Emrah Durgut
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Emrah Durgut has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Orhan Ozdemir
Department of Mineral Processing Engineering, Faculty of Mines, Istanbul Technical University, 34469 Istanbul, Türkiye
5 shared publications - Mustafa Cinar
ÇANAKKALE ONSEKİZ MART ÜNİVERSİTESİ, MÜHENDİSLİK FAKÜLTESİ, MADEN MÜHENDİSLİĞİ BÖLÜMÜ
3 shared publications - Ilgin Kursun
İstanbul Üniversitesi-Cerrahpaşa
2 shared publications - Mert Terzi
İstanbul Üniversitesi-Cerrahpaşa
2 shared publications - Yildiz Yildirim
R&D Department Director, Kaleseramik
2 shared publications Feridun Boylu
Istanbul Tech Univ, Dept Mineral Proc Engn, Maslak, Turkiye
1 shared publication
Latest Publications
- 15 March 2026
- Published by Black Sea Journal of Engineering and Science in Black Sea Journal of Engineering and Science
- Vol. 9 (2) , 971-979
Combined Gravity-Flotation Approach for Recovery of Unburned Carbon from Thermal Power Plant Slag
This study aimed to study unburned carbon recovery from thermal power plant slag using heavy-medium separation and flotation methods. In this context, firstly, the chemical, physical, and mineralogical properties of the slag sample were determined. Based on the data obtained from the chemical, physical, and mineralogical properties of the slag, heavy-medium separation and flotation experiments were carried out. Extensive mineralogical, physical, and microscopic characterization revealed that the slag contains quartz, cristobalite, mullite, hematite, and graphite, and had a porous structure rich in cenospheres and partially unburned coal fragments. The heavy medium separation process showed limited selectivity due to the presence of hollow spherical particles and mineral intergrowth. Thus, the lowest ash content was obtained from the -0.5+0.074 mm fraction with a density of 1.3 g/cm³ in heavy medium separation experiments. Flotation experiments showed that increasing collector dosage improved combustible recovery and reduced ash content, while decreasing pH increased the recovery but also increased the ash levels. The best flotation performance was obtained with 55.0% ash content and 14.4% combustible recovery using 600 g/t of montanol at natural pH (10.1). Overall, the complex mineralogical structure of the slag, particularly the abundance of cenospheres and the intimate association of carbon with inorganic phases, had significantly limited the efficiency of physical separation methods. In conclusion, the combined mineral processing and beneficiation processes, particularly the combination of fine-sized separation methods, are necessary for recovering unburned carbon with higher purity.
- 15 March 2026
- Published by Black Sea Journal of Engineering and Science in Black Sea Journal of Engineering and Science
- Vol. 9 (2) , 971-979
Combined Gravity-Flotation Approach for Recovery of Unburned Carbon from Thermal Power Plant Slag
This study aimed to study unburned carbon recovery from thermal power plant slag using heavy-medium separation and flotation methods. In this context, firstly, the chemical, physical, and mineralogical properties of the slag sample were determined. Based on the data obtained from the chemical, physical, and mineralogical properties of the slag, heavy-medium separation and flotation experiments were carried out. Extensive mineralogical, physical, and microscopic characterization revealed that the slag contains quartz, cristobalite, mullite, hematite, and graphite, and had a porous structure rich in cenospheres and partially unburned coal fragments. The heavy medium separation process showed limited selectivity due to the presence of hollow spherical particles and mineral intergrowth. Thus, the lowest ash content was obtained from the -0.5+0.074 mm fraction with a density of 1.3 g/cm³ in heavy medium separation experiments. Flotation experiments showed that increasing collector dosage improved combustible recovery and reduced ash content, while decreasing pH increased the recovery but also increased the ash levels. The best flotation performance was obtained with 55.0% ash content and 14.4% combustible recovery using 600 g/t of montanol at natural pH (10.1). Overall, the complex mineralogical structure of the slag, particularly the abundance of cenospheres and the intimate association of carbon with inorganic phases, had significantly limited the efficiency of physical separation methods. In conclusion, the combined mineral processing and beneficiation processes, particularly the combination of fine-sized separation methods, are necessary for recovering unburned carbon with higher purity.
- Open Access
- 15 October 2025
- Published by Politechnika Wroclawska Oficyna Wydawnicza in Mining Science
- Vol. 32, 155-167
The Industrial Effects of Ball Type on Ceramic Porcelain Tile Body Grinding
Raw materials such as feldspar, kaolin and illitic clay are used in the preparation of ceramic porcelain tile compositions according to their specific properties. Such raw materials are ground in ball mills in order to reduce the particle size to a certain value determined according to the operating conditions. In this study, it was aimed to compare capacity, time and energy spent in the grinding process of porcelain tile composition by using alumina and silica grinding medium from an industrial perspective. In this context, firstly, the grinding properties of the raw materials were determined with porcelain ball mill and Bond mill, separately. Bond Work Index values of magnesite, clay, kaolin and feldspar were determined as 8.7, 7.9, 12.3 and 14.2 kWh/ton, respectively. Then industrial grinding of a porcelain body was executed with a discontinuous horizontal ball mill. The industrial grinding studies showed that porcelain body was ground at 480 and 720 min to reach 2% sieve residue for +45 µm with alumina and silica ball, respectively, which resulted as 625 ton/h capacity difference. Lastly, the ground materials in alumina and silica medium were compared in terms of water absorption, shrinkage, color and SEM analysis after sintering in porcelain tile conditions.
- 15 October 2025
- Published by Politechnika Wroclawska Oficyna Wydawnicza in Mining Science
- Vol. 32, 155-167
Open AccessThe Industrial Effects of Ball Type on Ceramic Porcelain Tile Body Grinding
Raw materials such as feldspar, kaolin and illitic clay are used in the preparation of ceramic porcelain tile compositions according to their specific properties. Such raw materials are ground in ball mills in order to reduce the particle size to a certain value determined according to the operating conditions. In this study, it was aimed to compare capacity, time and energy spent in the grinding process of porcelain tile composition by using alumina and silica grinding medium from an industrial perspective. In this context, firstly, the grinding properties of the raw materials were determined with porcelain ball mill and Bond mill, separately. Bond Work Index values of magnesite, clay, kaolin and feldspar were determined as 8.7, 7.9, 12.3 and 14.2 kWh/ton, respectively. Then industrial grinding of a porcelain body was executed with a discontinuous horizontal ball mill. The industrial grinding studies showed that porcelain body was ground at 480 and 720 min to reach 2% sieve residue for +45 µm with alumina and silica ball, respectively, which resulted as 625 ton/h capacity difference. Lastly, the ground materials in alumina and silica medium were compared in terms of water absorption, shrinkage, color and SEM analysis after sintering in porcelain tile conditions.
- Open Access
Industrial-Based Comprehension on the Ceramic Body Composition by Continuous/Batch Grinding Methods
In this study, the effects of batch and continuous grinding on the ceramic floor tile body were investigated in terms of cost, capacity, and technical aspects. In batch milling, a changing speed during grinding was more efficient than a constant speed. Capacity and energy consumption increased as the mill rotation speed increased in continuous grinding. Specific energy consumptions were measured as 36 kW/ton and 43.1 kW/ton, with 1.6 ton/h and 8.375 t/h capacities. Additionally, d10, d50, and d90 values for ground ceramic floor tile bodies were determined to be 2.5, 9.5, and 47.2 µm and 2.5, 9.4, and 48.1 µm for batch and continuous grinding, respectively. No significant difference was observed in the color and shrinkage values, while water absorptions were calculated to be 1.1% and 0.3% as sintering properties for batch and continuous methods, respectively. In the phase analysis of a sintered body prepared using the continuous method, mullite and quartz were observed, while microcline was also analyzed differently from such minerals for the batch one. Structural changes, surface morphology, and roughness were also interpreted by DTA/TG, SEM, and AFM analysis. The presence of plastic clay minerals during the grinding process in batch milling caused non-plastic raw materials not to be ground sufficiently, and sintering characteristics changed.
Open AccessIndustrial-Based Comprehension on the Ceramic Body Composition by Continuous/Batch Grinding Methods
In this study, the effects of batch and continuous grinding on the ceramic floor tile body were investigated in terms of cost, capacity, and technical aspects. In batch milling, a changing speed during grinding was more efficient than a constant speed. Capacity and energy consumption increased as the mill rotation speed increased in continuous grinding. Specific energy consumptions were measured as 36 kW/ton and 43.1 kW/ton, with 1.6 ton/h and 8.375 t/h capacities. Additionally, d10, d50, and d90 values for ground ceramic floor tile bodies were determined to be 2.5, 9.5, and 47.2 µm and 2.5, 9.4, and 48.1 µm for batch and continuous grinding, respectively. No significant difference was observed in the color and shrinkage values, while water absorptions were calculated to be 1.1% and 0.3% as sintering properties for batch and continuous methods, respectively. In the phase analysis of a sintered body prepared using the continuous method, mullite and quartz were observed, while microcline was also analyzed differently from such minerals for the batch one. Structural changes, surface morphology, and roughness were also interpreted by DTA/TG, SEM, and AFM analysis. The presence of plastic clay minerals during the grinding process in batch milling caused non-plastic raw materials not to be ground sufficiently, and sintering characteristics changed.
- 1 October 2025
- Published by Bilimsel Madencilik Dergisi in Bilimsel Madencilik Dergisi
- Vol. 63 (2) , 95-100
Investigation of wet ground limestones on porous ceramic body properties
Limestone and clay group minerals are used in the production of ceramic wall tile compositions. Wall tiles must have a 10-20% water absorption depending on the EN 14411 standard. In order to meet this water absorption criterion, calcite and dolomite minerals which are in carbonated structure are used in wall tile body composition. Manufacturers supply these minerals from limestone sources close to the enterprises, which are abundant in nature. The size of raw materials must be reduced to finer sizes (-45 µm) for the production of ceramic bodies. For this reason, it is very important to control the size of the limestone during the grinding process limestone to a very fine size (-45 µm) in aqueous media in order to produce qualified wall tile body composition. In this context, this study aimed to investigate the effects of grinding of limestone samples obtained from the Derenti, Nevruz, and Terzialan regions of Çanakkale province, on ceramic wall tiles based on laboratory and industry-scale experiments/analyses. The limestone samples were firstly ground in a discontinuous mill, and the grinding performances were compared in terms of time-dependent particle size, energy consumption, and capacity. Second, the wall tile bodies were shaped and then fired in an industrial kiln, and finally analyzed in terms of sintering properties and TS EN 14411 standards. The results from this study showed that Bond Work Indexes of Derenti, Nevruz, and Terzialan limestone samples were determined as 12.8, 11.7, and 13.0 kWh/t, respectively. As a result of industrial-based discontinuous grinding studies, the energy consumption for grinding to 0.2% sieve residue for +45 µm increased from 67.4 to 73.4 kW/t and the capacity decreased from 1.34 t/h to 1.23 t/h with the increase of quartz content of limestone samples from 0.8% to 2.1%. The particle size analysis of the samples indicated the d90, d50, and d10 values of the ground samples in industrial-based grinding experiments were 16.97 µm, 1.85 µm, and 0.37 µm, respectively, As a result of the studies carried out within the scope of wall tile body composition development, the shrinkage value decreased from 0.43% to 0.31% with the increase in CaO content from 53.9% to 54.6% and wall tile with TS EN 14411 water absorption standard was obtained by using 13% limestone. In conclusion, the mineral content in limestone showed significant effects on particle size distribution, energy consumption, and capacity in the fine grinding process as well as on sintering properties of wall tile body composition.
- 1 October 2025
- Published by Bilimsel Madencilik Dergisi in Bilimsel Madencilik Dergisi
- Vol. 63 (2) , 95-100
Investigation of wet ground limestones on porous ceramic body properties
Limestone and clay group minerals are used in the production of ceramic wall tile compositions. Wall tiles must have a 10-20% water absorption depending on the EN 14411 standard. In order to meet this water absorption criterion, calcite and dolomite minerals which are in carbonated structure are used in wall tile body composition. Manufacturers supply these minerals from limestone sources close to the enterprises, which are abundant in nature. The size of raw materials must be reduced to finer sizes (-45 µm) for the production of ceramic bodies. For this reason, it is very important to control the size of the limestone during the grinding process limestone to a very fine size (-45 µm) in aqueous media in order to produce qualified wall tile body composition. In this context, this study aimed to investigate the effects of grinding of limestone samples obtained from the Derenti, Nevruz, and Terzialan regions of Çanakkale province, on ceramic wall tiles based on laboratory and industry-scale experiments/analyses. The limestone samples were firstly ground in a discontinuous mill, and the grinding performances were compared in terms of time-dependent particle size, energy consumption, and capacity. Second, the wall tile bodies were shaped and then fired in an industrial kiln, and finally analyzed in terms of sintering properties and TS EN 14411 standards. The results from this study showed that Bond Work Indexes of Derenti, Nevruz, and Terzialan limestone samples were determined as 12.8, 11.7, and 13.0 kWh/t, respectively. As a result of industrial-based discontinuous grinding studies, the energy consumption for grinding to 0.2% sieve residue for +45 µm increased from 67.4 to 73.4 kW/t and the capacity decreased from 1.34 t/h to 1.23 t/h with the increase of quartz content of limestone samples from 0.8% to 2.1%. The particle size analysis of the samples indicated the d90, d50, and d10 values of the ground samples in industrial-based grinding experiments were 16.97 µm, 1.85 µm, and 0.37 µm, respectively, As a result of the studies carried out within the scope of wall tile body composition development, the shrinkage value decreased from 0.43% to 0.31% with the increase in CaO content from 53.9% to 54.6% and wall tile with TS EN 14411 water absorption standard was obtained by using 13% limestone. In conclusion, the mineral content in limestone showed significant effects on particle size distribution, energy consumption, and capacity in the fine grinding process as well as on sintering properties of wall tile body composition.
- Open Access
- 22 March 2025
- Published by Politechnika Wroclawska Oficyna Wydawnicza in Physicochemical Problems of Mineral Processing
- Vol. 61 (3)
Fine-size separation of halloysite, kaolinite, and quartz minerals as binary systems using dispersion and sedimentation methods
Clay minerals are mainly composed of aluminum hydrosilicates. In some minerals, aluminum is completely or partially replaced by Fe or Mg. Alkaline minerals or alkali metals are present as major constituents of clay minerals. While some clay sources may contain a single clay mineral, they often contain different minerals such as quartz, calcite, feldspar, pyrite, etc. as impurities. They also contain organic matter and water-soluble salts. Halloysite is a clay mineral belonging to the kaolinite group and USA Environmental Protection Agency (EPA 4A) declared it as an innocuous/adaptable material to human health and the environment. Halloysite ore deposits are mainly found together with kaolinite and quartz minerals, but can also be found as a pure source. The degree of purity of halloysite ore determines the industrial area where it will be used and therefore its economic value. Since clay minerals are naturally composed of fine particles, it is necessary to disperse the clay particles in suspension to separate halloysite and kaolinite minerals. In addition, there are also fine-grained quartz minerals, and to recover pure halloysite minerals, it is necessary to determine their properties in the fine size fraction. In this study, the dispersion properties of halloysite, kaolinite, and quartz minerals in the presence of sodium silicate (SS), sodium tripolyphosphate (STPP), and sodium hexametaphosphate (SHMP) dispersants in fine-size fraction (-38 μm) were researched by particle size measurements and mineral separation properties were investigated by sedimentation experiments at different acidic, neutral, alkaline pH values. In dispersion experiments, the d90 values of halloysite, kaolinite, and quartz minerals were 74.0, 50.7, and 61.3 μm without any dispersant addition, and such values decreased to 54.7, 26.3, and 57.1 μm as SHMP increased to 10 kg/ton, respectively. d50 and d10 values showed a significant change for halloysite, while no important change was observed for kaolinite and halloysite. SHMP had the most effect on the particle size change in the dispersants especially on halloysite minerals. The least effect on particle size change was observed in the quartz sample with dispersant addition. The sedimentation experiments aimed to investigate the effects of pH on halloysite, kaolinite, and quartz recoveries in binary systems as settled products. Kaolinite settled more at acidic pH and halloysite at basic pH. There was no pH-dependent change in the settling behavior for halloysite and quartz. In the quartz-kaolinite system, quartz mineral settled more than kaolinite for all pH values. The settling experiments showed the importance of morphological differences between tubular halloysite and lamellar kaolinite minerals.
- 22 March 2025
- Published by Politechnika Wroclawska Oficyna Wydawnicza in Physicochemical Problems of Mineral Processing
- Vol. 61 (3)
Open AccessFine-size separation of halloysite, kaolinite, and quartz minerals as binary systems using dispersion and sedimentation methods
Clay minerals are mainly composed of aluminum hydrosilicates. In some minerals, aluminum is completely or partially replaced by Fe or Mg. Alkaline minerals or alkali metals are present as major constituents of clay minerals. While some clay sources may contain a single clay mineral, they often contain different minerals such as quartz, calcite, feldspar, pyrite, etc. as impurities. They also contain organic matter and water-soluble salts. Halloysite is a clay mineral belonging to the kaolinite group and USA Environmental Protection Agency (EPA 4A) declared it as an innocuous/adaptable material to human health and the environment. Halloysite ore deposits are mainly found together with kaolinite and quartz minerals, but can also be found as a pure source. The degree of purity of halloysite ore determines the industrial area where it will be used and therefore its economic value. Since clay minerals are naturally composed of fine particles, it is necessary to disperse the clay particles in suspension to separate halloysite and kaolinite minerals. In addition, there are also fine-grained quartz minerals, and to recover pure halloysite minerals, it is necessary to determine their properties in the fine size fraction. In this study, the dispersion properties of halloysite, kaolinite, and quartz minerals in the presence of sodium silicate (SS), sodium tripolyphosphate (STPP), and sodium hexametaphosphate (SHMP) dispersants in fine-size fraction (-38 μm) were researched by particle size measurements and mineral separation properties were investigated by sedimentation experiments at different acidic, neutral, alkaline pH values. In dispersion experiments, the d90 values of halloysite, kaolinite, and quartz minerals were 74.0, 50.7, and 61.3 μm without any dispersant addition, and such values decreased to 54.7, 26.3, and 57.1 μm as SHMP increased to 10 kg/ton, respectively. d50 and d10 values showed a significant change for halloysite, while no important change was observed for kaolinite and halloysite. SHMP had the most effect on the particle size change in the dispersants especially on halloysite minerals. The least effect on particle size change was observed in the quartz sample with dispersant addition. The sedimentation experiments aimed to investigate the effects of pH on halloysite, kaolinite, and quartz recoveries in binary systems as settled products. Kaolinite settled more at acidic pH and halloysite at basic pH. There was no pH-dependent change in the settling behavior for halloysite and quartz. In the quartz-kaolinite system, quartz mineral settled more than kaolinite for all pH values. The settling experiments showed the importance of morphological differences between tubular halloysite and lamellar kaolinite minerals.
- 6 March 2025
- Published by Taylor & Francis in Drying Technology
- Vol. 43 (5) , 937-948
Evaluation of the use of microwave energy on green floor/wall tile drying process
- 6 March 2025
- Published by Taylor & Francis in Drying Technology
- Vol. 43 (5) , 937-948
Evaluation of the use of microwave energy on green floor/wall tile drying process
- Open Access
- 15 April 2024
- Published by Politechnika Wroclawska Oficyna Wydawnicza in Physicochemical Problems of Mineral Processing
- Vol. 60 (2)
Effect of blunging process on purification of halloysite ore from ferrous impurities by dry magnetic separation
The objective of this research is to study the effects of feed particle size, splitter angle, and washing process on Fe2O3 removal efficiency in the separation of ferrous impurities from halloysite ore by dry magnetic separation in order to increase the purity of halloysite sample after crushing and blunging processes separately. Firstly, after crushing ore in a jaw crusher and sizing to -2+1 mm, -1+0.5 mm, and -0.5+0.212 mm fractions, the sized materials were fed to REMS-type dry magnetic separator at a constant belt speed of 300 rpm with the splitter angles of 0, 15, 30º separately. Maximum Fe2O3 removal efficiency (FRE) (97.1%) was obtained in the nonmagnetic product at -0.5+0.212 mm size fraction and 0º splitter angle. The minimum Fe2O3 content (1.3%) was reached in the nonmagnetic product obtained in the experiment with the feed size of -2+1 mm and a splitter angle of 0º. Secondly, dry magnetic separation was applied to the washed -2+0.212 mm size fraction after drying at room temperature to evaluate the coarse particle-sized halloysite ore that was gained by mechanical dispersion in the aqueous medium towards sodium hexametaphosphate (SHMP), while a significant part of the clay minerals went into fine size after the dispersion process. In the experiment performed with a 0º splitter angle after washing, it was determined that halloysite concentrate of 0.4% Fe2O3 content could be obtained with 98.8% Fe2O3 removal efficiency. As a result of dry magnetic separation experiments, it was seen that Fe2O3 removal efficiency decreased as the splitter angle increased, while Fe2O3 content in magnetic and nonmagnetic products increased. It was determined that washing and cleaning of fine-sized minerals plastered on particle surfaces after mechanical dispersion and particle release of minerals with different magnetic properties increased the dry magnetic separation efficiency, and nonmagnetic products with very low Fe2O3 (0.4%) and high Al2O3 (31.9%) content was obtained. The blunging process in the presence of dispersant caused the dispersion of clay minerals and allowed to liberating of the ferrous minerals from the halloysite ore, hence the increase in the FRE for the magnetic separation.
- 15 April 2024
- Published by Politechnika Wroclawska Oficyna Wydawnicza in Physicochemical Problems of Mineral Processing
- Vol. 60 (2)
Open AccessEffect of blunging process on purification of halloysite ore from ferrous impurities by dry magnetic separation
The objective of this research is to study the effects of feed particle size, splitter angle, and washing process on Fe2O3 removal efficiency in the separation of ferrous impurities from halloysite ore by dry magnetic separation in order to increase the purity of halloysite sample after crushing and blunging processes separately. Firstly, after crushing ore in a jaw crusher and sizing to -2+1 mm, -1+0.5 mm, and -0.5+0.212 mm fractions, the sized materials were fed to REMS-type dry magnetic separator at a constant belt speed of 300 rpm with the splitter angles of 0, 15, 30º separately. Maximum Fe2O3 removal efficiency (FRE) (97.1%) was obtained in the nonmagnetic product at -0.5+0.212 mm size fraction and 0º splitter angle. The minimum Fe2O3 content (1.3%) was reached in the nonmagnetic product obtained in the experiment with the feed size of -2+1 mm and a splitter angle of 0º. Secondly, dry magnetic separation was applied to the washed -2+0.212 mm size fraction after drying at room temperature to evaluate the coarse particle-sized halloysite ore that was gained by mechanical dispersion in the aqueous medium towards sodium hexametaphosphate (SHMP), while a significant part of the clay minerals went into fine size after the dispersion process. In the experiment performed with a 0º splitter angle after washing, it was determined that halloysite concentrate of 0.4% Fe2O3 content could be obtained with 98.8% Fe2O3 removal efficiency. As a result of dry magnetic separation experiments, it was seen that Fe2O3 removal efficiency decreased as the splitter angle increased, while Fe2O3 content in magnetic and nonmagnetic products increased. It was determined that washing and cleaning of fine-sized minerals plastered on particle surfaces after mechanical dispersion and particle release of minerals with different magnetic properties increased the dry magnetic separation efficiency, and nonmagnetic products with very low Fe2O3 (0.4%) and high Al2O3 (31.9%) content was obtained. The blunging process in the presence of dispersant caused the dispersion of clay minerals and allowed to liberating of the ferrous minerals from the halloysite ore, hence the increase in the FRE for the magnetic separation.
- 12 February 2024
- Published by Bilimsel Madencilik Dergisi in Bilimsel Madencilik Dergisi
- Vol. 62 (4) , 175-182
An overview of halloysite mineral
Halloysite is a type of clay mineral found in the kaolin group together with kaolinite, dickite, and nacrite minerals. Kaolinite is the most common mineral in this group, while dickite, nacrite, and halloysite are rarer. Although halloysite is primarily used in ceramic production, application in other industries is increasing and gaining economic value due to its unique properties. The use of halloysite is determined by the degree of purity and the properties of the nano-sized tubular structure. Naturally obtained halloysite mineral has a key position in the field of nanotechnology due to its unique physicochemical properties originating from its tubular structure. Also, due to its reserves in many parts of the world, halloysite is a more economical material for the sectors compared to artificially produced nanomaterials. And, they find many different application areas because of these features (morphological and physicochemical). Halloysite reserves known in Türkiye are located in the Çanakkale and Balıkesir regions. Although there are many useful studies on halloysite in different, additional studies are needed to understand the nano-sized properties of halloysite ore and to ensure its use that will provide maximum benefit. This study aimed to contribute to the studies on halloysite in terms of literature by compiling studies on the characterization of halloysite minerals, reserve information, physicochemical properties, enrichment methods, and usage areas.
- 12 February 2024
- Published by Bilimsel Madencilik Dergisi in Bilimsel Madencilik Dergisi
- Vol. 62 (4) , 175-182
An overview of halloysite mineral
Halloysite is a type of clay mineral found in the kaolin group together with kaolinite, dickite, and nacrite minerals. Kaolinite is the most common mineral in this group, while dickite, nacrite, and halloysite are rarer. Although halloysite is primarily used in ceramic production, application in other industries is increasing and gaining economic value due to its unique properties. The use of halloysite is determined by the degree of purity and the properties of the nano-sized tubular structure. Naturally obtained halloysite mineral has a key position in the field of nanotechnology due to its unique physicochemical properties originating from its tubular structure. Also, due to its reserves in many parts of the world, halloysite is a more economical material for the sectors compared to artificially produced nanomaterials. And, they find many different application areas because of these features (morphological and physicochemical). Halloysite reserves known in Türkiye are located in the Çanakkale and Balıkesir regions. Although there are many useful studies on halloysite in different, additional studies are needed to understand the nano-sized properties of halloysite ore and to ensure its use that will provide maximum benefit. This study aimed to contribute to the studies on halloysite in terms of literature by compiling studies on the characterization of halloysite minerals, reserve information, physicochemical properties, enrichment methods, and usage areas.
- Open Access
Evaluation of Different Dispersants on the Dispersion/Sedimentation Behavior of Halloysite, Kaolinite, and Quartz Suspensions in the Enrichment of Halloysite Ore by Mechanical Dispersion
In this study, the dispersion properties of pure halloysite, kaolinite, and quartz minerals in halloysite ore were determined in the absence and presence of dispersants (sodium silicate, STPP, SHMP). First of all, the samples were characterized by chemical, mineralogical, BET, FTIR, and TEM analyses. Afterward, the physico-chemical properties of these minerals were investigated by zeta potential measurements and dispersion/sedimentation experiments in the absence and presence of the dispersants. The zeta potential measurements showed that the surface charges of all minerals changed from negative to positive as the PH changed from basic to acidic. The presence of dispersants at natural pHs indicated that the mineral surface charges tended to become more negative as the concentration increased in the zeta potential measurements. SHMP showed the most effect on the zeta potential. In the dispersion/sedimentation experiments, settling was slowed down with the use of dispersants. Finally, the dispersion properties of halloysite ore in the presence of dispersants were explored using mechanical dispersion and pulp viscosity experiments based on the amount of material passing to 2O3 and 50.5% SiO2 content passed to 2O3 and 46.1% SiO2 content was gained in the use of 7.5 kg/ton SHMP, which was determined as the optimum within the scope of the study. In conclusion, dispersant use enhanced the mechanical dispersion effect for plastic clay mineral separation from hard minerals in an aqueous medium.
Open AccessEvaluation of Different Dispersants on the Dispersion/Sedimentation Behavior of Halloysite, Kaolinite, and Quartz Suspensions in the Enrichment of Halloysite Ore by Mechanical Dispersion
In this study, the dispersion properties of pure halloysite, kaolinite, and quartz minerals in halloysite ore were determined in the absence and presence of dispersants (sodium silicate, STPP, SHMP). First of all, the samples were characterized by chemical, mineralogical, BET, FTIR, and TEM analyses. Afterward, the physico-chemical properties of these minerals were investigated by zeta potential measurements and dispersion/sedimentation experiments in the absence and presence of the dispersants. The zeta potential measurements showed that the surface charges of all minerals changed from negative to positive as the PH changed from basic to acidic. The presence of dispersants at natural pHs indicated that the mineral surface charges tended to become more negative as the concentration increased in the zeta potential measurements. SHMP showed the most effect on the zeta potential. In the dispersion/sedimentation experiments, settling was slowed down with the use of dispersants. Finally, the dispersion properties of halloysite ore in the presence of dispersants were explored using mechanical dispersion and pulp viscosity experiments based on the amount of material passing to 2O3 and 50.5% SiO2 content passed to 2O3 and 46.1% SiO2 content was gained in the use of 7.5 kg/ton SHMP, which was determined as the optimum within the scope of the study. In conclusion, dispersant use enhanced the mechanical dispersion effect for plastic clay mineral separation from hard minerals in an aqueous medium.
- Open Access
Effect of Blunging/Dispersion Parameters on Separation of Halloysite Nanotubes from Gangue Minerals
Clay minerals need to be dispersed with blungers before their utilization in the related industries due to their plastic properties, and size reduction is carried out in a wet medium. Clay minerals also contain impurities such as nonplastic materials in their structure. Mechanical dispersion parameters are important in the separation of clay group minerals (halloysite and kaolinite) from their typical non-clayey gangue minerals (quartz and goethite). In this study, the removal of impurities from halloysite ore obtained from Kızıldam, Turkey, was examined in terms of mechanical dispersion parameters, namely, feed size, blunging time and speed, pulp concentration, pulp temperature, and the aging process. The effect of these parameters on halloysite dispersion was determined by particle size, chemical, and mineralogical analysis, and optical and scanning electron microscope images. The results obtained from the studies of the mechanical dispersing and particle size distribution of the products indicated that the optimum dispersion parameters were determined as −10 mm feed size, 8 h, and 1000 rpm blunging time, and speed, 35% pulp concentration at 25 °C pulp temperature. Under these optimum conditions, a 72.3% amount of −38 μm clay product containing 35.6% of halloysite, 46.5% of kaolinite, 12.0% quartz, 1.9% goethite, 0.9% gibbsite, and 3.2% other minerals were obtained from the halloysite ore, having 30.5% of halloysite, 43.4% of kaolinite, 19.1% quartz, 2.9% goethite, 1.4% gibbsite, and 2.7% other minerals. In this study, it was understood that feed size, pulp concentration, blunging time, and speed were important parameters, while pulp temperature and the aging process had no significant effect on the mechanical dispersion of Kızıldam halloysite. In addition, impurities such as quartz and iron-bearing minerals were separated from the ore by blunging and sieving.
Open AccessEffect of Blunging/Dispersion Parameters on Separation of Halloysite Nanotubes from Gangue Minerals
Clay minerals need to be dispersed with blungers before their utilization in the related industries due to their plastic properties, and size reduction is carried out in a wet medium. Clay minerals also contain impurities such as nonplastic materials in their structure. Mechanical dispersion parameters are important in the separation of clay group minerals (halloysite and kaolinite) from their typical non-clayey gangue minerals (quartz and goethite). In this study, the removal of impurities from halloysite ore obtained from Kızıldam, Turkey, was examined in terms of mechanical dispersion parameters, namely, feed size, blunging time and speed, pulp concentration, pulp temperature, and the aging process. The effect of these parameters on halloysite dispersion was determined by particle size, chemical, and mineralogical analysis, and optical and scanning electron microscope images. The results obtained from the studies of the mechanical dispersing and particle size distribution of the products indicated that the optimum dispersion parameters were determined as −10 mm feed size, 8 h, and 1000 rpm blunging time, and speed, 35% pulp concentration at 25 °C pulp temperature. Under these optimum conditions, a 72.3% amount of −38 μm clay product containing 35.6% of halloysite, 46.5% of kaolinite, 12.0% quartz, 1.9% goethite, 0.9% gibbsite, and 3.2% other minerals were obtained from the halloysite ore, having 30.5% of halloysite, 43.4% of kaolinite, 19.1% quartz, 2.9% goethite, 1.4% gibbsite, and 2.7% other minerals. In this study, it was understood that feed size, pulp concentration, blunging time, and speed were important parameters, while pulp temperature and the aging process had no significant effect on the mechanical dispersion of Kızıldam halloysite. In addition, impurities such as quartz and iron-bearing minerals were separated from the ore by blunging and sieving.