Zhenbiao Wang has a total of 12 co-authors. Here are the top co-authors by number of shared publications:


Latest Publications

  • Open Access

    Correction: Wang et al. Effect of the Deposition Process on High-Temperature Microstructure and Properties of the Direct Energy Deposition Al-Cu Alloy. Metals 2023, 13, 765

    by Zhenbiao Wang, Shuai Wang, Lingling Ren, Chengde Li, Wei Wang, Zhu Ming, Yuchun Zhai

  • Open Access

    Correction: Ren et al. The Effect of Cu Content on the Microstructure and Properties of the Wire Arc Additive Manufacturing Al-Cu Alloy. Materials 2023, 16, 2694

    by Lingling Ren, Zhenbiao Wang, Shuai Wang, Chengde Li, Wei Wang, Zhu Ming, Yuchun Zhai

  • Open Access

    Effect of the Deposition Process on High-Temperature Microstructure and Properties of the Direct Energy Deposition Al-Cu Alloy

    by Zhenbiao Wang, Shuai Wang, Lingling Ren, Chengde Li, Wei Wang, Zhu Ming, Yuchun Zhai

    The excellent microstructure and mechanical properties of Al-Cu alloy deposited using the Direct Energy Deposition (DED) process has been shown in previous studies, which is the most likely aluminum alloy material to meet the load-bearing requirements of hypersonic aircraft. However, its high-temperature performance and the law of microstructure transformation during the high-temperature process still need to be determined. In this paper, DED Al-Cu alloy samples were prepared using the Cold Metal Transfer (CMT) process, CMT Pulse process, and CMT Pulse Advanced process. The effect of different deposition processes on the microstructure and mechanical properties of the deposits was investigated at 200 °C for 30 min. The results show that the Al-Cu alloy’s main strengthening phase θ′ is excessively transformed into the equilibrium θ phase after the high-temperature process, which is the main reason for the degradation in the DED Al-Cu alloy’s properties at high temperatures. Different deposition processes have almost no effect on the high-temperature performance of the DED Al-Cu alloy, and the deposition process can be selected according to the product’s structure.


  • Open Access

    The Effect of Cu Content on the Microstructure and Properties of the Wire Arc Additive Manufacturing Al-Cu Alloy

    by Lingling Ren, Zhenbiao Wang, Shuai Wang, Chengde Li, Wei Wang, Zhu Ming, Yuchun Zhai

    Al-Cu alloy has broad application prospects in the field of aerospace due to its excellent performance. In this paper, deposits with different Cu contents were prepared by the wire arc additive manufacturing (WAAM) process, and the effects of Cu content on the microstructure and mechanical properties were investigated. The microstructure of Al-Cu alloy was investigated by metallography, scanning electron microscope (SEM), energy-dispersive spectrometer (EDS), and transmission electron microscope (TEM). The results show that both the number and size of the precipitated θ phases (Al2Cu) in the as-deposited material increase with the increase of Cu content. After the T4 treatment, the solid solution amount of Cu in the matrix showed a trend of first increasing and then remaining stable. When the content of Cu was greater than 5.65%, as the Cu content increased, the number and size of the remaining θ phases both increased. In the peak ageing state, the amount of precipitated θ’ phase showed a trend of increasing and then remaining stable. After the T6 treatment, the mechanical properties showed a trend of first increasing and then decreasing with the increase of the content of Cu. When the Cu content was 5.65%, the deposit achieved the best mechanical properties, and the anisotropy of the mechanical properties disappeared. The tensile strength, yield strength, and elongation reached 538 MPa, 478 MPa, and 10.5%, respectively. When the content of Cu was greater than 5.65%, the anisotropy of mechanical properties was obvious, and the fracture mode of the vertical specimen changed from ductile fracture to brittle fracture.


  • Open Access

    The Microstructure and Properties of an Al-Mg-0.3Sc Alloy Deposited by Wire Arc Additive Manufacturing

    by Lingling Ren, Huimin Gu, Wei Wang, Shuai Wang, Chengde Li, Zhenbiao Wang, Yuchun Zhai, Peihua Ma

    Al-Mg alloys can reach medium strength without a solid solution and quenching treatment, thereby avoiding product distortion caused by quenching, which has attracted the attention of wire arc additive manufacturing (WAAM) researchers. However, the mechanical properties of the WAAM Al-Mg alloy deposits obtained so far are poor. Herein, we describe the preparation of Al-Mg-0.3Sc alloy deposits by WAAM and detail the pores, microstructure, and mechanical properties of the alloy produced in this manner. The results showed that the number and sizes of the pores in WAAM Al-Mg-0.3Sc alloy deposits were equivalent to those in Al-Mg alloy deposits without Sc. The rapid cooling characteristics of the WAAM process make the precipitation morphology, size, and distribution of the primary and secondary Al3Sc phases unique and effectively improve the mechanical properties of the deposit. A primary Al3Sc phase less than 3 μm in size was found to precipitate from the WAAM Al-Mg-0.3Sc alloy deposits. The primary Al3Sc phase refines grains, changes the segregated β(Mg2Al3) phase morphology, and ensures that the mechanical properties of horizontal and vertical samples of the deposits are uniform. After heat treatment at 350 °C for 1 h, the WAAM Al-Mg-0.3Sc alloy deposits precipitated a secondary Al3Sc phase, which was spherical (diameter about 20 nm) and had high dispersity. This phase blocks dislocations and subgrain boundaries, causes a noticeable strengthening effect, and further improves the mechanical properties of the deposits, up to a horizontal samples tensile strength of 415 MPa, a yield strength of 279 MPa, and an elongation of 18.5%, a vertical samples tensile strength of 411 MPa, a yield strength of 279 MPa, and an elongation of 14.5%. This Al-Mg-Sc alloy is expected to be widely used in the WAAM field.


  • Open Access

    The Influence of Heat Input on the Microstructure and Properties of Wire-Arc-Additive-Manufactured Al-Cu-Sn Alloy Deposits

    by Shuai Wang, Huimin Gu, Wei Wang, Chengde Li, Lingling Ren, Zhenbiao Wang, Yuchun Zhai, Peihua Ma

    In this experiment, Al-Cu-Sn alloy was used as raw material to form deposits with different heat input using the wire-arc additive manufacturing (WAAM) process. The effects of heat input on microstructure and mechanical properties of Al-Cu-Sn alloy deposits were investigated by metallography, scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and transmission electron microscopy (TEM) and mechanical properties tests. The results show that with increased of heat input, the thickness of the deposits increased and the layer height of the deposits increased. The number and size of pores in the deposits also improved with the increased heat input. The grain size of the deposits in the as-deposited state gradually increased and changed from isometric crystals to columnar crystals, the precipitated θ phases gradually converged on the grain boundary from within the grains. After T6 heat treatment, with increased heat input, the number of unsolved θ phases on the grain boundary increased, and the number of θ phases precipitated out of the matrix decreased as the phase spacing increased. With the increased heat input, the mechanical properties of the deposits gradually decreased, and the fracture mode changed from ductile fracture to brittle fracture.


  • Open Access

    Study on Microstructural and Mechanical Properties of an Al–Cu–Sn Alloy Wall Deposited by Double-Wire Arc Additive Manufacturing Process

    by Shuai Wang, Huimin Gu, Wei Wang, Chengde Li, Lingling Ren, Zhenbiao Wang, Yuchun Zhai, Peihua Ma

    In this present study, single-wire and double-wire Al–Cu–Sn alloy walls were fabricated by an arc additive manufacturing process. The surface morphology, elemental composition, and microstructure were investigated by scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and transmission electron microscopy (TEM) techniques. The mechanical properties of both the single-wire and double-wire walls were studied by mechanical property testing. The results showed that the heat input of the double-wire wall was lower than that of the single-wire wall at the same wire feeding speed. The surface microstructure of the double-wire wall showed a more uniform surface than the single-wire wall. The grains of the double-wire wall were found to be isometric crystals in the as-deposited state. The θ phase of the double-wire wall was dispersed with a smaller grain size in the grain boundary. After T6 heat treatment, the θ phase of the double-wire wall was completely dissolved into the aluminum matrix, and a large amount of θ’ enhanced phases were precipitated with a phase spacing of about 15 nm. The mechanical properties of the double-wire wall were shown to have significantly improved performance, which further increased to 490 MPa, 420 MPa, and 12%, respectively. The transverse and longitudinal mechanical properties of the double-wire wall were consistent, and the fracture mode of both was ductile fracture.


  • Open Access

    Effect of Heat Input on Formability, Microstructure, and Properties of Al–7Si–0.6Mg Alloys Deposited by CMT-WAAM Process

    by Chengde Li, Huimin Gu, Wei Wang, Shuai Wang, Lingling Ren, Zhenbiao Wang, Zhu Ming, Yuchun Zhai

    In order to improve the forming efficiency of Al–7Si–0.6Mg fabricated by wire and arc additive manufacturing process (WAAM), wire with a diameter of 1.6 mm was selected as the raw material. The effect of heat input on the formability, microstructure, and properties of the WAAM alloy was investigated, and the forming model was established. The WAAM alloys were characterized by electronic universal testing, scanning electron microscopy, energy spectrum analysis, and metallographic microscopy. The results show that Al–7Si–0.6Mg alloy has a large processing window under the cold metal transfer (CMT) process, and it can be well formed with a large range of heat input. The secondary dendrite arm spacing and Fe-phase in the as-deposited alloy gradually increase with an increase in heat input, and slight overburning occurs in the heat affected zone at higher heat inputs. After solid solution and aging treatment (T6 heat treatment), the size of α-Al grain and eutectic silicon grain increases with the increase of heat input. Little anisotropy in the mechanical properties is observed except at higher heat inputs. The tensile strength is 354.5 MPa ± 7.5 MPa, yield strength is 310 MPa ± 5.5 MPa, and elongation is 6.3 ± 0.7%.


  • Open Access

    Effect of Mg Content on Microstructure and Properties of Al–Mg Alloy Produced by the Wire Arc Additive Manufacturing Method

    by Lingling Ren, Huimin Gu, Wei Wang, Shuai Wang, Chengde Li, Zhenbiao Wang, Yuchun Zhai, Peihua Ma

    In this study, an Al–Mg alloy was fabricated by wire arc additive manufacture (WAAM), and the effect of Mg content on the microstructure and properties of Al–Mg alloy deposits was investigated. The effects on the deposition surface oxidation, geometry, burn out rate of Mg, pores, microstructure, mechanical properties and fracture mechanisms were investigated. The results show that, when the Mg content increased, the surface oxidation degree increased; a “wave”-shaped deposition layer occurred when the Mg content reached 8%. When the Mg content was more than 6%, the burning loss rate of the Mg element increased significantly. With the increase of Mg content, the number of pores first decreased and then increased, and the size first decreased and then increased. When the Mg content reached 7% or above, obvious crystallization hot cracks appeared in the deposit bodies. When the Mg content increased, the precipitated phase (FeMn)Al6 and β(Mg2Al3) increased, and the grain size increased. When the Mg content was 6%, the comprehensive mechanical properties were best. The horizontal tensile strength, yield strength and elongation were 310 MPa, 225 MPa and 17%, respectively. The vertical tensile strength, yield strength and elongation were 300 MPa, 215 MPa and 15%, respectively. The fracture morphology was a ductile fracture.