Chengde Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Chengde Li has a total of 8 co-authors. Here are the top co-authors by number of shared publications:
- Huimin Gu
College of Metallurgy, Northeastern University, Shenyang, China
5 shared publications - Lingling Ren
College of Metallurgy, Northeastern University, Shenyang 110000, China
5 shared publications - Shuai Wang
College of Metallurgy, Northeastern University, Shenyang 110000, China
5 shared publications - Wei Wang
Inner Mongolia Metal Material Research Institute, Baotou 014000, China
5 shared publications - Yuchun Zhai
School of Materials and Metallurgy, Northeastern University, Shenyang 110819, China
5 shared publications - Zhenbiao Wang
North East Industrial Materials & Metallurgy Co., Ltd., Fushun 113000, China
5 shared publications
Latest Publications
- Open Access
The Microstructure and Properties of an Al-Mg-0.3Sc Alloy Deposited by Wire Arc Additive Manufacturing
Al-Mg alloys can reach medium strength without a solid solution and quenching treatment, thereby avoiding product distortion caused by quenching, which has attracted the attention of wire arc additive manufacturing (WAAM) researchers. However, the mechanical properties of the WAAM Al-Mg alloy deposits obtained so far are poor. Herein, we describe the preparation of Al-Mg-0.3Sc alloy deposits by WAAM and detail the pores, microstructure, and mechanical properties of the alloy produced in this manner. The results showed that the number and sizes of the pores in WAAM Al-Mg-0.3Sc alloy deposits were equivalent to those in Al-Mg alloy deposits without Sc. The rapid cooling characteristics of the WAAM process make the precipitation morphology, size, and distribution of the primary and secondary Al3Sc phases unique and effectively improve the mechanical properties of the deposit. A primary Al3Sc phase less than 3 μm in size was found to precipitate from the WAAM Al-Mg-0.3Sc alloy deposits. The primary Al3Sc phase refines grains, changes the segregated β(Mg2Al3) phase morphology, and ensures that the mechanical properties of horizontal and vertical samples of the deposits are uniform. After heat treatment at 350 °C for 1 h, the WAAM Al-Mg-0.3Sc alloy deposits precipitated a secondary Al3Sc phase, which was spherical (diameter about 20 nm) and had high dispersity. This phase blocks dislocations and subgrain boundaries, causes a noticeable strengthening effect, and further improves the mechanical properties of the deposits, up to a horizontal samples tensile strength of 415 MPa, a yield strength of 279 MPa, and an elongation of 18.5%, a vertical samples tensile strength of 411 MPa, a yield strength of 279 MPa, and an elongation of 14.5%. This Al-Mg-Sc alloy is expected to be widely used in the WAAM field.
Open AccessThe Microstructure and Properties of an Al-Mg-0.3Sc Alloy Deposited by Wire Arc Additive Manufacturing
Al-Mg alloys can reach medium strength without a solid solution and quenching treatment, thereby avoiding product distortion caused by quenching, which has attracted the attention of wire arc additive manufacturing (WAAM) researchers. However, the mechanical properties of the WAAM Al-Mg alloy deposits obtained so far are poor. Herein, we describe the preparation of Al-Mg-0.3Sc alloy deposits by WAAM and detail the pores, microstructure, and mechanical properties of the alloy produced in this manner. The results showed that the number and sizes of the pores in WAAM Al-Mg-0.3Sc alloy deposits were equivalent to those in Al-Mg alloy deposits without Sc. The rapid cooling characteristics of the WAAM process make the precipitation morphology, size, and distribution of the primary and secondary Al3Sc phases unique and effectively improve the mechanical properties of the deposit. A primary Al3Sc phase less than 3 μm in size was found to precipitate from the WAAM Al-Mg-0.3Sc alloy deposits. The primary Al3Sc phase refines grains, changes the segregated β(Mg2Al3) phase morphology, and ensures that the mechanical properties of horizontal and vertical samples of the deposits are uniform. After heat treatment at 350 °C for 1 h, the WAAM Al-Mg-0.3Sc alloy deposits precipitated a secondary Al3Sc phase, which was spherical (diameter about 20 nm) and had high dispersity. This phase blocks dislocations and subgrain boundaries, causes a noticeable strengthening effect, and further improves the mechanical properties of the deposits, up to a horizontal samples tensile strength of 415 MPa, a yield strength of 279 MPa, and an elongation of 18.5%, a vertical samples tensile strength of 411 MPa, a yield strength of 279 MPa, and an elongation of 14.5%. This Al-Mg-Sc alloy is expected to be widely used in the WAAM field.
- Open Access
The Influence of Heat Input on the Microstructure and Properties of Wire-Arc-Additive-Manufactured Al-Cu-Sn Alloy Deposits
In this experiment, Al-Cu-Sn alloy was used as raw material to form deposits with different heat input using the wire-arc additive manufacturing (WAAM) process. The effects of heat input on microstructure and mechanical properties of Al-Cu-Sn alloy deposits were investigated by metallography, scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and transmission electron microscopy (TEM) and mechanical properties tests. The results show that with increased of heat input, the thickness of the deposits increased and the layer height of the deposits increased. The number and size of pores in the deposits also improved with the increased heat input. The grain size of the deposits in the as-deposited state gradually increased and changed from isometric crystals to columnar crystals, the precipitated θ phases gradually converged on the grain boundary from within the grains. After T6 heat treatment, with increased heat input, the number of unsolved θ phases on the grain boundary increased, and the number of θ phases precipitated out of the matrix decreased as the phase spacing increased. With the increased heat input, the mechanical properties of the deposits gradually decreased, and the fracture mode changed from ductile fracture to brittle fracture.
Open AccessThe Influence of Heat Input on the Microstructure and Properties of Wire-Arc-Additive-Manufactured Al-Cu-Sn Alloy Deposits
In this experiment, Al-Cu-Sn alloy was used as raw material to form deposits with different heat input using the wire-arc additive manufacturing (WAAM) process. The effects of heat input on microstructure and mechanical properties of Al-Cu-Sn alloy deposits were investigated by metallography, scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and transmission electron microscopy (TEM) and mechanical properties tests. The results show that with increased of heat input, the thickness of the deposits increased and the layer height of the deposits increased. The number and size of pores in the deposits also improved with the increased heat input. The grain size of the deposits in the as-deposited state gradually increased and changed from isometric crystals to columnar crystals, the precipitated θ phases gradually converged on the grain boundary from within the grains. After T6 heat treatment, with increased heat input, the number of unsolved θ phases on the grain boundary increased, and the number of θ phases precipitated out of the matrix decreased as the phase spacing increased. With the increased heat input, the mechanical properties of the deposits gradually decreased, and the fracture mode changed from ductile fracture to brittle fracture.
- Open Access
Study on Microstructural and Mechanical Properties of an Al–Cu–Sn Alloy Wall Deposited by Double-Wire Arc Additive Manufacturing Process
In this present study, single-wire and double-wire Al–Cu–Sn alloy walls were fabricated by an arc additive manufacturing process. The surface morphology, elemental composition, and microstructure were investigated by scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and transmission electron microscopy (TEM) techniques. The mechanical properties of both the single-wire and double-wire walls were studied by mechanical property testing. The results showed that the heat input of the double-wire wall was lower than that of the single-wire wall at the same wire feeding speed. The surface microstructure of the double-wire wall showed a more uniform surface than the single-wire wall. The grains of the double-wire wall were found to be isometric crystals in the as-deposited state. The θ phase of the double-wire wall was dispersed with a smaller grain size in the grain boundary. After T6 heat treatment, the θ phase of the double-wire wall was completely dissolved into the aluminum matrix, and a large amount of θ’ enhanced phases were precipitated with a phase spacing of about 15 nm. The mechanical properties of the double-wire wall were shown to have significantly improved performance, which further increased to 490 MPa, 420 MPa, and 12%, respectively. The transverse and longitudinal mechanical properties of the double-wire wall were consistent, and the fracture mode of both was ductile fracture.
Open AccessStudy on Microstructural and Mechanical Properties of an Al–Cu–Sn Alloy Wall Deposited by Double-Wire Arc Additive Manufacturing Process
In this present study, single-wire and double-wire Al–Cu–Sn alloy walls were fabricated by an arc additive manufacturing process. The surface morphology, elemental composition, and microstructure were investigated by scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and transmission electron microscopy (TEM) techniques. The mechanical properties of both the single-wire and double-wire walls were studied by mechanical property testing. The results showed that the heat input of the double-wire wall was lower than that of the single-wire wall at the same wire feeding speed. The surface microstructure of the double-wire wall showed a more uniform surface than the single-wire wall. The grains of the double-wire wall were found to be isometric crystals in the as-deposited state. The θ phase of the double-wire wall was dispersed with a smaller grain size in the grain boundary. After T6 heat treatment, the θ phase of the double-wire wall was completely dissolved into the aluminum matrix, and a large amount of θ’ enhanced phases were precipitated with a phase spacing of about 15 nm. The mechanical properties of the double-wire wall were shown to have significantly improved performance, which further increased to 490 MPa, 420 MPa, and 12%, respectively. The transverse and longitudinal mechanical properties of the double-wire wall were consistent, and the fracture mode of both was ductile fracture.
- Open Access
- 20 December 2019
- Published by MDPI AG in Applied Sciences
- Vol. 10 (1) , 70
Effect of Heat Input on Formability, Microstructure, and Properties of Al–7Si–0.6Mg Alloys Deposited by CMT-WAAM Process
In order to improve the forming efficiency of Al–7Si–0.6Mg fabricated by wire and arc additive manufacturing process (WAAM), wire with a diameter of 1.6 mm was selected as the raw material. The effect of heat input on the formability, microstructure, and properties of the WAAM alloy was investigated, and the forming model was established. The WAAM alloys were characterized by electronic universal testing, scanning electron microscopy, energy spectrum analysis, and metallographic microscopy. The results show that Al–7Si–0.6Mg alloy has a large processing window under the cold metal transfer (CMT) process, and it can be well formed with a large range of heat input. The secondary dendrite arm spacing and Fe-phase in the as-deposited alloy gradually increase with an increase in heat input, and slight overburning occurs in the heat affected zone at higher heat inputs. After solid solution and aging treatment (T6 heat treatment), the size of α-Al grain and eutectic silicon grain increases with the increase of heat input. Little anisotropy in the mechanical properties is observed except at higher heat inputs. The tensile strength is 354.5 MPa ± 7.5 MPa, yield strength is 310 MPa ± 5.5 MPa, and elongation is 6.3 ± 0.7%.
- 20 December 2019
- Published by MDPI AG in Applied Sciences
- Vol. 10 (1) , 70
Open AccessEffect of Heat Input on Formability, Microstructure, and Properties of Al–7Si–0.6Mg Alloys Deposited by CMT-WAAM Process
In order to improve the forming efficiency of Al–7Si–0.6Mg fabricated by wire and arc additive manufacturing process (WAAM), wire with a diameter of 1.6 mm was selected as the raw material. The effect of heat input on the formability, microstructure, and properties of the WAAM alloy was investigated, and the forming model was established. The WAAM alloys were characterized by electronic universal testing, scanning electron microscopy, energy spectrum analysis, and metallographic microscopy. The results show that Al–7Si–0.6Mg alloy has a large processing window under the cold metal transfer (CMT) process, and it can be well formed with a large range of heat input. The secondary dendrite arm spacing and Fe-phase in the as-deposited alloy gradually increase with an increase in heat input, and slight overburning occurs in the heat affected zone at higher heat inputs. After solid solution and aging treatment (T6 heat treatment), the size of α-Al grain and eutectic silicon grain increases with the increase of heat input. Little anisotropy in the mechanical properties is observed except at higher heat inputs. The tensile strength is 354.5 MPa ± 7.5 MPa, yield strength is 310 MPa ± 5.5 MPa, and elongation is 6.3 ± 0.7%.
- Open Access
Effect of Mg Content on Microstructure and Properties of Al–Mg Alloy Produced by the Wire Arc Additive Manufacturing Method
In this study, an Al–Mg alloy was fabricated by wire arc additive manufacture (WAAM), and the effect of Mg content on the microstructure and properties of Al–Mg alloy deposits was investigated. The effects on the deposition surface oxidation, geometry, burn out rate of Mg, pores, microstructure, mechanical properties and fracture mechanisms were investigated. The results show that, when the Mg content increased, the surface oxidation degree increased; a “wave”-shaped deposition layer occurred when the Mg content reached 8%. When the Mg content was more than 6%, the burning loss rate of the Mg element increased significantly. With the increase of Mg content, the number of pores first decreased and then increased, and the size first decreased and then increased. When the Mg content reached 7% or above, obvious crystallization hot cracks appeared in the deposit bodies. When the Mg content increased, the precipitated phase (FeMn)Al6 and β(Mg2Al3) increased, and the grain size increased. When the Mg content was 6%, the comprehensive mechanical properties were best. The horizontal tensile strength, yield strength and elongation were 310 MPa, 225 MPa and 17%, respectively. The vertical tensile strength, yield strength and elongation were 300 MPa, 215 MPa and 15%, respectively. The fracture morphology was a ductile fracture.
Open AccessEffect of Mg Content on Microstructure and Properties of Al–Mg Alloy Produced by the Wire Arc Additive Manufacturing Method
In this study, an Al–Mg alloy was fabricated by wire arc additive manufacture (WAAM), and the effect of Mg content on the microstructure and properties of Al–Mg alloy deposits was investigated. The effects on the deposition surface oxidation, geometry, burn out rate of Mg, pores, microstructure, mechanical properties and fracture mechanisms were investigated. The results show that, when the Mg content increased, the surface oxidation degree increased; a “wave”-shaped deposition layer occurred when the Mg content reached 8%. When the Mg content was more than 6%, the burning loss rate of the Mg element increased significantly. With the increase of Mg content, the number of pores first decreased and then increased, and the size first decreased and then increased. When the Mg content reached 7% or above, obvious crystallization hot cracks appeared in the deposit bodies. When the Mg content increased, the precipitated phase (FeMn)Al6 and β(Mg2Al3) increased, and the grain size increased. When the Mg content was 6%, the comprehensive mechanical properties were best. The horizontal tensile strength, yield strength and elongation were 310 MPa, 225 MPa and 17%, respectively. The vertical tensile strength, yield strength and elongation were 300 MPa, 215 MPa and 15%, respectively. The fracture morphology was a ductile fracture.