Abdullah Sert
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Abdullah Sert has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- Fatih Hayati Çakir
Eskisehir Osmangazi University
3 shared publications Osman Nuri Celik
2 shared publicationsOsman Nuri Çelik
2 shared publications- Selim Gürgen
Eskisehir Osmangazi University
2 shared publications - Ali Armağan Diler
Departmant of Aviation Science and Technology, Institute of Science and Technology, Eskişehir Osmangazi University, Eskisehir, Turkey
1 shared publication - Gökçe Mehmet Ay
Department of Mechanical Engineering, School of Engineering and Architecture, Eskişehir Osmangazi University, Eskişehir, Turkey
1 shared publication
Latest Publications
- 2 July 2026
- Published by Springer Nature
- p. 99-115
Surface Polishing of an Al–Si–Cu–Ni–Mg Alloy Reinforced with SiC Particles
- 2 July 2026
- Published by Springer Nature
- p. 99-115
Surface Polishing of an Al–Si–Cu–Ni–Mg Alloy Reinforced with SiC Particles
- Open Access
- 17 June 2026
- Published by IOP Publishing in Materials Research Express
- Vol. 13 (12) , 126503
Characterization of the mechanical and microstructural properties of cryogenic and austempering heat treatments on Mo alloyed ductile cast iron
This study examines the combined effects of molybdenum (Mo) alloying and deep cryogenic treatment (DCT) on the microstructure and mechanical response of austempered ductile iron (ADI). Ductile irons with three Mo contents (0.388, 0.671, and 0.990 wt.%) were produced, austempered at 400 °C, and subsequently subjected to DCT at −196 °C for 360 min. Microstructural and phase analyses were conducted using optical microscopy, scanning electron microscopy, high-resolution transmission electron microscopy, and x-ray diffraction (XRD). Austempering resulted in a typical ausferritic matrix, while the subsequent cryogenic step was associated with further microstructural refinement and features indicative of partial transformation of retained austenite. In addition, fine secondary features were observed locally and attributed to carbide-like precipitates. Quantitative XRD analysis revealed the presence of α and γ reflections in all heat-treated conditions. Detailed diffraction scans exhibited a distinct peak shift toward lower 2 θ angles following DCT, indicating an expansion of the lattice parameters and a corresponding enrichment of carbon within the austenite phase. In terms of mechanical response, the integration of austempering and DCT led to a 16.6% increase in hardness compared to the as-cast state. Furthermore, the combined heat treatment cycle resulted in a 42.3% enhancement in impact energy relative to the initial cast condition, highlighting the potential of DCT to optimize the structural integrity and toughness of Mo-alloyed ADI.
- 17 June 2026
- Published by IOP Publishing in Materials Research Express
- Vol. 13 (12) , 126503
Open AccessCharacterization of the mechanical and microstructural properties of cryogenic and austempering heat treatments on Mo alloyed ductile cast iron
This study examines the combined effects of molybdenum (Mo) alloying and deep cryogenic treatment (DCT) on the microstructure and mechanical response of austempered ductile iron (ADI). Ductile irons with three Mo contents (0.388, 0.671, and 0.990 wt.%) were produced, austempered at 400 °C, and subsequently subjected to DCT at −196 °C for 360 min. Microstructural and phase analyses were conducted using optical microscopy, scanning electron microscopy, high-resolution transmission electron microscopy, and x-ray diffraction (XRD). Austempering resulted in a typical ausferritic matrix, while the subsequent cryogenic step was associated with further microstructural refinement and features indicative of partial transformation of retained austenite. In addition, fine secondary features were observed locally and attributed to carbide-like precipitates. Quantitative XRD analysis revealed the presence of α and γ reflections in all heat-treated conditions. Detailed diffraction scans exhibited a distinct peak shift toward lower 2 θ angles following DCT, indicating an expansion of the lattice parameters and a corresponding enrichment of carbon within the austenite phase. In terms of mechanical response, the integration of austempering and DCT led to a 16.6% increase in hardness compared to the as-cast state. Furthermore, the combined heat treatment cycle resulted in a 42.3% enhancement in impact energy relative to the initial cast condition, highlighting the potential of DCT to optimize the structural integrity and toughness of Mo-alloyed ADI.
- 22 August 2025
- Published by Eskisehir Osmangazi Universitesi Muhendislik ve Mimarlik Fakultesi Dergisi in Eskişehir Osmangazi Üniversitesi Mühendislik ve Mimarlık Fakültesi Dergisi
- Vol. 33 (2) , 1809-1818
MICROSTRUCTURAL AND TRIBOLOGICAL PROPERTIES OF NICKEL-BASED HARDFACING COATINGS APPLIED ON NITRIDING STEELS BY PLASMA TRANSFERRED ARC WELDING
Plasma Transferred Arc (PTA) coatings are widely used for the surface modification of metals due to their ability to achieve high coating thickness, low thermal stress, and high energy density. This technique is commonly applied to glass and ceramic molds, automotive valves, petrochemical vanes, lamination cylinders, as well as plastic extrusion molds and screws. In plastic injection machine screws, high hardness and wear resistance are essential for durability. To achieve these properties, the steels used in plastic injection screws are first hardfaced on the thread crests using the PTA coating method and then nitrided. In this study, 1.8550 and 1.8519 steels, commonly used in plastic injection screw manufacturing, were coated with two different powders: FeCrBSi with a nickel (Ni) balance, either with or without tungsten (W) addition. The tribological properties of the coated samples were evaluated through ball-on-disc wear tests. The samples were characterized using X-ray diffraction (XRD), scanning electron microscopy (SEM), energy-dispersive spectroscopy (EDS), and optical microscopy. The depth and width of wear tracks were measured using a profilometer. Results indicated that increasing W content leads to a higher coefficient of friction, but the best wear performance was observed with W-containing coatings. The optimal combination was found to be the 1.8550 steel substrate paired with the FeCrBSi-W coating, which demonstrated a 5% higher coefficient of friction but a 47% lower specific wear rate compared to the non-W coating.
- 22 August 2025
- Published by Eskisehir Osmangazi Universitesi Muhendislik ve Mimarlik Fakultesi Dergisi in Eskişehir Osmangazi Üniversitesi Mühendislik ve Mimarlık Fakültesi Dergisi
- Vol. 33 (2) , 1809-1818
MICROSTRUCTURAL AND TRIBOLOGICAL PROPERTIES OF NICKEL-BASED HARDFACING COATINGS APPLIED ON NITRIDING STEELS BY PLASMA TRANSFERRED ARC WELDING
Plasma Transferred Arc (PTA) coatings are widely used for the surface modification of metals due to their ability to achieve high coating thickness, low thermal stress, and high energy density. This technique is commonly applied to glass and ceramic molds, automotive valves, petrochemical vanes, lamination cylinders, as well as plastic extrusion molds and screws. In plastic injection machine screws, high hardness and wear resistance are essential for durability. To achieve these properties, the steels used in plastic injection screws are first hardfaced on the thread crests using the PTA coating method and then nitrided. In this study, 1.8550 and 1.8519 steels, commonly used in plastic injection screw manufacturing, were coated with two different powders: FeCrBSi with a nickel (Ni) balance, either with or without tungsten (W) addition. The tribological properties of the coated samples were evaluated through ball-on-disc wear tests. The samples were characterized using X-ray diffraction (XRD), scanning electron microscopy (SEM), energy-dispersive spectroscopy (EDS), and optical microscopy. The depth and width of wear tracks were measured using a profilometer. Results indicated that increasing W content leads to a higher coefficient of friction, but the best wear performance was observed with W-containing coatings. The optimal combination was found to be the 1.8550 steel substrate paired with the FeCrBSi-W coating, which demonstrated a 5% higher coefficient of friction but a 47% lower specific wear rate compared to the non-W coating.
- 5 October 2022
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications
- Vol. 237 (4) , 925-940
Failure analysis of an axle shaft in an airport ground support vehicle
In this study, failure analysis of an axle shaft in an airport ground support vehicle was carried out to determine failure mechanism, failure root causes and preventive actions. Macroscopic observation, numerical analysis, metallographic analysis, chemical composition analysis, hardness measurement and tensile test methods were used in failure analysis. In numerical fatigue analyses, axle shaft was modelled as a functionally graded material due to mechanical properties changing in the material radial section as a result of induction surface hardening. The analysis results showed that the failure mechanism of fractured axle shaft was torsional fatigue. High surface roughness and insufficient mechanical properties were found as failure root causes. Making finish cut with low depth and even grinding in surface finishing process were proposed as a prevention to increase surface quality, reduce surface roughness and stress concentrations in machining of axle shaft. In addition, using another material with higher yield strength (EN 37Cr4) was proposed instead of EN 34Cr4 alloy steel as the axle shaft material.
- 5 October 2022
- Published by SAGE Publications in Proceedings of the Institution of Mechanical Engineers, Part L: Journal of Materials: Design and Applications
- Vol. 237 (4) , 925-940
Failure analysis of an axle shaft in an airport ground support vehicle
In this study, failure analysis of an axle shaft in an airport ground support vehicle was carried out to determine failure mechanism, failure root causes and preventive actions. Macroscopic observation, numerical analysis, metallographic analysis, chemical composition analysis, hardness measurement and tensile test methods were used in failure analysis. In numerical fatigue analyses, axle shaft was modelled as a functionally graded material due to mechanical properties changing in the material radial section as a result of induction surface hardening. The analysis results showed that the failure mechanism of fractured axle shaft was torsional fatigue. High surface roughness and insufficient mechanical properties were found as failure root causes. Making finish cut with low depth and even grinding in surface finishing process were proposed as a prevention to increase surface quality, reduce surface roughness and stress concentrations in machining of axle shaft. In addition, using another material with higher yield strength (EN 37Cr4) was proposed instead of EN 34Cr4 alloy steel as the axle shaft material.
- 24 November 2021
- Published by IOP Publishing in Surface Topography: Metrology and Properties
- Vol. 9 (4) , 045026
Improvement of tool life of a commercial drill bits by cryogenic treatment while machining widmanstatten Ti-6Al-4V
In this study, the performance of Ø 8 mm WC-Co (10%) drill bits with a TiAlN coating was tested for machining of Ti6Al4V alloy with a Widmanstatten structure. In order to improve the tool life, cutting tools were subjected to deep cryogenic treatment. In total, three groups of tools were prepared for this study. The first group was used for reference as the supplied state; the second group was subjected to 24 h deep cryogenic treatment at −196 °C, and the third group was subjected to 24 h deep cryogenic at −196 °C, additionally was tempered 2 h at 200 °C. Machining experiments were done by drilling and a set of 60 holes were drilled with each drill bit, and tool wear were observed and recorded with a stereo microscope. Additionally, Scanning Electron Microscope (SEM) and Energy Dispersive Spectroscopy (EDS) analyses were carried on to understand the tool wear better. The microhardness of Cryo-treated and tempered cutting tools hardness increased up to 20 Hv (about 1%), and the toughness value did not change significantly. Cutting performance was observed by measuring the cutting forces during drilling experiments. According to these results, deep cryogenic treatment on WC-Co-based inserts decreased cutting forces by approximately 7% compared to the reference drill bit, which affected the cutting tool life. The dominant wear mechanism was Built-up edge (BUE) formation, and cryo-treatment lowered the BUE amount 8% and cryo-treated and tempered drill bit 45% compared to the reference drill bit.
- 24 November 2021
- Published by IOP Publishing in Surface Topography: Metrology and Properties
- Vol. 9 (4) , 045026
Improvement of tool life of a commercial drill bits by cryogenic treatment while machining widmanstatten Ti-6Al-4V
In this study, the performance of Ø 8 mm WC-Co (10%) drill bits with a TiAlN coating was tested for machining of Ti6Al4V alloy with a Widmanstatten structure. In order to improve the tool life, cutting tools were subjected to deep cryogenic treatment. In total, three groups of tools were prepared for this study. The first group was used for reference as the supplied state; the second group was subjected to 24 h deep cryogenic treatment at −196 °C, and the third group was subjected to 24 h deep cryogenic at −196 °C, additionally was tempered 2 h at 200 °C. Machining experiments were done by drilling and a set of 60 holes were drilled with each drill bit, and tool wear were observed and recorded with a stereo microscope. Additionally, Scanning Electron Microscope (SEM) and Energy Dispersive Spectroscopy (EDS) analyses were carried on to understand the tool wear better. The microhardness of Cryo-treated and tempered cutting tools hardness increased up to 20 Hv (about 1%), and the toughness value did not change significantly. Cutting performance was observed by measuring the cutting forces during drilling experiments. According to these results, deep cryogenic treatment on WC-Co-based inserts decreased cutting forces by approximately 7% compared to the reference drill bit, which affected the cutting tool life. The dominant wear mechanism was Built-up edge (BUE) formation, and cryo-treatment lowered the BUE amount 8% and cryo-treated and tempered drill bit 45% compared to the reference drill bit.
- 1 March 2021
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 41 (3) , 1878-1890
Anisotropic mechanical and tribological properties of SiAlON matrix composites containing different types of GNPs
- 1 March 2021
- Published by Elsevier in Journal of the European Ceramic Society
- Vol. 41 (3) , 1878-1890
Anisotropic mechanical and tribological properties of SiAlON matrix composites containing different types of GNPs
- 3 November 2020
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 138 (16)
An investigation on wear behavior of UHMWPE/carbide composites at elevated temperatures
Ultra‐high molecular weight polyethylene (UHMWPE) is extensively used in frictional applications due to its advanced wear resistance. This advanced polymer is reinforced with hard particulate fillers for further developments against wear conditions. Since elevated temperatures prevail in the service conditions, wear behavior of UHMWPE composites is an important issue for the engineering applications. In the present work, UHMWPE‐based composites including silicon carbide (SiC) fillers were fabricated in a compression molding chamber. In the specimen preparation stage, molding pressure, filler amount, and filler particle size were varied to investigate the influence of these variables. Upon deciding the optimum parameters from the wear tests conducted at room temperature, the wear experiments were repeated for the optimum specimen at elevated temperatures, such as 40 and 60°C. According to the results, the wear behavior of the SiC/UHMWPE composites is heavily changed by the effect of elevated temperature. Adhesive effect is pronounced at elevated temperatures while the wear characteristics possess the abrasive effect in the sliding path. In addition, the composites exhibit an accelerated material loss as temperature increases during the frictional system.
- 3 November 2020
- Published by Wiley in Journal of Applied Polymer Science
- Vol. 138 (16)
An investigation on wear behavior of UHMWPE/carbide composites at elevated temperatures
Ultra‐high molecular weight polyethylene (UHMWPE) is extensively used in frictional applications due to its advanced wear resistance. This advanced polymer is reinforced with hard particulate fillers for further developments against wear conditions. Since elevated temperatures prevail in the service conditions, wear behavior of UHMWPE composites is an important issue for the engineering applications. In the present work, UHMWPE‐based composites including silicon carbide (SiC) fillers were fabricated in a compression molding chamber. In the specimen preparation stage, molding pressure, filler amount, and filler particle size were varied to investigate the influence of these variables. Upon deciding the optimum parameters from the wear tests conducted at room temperature, the wear experiments were repeated for the optimum specimen at elevated temperatures, such as 40 and 60°C. According to the results, the wear behavior of the SiC/UHMWPE composites is heavily changed by the effect of elevated temperature. Adhesive effect is pronounced at elevated temperatures while the wear characteristics possess the abrasive effect in the sliding path. In addition, the composites exhibit an accelerated material loss as temperature increases during the frictional system.
- 1 October 2019
- Published by Elsevier in Composites Part B: Engineering
- Vol. 175
Polishing operation of a steel bar in a shear thickening fluid medium
- 1 October 2019
- Published by Elsevier in Composites Part B: Engineering
- Vol. 175
Polishing operation of a steel bar in a shear thickening fluid medium
- Open Access
- 31 August 2019
- Published by Turkish Journal of Public Health in Türkiye Halk Sağlığı Dergisi
- Vol. 17 (2) , 132-142
Healthy lifestyle behaviors of medical and vocational high school students and related socio-demographic factors
Amaç: Bu çalışmada Yüzüncü Yıl Üniversitesi Tıp Fakültesi ve Van Meslek Yüksek Okulu’nda eğitim gören öğrencilerin sağlıklı yaşam biçimi davranışlarının değerlendirilmesi ve bu davranışlarla ilişkili sosyo-demografik özelliklerin saptanması amaçlanmıştır. Yöntem: Çalışmanın evreni Yüzüncü Yıl Üniversitesi Tıp Fakültesi ve Van Meslek Yüksek Okulu’nda eğitim gören 1842 öğrenci oluşturmaktadır. Tabakalı ve sistematik yöntemle seçilen 470 öğrenci örnek grubunu oluşturmaktadır. Verilerin toplanmasında öğrencilerin sosyo-demografik özelliklerini ve sağlıklarıyla ilgili bazı konuları sorgulayan bir anket ile Sağlıklı Yaşam Biçimi Davranışları-II (SYBD-II) ölçeği gözetim altında uygulanmıştır. Bulgular: Öğrencilerin 313’ü (%66.6) Meslek Yüksekokulu’nda, 157’si (%33.4) Tıp Fakültesinde öğrenim görmektedir. Araştırmaya katılan öğrencilerin 199’u (%42.6) kız, 268’i (%57.4) erkektir. Öğrencilerin yaşlarının ortanca değeri 22’dir (en küçük-en büyük=17-60). Öğrencilerin sağlıklı yaşam biçimi davranışları ölçeğinden aldıkları puanın ortalaması 123.2±20.6’dir. Fakülteler arasında SYBD toplam puanı açısından istatistik olarak anlamlı fark bulunmamıştır (p=0.05). Sonuç: Öğrencilerin SYBD toplam puanı ortalaması orta düzeyde bulunmuştur. SYBD düzeyinin artırılması için farkındalık yaratma ve bilinçlendirme çalışmaları yapılmalıdır.
- 31 August 2019
- Published by Turkish Journal of Public Health in Türkiye Halk Sağlığı Dergisi
- Vol. 17 (2) , 132-142
Open AccessHealthy lifestyle behaviors of medical and vocational high school students and related socio-demographic factors
Amaç: Bu çalışmada Yüzüncü Yıl Üniversitesi Tıp Fakültesi ve Van Meslek Yüksek Okulu’nda eğitim gören öğrencilerin sağlıklı yaşam biçimi davranışlarının değerlendirilmesi ve bu davranışlarla ilişkili sosyo-demografik özelliklerin saptanması amaçlanmıştır. Yöntem: Çalışmanın evreni Yüzüncü Yıl Üniversitesi Tıp Fakültesi ve Van Meslek Yüksek Okulu’nda eğitim gören 1842 öğrenci oluşturmaktadır. Tabakalı ve sistematik yöntemle seçilen 470 öğrenci örnek grubunu oluşturmaktadır. Verilerin toplanmasında öğrencilerin sosyo-demografik özelliklerini ve sağlıklarıyla ilgili bazı konuları sorgulayan bir anket ile Sağlıklı Yaşam Biçimi Davranışları-II (SYBD-II) ölçeği gözetim altında uygulanmıştır. Bulgular: Öğrencilerin 313’ü (%66.6) Meslek Yüksekokulu’nda, 157’si (%33.4) Tıp Fakültesinde öğrenim görmektedir. Araştırmaya katılan öğrencilerin 199’u (%42.6) kız, 268’i (%57.4) erkektir. Öğrencilerin yaşlarının ortanca değeri 22’dir (en küçük-en büyük=17-60). Öğrencilerin sağlıklı yaşam biçimi davranışları ölçeğinden aldıkları puanın ortalaması 123.2±20.6’dir. Fakülteler arasında SYBD toplam puanı açısından istatistik olarak anlamlı fark bulunmamıştır (p=0.05). Sonuç: Öğrencilerin SYBD toplam puanı ortalaması orta düzeyde bulunmuştur. SYBD düzeyinin artırılması için farkındalık yaratma ve bilinçlendirme çalışmaları yapılmalıdır.
- 1 April 2019
- Published by Elsevier in Materials Characterization
- Vol. 150, 1-7
Characterization of the mechanism of cryogenic treatment on the microstructural changes in tungsten carbide cutting tools
- 1 April 2019
- Published by Elsevier in Materials Characterization
- Vol. 150, 1-7
Characterization of the mechanism of cryogenic treatment on the microstructural changes in tungsten carbide cutting tools