Alireza Bagheri Bami
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Alireza Bagheri Bami has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
Saeid Amini
3 shared publications- Farhang Honarvar
NDE Lab, Faculty of Mechanical Engineering, K. N. Toosi University of Technology, Tehran, Iran
2 shared publications Reza Teimouri
2 shared publications- Saeid Amini
Department of Manufacturing, Faculty of Mechanical Engineering, University of Kashan, Kashan, Iran
2 shared publications A. Amanov
1 shared publicationAli Alaei
1 shared publication
Latest Publications
- 1 November 2026
- Published by NDT.net GmbH & Co. KG in e-Journal of Nondestructive Testing
- Vol. 31 (11)
Experimental Analysis of Frequency-Dependent Ultrasonic Attenuation and Velocity in Additively Manufactured Polymers
Ultrasonic velocity and attenuation in non-metallic materials such as polymers exhibit strong frequency-dependent behavior, unlike the largely frequency-independent attenuation observed in metals, which limits penetration depth and measurement resolution in non-destructive evaluation (NDE). This study investigates the frequency-dependent ultrasonic velocity and attenuation characteristics of additively manufactured polymer materials by evaluating four attenuation coefficients—standard time-domain exponential fitting, frequency-domain exponential fitting, Welch-based frequency-domain exponential fitting, and frequency-dependent attenuation at the nominal transducer frequency—and two velocity measures: standard constant longitudinal velocity and frequency-dependent velocity. Eight fused-deposition-modeled polymer samples were fabricated with varying nozzle temperatures (195°C and 205°C), nozzle diameters (0.4 mm and 0.6 mm), and raster angles (25° and 50°). Results show that higher nozzle temperatures and larger nozzle diameters reduce attenuation and increase ultrasonic velocity by improving interlayer bonding, reducing porosity, and enhancing material homogeneity. Statistical analysis using Minitab identified 205°C and a 0.6 mm nozzle diameter as the optimal combination for minimizing attenuation and maximizing velocity in NDE applications, while lower temperatures, smaller diameters, and 50° raster angles were more suitable for sound-absorption and damping applications. The proposed frequency-dependent characterization methodology was validated using standard samples and established literature data, providing a systematic framework for evaluating acoustic properties in additively manufactured polymers and bridging the gap between conventional frequency-independent approaches and advanced signal-processing-based techniques.
- 1 November 2026
- Published by NDT.net GmbH & Co. KG in e-Journal of Nondestructive Testing
- Vol. 31 (11)
Experimental Analysis of Frequency-Dependent Ultrasonic Attenuation and Velocity in Additively Manufactured Polymers
Ultrasonic velocity and attenuation in non-metallic materials such as polymers exhibit strong frequency-dependent behavior, unlike the largely frequency-independent attenuation observed in metals, which limits penetration depth and measurement resolution in non-destructive evaluation (NDE). This study investigates the frequency-dependent ultrasonic velocity and attenuation characteristics of additively manufactured polymer materials by evaluating four attenuation coefficients—standard time-domain exponential fitting, frequency-domain exponential fitting, Welch-based frequency-domain exponential fitting, and frequency-dependent attenuation at the nominal transducer frequency—and two velocity measures: standard constant longitudinal velocity and frequency-dependent velocity. Eight fused-deposition-modeled polymer samples were fabricated with varying nozzle temperatures (195°C and 205°C), nozzle diameters (0.4 mm and 0.6 mm), and raster angles (25° and 50°). Results show that higher nozzle temperatures and larger nozzle diameters reduce attenuation and increase ultrasonic velocity by improving interlayer bonding, reducing porosity, and enhancing material homogeneity. Statistical analysis using Minitab identified 205°C and a 0.6 mm nozzle diameter as the optimal combination for minimizing attenuation and maximizing velocity in NDE applications, while lower temperatures, smaller diameters, and 50° raster angles were more suitable for sound-absorption and damping applications. The proposed frequency-dependent characterization methodology was validated using standard samples and established literature data, providing a systematic framework for evaluating acoustic properties in additively manufactured polymers and bridging the gap between conventional frequency-independent approaches and advanced signal-processing-based techniques.
- Open Access
- 27 May 2026
- Published by Elsevier in Materials Today Communications
- Vol. 53
Multi-scale modelling of the microstructure evolution during ultrasonic nanocrystal surface modification of WE54 Mg alloy
- 27 May 2026
- Published by Elsevier in Materials Today Communications
- Vol. 53
Open AccessMulti-scale modelling of the microstructure evolution during ultrasonic nanocrystal surface modification of WE54 Mg alloy
- 14 July 2024
- Published by Wiley in Polymer Engineering & Science
- Vol. 64 (9) , 4210-4233
Anisotropic polymer components with desired elastic properties manufactured through fused filament fabrication additive manufacturing
Fused filament fabrication (FFF) is a popular additive manufacturing (AM) process, primarily used for fabricating polymer components. Optimizing the mechanical properties of FFF components, such as their elastic moduli, is crucial in many applications. This study focuses on adjusting the elastic properties of polymer components manufactured through FFF process by selecting appropriate process parameters. The elastic constants of the anisotropic FFF components are measured by using ultrasonic testing (UT). Response surface methodology (RSM) is employed to determine the optimal settings for these parameters to achieve the desired elastic properties. The effects of layer thickness, printing speed, and raster angle on Young's modulus are explored. Analysis of variance (ANOVA) is used to identify the contributions of each process factor on the output responses. According to ANOVA results, the optimal conditions identified are: a printing speed of 2040 mm/min, a layer thickness of 0.2 mm, and a raster angle of 29°. These conditions collectively achieved the maximum Young's modulus. The differences between the predicted and measured moduli for all responses are less than 5%. The structural factors influencing the results are examined by analyzing the fracture surfaces of the tensile testing (TT) specimens with field emission scanning electron microscopy. Additional measurements of other properties, including ultrasound velocity and wave attenuation, are conducted on the samples. The findings indicate that optimizing the parameters by setting them to their minimum values does not only improve the maximum elastic modulus in specific directions but also reduces attenuation. It is concluded that the desired elastic modulus for a component can be achieved by properly adjusting the process parameters.Highlights: Optimizing AM parameters to achieve the desired elastic properties of FFF samples. Examining the effects of each AM parameter by utilizing ANOVA and RSM methods. Measuring the anisotropic elastic properties of AM samples by UT. Verifying UT results through TT and measuring attenuation.
- 14 July 2024
- Published by Wiley in Polymer Engineering & Science
- Vol. 64 (9) , 4210-4233
Anisotropic polymer components with desired elastic properties manufactured through fused filament fabrication additive manufacturing
Fused filament fabrication (FFF) is a popular additive manufacturing (AM) process, primarily used for fabricating polymer components. Optimizing the mechanical properties of FFF components, such as their elastic moduli, is crucial in many applications. This study focuses on adjusting the elastic properties of polymer components manufactured through FFF process by selecting appropriate process parameters. The elastic constants of the anisotropic FFF components are measured by using ultrasonic testing (UT). Response surface methodology (RSM) is employed to determine the optimal settings for these parameters to achieve the desired elastic properties. The effects of layer thickness, printing speed, and raster angle on Young's modulus are explored. Analysis of variance (ANOVA) is used to identify the contributions of each process factor on the output responses. According to ANOVA results, the optimal conditions identified are: a printing speed of 2040 mm/min, a layer thickness of 0.2 mm, and a raster angle of 29°. These conditions collectively achieved the maximum Young's modulus. The differences between the predicted and measured moduli for all responses are less than 5%. The structural factors influencing the results are examined by analyzing the fracture surfaces of the tensile testing (TT) specimens with field emission scanning electron microscopy. Additional measurements of other properties, including ultrasound velocity and wave attenuation, are conducted on the samples. The findings indicate that optimizing the parameters by setting them to their minimum values does not only improve the maximum elastic modulus in specific directions but also reduces attenuation. It is concluded that the desired elastic modulus for a component can be achieved by properly adjusting the process parameters.Highlights: Optimizing AM parameters to achieve the desired elastic properties of FFF samples. Examining the effects of each AM parameter by utilizing ANOVA and RSM methods. Measuring the anisotropic elastic properties of AM samples by UT. Verifying UT results through TT and measuring attenuation.
- Open Access
- 1 September 2021
- Published by KEAI Publishing in International Journal of Lightweight Materials and Manufacture
- Vol. 4 (3) , 315-322
Ultrasonic-assisted friction drilling process of aerospace aluminum alloy (AA7075): FEA and experimental study
- 1 September 2021
- Published by KEAI Publishing in International Journal of Lightweight Materials and Manufacture
- Vol. 4 (3) , 315-322
Open AccessUltrasonic-assisted friction drilling process of aerospace aluminum alloy (AA7075): FEA and experimental study
- 10 October 2019
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine
- Vol. 233 (12) , 1226-1236
Improving the surface energy of titanium implants by the creation of hierarchical textures on the surface via three-dimensional elliptical vibration turning for enhanced osseointegration
An increase in bone-implant contact and an increase in surface hydrophilicity are the two important factors involved in improving osseointegration. Therefore, three-dimensional elliptical vibration turning method is applied to increase the hydrophilicity of titanium surface by the generation of hierarchical nano- and micro-textures. That being the case, face turning process at different cutting conditions is carried out in this research. Surface roughness and the contact angle of water drops with machined surfaces were selected to be measured for the analysis of surface hydrophilicity. The results show that an additional surface area can be achieved by the generation of micro- or nano-textures, resulting in a lower contact angle. Furthermore, intermittent movement of cutting tool in vibration cutting causes the process to be more stable, achieving the desired range of surface roughness.
- 10 October 2019
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part H: Journal of Engineering in Medicine
- Vol. 233 (12) , 1226-1236
Improving the surface energy of titanium implants by the creation of hierarchical textures on the surface via three-dimensional elliptical vibration turning for enhanced osseointegration
An increase in bone-implant contact and an increase in surface hydrophilicity are the two important factors involved in improving osseointegration. Therefore, three-dimensional elliptical vibration turning method is applied to increase the hydrophilicity of titanium surface by the generation of hierarchical nano- and micro-textures. That being the case, face turning process at different cutting conditions is carried out in this research. Surface roughness and the contact angle of water drops with machined surfaces were selected to be measured for the analysis of surface hydrophilicity. The results show that an additional surface area can be achieved by the generation of micro- or nano-textures, resulting in a lower contact angle. Furthermore, intermittent movement of cutting tool in vibration cutting causes the process to be more stable, achieving the desired range of surface roughness.
- 1 February 2018
- Published by Elsevier in Measurement
- Vol. 116, 129-139
Evaluation of optimized surface properties and residual stress in ultrasonic assisted ball burnishing of AA6061-T6
- 1 February 2018
- Published by Elsevier in Measurement
- Vol. 116, 129-139
Evaluation of optimized surface properties and residual stress in ultrasonic assisted ball burnishing of AA6061-T6
- 8 June 2017
- Published by Taylor & Francis in Materials and Manufacturing Processes
- Vol. 33 (11) , 1250-1259
Ultrasonic-assisted ball burnishing of aluminum 6061 and AISI 1045 steel
In the present work, experimental study was carried out to enhance the surface properties of aluminum 6061 and AISI 1045 steel plates by ultrasonic-assisted ball burnishing process. Full factorial experimental design was utilized here to find the effect of ultrasonic vibration, feed rate, and pass number on surface roughness and hardness. The results were discussed according to interaction effect of process factors for different material. It is found from the results that for conventional burnishing process, the highest surface hardness is attained at 5000 mm/min feed rate and 5 pass number, while for ultrasonic-assisted burnishing, the highest hardness is attained at 1000 mm/min feed rate and 5 pass number. On the other hand, it is found from the results that exerting ultrasonic vibration significantly enhances the hardness value and hardened depth. Also, it is found that irrespective of type of operation and material, increase in feed rate causes higher roughness, whereas increase in pass number causes reduction in roughness. Furthermore, surface roughness of ultrasonic-assisted burnishing is lower than that of conventional burnishing process. This enhancement is due to the association of both static and dynamic loading in ultrasonic-assisted burnishing process that causes microstructure modification and limits the elastic recovery of the surface.
- 8 June 2017
- Published by Taylor & Francis in Materials and Manufacturing Processes
- Vol. 33 (11) , 1250-1259
Ultrasonic-assisted ball burnishing of aluminum 6061 and AISI 1045 steel
In the present work, experimental study was carried out to enhance the surface properties of aluminum 6061 and AISI 1045 steel plates by ultrasonic-assisted ball burnishing process. Full factorial experimental design was utilized here to find the effect of ultrasonic vibration, feed rate, and pass number on surface roughness and hardness. The results were discussed according to interaction effect of process factors for different material. It is found from the results that for conventional burnishing process, the highest surface hardness is attained at 5000 mm/min feed rate and 5 pass number, while for ultrasonic-assisted burnishing, the highest hardness is attained at 1000 mm/min feed rate and 5 pass number. On the other hand, it is found from the results that exerting ultrasonic vibration significantly enhances the hardness value and hardened depth. Also, it is found that irrespective of type of operation and material, increase in feed rate causes higher roughness, whereas increase in pass number causes reduction in roughness. Furthermore, surface roughness of ultrasonic-assisted burnishing is lower than that of conventional burnishing process. This enhancement is due to the association of both static and dynamic loading in ultrasonic-assisted burnishing process that causes microstructure modification and limits the elastic recovery of the surface.