Hui Wang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Hui Wang has a total of 6 co-authors. Here are the top co-authors by number of shared publications:
- Weilong Cong
Department of Industrial, Manufacturing, and System Engineering, Texas Tech University, Lubbock, TX 79409, USA
2 shared publications - Bo Zhao
Texas Tech University, Lubbock, USA
1 shared publication - Dayue Jiang
Department of Systems Science and Industrial Engineering, State University of New York at Binghamton, Binghamton, NY 13902
1 shared publication - Fuda Ning
State University of New York at Binghamton, Binghamton, USA
1 shared publication - Yingbin Hu
Department of Industrial, Manufacturing, and Systems Engineering, Texas Tech University, Lubbock, TX 79409
1 shared publication - Zhichao Liu
West Virginia University, Morgantown, USA
1 shared publication
Latest Publications
- 11 November 2020
- Published by ASME International in Journal of Manufacturing Science and Engineering
- Vol. 143 (5) , 1-30
Ultrasonic Frequency Effects on the Melt Pool Formation, Porosity, and Thermal-Dependent Property of Inconel 718 Fabricated by Ultrasonic Vibration-Assisted Directed Energy Deposition
Ultrasonic vibration-assisted (UV-A) directed energy deposition (DED) has become a promising technology to improve the as-built quality and mechanical performance of metal parts. Ultrasonic frequency, a critical parameter of the ultrasonic vibration, can remarkably affect the ultrasonic vibration behaviors in assisting DED processes. However, leveraging varied ultrasonic frequencies in UV-A DED attracts little attention, and the effects of ultrasonic frequency have been thus overlooked. Linking ultrasonic frequency and part performance emphasizes the need for an understanding of the underlying thermodynamics in the melt pool due to the key role of thermal history in the DED process. In this work, we fabricated Inconel 718 (IN718) parts using the UV-A DED process under different levels of ultrasonic vibration frequency (including 0, 25 kHz, 33 kHz, and 41 kHz). For the first time, melt pool size, temperature distribution, and peak temperature within the melt pool, as well as the peak temperature fluctuation within a layer deposition, were studied. Porosity and thermal-dependent properties including grain size and microhardness were also investigated. The results indicated that the increase in ultrasonic frequency led to an increase in both melt pool size and peak temperature. Moreover, the lowest porosity was obtained at an ultrasonic frequency of 25 kHz, while grain refinement and microhardness enhancement were achieved at the highest frequency of 41 kHz. This investigation provides great insights into the link among ultrasonic frequency, melt pool formation, temperature field, porosity, and thermal-dependent properties in the UV-A DED-built IN718 parts.
- 11 November 2020
- Published by ASME International in Journal of Manufacturing Science and Engineering
- Vol. 143 (5) , 1-30
Ultrasonic Frequency Effects on the Melt Pool Formation, Porosity, and Thermal-Dependent Property of Inconel 718 Fabricated by Ultrasonic Vibration-Assisted Directed Energy Deposition
Ultrasonic vibration-assisted (UV-A) directed energy deposition (DED) has become a promising technology to improve the as-built quality and mechanical performance of metal parts. Ultrasonic frequency, a critical parameter of the ultrasonic vibration, can remarkably affect the ultrasonic vibration behaviors in assisting DED processes. However, leveraging varied ultrasonic frequencies in UV-A DED attracts little attention, and the effects of ultrasonic frequency have been thus overlooked. Linking ultrasonic frequency and part performance emphasizes the need for an understanding of the underlying thermodynamics in the melt pool due to the key role of thermal history in the DED process. In this work, we fabricated Inconel 718 (IN718) parts using the UV-A DED process under different levels of ultrasonic vibration frequency (including 0, 25 kHz, 33 kHz, and 41 kHz). For the first time, melt pool size, temperature distribution, and peak temperature within the melt pool, as well as the peak temperature fluctuation within a layer deposition, were studied. Porosity and thermal-dependent properties including grain size and microhardness were also investigated. The results indicated that the increase in ultrasonic frequency led to an increase in both melt pool size and peak temperature. Moreover, the lowest porosity was obtained at an ultrasonic frequency of 25 kHz, while grain refinement and microhardness enhancement were achieved at the highest frequency of 41 kHz. This investigation provides great insights into the link among ultrasonic frequency, melt pool formation, temperature field, porosity, and thermal-dependent properties in the UV-A DED-built IN718 parts.
- 17 December 2019
- Published by ASME International in Journal of Manufacturing Science and Engineering
- Vol. 142 (2) , 1-20
Directed Energy Deposition of Zirconia-Toughened Alumina Ceramic: Novel Microstructure Formation and Mechanical Performance
Over the past two decades, a considerable amount of work has been done on zirconia toughened alumina (ZTA) to take advantage of the recognized toughening effect induced by ZrO2. In fabricating customized or complex-shaped ZTA parts, conventional manufacturing processes, including slip casting and powder metallurgy, are regarded as time-consuming and cost-intensive. In response to these problems, directed energy deposition (DED) has been proposed and utilized to fabricate customized ZTA parts with highly flexible features in a shorter cycle time at a lower cost. Investigations have been reported on studying effects of input variables (such as laser power) in DED of ZTA parts, however, there are very limited investigations on effects of ZrO2 content. In this investigation, the effects of ZrO2 content on microstructures and mechanical properties of DED fabricated ZTA parts are studied. Experimental results show that at lower levels of ZrO2 contents (5 wt.%, 10 wt.%, and 20 wt.%), a novel three-dimensional quasi-continuous network (3DQCN) microstructure is tailored, whereas at higher levels of ZrO2 contents (30 wt.%, 35 wt.%, and 41.5 wt.%), eutectic microstructure dominates the whole part. Both the 3DQCN microstructure and the eutectic microstructure are beneficial for toughening ZTA parts. In addition, the 3DQCN microstructure contributes to hardening ZTA parts.
- 17 December 2019
- Published by ASME International in Journal of Manufacturing Science and Engineering
- Vol. 142 (2) , 1-20
Directed Energy Deposition of Zirconia-Toughened Alumina Ceramic: Novel Microstructure Formation and Mechanical Performance
Over the past two decades, a considerable amount of work has been done on zirconia toughened alumina (ZTA) to take advantage of the recognized toughening effect induced by ZrO2. In fabricating customized or complex-shaped ZTA parts, conventional manufacturing processes, including slip casting and powder metallurgy, are regarded as time-consuming and cost-intensive. In response to these problems, directed energy deposition (DED) has been proposed and utilized to fabricate customized ZTA parts with highly flexible features in a shorter cycle time at a lower cost. Investigations have been reported on studying effects of input variables (such as laser power) in DED of ZTA parts, however, there are very limited investigations on effects of ZrO2 content. In this investigation, the effects of ZrO2 content on microstructures and mechanical properties of DED fabricated ZTA parts are studied. Experimental results show that at lower levels of ZrO2 contents (5 wt.%, 10 wt.%, and 20 wt.%), a novel three-dimensional quasi-continuous network (3DQCN) microstructure is tailored, whereas at higher levels of ZrO2 contents (30 wt.%, 35 wt.%, and 41.5 wt.%), eutectic microstructure dominates the whole part. Both the 3DQCN microstructure and the eutectic microstructure are beneficial for toughening ZTA parts. In addition, the 3DQCN microstructure contributes to hardening ZTA parts.