518
Preparation of B 4 C composites toughened by MoB 2 /Mo 2 B 5 ‐SiC interlocking structure via reactive hot pressing
B 4 C composites toughened by MoB 2 /Mo 2 B 5 ‐SiC interlocking structure were prepared via reactive hot pressing with B 4 C and MoSi 2 as raw materials. The phase composition, microstructure, and mechanical properties of the fabricated B 4 C composites were studied. The crack propagation and fracture surface were observed, and the toughening mechanism was analyzed. The results indicate that the interlocking structure of MoB 2 /Mo 2 B 5 ‐SiC is formed in the obtained B 4 C composites. The relative density, flexural strength, and fracture toughness of the B 4 C composites reach 99.3%, 480 MPa, and 5.2 MPa·m 1/2 , respectively, when the MoSi 2 content is 30 wt%. The hardness is 33 GPa when the MoSi 2 content is 20 wt%. The special laminar fracture of the interlocking structure of MoB 2 /Mo 2 B 5 ‐SiC elongates the crack extending path and thus consumes more energy of crack extension. The phenomena of crack bridging and branching and the special laminar fracture of the interlocking structure have a synergistic effect on promoting the overall fracture toughness.