Erkul Karacaoglu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Erkul Karacaoglu has a total of 45 co-authors. Here are the top co-authors by number of shared publications:
- Esra Öztürk
Department of Chemistry, Faculty of Science Hacettepe University Ankara Turkiye
8 shared publications Bekir Karasu
Karamanoglu Mehmetbey University
5 shared publicationsEsra Öztürk
5 shared publications- Burak Demir
BİNGÖL ÜNİVERSİTESİ MÜHENDİSLİK VE MİMARLIK FAKÜLTESİ
4 shared publications Erhan Ayas
4 shared publicationsMert Gul
Materials Science and Engineering, Eskisehir Technical University, Eskisehir, Türkiye
4 shared publications
Latest Publications
- Open Access
- 24 June 2026
- Published by Wiley in Polymer Composites
- Vol. 47 (18) , 16499-16510
Low‐Loading Toughening and Interfacial Effects of TiO 2 ALD ‐Coated SrAL 2 O 4 :Eu 2+ ,Dy 3+ Phosphor–Epoxy Composites
This study investigates the mechanical performance and photoluminescence of SrAl 2 O 4 :Eu 2+ ,Dy 3+ phosphor–epoxy composites as a function of filler loading. SrAl 2 O 4 :Eu 2+ ,Dy 3+ (SA2‐Green) long afterglow phosphor particles (25–75 μm), synthesized via a solid‐state reaction, are incorporated into an epoxy matrix in both uncoated and ~13 nm TiO 2 ‐coated forms using atomic layer deposition (ALD). The composites are fabricated as dog‐bone‐shaped specimens and evaluated using uniaxial tensile testing. Structural and photoluminescence (PL) analyses confirm that the crystalline structure and emission properties of the phosphor particles are preserved after embedding them in the epoxy matrix. The mechanical results show that the composites with 0.5 wt.% phosphor loading exhibit the highest tensile strength, toughness, and elongation, following the trend 0.5 wt.% > 1 wt.% > 2 wt.% > pure epoxy. The enhancement at low loading is attributed to particle‐induced toughening mechanisms, such as crack deflection, interfacial debonding, and crack–particle interactions, whereas higher loadings lead to particle agglomeration and stress concentration, reducing performance. TiO 2 ALD coatings increase the Young's modulus owing to improved interfacial adhesion and stress transfer but reduce the toughness by suppressing energy‐dissipating mechanisms. These findings highlight the critical role of interfacial engineering and particle dispersion in the design of multifunctional phosphor–epoxy composites with potential applications in mechanoluminescent sensing and smart materials.
- 24 June 2026
- Published by Wiley in Polymer Composites
- Vol. 47 (18) , 16499-16510
Open AccessLow‐Loading Toughening and Interfacial Effects of TiO 2 ALD ‐Coated SrAL 2 O 4 :Eu 2+ ,Dy 3+ Phosphor–Epoxy Composites
This study investigates the mechanical performance and photoluminescence of SrAl 2 O 4 :Eu 2+ ,Dy 3+ phosphor–epoxy composites as a function of filler loading. SrAl 2 O 4 :Eu 2+ ,Dy 3+ (SA2‐Green) long afterglow phosphor particles (25–75 μm), synthesized via a solid‐state reaction, are incorporated into an epoxy matrix in both uncoated and ~13 nm TiO 2 ‐coated forms using atomic layer deposition (ALD). The composites are fabricated as dog‐bone‐shaped specimens and evaluated using uniaxial tensile testing. Structural and photoluminescence (PL) analyses confirm that the crystalline structure and emission properties of the phosphor particles are preserved after embedding them in the epoxy matrix. The mechanical results show that the composites with 0.5 wt.% phosphor loading exhibit the highest tensile strength, toughness, and elongation, following the trend 0.5 wt.% > 1 wt.% > 2 wt.% > pure epoxy. The enhancement at low loading is attributed to particle‐induced toughening mechanisms, such as crack deflection, interfacial debonding, and crack–particle interactions, whereas higher loadings lead to particle agglomeration and stress concentration, reducing performance. TiO 2 ALD coatings increase the Young's modulus owing to improved interfacial adhesion and stress transfer but reduce the toughness by suppressing energy‐dissipating mechanisms. These findings highlight the critical role of interfacial engineering and particle dispersion in the design of multifunctional phosphor–epoxy composites with potential applications in mechanoluminescent sensing and smart materials.
- 24 December 2025
- Published by Elsevier in Ceramics International
- Vol. 52 (5) , 5789-5797
Enhancing the photoluminescence performance of Sm-doped fluorapatite with Dy co-doping
- 24 December 2025
- Published by Elsevier in Ceramics International
- Vol. 52 (5) , 5789-5797
Enhancing the photoluminescence performance of Sm-doped fluorapatite with Dy co-doping
- 20 June 2023
- Published by Springer Nature in Journal of Materials Research
- Vol. 38 (14) , 3536-3547
Effect of lanthanum doping on structural, optical, and photocatalytic properties of YVO4
- 20 June 2023
- Published by Springer Nature in Journal of Materials Research
- Vol. 38 (14) , 3536-3547
Effect of lanthanum doping on structural, optical, and photocatalytic properties of YVO4
- 25 January 2023
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 298
Aqueous degradation and atomic layer deposition (ALD) stabilization of BaAl2O4: Eu2+, Dy3+ long afterglow phosphors
- 25 January 2023
- Published by Elsevier in Materials Chemistry and Physics
- Vol. 298
Aqueous degradation and atomic layer deposition (ALD) stabilization of BaAl2O4: Eu2+, Dy3+ long afterglow phosphors
- Open Access
- 10 January 2023
- Published by Springer Nature in Research Square
Effect of lanthanum doping on structural, optical, and photocatalytic properties of YVO4
Yttrium vanadate (YVO4) based undoped and La3+-doped powders were prepared through a solid-state reaction method. The structural characterization carried out with XRD indicating that the samples are crystalline tetragonal type crystal structure of YVO4. XRD of the YVO4: La3+ powder contain same YVO4 diffraction lines and no other lanthanum related impurity and/or secondary phases were detected. Both undoped and La3+-doped YVO4 samples show combined white light emission peaks appeared at 478, 571 and 613 nm. The higher intensity of peaks located at 478 and 571 nm in YVO4: La3+ sample can be attributed to O2−-La3+ and O2−-V5+ charge transfer mechanisms. Besides, photocatalytic activities of the undoped and La3+ doped YVO4 samples were investigated under the UV light irradiation monitoring the aqueous solution of methylene blue (MB) dye. Hence, the effects of La3+ dopant ion on the photoluminescence properties are discussed in detail. While the degradation of MB reaches to 38.8% after 180 minutes of UV light exposure with undoped YVO4, the degradation efficiency of La3+ doped YVO4 reaches 76.7%. Pseudo-first-order reaction rate constant (k) of La3+-doped YVO4 (0.00846 min− 1) is determined 66% greater than undoped one (0.00287 min− 1).
- 10 January 2023
- Published by Springer Nature in Research Square
Open AccessEffect of lanthanum doping on structural, optical, and photocatalytic properties of YVO4
Yttrium vanadate (YVO4) based undoped and La3+-doped powders were prepared through a solid-state reaction method. The structural characterization carried out with XRD indicating that the samples are crystalline tetragonal type crystal structure of YVO4. XRD of the YVO4: La3+ powder contain same YVO4 diffraction lines and no other lanthanum related impurity and/or secondary phases were detected. Both undoped and La3+-doped YVO4 samples show combined white light emission peaks appeared at 478, 571 and 613 nm. The higher intensity of peaks located at 478 and 571 nm in YVO4: La3+ sample can be attributed to O2−-La3+ and O2−-V5+ charge transfer mechanisms. Besides, photocatalytic activities of the undoped and La3+ doped YVO4 samples were investigated under the UV light irradiation monitoring the aqueous solution of methylene blue (MB) dye. Hence, the effects of La3+ dopant ion on the photoluminescence properties are discussed in detail. While the degradation of MB reaches to 38.8% after 180 minutes of UV light exposure with undoped YVO4, the degradation efficiency of La3+ doped YVO4 reaches 76.7%. Pseudo-first-order reaction rate constant (k) of La3+-doped YVO4 (0.00846 min− 1) is determined 66% greater than undoped one (0.00287 min− 1).
- 17 November 2022
- Published by Springer Nature in Applied Physics A
- Vol. 128 (12) , 1-10
Luminescence properties and aqueous degradation of Eu2+/3+-activated (Zn,Sr)Al2O4 phosphors
- 17 November 2022
- Published by Springer Nature in Applied Physics A
- Vol. 128 (12) , 1-10
Luminescence properties and aqueous degradation of Eu2+/3+-activated (Zn,Sr)Al2O4 phosphors
- 9 October 2022
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2022-02 (51) , 1974
Investigation of Atomic Layer Deposition Post-Coating Properties of Phosphorescent SrAl2O4: Eu2+, Dy3+ Fibers Produced By Electrospinning
In this research, phosphorescent SrAl2O4:Eu2+, Dy3+ fibers were produced by electrospinning and coated with atomic layer deposition (ALD) technique to enhance the photoluminescence (PL) properties, and water & thermal resistance. Particle form of Eu2+-activated strontium aluminate phosphors possess many remarkable features that have been reported over and over, for example, nontoxic, stable, efficient. PL enhancement and stability in water of these particles were provided by nano encapsulation process by ALD that has just been published in our previous paper. In this study, for the first time, SrAl2O4 based long persistence phosphor fibers were coated with the ALD method to both improve their PL and provide water & thermal resistance property. In this successfully carried out study, luminescence, optic, chemical and structural properties of phosphor in fiber form were investigated in detail. These improved submicron afterglow fibers which are SrAl2O4:Eu2+, Dy3+ based are promising materials for applications such as solar cells, luminescent labels for bioimaging, mechanoluminescence sensor, etc.
- 9 October 2022
- Published by The Electrochemical Society in ECS Meeting Abstracts
- Vol. MA2022-02 (51) , 1974
Investigation of Atomic Layer Deposition Post-Coating Properties of Phosphorescent SrAl2O4: Eu2+, Dy3+ Fibers Produced By Electrospinning
In this research, phosphorescent SrAl2O4:Eu2+, Dy3+ fibers were produced by electrospinning and coated with atomic layer deposition (ALD) technique to enhance the photoluminescence (PL) properties, and water & thermal resistance. Particle form of Eu2+-activated strontium aluminate phosphors possess many remarkable features that have been reported over and over, for example, nontoxic, stable, efficient. PL enhancement and stability in water of these particles were provided by nano encapsulation process by ALD that has just been published in our previous paper. In this study, for the first time, SrAl2O4 based long persistence phosphor fibers were coated with the ALD method to both improve their PL and provide water & thermal resistance property. In this successfully carried out study, luminescence, optic, chemical and structural properties of phosphor in fiber form were investigated in detail. These improved submicron afterglow fibers which are SrAl2O4:Eu2+, Dy3+ based are promising materials for applications such as solar cells, luminescent labels for bioimaging, mechanoluminescence sensor, etc.
- 1 October 2022
- Published by The Electrochemical Society in ECS Journal of Solid State Science and Technology
- Vol. 11 (10) , 106001
Synthesis and Characterization of Luminescent Er3+-Doped Natural Fluorapatite
Ca10(PO4)6F2:xEr3+ (x = 0.1, 0.3 and 0.5) was synthesized using solid-state powder process (1150 °C, 1h), conventional sintering (1150 °C, 1h), and spark plasma sintering (SPS) techniques (1150 °C, 10 min, and 50 MPa). XRD analysis revealed that all samples are generally composed of fluorapatite (FAP) containing quartz as a minor phase, and the presence of Er2O3 peaks is becoming more evident as Er-doped increases. In the SEM microstructure images, non-diffused Er2O3 particles also increase with doping in powder and pellet samples. However, the PL analysis showed that the luminescence intensity did not increase proportionally with the doping content caused by the concentration quenching effect. FAP samples doped with 0.3 mol Er have higher luminescence intensity than 0.1 and 0.5 mol Er-doped samples. In addition, powder samples have the highest luminescence intensity due to increased luminescence intensity with increasing crystallite size. The characteristic 2H11/2 to 4I15/2 emission bands of Er3+ at ∼530 nm are seen in all samples. The maximum average lifetime was obtained in 125 μs in the powder sample with 0.3 mol Er. CIE color coordinates demonstrate the standard green color under ∼ 275 nm excitation; eventually, these phosphors can be utilized as green phosphors for optical applications.
- 1 October 2022
- Published by The Electrochemical Society in ECS Journal of Solid State Science and Technology
- Vol. 11 (10) , 106001
Synthesis and Characterization of Luminescent Er3+-Doped Natural Fluorapatite
Ca10(PO4)6F2:xEr3+ (x = 0.1, 0.3 and 0.5) was synthesized using solid-state powder process (1150 °C, 1h), conventional sintering (1150 °C, 1h), and spark plasma sintering (SPS) techniques (1150 °C, 10 min, and 50 MPa). XRD analysis revealed that all samples are generally composed of fluorapatite (FAP) containing quartz as a minor phase, and the presence of Er2O3 peaks is becoming more evident as Er-doped increases. In the SEM microstructure images, non-diffused Er2O3 particles also increase with doping in powder and pellet samples. However, the PL analysis showed that the luminescence intensity did not increase proportionally with the doping content caused by the concentration quenching effect. FAP samples doped with 0.3 mol Er have higher luminescence intensity than 0.1 and 0.5 mol Er-doped samples. In addition, powder samples have the highest luminescence intensity due to increased luminescence intensity with increasing crystallite size. The characteristic 2H11/2 to 4I15/2 emission bands of Er3+ at ∼530 nm are seen in all samples. The maximum average lifetime was obtained in 125 μs in the powder sample with 0.3 mol Er. CIE color coordinates demonstrate the standard green color under ∼ 275 nm excitation; eventually, these phosphors can be utilized as green phosphors for optical applications.