Hongfeng Huang
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Research Interests
Hongfeng Huang has a total of 19 co-authors. Here are the top co-authors by number of shared publications:
- K. Suzuki
Monash University
3 shared publications A. Kato
Toyota Motor Corporation 4 , Mishuku, Susono, Shizuoka 410-1193, Japan
2 shared publications- R. Parsons
Department of Materials Science and Engineering, Monash University 1 , Clayton, VIC 3800, Australia
2 shared publications T. Shoji
Toyota Motor Corporation 4 , Mishuku, Susono, Shizuoka 410-1193, Japan
2 shared publications- Akira Kato
Toyota Motor Corporation, Mishuku, Susono, Shizuoka 410-1193, Japan
1 shared publication B. Zang
Department of Materials Science and Engineering, Monash University 1 , Clayton, VIC 3800, Australia
1 shared publication
Latest Publications
- 8 March 2024
- Published by American Physical Society (APS) in Physical Review B
- Vol. 109 (10) , 104408
Origin of excess core loss in amorphous and nanocrystalline soft magnetic materials
Core losses of amorphous and nanocrystalline soft magnetic ribbons with a range of saturation magnetostriction constants () from near zero to have been investigated experimentally with complementary micromagnetic simulations in order to clarify the effect of magnetostriction on the excess loss, i.e., the core loss component unaccounted for by the hysteresis and classical eddy-current losses. The excess loss at 400 Hz and a peak polarization of 1.0 T () has been found to increase linearly with , and varies considerably between for near zero-magnetostrictive nc- and for amorphous with . By substituting the domain wall damping coefficient () for the eddy current one in Bertotti's statistical model of core losses, the excess loss is predicted to be proportional to , indicating that the observed linear increase of is caused by mechanisms where increases with . Such a quadratic relationship is confirmed by modeling a free wall damping process with lattice anelasticity, suggesting that the anelastic lattice relaxation mediated by magnetostriction could be a potential mechanism. However, the absolute value of remains open because of the uncertainty of the viscosity, and further investigation is needed to validate the mechanism of the excess loss induced by magnetostriction. Our results show that magnetostriction plays a significant role in determining the excess loss in the exchange-softened magnetic materials, and lowering the saturation magnetostriction is crucial for reducing the wall damping effect and the core loss at high frequencies.- 8 March 2024
- Published by American Physical Society (APS) in Physical Review B
- Vol. 109 (10) , 104408
Origin of excess core loss in amorphous and nanocrystalline soft magnetic materials
Core losses of amorphous and nanocrystalline soft magnetic ribbons with a range of saturation magnetostriction constants () from near zero to have been investigated experimentally with complementary micromagnetic simulations in order to clarify the effect of magnetostriction on the excess loss, i.e., the core loss component unaccounted for by the hysteresis and classical eddy-current losses. The excess loss at 400 Hz and a peak polarization of 1.0 T () has been found to increase linearly with , and varies considerably between for near zero-magnetostrictive nc- and for amorphous with . By substituting the domain wall damping coefficient () for the eddy current one in Bertotti's statistical model of core losses, the excess loss is predicted to be proportional to , indicating that the observed linear increase of is caused by mechanisms where increases with . Such a quadratic relationship is confirmed by modeling a free wall damping process with lattice anelasticity, suggesting that the anelastic lattice relaxation mediated by magnetostriction could be a potential mechanism. However, the absolute value of remains open because of the uncertainty of the viscosity, and further investigation is needed to validate the mechanism of the excess loss induced by magnetostriction. Our results show that magnetostriction plays a significant role in determining the excess loss in the exchange-softened magnetic materials, and lowering the saturation magnetostriction is crucial for reducing the wall damping effect and the core loss at high frequencies.- Open Access
- 1 February 2023
- Published by AIP Publishing in AIP Advances
- Vol. 13 (2) , 025304
Effect of grain size on the core loss of nanocrystalline Fe86B13Cu1 prepared by ultra-rapid annealing
Nanocrystalline alloy samples with the same chemistry (Fe86B13Cu1) but with a range of mean grain sizes were prepared in order to investigate the effect of the grain size (D) on the core losses in nanocrystalline alloys. The core loss was measured on an Epstein frame in a frequency range between 10 Hz and 30 kHz. The measured core loss was separated into 3 parts, i.e. the hysteresis loss, classical eddy current loss and the excess loss. The classical eddy current loss is only a minor component due to the small thickness and moderately high electrical resistivity of the samples. Both the coercivity and the cycle hysteresis loss are found to follow roughly a D3 dependence. The excess loss at the maximum polarization (Jm) between 0.6 and 1.0 T is described universally by a simple power dependence of (Jm·f)n with an exponent of about 1.4 over a wide frequency (f) range between 10 Hz to 30 kHz. The excess loss at low frequencies appears almost independent of the grain size. Thus, the grain size effect on the total loss at low frequencies is attributable to the change in the hysteresis loss which reflects the static coercivity. However, the excess loss at 30 kHz shows a clear increase with an increase in D, indicating that the excess loss also becomes influential to the grain size dependence of the total core loss at high frequencies.
- 1 February 2023
- Published by AIP Publishing in AIP Advances
- Vol. 13 (2) , 025304
Open AccessEffect of grain size on the core loss of nanocrystalline Fe86B13Cu1 prepared by ultra-rapid annealing
Nanocrystalline alloy samples with the same chemistry (Fe86B13Cu1) but with a range of mean grain sizes were prepared in order to investigate the effect of the grain size (D) on the core losses in nanocrystalline alloys. The core loss was measured on an Epstein frame in a frequency range between 10 Hz and 30 kHz. The measured core loss was separated into 3 parts, i.e. the hysteresis loss, classical eddy current loss and the excess loss. The classical eddy current loss is only a minor component due to the small thickness and moderately high electrical resistivity of the samples. Both the coercivity and the cycle hysteresis loss are found to follow roughly a D3 dependence. The excess loss at the maximum polarization (Jm) between 0.6 and 1.0 T is described universally by a simple power dependence of (Jm·f)n with an exponent of about 1.4 over a wide frequency (f) range between 10 Hz to 30 kHz. The excess loss at low frequencies appears almost independent of the grain size. Thus, the grain size effect on the total loss at low frequencies is attributable to the change in the hysteresis loss which reflects the static coercivity. However, the excess loss at 30 kHz shows a clear increase with an increase in D, indicating that the excess loss also becomes influential to the grain size dependence of the total core loss at high frequencies.
- 17 July 2022
- Published by Wiley in Advanced Materials Interfaces
- Vol. 9 (23)
Substrate Modification for High‐Performance Thermoelectric Materials and Generators Based on Polymer and Carbon Nanotube Composite
Polymer and carbon nanotube composites have aroused extensive attention for thermoelectric materials owing to the combination of low thermal conductivity of polymer and high electrical conductivity of carbon nanotubes. Surface properties of the substrate are of great importance for the charge transport behaviors of semiconducting thin films, which are less explored in thermoelectric applications. Herein, self‐assembled monolayers (SAMs) are used to modify the substrate for thermoelectric polymer composites. The trifluoromethyl (CF3)‐terminated SAM is beneficial for an improved electrical conductivity; while the SAM with amino group is found to improve their Seebeck coefficient and decrease the electrical conductivity. As a result, polymer composites on CF3‐SAM‐modified substrate show a high room‐temperature power factor of 285 µW m−1 K−2 and a large output power of 2.36 µW for thermoelectric generator at a temperature gradient of 50 K. This work demonstrates that surface modification by SAMs is a promising strategy for improving performance of thermoelectric materials and devices.
- 17 July 2022
- Published by Wiley in Advanced Materials Interfaces
- Vol. 9 (23)
Substrate Modification for High‐Performance Thermoelectric Materials and Generators Based on Polymer and Carbon Nanotube Composite
Polymer and carbon nanotube composites have aroused extensive attention for thermoelectric materials owing to the combination of low thermal conductivity of polymer and high electrical conductivity of carbon nanotubes. Surface properties of the substrate are of great importance for the charge transport behaviors of semiconducting thin films, which are less explored in thermoelectric applications. Herein, self‐assembled monolayers (SAMs) are used to modify the substrate for thermoelectric polymer composites. The trifluoromethyl (CF3)‐terminated SAM is beneficial for an improved electrical conductivity; while the SAM with amino group is found to improve their Seebeck coefficient and decrease the electrical conductivity. As a result, polymer composites on CF3‐SAM‐modified substrate show a high room‐temperature power factor of 285 µW m−1 K−2 and a large output power of 2.36 µW for thermoelectric generator at a temperature gradient of 50 K. This work demonstrates that surface modification by SAMs is a promising strategy for improving performance of thermoelectric materials and devices.
- Open Access
- 1 January 2020
- Published by AIP Publishing in AIP Advances
- Vol. 10 (1) , 015105
Effect of latent heat during primary crystallization on the nanostructural formation process in nanocrystalline soft magnetic materials
Nanocrystalline soft magnetic materials are known to be prepared by primary crystallization of Fe-based amorphous precursors. Since the crystallization reaction is exothermic, the amorphous precursor may experience a temporary rise in its temperature relative to its surroundings during the process of nanocrystallization. Given the typical latent heat of primary crystallization (∼ 100 kJ/kg), this temperature rise may exceed hundreds of degrees if not adequately controlled and thus, lead to the formation of unwanted magnetically hard compounds. This effect is generally small for isolated ribbons annealed with a moderate heating rate. However, the recent adoption of high heating rates and short annealing times has caused the self-heating effect to become relevant even for small sample sizes. In this work, the effect of self-heating on the microstructure and magnetic properties of nanocrystalline Fe86B14 is investigated. It is found that magnetically hard Fe-B compounds cannot be avoided when annealing under vacuum in an infrared furnace with a heating rate ≥3 K/s due to the self-heating effect. However, the high thermal conductivity of the copper blocks used by the ultra-rapid annealing process can successfully prevent a self-heating induced temperature rise during annealing, avoiding unwanted compound formation. Finite Element Analysis is also used for predicting the extent of self-heating during infrared annealing.
- 1 January 2020
- Published by AIP Publishing in AIP Advances
- Vol. 10 (1) , 015105
Open AccessEffect of latent heat during primary crystallization on the nanostructural formation process in nanocrystalline soft magnetic materials
Nanocrystalline soft magnetic materials are known to be prepared by primary crystallization of Fe-based amorphous precursors. Since the crystallization reaction is exothermic, the amorphous precursor may experience a temporary rise in its temperature relative to its surroundings during the process of nanocrystallization. Given the typical latent heat of primary crystallization (∼ 100 kJ/kg), this temperature rise may exceed hundreds of degrees if not adequately controlled and thus, lead to the formation of unwanted magnetically hard compounds. This effect is generally small for isolated ribbons annealed with a moderate heating rate. However, the recent adoption of high heating rates and short annealing times has caused the self-heating effect to become relevant even for small sample sizes. In this work, the effect of self-heating on the microstructure and magnetic properties of nanocrystalline Fe86B14 is investigated. It is found that magnetically hard Fe-B compounds cannot be avoided when annealing under vacuum in an infrared furnace with a heating rate ≥3 K/s due to the self-heating effect. However, the high thermal conductivity of the copper blocks used by the ultra-rapid annealing process can successfully prevent a self-heating induced temperature rise during annealing, avoiding unwanted compound formation. Finite Element Analysis is also used for predicting the extent of self-heating during infrared annealing.