Chuanbing Huang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Chuanbing Huang has a total of 18 co-authors. Here are the top co-authors by number of shared publications:
- Weigang Zhang
School of Rare Earths, University of Science and Technology of China, Hefei 230026, China
5 shared publications - Huifeng Zhang
School of Rare Earths, University of Science and Technology of China, Hefei 230026, China
4 shared publications - Hao Lan
Ganjiang Innovation Academy, Chinese Academy of Sciences, Ganzhou 341119, China
2 shared publications - Hao Lan
State Key Laboratory of Multi-phase Complex Systems, Institute of Process Engineering, Chinese Academy of Sciences, Beijing 100190, China
1 shared publication - Haozhong Lv
Institute of Process Engineering, Chinese Academy of Sciences, Beijing 100190, China
1 shared publication - Junnan Jin
Ganjiang Innovation Academy, Chinese Academy of Sciences, Ganzhou 341119, China
1 shared publication
Latest Publications
- Open Access
- 21 July 2026
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 10 (7) , 255
Laser Remelting-Induced Microstructure Refinement and Strengthening of (TaWZrHf)95Y5 Refractory High-Entropy Alloy
A novel (TaWZrHf)95Y5 refractory high-entropy alloy (RHEA) matrix was fabricated via vacuum hot pressing (VHP) sintering and subsequently modified through laser remelting (LR) surface treatment. Thermodynamic phase diagram calculations predicted the alloy’s dual-phase BCC structure, and the effects of LR on phase composition, microstructure, and mechanical properties were systematically investigated. LR induced a significant phase transition, promoting rapid solidification and substantial grain refinement. The surface hardness increased to 848 HV0.2, approximately 1.5 times higher than that of the matrix, while the compressive strength reached 1635 MPa, surpassing the matrix by 200 MPa without compromising ductility. Importantly, the LR process effectively mitigated rare-earth (yttrium) segregation and loss, a common challenge in conventional arc melting of refractory HEAs, thereby enhancing solid solution strengthening and phase stability. This work pioneers the application of laser surface engineering to VHP-sintered refractory HEAs, bridging critical gaps in fabrication, microstructural optimization, and performance enhancement, and offering valuable insights for the future design of high-performance multi-principal element alloy development.
- 21 July 2026
- Published by MDPI AG in Journal of Manufacturing and Materials Processing
- Vol. 10 (7) , 255
Open AccessLaser Remelting-Induced Microstructure Refinement and Strengthening of (TaWZrHf)95Y5 Refractory High-Entropy Alloy
A novel (TaWZrHf)95Y5 refractory high-entropy alloy (RHEA) matrix was fabricated via vacuum hot pressing (VHP) sintering and subsequently modified through laser remelting (LR) surface treatment. Thermodynamic phase diagram calculations predicted the alloy’s dual-phase BCC structure, and the effects of LR on phase composition, microstructure, and mechanical properties were systematically investigated. LR induced a significant phase transition, promoting rapid solidification and substantial grain refinement. The surface hardness increased to 848 HV0.2, approximately 1.5 times higher than that of the matrix, while the compressive strength reached 1635 MPa, surpassing the matrix by 200 MPa without compromising ductility. Importantly, the LR process effectively mitigated rare-earth (yttrium) segregation and loss, a common challenge in conventional arc melting of refractory HEAs, thereby enhancing solid solution strengthening and phase stability. This work pioneers the application of laser surface engineering to VHP-sintered refractory HEAs, bridging critical gaps in fabrication, microstructural optimization, and performance enhancement, and offering valuable insights for the future design of high-performance multi-principal element alloy development.
- Open Access
Microstructure and High-Temperature Ablation Behaviour of Hafnium-Doped Tungsten-Yttrium Alloys
W is a widely used refractory metal with ultra-high melting point up to 3410 °C. However, its applications are limited by poor ablation resistance under high-temperature flame and air flow, which is crucial for aerospace vehicles. To improve the ablation resistance of W under extreme conditions, W-Y alloys doped with different Hf mass fractions (0, 10, 20, and 30) were prepared using the fast hot pressing sintering method. Microstructure and ablation behaviours at 2000 °C were investigated. Results showed that adding an appropriate amount of Hf improved the properties of the W-Y alloy evidently. In particular, the hardness of the alloy increased with the increased content of Hf. The formation of the HfO2 layer on the surface during ablation decreased the mass and linear ablation rates, indicating enhanced ablation resistance. However, excessive Hf addition will result in crack behaviour during ablation. With a Hf content of 20 wt.%, the alloy exhibited high stability and an excellent ablation resistance.
Open AccessMicrostructure and High-Temperature Ablation Behaviour of Hafnium-Doped Tungsten-Yttrium Alloys
W is a widely used refractory metal with ultra-high melting point up to 3410 °C. However, its applications are limited by poor ablation resistance under high-temperature flame and air flow, which is crucial for aerospace vehicles. To improve the ablation resistance of W under extreme conditions, W-Y alloys doped with different Hf mass fractions (0, 10, 20, and 30) were prepared using the fast hot pressing sintering method. Microstructure and ablation behaviours at 2000 °C were investigated. Results showed that adding an appropriate amount of Hf improved the properties of the W-Y alloy evidently. In particular, the hardness of the alloy increased with the increased content of Hf. The formation of the HfO2 layer on the surface during ablation decreased the mass and linear ablation rates, indicating enhanced ablation resistance. However, excessive Hf addition will result in crack behaviour during ablation. With a Hf content of 20 wt.%, the alloy exhibited high stability and an excellent ablation resistance.
- Open Access
Fabrication of C/C–SiC–ZrB2 Ultra-High Temperature Composites through Liquid–Solid Chemical Reaction
In this paper, we aimed to improve the oxidation and ablation resistance of carbon fiber-reinforced carbon (CFC) composites at temperatures above 2000 °C. C/C–SiC–ZrB2 ultra-high temperature ceramic composites were fabricated through a complicated liquid–solid reactive process combining slurry infiltration (SI) and reactive melt infiltration (RMI). A liquid Si–Zr10 eutectic alloy was introduced, at 1600 °C, into porous CFC composites containing two kinds of boride particles (B4C and ZrB2, respectively) to form a SiC–ZrB2 matrix. The effects and mechanism of the introduced B4C and ZrB2 particles on the formation reaction and microstructure of the final C/C–SiC–ZrB2 composites were investigated in detail. It was found that the composite obtained from a C/C–B4C preform displayed a porous and loose structure, and the formed SiC–ZrB2 matrix distributed heterogeneously in the composite due to the asynchronous generation of the SiC and ZrB2 ceramics. However, the C/C–SiC–ZrB2 composite, prepared from a C/C–ZrB2 preform, showed a very dense matrix between the fiber bundles, and elongated plate-like ZrB2 ceramics appeared in the matrix, which were derived from the dissolution–diffusion–precipitation mechanism of the ZrB2 clusters. The latter composite exhibited a relatively higher ZrB2 content (9.51%) and bulk density (2.82 g/cm3), along with lower open porosity (3.43%), which endowed this novel composite with good mechanical properties, including pseudo-plastic fracture behavior.
Open AccessFabrication of C/C–SiC–ZrB2 Ultra-High Temperature Composites through Liquid–Solid Chemical Reaction
In this paper, we aimed to improve the oxidation and ablation resistance of carbon fiber-reinforced carbon (CFC) composites at temperatures above 2000 °C. C/C–SiC–ZrB2 ultra-high temperature ceramic composites were fabricated through a complicated liquid–solid reactive process combining slurry infiltration (SI) and reactive melt infiltration (RMI). A liquid Si–Zr10 eutectic alloy was introduced, at 1600 °C, into porous CFC composites containing two kinds of boride particles (B4C and ZrB2, respectively) to form a SiC–ZrB2 matrix. The effects and mechanism of the introduced B4C and ZrB2 particles on the formation reaction and microstructure of the final C/C–SiC–ZrB2 composites were investigated in detail. It was found that the composite obtained from a C/C–B4C preform displayed a porous and loose structure, and the formed SiC–ZrB2 matrix distributed heterogeneously in the composite due to the asynchronous generation of the SiC and ZrB2 ceramics. However, the C/C–SiC–ZrB2 composite, prepared from a C/C–ZrB2 preform, showed a very dense matrix between the fiber bundles, and elongated plate-like ZrB2 ceramics appeared in the matrix, which were derived from the dissolution–diffusion–precipitation mechanism of the ZrB2 clusters. The latter composite exhibited a relatively higher ZrB2 content (9.51%) and bulk density (2.82 g/cm3), along with lower open porosity (3.43%), which endowed this novel composite with good mechanical properties, including pseudo-plastic fracture behavior.
- Open Access
Characterization and Microstructural Evolution of Continuous BN Ceramic Fibers Containing Amorphous Silicon Nitride
Boron nitride (BN) ceramic fibers containing amounts of silicon nitride (Si3N4) were prepared using hybrid precursors of poly(tri(methylamino)borazine) (PBN) and polycarbosilane (PCS) via melt-spinning, curing, decarburization under NH3 to 1000 °C and pyrolysis up to 1600 °C under N2. The effect of Si3N4 contents on the microstructure of the BN/Si3N4 composite ceramics was investigated. Series of the BN/Si3N4 composite fibers containing various amounts of Si3N4 from 5 wt% to 25 wt% were fabricated. It was found that the crystallization of Si3N4 could be totally restrained when its content was below 25 wt% in the BN/Si3N4 composite ceramics at 1600 °C, and the amorphous BN/Si3N4 composite ceramic could be obtained with a certain ratio. The mean tensile strength and Young’s modulus of the composite fibers correlated positively with the Si3N4 mass content, while an obvious BN (shell)/Si3N4 (core) was formed only when the Si3N4 content reached 25 wt%.
Open AccessCharacterization and Microstructural Evolution of Continuous BN Ceramic Fibers Containing Amorphous Silicon Nitride
Boron nitride (BN) ceramic fibers containing amounts of silicon nitride (Si3N4) were prepared using hybrid precursors of poly(tri(methylamino)borazine) (PBN) and polycarbosilane (PCS) via melt-spinning, curing, decarburization under NH3 to 1000 °C and pyrolysis up to 1600 °C under N2. The effect of Si3N4 contents on the microstructure of the BN/Si3N4 composite ceramics was investigated. Series of the BN/Si3N4 composite fibers containing various amounts of Si3N4 from 5 wt% to 25 wt% were fabricated. It was found that the crystallization of Si3N4 could be totally restrained when its content was below 25 wt% in the BN/Si3N4 composite ceramics at 1600 °C, and the amorphous BN/Si3N4 composite ceramic could be obtained with a certain ratio. The mean tensile strength and Young’s modulus of the composite fibers correlated positively with the Si3N4 mass content, while an obvious BN (shell)/Si3N4 (core) was formed only when the Si3N4 content reached 25 wt%.
- Open Access
Formation of Diffusion Layer on Ti-6Al-4V Alloy during Longtime Friction with Al
Elements’ diffusion between Ti-6Al-4V alloy and Al in the process of sliding was investigated from 400 °C to 600 °C. The results showed that the atoms were diffused at the Ti-6Al-4V/Al interface. When sliding at 400 °C and 500 °C, no intermetallic compound was detected on the surface of Ti-6Al-4V alloy. When sliding at 600 °C, intermetallic TiAl3 was formed and grew on the surface of Ti-6Al-4V alloy. The diffusion thickness of Al atoms on the surface of Ti-6Al-4V alloy increased with increasing time and temperature. The diffusion kinetic equation of Al atoms on the surface of Ti-6Al-4V alloy was successfully established. The diffusion activation energy of Al atoms in the sliding process was calculated to be 28.22 kJ·mol−1 and the dynamic index n was 0.5. The diffusion growth of Al atoms was controlled by normal parabolic law with time.
Open AccessFormation of Diffusion Layer on Ti-6Al-4V Alloy during Longtime Friction with Al
Elements’ diffusion between Ti-6Al-4V alloy and Al in the process of sliding was investigated from 400 °C to 600 °C. The results showed that the atoms were diffused at the Ti-6Al-4V/Al interface. When sliding at 400 °C and 500 °C, no intermetallic compound was detected on the surface of Ti-6Al-4V alloy. When sliding at 600 °C, intermetallic TiAl3 was formed and grew on the surface of Ti-6Al-4V alloy. The diffusion thickness of Al atoms on the surface of Ti-6Al-4V alloy increased with increasing time and temperature. The diffusion kinetic equation of Al atoms on the surface of Ti-6Al-4V alloy was successfully established. The diffusion activation energy of Al atoms in the sliding process was calculated to be 28.22 kJ·mol−1 and the dynamic index n was 0.5. The diffusion growth of Al atoms was controlled by normal parabolic law with time.