Mert Terzi
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Mert Terzi has a total of 15 co-authors. Here are the top co-authors by number of shared publications:
- Ilgin Kursun
İstanbul Üniversitesi-Cerrahpaşa
12 shared publications - Orhan Ozdemir
Department of Mineral Processing Engineering, Faculty of Mines, Istanbul Technical University, 34469 Istanbul, Türkiye
6 shared publications - Can Gungoren
Mining Engineering Department, Engineering Faculty, Istanbul University-Cerrahapasa, 34320 Istanbul, Türkiye
3 shared publications - Emrah Durgut
Mining and Extraction Department, Can Vocational School, Canakkale Onsekiz Mart University, Canakkale 17400, Türkiye
2 shared publications - Mustafa Cinar
ÇANAKKALE ONSEKİZ MART ÜNİVERSİTESİ, MÜHENDİSLİK FAKÜLTESİ, MADEN MÜHENDİSLİĞİ BÖLÜMÜ
2 shared publications - Saleban Mohamed Muse
İstanbul Üniversitesi-Cerrahpaşa
2 shared publications
Latest Publications
- Open Access
Effect of Nitrogen Gas on Sulfide Gold Ore Flotation in the Presence of Combined Collectors
In this study, the effects of the nitrogen gas (N2) phase on bench-scale flotation efficiency and kinetics were investigated by a series of flotation experiments on a complex Au-bearing sulfide ore using sodium isobutyl xanthate (SIBX), monothiophosphate (Aero S-8045) and an isopropylethyl thiocarbamate-dominant reagent (Aero Float MX-505). In the presence of nitrogen, the use of both the SIBX-S-8045 binary system and MX-505 resulted in improvements compared to the use of air, across nearly all collector dosages examined in terms of both Au recovery and grade. On the other hand, flotation results with the SIBX-MX-505 binary collector system showed improvements of 4% in Au recovery in the presence of N2 compared to air under the same flotation conditions. Furthermore, it has been observed that this increase in recovery is accompanied by a slight decrease in the Au grade. The results of the flotation kinetics evaluations have shown that the second-order and first-order model with rectangular distribution of flotabilities generally has the highest correlation with the experimental results compared to the other models for SIBX-S-8045 and SIBX-MX-505, respectively. In the presence of air and N2, the flotation rate constant (k) in the second-order model with rectangular distribution of flotabilities was determined as 4.425 (R2 = 0.9947) and 8.2402 (R2 = 0.9977) for the SIBX-S-8045 system. Moreover, k was determined as 4.7257 (R2 = 0.9503) and 6.3775 (R2 = 0.9728) in the same model for the SIBX-MX-505 system in the presence of air and N2, respectively. Therefore, it was determined that the N2 phase had significantly faster kinetics compared to the air phase in both binary collector systems.
Open AccessEffect of Nitrogen Gas on Sulfide Gold Ore Flotation in the Presence of Combined Collectors
In this study, the effects of the nitrogen gas (N2) phase on bench-scale flotation efficiency and kinetics were investigated by a series of flotation experiments on a complex Au-bearing sulfide ore using sodium isobutyl xanthate (SIBX), monothiophosphate (Aero S-8045) and an isopropylethyl thiocarbamate-dominant reagent (Aero Float MX-505). In the presence of nitrogen, the use of both the SIBX-S-8045 binary system and MX-505 resulted in improvements compared to the use of air, across nearly all collector dosages examined in terms of both Au recovery and grade. On the other hand, flotation results with the SIBX-MX-505 binary collector system showed improvements of 4% in Au recovery in the presence of N2 compared to air under the same flotation conditions. Furthermore, it has been observed that this increase in recovery is accompanied by a slight decrease in the Au grade. The results of the flotation kinetics evaluations have shown that the second-order and first-order model with rectangular distribution of flotabilities generally has the highest correlation with the experimental results compared to the other models for SIBX-S-8045 and SIBX-MX-505, respectively. In the presence of air and N2, the flotation rate constant (k) in the second-order model with rectangular distribution of flotabilities was determined as 4.425 (R2 = 0.9947) and 8.2402 (R2 = 0.9977) for the SIBX-S-8045 system. Moreover, k was determined as 4.7257 (R2 = 0.9503) and 6.3775 (R2 = 0.9728) in the same model for the SIBX-MX-505 system in the presence of air and N2, respectively. Therefore, it was determined that the N2 phase had significantly faster kinetics compared to the air phase in both binary collector systems.
- Open Access
- 6 October 2026
- Published by Afyon Kocatepe Universitesi Fen Ve Muhendislik Bilimleri Dergisi in Afyon Kocatepe University Journal of Sciences and Engineering
- Vol. 26 (5) , 1194-1201
Çözünmüş İyon Konsantrasyonunun Galenin Islanabilirliği ve Flotasyon Davranışı Üzerindeki Etkisi
Minerallerin flotasyon davranışı, flotasyon suyunda bulunan çözünmüş iyonların mineral ıslanabilirliği ve kabarcık-tane etkileşimleri üzerindeki etkileri nedeniyle değişebilmektedir. Bu çalışmada, yapay flotasyon sularında bulunan çözünmüş iyonların karmaşık bir sülfürlü cevherdeki galenin hidrofobluğu ve flotasyon davranışı üzerindeki birleşik etkisi araştırılmıştır. Na+, Ca2+, Mg2+, Pb2+, Zn2+, Cu2+, Fe3+, Cl-, NO3-, CO32- ve SO42- iyonlarını içeren yapay sular dört farklı konsantrasyon seviyesinde (APW1, APW3, APW5 ve APW10) hazırlanmıştır; daha yüksek konsantrasyonlu suların elde edilmesi için APW1’deki iyon konsantrasyonları sırasıyla üç, beş ve on kat artırılmıştır. Artan iyon konsantrasyonunun galenin davranışı üzerindeki etkisini değerlendirmek amacıyla cevher karakterizasyonu, pH profili deneyleri, dinamik temas açısı ölçümleri ve kesikli flotasyon deneyleri gerçekleştirilmiştir. Galen cevherinin yaklaşık 8 tampon pH değerine sahip olduğu belirlenmiştir. Saf suda 39° olan başlangıç temas açısı APW1 varlığında 54°’ye yükselmiş ve 50 g/t potasyum etil ksantat (KEX) varlığında 60°’ye ulaşmıştır. Bununla birlikte, iyon konsantrasyonunun daha fazla artırılması hem KEX yokluğunda hem de varlığında galenin hidrofobluğunu kademeli olarak azaltmıştır. Flotasyon deneylerinde galen kazanma verimi saf suda %79,1 iken APW1 varlığında hafif bir artışla %82,0’ye yükselmiş, ancak APW konsantrasyonunun daha fazla artırılması kazanma veriminde veya konsantre Pb tenöründe belirgin bir iyileşme sağlamamıştır. Bu sonuçlar, çözünmüş iyonların orta düzeydeki konsantrasyonlarının galenin ıslanabilirliğini ve flotasyon davranışını iyileştirebildiğini, ancak toplam iyon konsantrasyonunun belirli bir seviyenin üzerine çıkarılmasının flotasyon açısından ilave bir fayda sağlamadığını göstermektedir. Bulgular, karmaşık sülfürlü cevherlerin zenginleştirilmesinde geri dönüştürülmüş veya iyon bakımından zengin sular kullanıldığında, flotasyon suyunun genel iyonik ortamının kontrol edilmesinin önemini ortaya koymaktadır.
- 6 October 2026
- Published by Afyon Kocatepe Universitesi Fen Ve Muhendislik Bilimleri Dergisi in Afyon Kocatepe University Journal of Sciences and Engineering
- Vol. 26 (5) , 1194-1201
Open AccessÇözünmüş İyon Konsantrasyonunun Galenin Islanabilirliği ve Flotasyon Davranışı Üzerindeki Etkisi
Minerallerin flotasyon davranışı, flotasyon suyunda bulunan çözünmüş iyonların mineral ıslanabilirliği ve kabarcık-tane etkileşimleri üzerindeki etkileri nedeniyle değişebilmektedir. Bu çalışmada, yapay flotasyon sularında bulunan çözünmüş iyonların karmaşık bir sülfürlü cevherdeki galenin hidrofobluğu ve flotasyon davranışı üzerindeki birleşik etkisi araştırılmıştır. Na+, Ca2+, Mg2+, Pb2+, Zn2+, Cu2+, Fe3+, Cl-, NO3-, CO32- ve SO42- iyonlarını içeren yapay sular dört farklı konsantrasyon seviyesinde (APW1, APW3, APW5 ve APW10) hazırlanmıştır; daha yüksek konsantrasyonlu suların elde edilmesi için APW1’deki iyon konsantrasyonları sırasıyla üç, beş ve on kat artırılmıştır. Artan iyon konsantrasyonunun galenin davranışı üzerindeki etkisini değerlendirmek amacıyla cevher karakterizasyonu, pH profili deneyleri, dinamik temas açısı ölçümleri ve kesikli flotasyon deneyleri gerçekleştirilmiştir. Galen cevherinin yaklaşık 8 tampon pH değerine sahip olduğu belirlenmiştir. Saf suda 39° olan başlangıç temas açısı APW1 varlığında 54°’ye yükselmiş ve 50 g/t potasyum etil ksantat (KEX) varlığında 60°’ye ulaşmıştır. Bununla birlikte, iyon konsantrasyonunun daha fazla artırılması hem KEX yokluğunda hem de varlığında galenin hidrofobluğunu kademeli olarak azaltmıştır. Flotasyon deneylerinde galen kazanma verimi saf suda %79,1 iken APW1 varlığında hafif bir artışla %82,0’ye yükselmiş, ancak APW konsantrasyonunun daha fazla artırılması kazanma veriminde veya konsantre Pb tenöründe belirgin bir iyileşme sağlamamıştır. Bu sonuçlar, çözünmüş iyonların orta düzeydeki konsantrasyonlarının galenin ıslanabilirliğini ve flotasyon davranışını iyileştirebildiğini, ancak toplam iyon konsantrasyonunun belirli bir seviyenin üzerine çıkarılmasının flotasyon açısından ilave bir fayda sağlamadığını göstermektedir. Bulgular, karmaşık sülfürlü cevherlerin zenginleştirilmesinde geri dönüştürülmüş veya iyon bakımından zengin sular kullanıldığında, flotasyon suyunun genel iyonik ortamının kontrol edilmesinin önemini ortaya koymaktadır.
- Open Access
- 30 September 2024
- Published by Canakkale Onsekiz Mart University in Journal of Advanced Research in Natural and Applied Sciences
- Vol. 10 (3) , 587-600
Particle Shape-Based Evaluation of the Leaching of Sphalerite Ore in Dilute Acid Solutions
In this study, the effects of changes in particle shapes on dissolution efficiencies in zinc (Zn) recovery from a lead-zinc (Pb-Zn) ore by acid leaching method were investigated. In the experiments with nitric acid (HNO3), sulfuric acid (H2SO4), and hydrochloric acid (HCl), particle size (75-106-150 µm), solids ratio (5-10-15-20-25%), leaching time (30-60-120-180-240 min), acid dosage (0.25-0.5-1-2-5 M) and pulp temperature (30-40-50-60-70 oC) parameters were analyzed. Optimum results were obtained under the conditions of 75 µm particle size, 15% solids ratio, 120 min leaching time, 0.5 M acid dosage, and 50°C pulp temperature for H2SO4; 106 µm particle size, 25% solids ratio, 60 min leaching time, 0.5 M acid dosage, and 70°C pulp temperature for HCl; 75 µm particle size, 20% solids ratio, 60 min leaching time, 1 M acid dosage, and 50°C pulp temperature for HNO3. As a consequence of the tests performed under these optimized conditions, 97.32%, 96.38% and 96.06% Zn dissolution efficiencies were obtained. Within the context of particle shape factor research, microscope images of the leaching residues were obtained from the experiments in which the pulp temperature, acid dosage, and leaching time parameters were examined. The samples obtained from the experiments with all three acids were compared with the ore samples, and the impacts of changes in circularity, roundness, and solidity values on dissolution efficiencies were interpreted.
- 30 September 2024
- Published by Canakkale Onsekiz Mart University in Journal of Advanced Research in Natural and Applied Sciences
- Vol. 10 (3) , 587-600
Open AccessParticle Shape-Based Evaluation of the Leaching of Sphalerite Ore in Dilute Acid Solutions
In this study, the effects of changes in particle shapes on dissolution efficiencies in zinc (Zn) recovery from a lead-zinc (Pb-Zn) ore by acid leaching method were investigated. In the experiments with nitric acid (HNO3), sulfuric acid (H2SO4), and hydrochloric acid (HCl), particle size (75-106-150 µm), solids ratio (5-10-15-20-25%), leaching time (30-60-120-180-240 min), acid dosage (0.25-0.5-1-2-5 M) and pulp temperature (30-40-50-60-70 oC) parameters were analyzed. Optimum results were obtained under the conditions of 75 µm particle size, 15% solids ratio, 120 min leaching time, 0.5 M acid dosage, and 50°C pulp temperature for H2SO4; 106 µm particle size, 25% solids ratio, 60 min leaching time, 0.5 M acid dosage, and 70°C pulp temperature for HCl; 75 µm particle size, 20% solids ratio, 60 min leaching time, 1 M acid dosage, and 50°C pulp temperature for HNO3. As a consequence of the tests performed under these optimized conditions, 97.32%, 96.38% and 96.06% Zn dissolution efficiencies were obtained. Within the context of particle shape factor research, microscope images of the leaching residues were obtained from the experiments in which the pulp temperature, acid dosage, and leaching time parameters were examined. The samples obtained from the experiments with all three acids were compared with the ore samples, and the impacts of changes in circularity, roundness, and solidity values on dissolution efficiencies were interpreted.
- Open Access
Synergistic Effect of Frequently Found Ions in the Flotation of Pb-Zn Sulfide Ores on Air/Water Interface
The aqueous ions influence the properties of air bubbles and, therefore, the recovery of flotation. This study aims to reveal the synergistic effect of frequently found ions in the flotation of Pb-Zn sulfide ores. In this context, dynamic surface tension measurements, bubble coalescence time, Sauter mean diameter (SMD), bubble size distribution (BSD), and dynamic foam stability (DFS) measurements were carried out using artificial process waters (APWs). APW with the minimum ion concentration is expressed as “APW1” with the ionic strength (I) of 0.03 mol/dm3. The concentration of the ions in APW1 was increased by 3, 5, and 10 times, and thus APW3 (I = 0.08 mol/dm3), APW5 (I = 0.13 mol/dm3), and APW10 (I = 0.26 mol/dm3) were prepared, respectively. The results of this study indicated that the surface tension increased slightly in the presence of APW related to the ion concentration. Potassium ethyl xanthate (KEX) at high concentrations was effective in the reduction of surface tension. As the APW concentration increased, finer bubbles were obtained with a narrower size range. The stability of the foam increased with butyl glycol (BG) and APW concentration. There was no need to use a frother (BG) for the flotation experiments in the presence of APW1 or APWs with higher ionic strength.
Open AccessSynergistic Effect of Frequently Found Ions in the Flotation of Pb-Zn Sulfide Ores on Air/Water Interface
The aqueous ions influence the properties of air bubbles and, therefore, the recovery of flotation. This study aims to reveal the synergistic effect of frequently found ions in the flotation of Pb-Zn sulfide ores. In this context, dynamic surface tension measurements, bubble coalescence time, Sauter mean diameter (SMD), bubble size distribution (BSD), and dynamic foam stability (DFS) measurements were carried out using artificial process waters (APWs). APW with the minimum ion concentration is expressed as “APW1” with the ionic strength (I) of 0.03 mol/dm3. The concentration of the ions in APW1 was increased by 3, 5, and 10 times, and thus APW3 (I = 0.08 mol/dm3), APW5 (I = 0.13 mol/dm3), and APW10 (I = 0.26 mol/dm3) were prepared, respectively. The results of this study indicated that the surface tension increased slightly in the presence of APW related to the ion concentration. Potassium ethyl xanthate (KEX) at high concentrations was effective in the reduction of surface tension. As the APW concentration increased, finer bubbles were obtained with a narrower size range. The stability of the foam increased with butyl glycol (BG) and APW concentration. There was no need to use a frother (BG) for the flotation experiments in the presence of APW1 or APWs with higher ionic strength.
- Open Access
Evaluation of Different Dispersants on the Dispersion/Sedimentation Behavior of Halloysite, Kaolinite, and Quartz Suspensions in the Enrichment of Halloysite Ore by Mechanical Dispersion
In this study, the dispersion properties of pure halloysite, kaolinite, and quartz minerals in halloysite ore were determined in the absence and presence of dispersants (sodium silicate, STPP, SHMP). First of all, the samples were characterized by chemical, mineralogical, BET, FTIR, and TEM analyses. Afterward, the physico-chemical properties of these minerals were investigated by zeta potential measurements and dispersion/sedimentation experiments in the absence and presence of the dispersants. The zeta potential measurements showed that the surface charges of all minerals changed from negative to positive as the PH changed from basic to acidic. The presence of dispersants at natural pHs indicated that the mineral surface charges tended to become more negative as the concentration increased in the zeta potential measurements. SHMP showed the most effect on the zeta potential. In the dispersion/sedimentation experiments, settling was slowed down with the use of dispersants. Finally, the dispersion properties of halloysite ore in the presence of dispersants were explored using mechanical dispersion and pulp viscosity experiments based on the amount of material passing to 2O3 and 50.5% SiO2 content passed to 2O3 and 46.1% SiO2 content was gained in the use of 7.5 kg/ton SHMP, which was determined as the optimum within the scope of the study. In conclusion, dispersant use enhanced the mechanical dispersion effect for plastic clay mineral separation from hard minerals in an aqueous medium.
Open AccessEvaluation of Different Dispersants on the Dispersion/Sedimentation Behavior of Halloysite, Kaolinite, and Quartz Suspensions in the Enrichment of Halloysite Ore by Mechanical Dispersion
In this study, the dispersion properties of pure halloysite, kaolinite, and quartz minerals in halloysite ore were determined in the absence and presence of dispersants (sodium silicate, STPP, SHMP). First of all, the samples were characterized by chemical, mineralogical, BET, FTIR, and TEM analyses. Afterward, the physico-chemical properties of these minerals were investigated by zeta potential measurements and dispersion/sedimentation experiments in the absence and presence of the dispersants. The zeta potential measurements showed that the surface charges of all minerals changed from negative to positive as the PH changed from basic to acidic. The presence of dispersants at natural pHs indicated that the mineral surface charges tended to become more negative as the concentration increased in the zeta potential measurements. SHMP showed the most effect on the zeta potential. In the dispersion/sedimentation experiments, settling was slowed down with the use of dispersants. Finally, the dispersion properties of halloysite ore in the presence of dispersants were explored using mechanical dispersion and pulp viscosity experiments based on the amount of material passing to 2O3 and 50.5% SiO2 content passed to 2O3 and 46.1% SiO2 content was gained in the use of 7.5 kg/ton SHMP, which was determined as the optimum within the scope of the study. In conclusion, dispersant use enhanced the mechanical dispersion effect for plastic clay mineral separation from hard minerals in an aqueous medium.
- Open Access
Effect of Blunging/Dispersion Parameters on Separation of Halloysite Nanotubes from Gangue Minerals
Clay minerals need to be dispersed with blungers before their utilization in the related industries due to their plastic properties, and size reduction is carried out in a wet medium. Clay minerals also contain impurities such as nonplastic materials in their structure. Mechanical dispersion parameters are important in the separation of clay group minerals (halloysite and kaolinite) from their typical non-clayey gangue minerals (quartz and goethite). In this study, the removal of impurities from halloysite ore obtained from Kızıldam, Turkey, was examined in terms of mechanical dispersion parameters, namely, feed size, blunging time and speed, pulp concentration, pulp temperature, and the aging process. The effect of these parameters on halloysite dispersion was determined by particle size, chemical, and mineralogical analysis, and optical and scanning electron microscope images. The results obtained from the studies of the mechanical dispersing and particle size distribution of the products indicated that the optimum dispersion parameters were determined as −10 mm feed size, 8 h, and 1000 rpm blunging time, and speed, 35% pulp concentration at 25 °C pulp temperature. Under these optimum conditions, a 72.3% amount of −38 μm clay product containing 35.6% of halloysite, 46.5% of kaolinite, 12.0% quartz, 1.9% goethite, 0.9% gibbsite, and 3.2% other minerals were obtained from the halloysite ore, having 30.5% of halloysite, 43.4% of kaolinite, 19.1% quartz, 2.9% goethite, 1.4% gibbsite, and 2.7% other minerals. In this study, it was understood that feed size, pulp concentration, blunging time, and speed were important parameters, while pulp temperature and the aging process had no significant effect on the mechanical dispersion of Kızıldam halloysite. In addition, impurities such as quartz and iron-bearing minerals were separated from the ore by blunging and sieving.
Open AccessEffect of Blunging/Dispersion Parameters on Separation of Halloysite Nanotubes from Gangue Minerals
Clay minerals need to be dispersed with blungers before their utilization in the related industries due to their plastic properties, and size reduction is carried out in a wet medium. Clay minerals also contain impurities such as nonplastic materials in their structure. Mechanical dispersion parameters are important in the separation of clay group minerals (halloysite and kaolinite) from their typical non-clayey gangue minerals (quartz and goethite). In this study, the removal of impurities from halloysite ore obtained from Kızıldam, Turkey, was examined in terms of mechanical dispersion parameters, namely, feed size, blunging time and speed, pulp concentration, pulp temperature, and the aging process. The effect of these parameters on halloysite dispersion was determined by particle size, chemical, and mineralogical analysis, and optical and scanning electron microscope images. The results obtained from the studies of the mechanical dispersing and particle size distribution of the products indicated that the optimum dispersion parameters were determined as −10 mm feed size, 8 h, and 1000 rpm blunging time, and speed, 35% pulp concentration at 25 °C pulp temperature. Under these optimum conditions, a 72.3% amount of −38 μm clay product containing 35.6% of halloysite, 46.5% of kaolinite, 12.0% quartz, 1.9% goethite, 0.9% gibbsite, and 3.2% other minerals were obtained from the halloysite ore, having 30.5% of halloysite, 43.4% of kaolinite, 19.1% quartz, 2.9% goethite, 1.4% gibbsite, and 2.7% other minerals. In this study, it was understood that feed size, pulp concentration, blunging time, and speed were important parameters, while pulp temperature and the aging process had no significant effect on the mechanical dispersion of Kızıldam halloysite. In addition, impurities such as quartz and iron-bearing minerals were separated from the ore by blunging and sieving.
- 1 September 2021
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 62 (5) , 514-521
Gold Extraction from an Oxide Ore by Thiourea Leaching with Hydrogen Peroxide as an Oxidant
In this study, the effects of thiourea (CH4N2S) on the efficiency of gold dissolution were investigated for the extraction of gold from an oxide gold ore o
- 1 September 2021
- Published by Allerton Press in Russian Journal of Non-Ferrous Metals
- Vol. 62 (5) , 514-521
Gold Extraction from an Oxide Ore by Thiourea Leaching with Hydrogen Peroxide as an Oxidant
In this study, the effects of thiourea (CH4N2S) on the efficiency of gold dissolution were investigated for the extraction of gold from an oxide gold ore o
- 13 March 2021
- Published by Politechnika Wroclawska Oficyna Wydawnicza in Physicochemical Problems of Mineral Processing
- Vol. 57 (3) , 21-35
Digital image processing (DIP) application on the evaluation of iron-rich heavy mineral concentrates produced from river sand using a sequential mineral processing approach
In this study, the iron-rich heavy mineral concentrate production from river sand as a by-product of an alternative resource by gravity, magnetic separation, and flotation methods were investigated in detail. For the physical separation of the sample and increasing the Fe2O3 content, a shaking...
- 13 March 2021
- Published by Politechnika Wroclawska Oficyna Wydawnicza in Physicochemical Problems of Mineral Processing
- Vol. 57 (3) , 21-35
Digital image processing (DIP) application on the evaluation of iron-rich heavy mineral concentrates produced from river sand using a sequential mineral processing approach
In this study, the iron-rich heavy mineral concentrate production from river sand as a by-product of an alternative resource by gravity, magnetic separation, and flotation methods were investigated in detail. For the physical separation of the sample and increasing the Fe2O3 content, a shaking...
- Open Access
- 1 December 2018
- Published by Bilimsel Madencilik Dergisi in Bilimsel Madencilik Dergisi
- Vol. 57 (4) , 267-280
ISPARTA ÇANAKLI CEVHERİNDEN SÜLFÜRİK ASİT LİÇİ İLE NTE EKSTRAKSİYONUNUN DENEYSEL TASARIMI
Bu çalışmada, Isparta Çanaklı yöresine ait nadir toprak elementleri (NTE) içeren ayrışmış piroklastik cevherden sülfürik asitli ortamda farklı liç koşullarında NTE çözünme verimleri incelenmiştir. Deneylerde 2n faktöriyel tasarımı ve Yates deneysel düzen tekniği kullanılmış olup, liç işlemlerinde asit konsantrasyonu, çözündürme süresi ve pülp sıcaklığı temel değişkenler olarak seçilmiştir. Deneylerde en iyi sonuçlar 5M H2SO4 konsantrasyonu, 5 saat liç süresi ve 100oC pülp sıcaklığı şartlarında elde edilmiş ve toplam NTE (TNTE), hafif NTE (HNTE), ağır NTE (ANTE), Ce, La ve Nd çözünme verimleri sırasıyla %65,34, %61,80, %65,22, %66,09, %66,86 ve %68,38 olmuştur. ANOVA analizi ile etken olduğu belirlenen parametreler için Minitab yazılımı kullanılarak modeller oluşturulmuş ve deneysel sonuçlar ile modelden elde edilen teorik sonuçlar arasında korelasyon analizleri gerçekleştirilmiştir. TNTE, HNTE, ANTE, Ce, La ve Nd çözünme verimleri için deneysel ve teorik sonuçlar arasındaki korelasyon katsayısı (R2) sırasıyla 0,7933, 0,7721, 0,9323, 0,6700, 0,8312 ve 0,8183 olarak hesaplanmıştır.
- 1 December 2018
- Published by Bilimsel Madencilik Dergisi in Bilimsel Madencilik Dergisi
- Vol. 57 (4) , 267-280
Open AccessISPARTA ÇANAKLI CEVHERİNDEN SÜLFÜRİK ASİT LİÇİ İLE NTE EKSTRAKSİYONUNUN DENEYSEL TASARIMI
Bu çalışmada, Isparta Çanaklı yöresine ait nadir toprak elementleri (NTE) içeren ayrışmış piroklastik cevherden sülfürik asitli ortamda farklı liç koşullarında NTE çözünme verimleri incelenmiştir. Deneylerde 2n faktöriyel tasarımı ve Yates deneysel düzen tekniği kullanılmış olup, liç işlemlerinde asit konsantrasyonu, çözündürme süresi ve pülp sıcaklığı temel değişkenler olarak seçilmiştir. Deneylerde en iyi sonuçlar 5M H2SO4 konsantrasyonu, 5 saat liç süresi ve 100oC pülp sıcaklığı şartlarında elde edilmiş ve toplam NTE (TNTE), hafif NTE (HNTE), ağır NTE (ANTE), Ce, La ve Nd çözünme verimleri sırasıyla %65,34, %61,80, %65,22, %66,09, %66,86 ve %68,38 olmuştur. ANOVA analizi ile etken olduğu belirlenen parametreler için Minitab yazılımı kullanılarak modeller oluşturulmuş ve deneysel sonuçlar ile modelden elde edilen teorik sonuçlar arasında korelasyon analizleri gerçekleştirilmiştir. TNTE, HNTE, ANTE, Ce, La ve Nd çözünme verimleri için deneysel ve teorik sonuçlar arasındaki korelasyon katsayısı (R2) sırasıyla 0,7933, 0,7721, 0,9323, 0,6700, 0,8312 ve 0,8183 olarak hesaplanmıştır.
- 22 August 2018
- Published by Springer Nature in Arabian Journal of Geosciences
- Vol. 11 (16) , 462
Evaluation of digital image processing (DIP) in analysis of magnetic separation fractions from Na-feldspar ore
- 22 August 2018
- Published by Springer Nature in Arabian Journal of Geosciences
- Vol. 11 (16) , 462
Evaluation of digital image processing (DIP) in analysis of magnetic separation fractions from Na-feldspar ore