Verena Müller
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Verena Müller has a total of 12 co-authors. Here are the top co-authors by number of shared publications:
- Michael A. Danzer
Chair of Electrical Energy Systems, University of Bayreuth, Bayreuth, Germany
2 shared publications Michaela Memm
Zentrum für Sonnenenergie- und Wasserstoff-Forschung Baden-Württemberg Lise-Meitner-Str. 24 89081 Ulm Germany
2 shared publicationsJennifer Wegener
Wacker Chemie AG Consortium für Elektrochemische Industrie Zielstattstr. 20 81379 Munich Germany
1 shared publicationJürgen Pfeiffer
Wacker Chemie AG Consortium für Elektrochemische Industrie Zielstattstr. 20 81379 Munich Germany
1 shared publicationKarsten Richter
Zentrum für Sonnenenergie-und Wasserstoffforschung Baden-Württemberg, 89081 Ulm, Germany
1 shared publicationMargret Wohlfahrt-Mehrens
Zentrum für Sonnenenergie-und Wasserstoffforschung Baden-Württemberg, 89081 Ulm, Germany
1 shared publication
Latest Publications
- 1 May 2020
- Published by Wiley in Energy Technology
- Vol. 8 (7)
Evaluation of Scalable Porous Si‐Rich Si/C Composites with Low Volume Expansion in Coin Cells to Prismatic Cell Formats
Li‐ion battery cells on the basis of Si‐containing anodes suffer from their large volume expansion of up to 300%, impeding their extensive application in the automotive field. Herein, the synthesis of a Si‐rich Si/C composite is introduced. The implemented porosity of the composite has a buffering effect on the Si volume changes during cycling. The scalability of the material from lab‐scale to industrial‐scale batch sizes as well as from coin cell (<5 mAh), to pouch cell (≈0.75 Ah), and to prismatic (PHEV) cells (≈26 Ah) is demonstrated. The performance of the pouch cells and PHEV cells is further improved by cycling under an external mechanical pressure. The irreversible swelling of the pouch and the PHEV cells stays below 6% during cycling. Reproducible aging and swelling behavior of different cell types is observed and investigated in detail. The low irreversible volume increase is confirmed by X‐ray computer tomography (CT) measurements of the PHEV cells before and after cycling.
- 1 May 2020
- Published by Wiley in Energy Technology
- Vol. 8 (7)
Evaluation of Scalable Porous Si‐Rich Si/C Composites with Low Volume Expansion in Coin Cells to Prismatic Cell Formats
Li‐ion battery cells on the basis of Si‐containing anodes suffer from their large volume expansion of up to 300%, impeding their extensive application in the automotive field. Herein, the synthesis of a Si‐rich Si/C composite is introduced. The implemented porosity of the composite has a buffering effect on the Si volume changes during cycling. The scalability of the material from lab‐scale to industrial‐scale batch sizes as well as from coin cell (<5 mAh), to pouch cell (≈0.75 Ah), and to prismatic (PHEV) cells (≈26 Ah) is demonstrated. The performance of the pouch cells and PHEV cells is further improved by cycling under an external mechanical pressure. The irreversible swelling of the pouch and the PHEV cells stays below 6% during cycling. Reproducible aging and swelling behavior of different cell types is observed and investigated in detail. The low irreversible volume increase is confirmed by X‐ray computer tomography (CT) measurements of the PHEV cells before and after cycling.
- Open Access
- 14 November 2019
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 166 (15) , A3796-A3805
Effects of Mechanical Compression on the Aging and the Expansion Behavior of Si/C-Composite|NMC811 in Different Lithium-Ion Battery Cell Formats
Due to their extreme volume expansion, Si/C-composites suffer from fracture or delamination and consequent capacity fading during the Li-ion cell operation. One approach to reduce the electrical contact loss and improve the performance is the application of mechanical pressure on the cell. Therefore, a comprehensive aging study of Si/C|NMC811 pouch cells is conducted with cells in different compression configurations as uncompressed and under flexible and fixed compression at pressure levels in the range of 0.08 MPa, 0.42 MPa, and 0.84 MPa. In-situ swelling measurements by dilation as well as in-operando mapping of the pressure distribution on the cell surfaces reveal the positive influence of the low pressure fixed and the middle pressure flexible compression on the cycle life. For the heavily fixed compressed cells, an inhomogeneous pressure distribution and occurring pressure hot -spots close to the cell current collectors of up to 5.2 MPa are found. An extensive post-mortem analysis including SEM cross-sectioning and EIS measurements of the aged anodes and the separator confirms cell failure by different aging mechanisms depending on the type of compression. Aging experiments of Si/C|NMC811 cylindrical 18650-cells show local differences along the jelly roll which are explained by the help of the pouch cell results.
- 14 November 2019
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 166 (15) , A3796-A3805
Open AccessEffects of Mechanical Compression on the Aging and the Expansion Behavior of Si/C-Composite|NMC811 in Different Lithium-Ion Battery Cell Formats
Due to their extreme volume expansion, Si/C-composites suffer from fracture or delamination and consequent capacity fading during the Li-ion cell operation. One approach to reduce the electrical contact loss and improve the performance is the application of mechanical pressure on the cell. Therefore, a comprehensive aging study of Si/C|NMC811 pouch cells is conducted with cells in different compression configurations as uncompressed and under flexible and fixed compression at pressure levels in the range of 0.08 MPa, 0.42 MPa, and 0.84 MPa. In-situ swelling measurements by dilation as well as in-operando mapping of the pressure distribution on the cell surfaces reveal the positive influence of the low pressure fixed and the middle pressure flexible compression on the cycle life. For the heavily fixed compressed cells, an inhomogeneous pressure distribution and occurring pressure hot -spots close to the cell current collectors of up to 5.2 MPa are found. An extensive post-mortem analysis including SEM cross-sectioning and EIS measurements of the aged anodes and the separator confirms cell failure by different aging mechanisms depending on the type of compression. Aging experiments of Si/C|NMC811 cylindrical 18650-cells show local differences along the jelly roll which are explained by the help of the pouch cell results.