Shailesh Kumar Shukla
Research Subjects
Shailesh Kumar Shukla has a total of 3 co-authors. Here are the top co-authors by number of shared publications:
- Deepak Srivastava
Department of Plastic Technology, H. B. Technological Institute, Kanpur 208 002, India
2 shared publications - Deepak Srivastava
Gladstone Institutes, San Francisco, California 94158, USA
1 shared publication - Pramod Kumar
Department of Space Engineering and Rocketry, Birla Institute of Technology, Mesra, Ranchi, India
1 shared publication
Latest Publications
- 15 January 2007
- Published by Springer Nature in Journal of Materials Science
- Vol. 42 (9) , 3215-3222
Studies on the blends of modified epoxy resin and carboxyl-terminated polybutadiene (CTPB)—II: thermal and mechanical characteristics
- 15 January 2007
- Published by Springer Nature in Journal of Materials Science
- Vol. 42 (9) , 3215-3222
Studies on the blends of modified epoxy resin and carboxyl-terminated polybutadiene (CTPB)—II: thermal and mechanical characteristics
- 24 January 2006
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 100 (3) , 1802-1808
Blends of modified epoxy resin and carboxyl‐terminated polybutadiene. I
Six blend samples were prepared by the physical mixing of epoxidized resole (EDR) with different weight ratios of carboxyl‐terminated polybutadiene (CTPB) liquid rubber ranging from 0 to 25 wt % in intervals of 5 wt %. The formation of various reaction products during the curing of unblended EDR and CTPB‐blended EDR were studied with Fourier transform infrared spectroscopy. The curing time at 100°C for the blend sample containing 15 wt % CTPB was the least among all of the blend samples. This blend sample, also, showed the highest initial degradation temperature, as obtained from thermogravimetric analysis thermograms, which indicated that it was the most thermally stable matrix system. The films of coatings based on the blend of EDR with 15 wt % CTPB offered the highest resistance toward different concentrations of acids and alkalis compared to the films having 5, 10, 20, and 25 wt % CTPB in the EDR/CTPB blends. Solvents showed almost the same behavior as acids and alkalis for these films except for hydrocarbon solvents such as mineral turpentine oil, toluene, and xylene. The resistance toward these solvents was poor and slightly inferior to those found with EDR unblended with CTPB. The tensile, flexural, and impact strengths of the molded specimens derived from the EDR/CTPB blends initially increased up to 15 wt % CTPB addition in the blend and then decreased, whereas the elongation at break remained constant for all blend compositions. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 100: 1802–1808, 2006
- 24 January 2006
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 100 (3) , 1802-1808
Blends of modified epoxy resin and carboxyl‐terminated polybutadiene. I
Six blend samples were prepared by the physical mixing of epoxidized resole (EDR) with different weight ratios of carboxyl‐terminated polybutadiene (CTPB) liquid rubber ranging from 0 to 25 wt % in intervals of 5 wt %. The formation of various reaction products during the curing of unblended EDR and CTPB‐blended EDR were studied with Fourier transform infrared spectroscopy. The curing time at 100°C for the blend sample containing 15 wt % CTPB was the least among all of the blend samples. This blend sample, also, showed the highest initial degradation temperature, as obtained from thermogravimetric analysis thermograms, which indicated that it was the most thermally stable matrix system. The films of coatings based on the blend of EDR with 15 wt % CTPB offered the highest resistance toward different concentrations of acids and alkalis compared to the films having 5, 10, 20, and 25 wt % CTPB in the EDR/CTPB blends. Solvents showed almost the same behavior as acids and alkalis for these films except for hydrocarbon solvents such as mineral turpentine oil, toluene, and xylene. The resistance toward these solvents was poor and slightly inferior to those found with EDR unblended with CTPB. The tensile, flexural, and impact strengths of the molded specimens derived from the EDR/CTPB blends initially increased up to 15 wt % CTPB addition in the blend and then decreased, whereas the elongation at break remained constant for all blend compositions. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 100: 1802–1808, 2006
- 31 March 2001
- Published by Taylor & Francis in Materials and Manufacturing Processes
- Vol. 16 (2) , 281-289
STUDY OF DEGRADATION KINETICS OF BLENDS OF EPOXY AND RESOLE: A STATISTICAL APPROACH
Blends of resole and epoxy were prepared by physical mixing, and cured with 30% polyamide based on blend resin and polyamide. Degradation of each sample was studied by dynamic thermogravimetric analysis in nitrogen atmosphere at a heating rate of 10°C min−1. The degradation of blends of epoxy and resole having 30 wt % polyamide proceeded with 0.50th order. This result was found with the Coats-Redfern equation using best-fit analysis, and further confirmed by linear regression analysis. The validity of data was checked by t test analysis. From this value of reaction order, activation energy (E) and pre-exponential factor (Z) were calculated. The values of activation energy increased, whereas the values of pre-exponential factor decreased as the resole content in the blend decreased from 100 to 0 wt %.
- 31 March 2001
- Published by Taylor & Francis in Materials and Manufacturing Processes
- Vol. 16 (2) , 281-289
STUDY OF DEGRADATION KINETICS OF BLENDS OF EPOXY AND RESOLE: A STATISTICAL APPROACH
Blends of resole and epoxy were prepared by physical mixing, and cured with 30% polyamide based on blend resin and polyamide. Degradation of each sample was studied by dynamic thermogravimetric analysis in nitrogen atmosphere at a heating rate of 10°C min−1. The degradation of blends of epoxy and resole having 30 wt % polyamide proceeded with 0.50th order. This result was found with the Coats-Redfern equation using best-fit analysis, and further confirmed by linear regression analysis. The validity of data was checked by t test analysis. From this value of reaction order, activation energy (E) and pre-exponential factor (Z) were calculated. The values of activation energy increased, whereas the values of pre-exponential factor decreased as the resole content in the blend decreased from 100 to 0 wt %.