Shouquan Yu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Shouquan Yu has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Min Ge
State Key Laboratory of Multi-phase Complex Systems, Institute of Process Engineering, Chinese Academy of Sciences, Beijing 100190, China
3 shared publications - Weigang Zhang
School of Rare Earths, University of Science and Technology of China, Hefei 230026, China
3 shared publications - Zhenxi Lu
State Key Laboratory of Multi-phase Complex Systems, Institute of Process Engineering, Chinese Academy of Sciences, Beijing 100190, China
2 shared publications - Chuanbing Huang
Institute of Process Engineering, Chinese Academy of Sciences, Beijing 100190, China
1 shared publication - Hao Zhang
State Key Laboratory of Multi-phase Complex Systems, Institute of Process Engineering, Chinese Academy of Sciences, Beijing 100190, China
1 shared publication - Huifeng Zhang
School of Rare Earths, University of Science and Technology of China, Hefei 230026, China
1 shared publication
Latest Publications
- Open Access
Characterization and Microstructural Evolution of Continuous BN Ceramic Fibers Containing Amorphous Silicon Nitride
Boron nitride (BN) ceramic fibers containing amounts of silicon nitride (Si3N4) were prepared using hybrid precursors of poly(tri(methylamino)borazine) (PBN) and polycarbosilane (PCS) via melt-spinning, curing, decarburization under NH3 to 1000 °C and pyrolysis up to 1600 °C under N2. The effect of Si3N4 contents on the microstructure of the BN/Si3N4 composite ceramics was investigated. Series of the BN/Si3N4 composite fibers containing various amounts of Si3N4 from 5 wt% to 25 wt% were fabricated. It was found that the crystallization of Si3N4 could be totally restrained when its content was below 25 wt% in the BN/Si3N4 composite ceramics at 1600 °C, and the amorphous BN/Si3N4 composite ceramic could be obtained with a certain ratio. The mean tensile strength and Young’s modulus of the composite fibers correlated positively with the Si3N4 mass content, while an obvious BN (shell)/Si3N4 (core) was formed only when the Si3N4 content reached 25 wt%.
Open AccessCharacterization and Microstructural Evolution of Continuous BN Ceramic Fibers Containing Amorphous Silicon Nitride
Boron nitride (BN) ceramic fibers containing amounts of silicon nitride (Si3N4) were prepared using hybrid precursors of poly(tri(methylamino)borazine) (PBN) and polycarbosilane (PCS) via melt-spinning, curing, decarburization under NH3 to 1000 °C and pyrolysis up to 1600 °C under N2. The effect of Si3N4 contents on the microstructure of the BN/Si3N4 composite ceramics was investigated. Series of the BN/Si3N4 composite fibers containing various amounts of Si3N4 from 5 wt% to 25 wt% were fabricated. It was found that the crystallization of Si3N4 could be totally restrained when its content was below 25 wt% in the BN/Si3N4 composite ceramics at 1600 °C, and the amorphous BN/Si3N4 composite ceramic could be obtained with a certain ratio. The mean tensile strength and Young’s modulus of the composite fibers correlated positively with the Si3N4 mass content, while an obvious BN (shell)/Si3N4 (core) was formed only when the Si3N4 content reached 25 wt%.
- Open Access
Microstructures of a SiC–ZrC Ceramic Fiber Derived from a Polymeric Precursor
Continuous ceramic fiber comprising silicon carbide–zirconium carbide (SiC–ZrC) binary phases was obtained through melt spinning, electron-beam curing and pyrolysis of a pre-ceramic precursor of polyzirconocenecarbosilanes (PZCS). After pyrolysis and heat treatment, ZrC particles with mean diameters of 15–20 nm were formed and homogeneously dispersed in a matrix of fine crystalline β-SiC with an average grain size of 6–10 nm. Concentration of Zr in the fiber varies from 14.88% to 17.45% by mass. Fibers consisting of near-stoichiometric ZrC and SiC with little free carbon can be obtained through pyrolysis decarbonization of the as-cured fiber in hydrogen from room temperature to 1000 °C, and subsequently heat treatment in argon up to 1600 °C for 1 h. High-temperature treatment of these amorphous inorganic fibers leads to crystallization of the binary phases of β-SiC and ZrC. The removal of free carbon under hydrogen results in more rapid growth of β-SiC and ZrC crystals, in which obvious aggregation of the dispersed ZrC particles among the continuous β-SiC matrix can be ascribed to a fast migration of Zr cation.
Open AccessMicrostructures of a SiC–ZrC Ceramic Fiber Derived from a Polymeric Precursor
Continuous ceramic fiber comprising silicon carbide–zirconium carbide (SiC–ZrC) binary phases was obtained through melt spinning, electron-beam curing and pyrolysis of a pre-ceramic precursor of polyzirconocenecarbosilanes (PZCS). After pyrolysis and heat treatment, ZrC particles with mean diameters of 15–20 nm were formed and homogeneously dispersed in a matrix of fine crystalline β-SiC with an average grain size of 6–10 nm. Concentration of Zr in the fiber varies from 14.88% to 17.45% by mass. Fibers consisting of near-stoichiometric ZrC and SiC with little free carbon can be obtained through pyrolysis decarbonization of the as-cured fiber in hydrogen from room temperature to 1000 °C, and subsequently heat treatment in argon up to 1600 °C for 1 h. High-temperature treatment of these amorphous inorganic fibers leads to crystallization of the binary phases of β-SiC and ZrC. The removal of free carbon under hydrogen results in more rapid growth of β-SiC and ZrC crystals, in which obvious aggregation of the dispersed ZrC particles among the continuous β-SiC matrix can be ascribed to a fast migration of Zr cation.
- Open Access
Microstructures and Properties of Ceramic Fibers of h-BN Containing Amorphous Si3N4
Composite ceramic fibers comprising about 80 wt% boron nitride (h-BN) and 20 wt% Si3N4 were fabricated through melt-spinning, electron-beam curing, and pyrolysis up to 1600 °C in atmospheres of NH3 and N2, using a mixture of poly[tri(methylamino)borazine] (PBN) and polysilazane (PSZ). By analyzing the microstructure and composition of the pyrolyzed ceramic fibers, we found the formation of binary phases including crystalline h-BN and amorphous Si3N4. Further investigations confirmed that this heterogeneous microstructure can only be formed when the introduced ratio of Si3N4 is below 30% in mass. The mean modulus and tensile strength of the fabricated composite fibers were about 90 GPa and 1040 MPa, twice the average of the pure h-BN fiber. The dielectric constant and dielectric loss tangent of the composite fibers is 3.06 and 2.94 × 10−3.
Open AccessMicrostructures and Properties of Ceramic Fibers of h-BN Containing Amorphous Si3N4
Composite ceramic fibers comprising about 80 wt% boron nitride (h-BN) and 20 wt% Si3N4 were fabricated through melt-spinning, electron-beam curing, and pyrolysis up to 1600 °C in atmospheres of NH3 and N2, using a mixture of poly[tri(methylamino)borazine] (PBN) and polysilazane (PSZ). By analyzing the microstructure and composition of the pyrolyzed ceramic fibers, we found the formation of binary phases including crystalline h-BN and amorphous Si3N4. Further investigations confirmed that this heterogeneous microstructure can only be formed when the introduced ratio of Si3N4 is below 30% in mass. The mean modulus and tensile strength of the fabricated composite fibers were about 90 GPa and 1040 MPa, twice the average of the pure h-BN fiber. The dielectric constant and dielectric loss tangent of the composite fibers is 3.06 and 2.94 × 10−3.