SBSebastian Bolz

Sebastian Bolz

*This is an algorithmically generated author record based on publicly available information.

Current Organizations / Institutes

The organizations/institutes from the scholar's latest article


Sebastian Bolz has a total of 11 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Oxidation Behavior of Zr–1Nb Corroded in Air at 400 °C after Plasma Immersion Titanium Implantation

    by Aleksei Obrosov, Alina N. Sutygina, Anton Manakhov, Sebastian Bolz, Sabine Weiß, Egor B. Kashkarov

    In this paper, the influence of plasma immersion titanium implantation into the zirconium alloy Zr-1Nb on the oxidation behavior at 400 °C for 5, 24, 72, and 240 h in air under normal atmospheric pressure (101.3 kPa) was shown. The influence of implantation on the protective properties of the modified layer was shown. The valence of the oxides before and after implantation was analyzed by means of X-ray photoelectron spectroscopy (XPS). Grazing incidence X-ray diffraction (GIXRD) was carried out to examine the phase composition after titanium ion implantation and oxidation. Differential scanning calorimetry (DSC) revealed that titanium implantation exhibited effects of stabilizing the β phase. The formation of the t-ZrO2 and m-ZrO2 was observed during the oxidation of the as-received and modified Zr-1Nb. The measurement of weight gain showed an improvement in oxidation resistance of Ti implanted Zr-1Nb at the oxidation up to 24 h when compared with that of the as-received Zr-1Nb. However, at longer oxidation cycle the oxidation rate of Ti-implanted zirconium alloy is the same with the as-received alloy, which attributed to the layer thickness. Nevertheless, the corrosion of the Ti-implanted alloy is more uniform, while a local corrosion and cracks was detected on the surface of the as-received alloy.


  • Open Access

    XPS and AFM Investigations of Ti-Al-N Coatings Fabricated Using DC Magnetron Sputtering at Various Nitrogen Flow Rates and Deposition Temperatures

    by Aleksei Obrosov, Roman Gulyaev, Markus Ratzke, Alex A. Volinsky, Sebastian Bolz, Muhammad Naveed, Sabine Weiß

    Ti-Al-N coatings were deposited by direct current magnetron sputtering (DCMS) onto IN 718 at different nitrogen flow rates and deposition temperatures. The coatings’ properties were characterized using atomic force microscopy (AFM), X-ray photoelectron spectroscopy (XPS) as well as nanoindentation. It was found that higher deposition temperature leads to higher surface roughness and nitrogen flux influences the shape of grains. According to XPS, the bonding structure of all coatings exhibited the (Ti,Al)N phase. Mechanical properties depend on the Al content within the films. The coating with the best mechanical properties (deposited at 500 °C and 20 standard cubic centimeters per minute (sccm)) was further deposited onto tungsten carbide (WC) cutting tools for cylindrical turning experiments. A quasi-constant flank wear was observed until a machining volume of 23,500 mm3.


  • Open Access

    Devising Strain Hardening Models Using Kocks–Mecking Plots—A Comparison of Model Development for Titanium Aluminides and Case Hardening Steel

    by Markus Bambach, Irina Sizova, Sebastian Bolz, Sabine Weiß

    The present study focuses on the development of strain hardening models taking into account the peculiarities of titanium aluminides. In comparison to steels, whose behavior has been studied extensively in the past, titanium aluminides possess a much larger initial work hardening rate, a sharp peak stress and pronounced softening. The work hardening behavior of a TNB-V4 (Ti–44.5Al–6.25Nb–0.8Mo–0.1B) alloy is studied using isothermal hot compression tests conducted on a Gleeble 3500 simulator, and compared to the typical case hardening steel 25MoCrS4. The behavior is analyzed with the help of the Kocks-Mecking plots. In contrast to steel the TNB-V4 alloy shows a non-linear course of θ (i.e., no stage-III hardening) initially and exhibits neither a plateau (stage IV hardening) nor an inflection point at all deformation conditions. The present paper describes the development and application of a methodology for the design of strain hardening models for the TNB-V4 alloy and the 25CrMoS4 steel by taking the course of the Kocks-Mecking plots into account. Both models use different approaches for the hardening and softening mechanisms and accurately predict the flow stress over a wide range of deformation conditions. The methodology may hence assist in further developments of more sophisticated physically-based strain hardening models for TiAl-alloys.


  • Development of a dynamic recrystallization model for a β-solidifying titanium aluminide alloy using Kocks-Mecking plots

    by Markus Bambach, Irina Sizova, Sebastian Bolz, Sabine Weiß

    Intermetallic titanium aluminide alloys are of growing interest for aerospace and automotive industries due to their remarkable mechanical properties at elevated temperature. The present study focusses on the investigation of the high-temperature deformation behavior of an intermetallic alloy with the nominal composition Ti–44.5Al–6.25Nb–0.8Mo–0.1B. Isothermal compression tests were conducted on a Gleeble 3500 simulator. The flow curves were transformed into Kocks-Mecking plots, where remarkable features such as the absence of stage-III hardening and an inflection point marking the onset of dynamic recrystallization were observed. Based on these observations, a phenomenological flow stress model was devised which incorporates the observations revealed through the Kocks-Mecking plots and reproduces the course of flow stress up to the peak stress and towards the steady-state well. The model may hence be used in finite element simulations of isothermal forging of titanium aluminides.