Mohammed S. Aboraia
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Mohammed S. Aboraia has a total of 20 co-authors. Here are the top co-authors by number of shared publications:
- M. A. Doheim
Mining and Metallurgical Engineering Department, Assiut University, Assiut71516, Egypt
3 shared publications - S. A. Karrab
Faculty of Engineering, Materials Science Department, Misurata University, Misurata, Libya
3 shared publications - Shemy M. Ahmed
Mechanical Engineering Department, Faculty of Engineering, Majmaah University, North Riyadh, Kingdom of Saudi Arabia
3 shared publications A E Rizk
1 shared publicationB. Reitinger
1 shared publicationC. Hofer
1 shared publication
Latest Publications
- 26 July 2020
- Published by Egyptian Knowledge Bank in Journal of Petroleum and Mining Engineering
- p. 1-7
Joint Addition of Zirconium, Titanium and Chromium to Commercial Pure Aluminium
The effect of joint addition of Zr, Ti and Cr on the grain refinement of commercial pure aluminium (99.7% Al) has been investigated by optical microscopy and scanning electron microscopy (SEM) as well as Energy Dispersive X-ray Spectroscopy (EDS). It was found that joint addition of 0.15 wt% Zr and 0.025 wt% Ti to Al can result in a remarkable refinement with an average grain size of 102 μm. It was found the optimum addition level of Ti to be 0.025 wt% in the presence of 0.1 % Zr and any increase in the Ti beyond 0.025wt% results in coarse grain size. Joint additions of 0.15 wt% Zr, 0.025 wt% Ti and 0.15 wt% Cr to Al facilitate better grain refinement and the average grain size was 75 μm. The grain refining performance of joint addition of 0.1 wt.% Zr and different additions of either Ti or Cr is higher than refining with zirconium alone. EDS and SEM analysis of the precipitated phases observed at or near the centers of the refined aluminium with joint addition of Zr and Ti was found to be Al3(Zr1-xTix). These Al3(Zr1-xTix) particles act as heterogeneous nucleation sites for α-Al during solidification and resulted in better grain refinement.
- 26 July 2020
- Published by Egyptian Knowledge Bank in Journal of Petroleum and Mining Engineering
- p. 1-7
Joint Addition of Zirconium, Titanium and Chromium to Commercial Pure Aluminium
The effect of joint addition of Zr, Ti and Cr on the grain refinement of commercial pure aluminium (99.7% Al) has been investigated by optical microscopy and scanning electron microscopy (SEM) as well as Energy Dispersive X-ray Spectroscopy (EDS). It was found that joint addition of 0.15 wt% Zr and 0.025 wt% Ti to Al can result in a remarkable refinement with an average grain size of 102 μm. It was found the optimum addition level of Ti to be 0.025 wt% in the presence of 0.1 % Zr and any increase in the Ti beyond 0.025wt% results in coarse grain size. Joint additions of 0.15 wt% Zr, 0.025 wt% Ti and 0.15 wt% Cr to Al facilitate better grain refinement and the average grain size was 75 μm. The grain refining performance of joint addition of 0.1 wt.% Zr and different additions of either Ti or Cr is higher than refining with zirconium alone. EDS and SEM analysis of the precipitated phases observed at or near the centers of the refined aluminium with joint addition of Zr and Ti was found to be Al3(Zr1-xTix). These Al3(Zr1-xTix) particles act as heterogeneous nucleation sites for α-Al during solidification and resulted in better grain refinement.
- 21 September 2018
- Published by IOP Publishing in Materials Research Express
- Vol. 5 (12) , 126511
The effect of sodium citrate as a complex agent on the corrosion properties of the electroless Ni-P coating
- 21 September 2018
- Published by IOP Publishing in Materials Research Express
- Vol. 5 (12) , 126511
The effect of sodium citrate as a complex agent on the corrosion properties of the electroless Ni-P coating
- 7 April 2017
- Published by SAGE Publications in Journal of Reinforced Plastics and Composites
- Vol. 36 (15) , 1092-1098
Notch sensitivity of short and 2D plain woven glass fibres reinforced with different polymer matrix composites
This research article investigated the notch sensitivity of two different glass fibre architectures, namely short and 2D plain-woven glass fibres reinforced with unsaturated polyester and epoxy matrix composites fabricated by the hand lay-up technique. This was carried out through open hole tension tests at different ratios of the specimen hole diameter to the specimen with three different values (0.1, 0.2, 0.5) compared to the unnotched specimen. The notch sensitivity of these composites was evaluated using the residual tensile strength by the application of Whitney–Nuismer Mathematical Model. The results showed that by using polyester matrix, the notch sensitivity of composites reinforced with plain-woven glass fibre is higher than that of short glass fibre at different D/W ratios. On the other hand, on testing epoxy matrixes, the notch sensitivity of composites reinforced with plain-woven glass fibre is lower than that of short glass fibre at different D/W ratios.
- 7 April 2017
- Published by SAGE Publications in Journal of Reinforced Plastics and Composites
- Vol. 36 (15) , 1092-1098
Notch sensitivity of short and 2D plain woven glass fibres reinforced with different polymer matrix composites
This research article investigated the notch sensitivity of two different glass fibre architectures, namely short and 2D plain-woven glass fibres reinforced with unsaturated polyester and epoxy matrix composites fabricated by the hand lay-up technique. This was carried out through open hole tension tests at different ratios of the specimen hole diameter to the specimen with three different values (0.1, 0.2, 0.5) compared to the unnotched specimen. The notch sensitivity of these composites was evaluated using the residual tensile strength by the application of Whitney–Nuismer Mathematical Model. The results showed that by using polyester matrix, the notch sensitivity of composites reinforced with plain-woven glass fibre is higher than that of short glass fibre at different D/W ratios. On the other hand, on testing epoxy matrixes, the notch sensitivity of composites reinforced with plain-woven glass fibre is lower than that of short glass fibre at different D/W ratios.
- 31 July 2015
- Published by Wiley
- p. 87-97
Effect of Electroless Ni‐Co‐P and Co‐P Coatings on Cavitation Erosion Resistance
- 31 July 2015
- Published by Wiley
- p. 87-97
Effect of Electroless Ni‐Co‐P and Co‐P Coatings on Cavitation Erosion Resistance
- 1 January 2012
- Published by ASME International in Journal of Tribology
- Vol. 134 (1) , 011602
Study of Cavitation Erosion Pits on 1045 Carbon Steel Surface in Corrosive Waters
Cavitation erosion resistance of steels is important in many applications. The investigation of such resistance, under different conditions, should be very useful. Cavitation erosion tests were carried out on carbon steel AISI-1045 using an ultrasonic induced cavitation facility. Cavitation erosion pits and their effect on the localized corrosion were investigated in detail in three different corrosive media: distilled water, tap water, and 3% NaCl water.The results of the investigation using SEM indicated the formation of three types of pits on cavitating specimen surfaces: corrosion pits, erosion pits, and erosion-corrosion pits. The corrosion pits have different shapes, however, the lamellar structure is the dominant structure, and has a large size of about 100 μm. The erosion pits that were formed by the cavitation microjet impacts have sizes of a few micrometers. The erosion-corrosion pits were similar to the corrosion pits, except the erosion pits formed on the corrosion pit surface due to dissolution. The eroded surface removal was the largest in the case of saline water.
- 1 January 2012
- Published by ASME International in Journal of Tribology
- Vol. 134 (1) , 011602
Study of Cavitation Erosion Pits on 1045 Carbon Steel Surface in Corrosive Waters
Cavitation erosion resistance of steels is important in many applications. The investigation of such resistance, under different conditions, should be very useful. Cavitation erosion tests were carried out on carbon steel AISI-1045 using an ultrasonic induced cavitation facility. Cavitation erosion pits and their effect on the localized corrosion were investigated in detail in three different corrosive media: distilled water, tap water, and 3% NaCl water.The results of the investigation using SEM indicated the formation of three types of pits on cavitating specimen surfaces: corrosion pits, erosion pits, and erosion-corrosion pits. The corrosion pits have different shapes, however, the lamellar structure is the dominant structure, and has a large size of about 100 μm. The erosion pits that were formed by the cavitation microjet impacts have sizes of a few micrometers. The erosion-corrosion pits were similar to the corrosion pits, except the erosion pits formed on the corrosion pit surface due to dissolution. The eroded surface removal was the largest in the case of saline water.
- 24 December 2011
- Published by Springer Nature in Tribology Letters
- Vol. 45 (3) , 437-444
Investigation of the Ring Area Formed Around Cavitation Erosion Pits on the Surface of Carbon Steel
- 24 December 2011
- Published by Springer Nature in Tribology Letters
- Vol. 45 (3) , 437-444
Investigation of the Ring Area Formed Around Cavitation Erosion Pits on the Surface of Carbon Steel
- Open Access
- 1 March 2011
- Published by Egyptian Knowledge Bank in JES. Journal of Engineering Sciences
- Vol. 39 (2) , 441-451
PRODUCTION OF ALUMINIUM FOAM AND THE EFFECT OF CALCIUM CARBONATE AS A FOAMING AGENT
- 1 March 2011
- Published by Egyptian Knowledge Bank in JES. Journal of Engineering Sciences
- Vol. 39 (2) , 441-451
Open AccessPRODUCTION OF ALUMINIUM FOAM AND THE EFFECT OF CALCIUM CARBONATE AS A FOAMING AGENT
- 1 February 2005
- Published by Elsevier in Composites Science and Technology
- Vol. 65 (2) , 301-306
Non-contact determination of elastic moduli of continuous fiber reinforced metals
- 1 February 2005
- Published by Elsevier in Composites Science and Technology
- Vol. 65 (2) , 301-306
Non-contact determination of elastic moduli of continuous fiber reinforced metals