Hiroki Mano
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Hiroki Mano has a total of 50 co-authors. Here are the top co-authors by number of shared publications:
- Takashi Murakami
Advanced Manufacturing Research Institute, National Institute of Advanced Industrial Science and Technology (AIST)
9 shared publications - Atsushi Korenaga
National Institute of Advanced Industrial Science and Technology (AIST)
7 shared publications - Yuko Hibi
National Institute of Advanced Industrial Science and Technology (AIST)
6 shared publications - Koji Miyake
AIST
5 shared publications - Miki Nakano
National Institute of Advanced Industrial Science and Technology (AIST)
5 shared publications S. Sasaki
Tokyo University of Science, Tokyo 102-0073, Japan
4 shared publications
Latest Publications
- 27 May 2022
- Published by Elsevier in Precision Engineering
- Vol. 77, 220-226
Propagation characteristics of acoustic emission waves in liquid media in near-field
- 27 May 2022
- Published by Elsevier in Precision Engineering
- Vol. 77, 220-226
Propagation characteristics of acoustic emission waves in liquid media in near-field
- 1 October 2018
- Published by Elsevier in Biochemical and Biophysical Research Communications
- Vol. 505 (2) , 460-465
Novel biosensor using split-luciferase for detecting vitamin D receptor ligands based on the interaction between vitamin D receptor and coactivator
- 1 October 2018
- Published by Elsevier in Biochemical and Biophysical Research Communications
- Vol. 505 (2) , 460-465
Novel biosensor using split-luciferase for detecting vitamin D receptor ligands based on the interaction between vitamin D receptor and coactivator
- 18 September 2015
- Published by American Chemical Society (ACS) in Bioconjugate Chemistry
- Vol. 26 (10) , 2038-2045
Development of Novel Bioluminescent Sensor to Detect and Discriminate between Vitamin D Receptor Agonists and Antagonists in Living Cells
Active forms of vitamin D regulate the expression of multiple genes that play essential roles in calcium and phosphate homeostasis, cell differentiation, and the immune system via the vitamin D receptor (VDR). Many vitamin D analogs have been synthesized for clinical use in the treatment of type I rickets, osteoporosis, renal osteodystrophy, psoriasis, leukemia, and breast cancer. We have constructed two fusion proteins containing split-luciferase and the ligand binding domain (LBD) of the VDR designated as LucN-LBD-LucC and LucC-LBD-LucN. Remarkably, the LucC-LBD-LucN, which has the C-terminal domain of luciferase at the N-terminus of the fusion protein, was a significantly better biosensor than LucN-LBD-LucC. Addition of the VDR agonists to COS-7 cells expressing LucC-LBD-LucN dramatically reduced luciferase activity. In contrast, the VDR antagonist significantly increased the chimeric luciferase activity in a dose- and time-dependent manner. Our results on chimeric luciferases containing the LBDs of mutant VDRs derived from patients with vitamin D-dependent type II rickets indicated that our system could detect a conformational change of the LBD of the VDR likely based on a positional change of the helix 12, which occurs upon ligand binding. This novel system to detect and discriminate between VDR agonists and antagonists could be useful for the screening and identification of chemical compounds that bind to normal or mutant VDRs with high affinity.
- 18 September 2015
- Published by American Chemical Society (ACS) in Bioconjugate Chemistry
- Vol. 26 (10) , 2038-2045
Development of Novel Bioluminescent Sensor to Detect and Discriminate between Vitamin D Receptor Agonists and Antagonists in Living Cells
Active forms of vitamin D regulate the expression of multiple genes that play essential roles in calcium and phosphate homeostasis, cell differentiation, and the immune system via the vitamin D receptor (VDR). Many vitamin D analogs have been synthesized for clinical use in the treatment of type I rickets, osteoporosis, renal osteodystrophy, psoriasis, leukemia, and breast cancer. We have constructed two fusion proteins containing split-luciferase and the ligand binding domain (LBD) of the VDR designated as LucN-LBD-LucC and LucC-LBD-LucN. Remarkably, the LucC-LBD-LucN, which has the C-terminal domain of luciferase at the N-terminus of the fusion protein, was a significantly better biosensor than LucN-LBD-LucC. Addition of the VDR agonists to COS-7 cells expressing LucC-LBD-LucN dramatically reduced luciferase activity. In contrast, the VDR antagonist significantly increased the chimeric luciferase activity in a dose- and time-dependent manner. Our results on chimeric luciferases containing the LBDs of mutant VDRs derived from patients with vitamin D-dependent type II rickets indicated that our system could detect a conformational change of the LBD of the VDR likely based on a positional change of the helix 12, which occurs upon ligand binding. This novel system to detect and discriminate between VDR agonists and antagonists could be useful for the screening and identification of chemical compounds that bind to normal or mutant VDRs with high affinity.
- 1 November 2013
- Published by Elsevier in Biochemical and Biophysical Research Communications
- Vol. 441 (1) , 25-30
Possible involvement of Hcn1 ion channel in learning and memory dysfunction in SAMP8 mice
- 1 November 2013
- Published by Elsevier in Biochemical and Biophysical Research Communications
- Vol. 441 (1) , 25-30
Possible involvement of Hcn1 ion channel in learning and memory dysfunction in SAMP8 mice
- 12 September 2013
- Published by Elsevier in Tribology International
- Vol. 69, 61-69
Friction and wear properties of αFeSi2–Si alloy, ReSi1.8 and MoSi2 in ethyl alcohol
- 12 September 2013
- Published by Elsevier in Tribology International
- Vol. 69, 61-69
Friction and wear properties of αFeSi2–Si alloy, ReSi1.8 and MoSi2 in ethyl alcohol
- 1 December 2012
- Published by Elsevier in Tribology International
- Vol. 56, 1-8
Friction and wear properties of Fe7Mo6- and αFeSi2-based alloys in rapeseed oil
- 1 December 2012
- Published by Elsevier in Tribology International
- Vol. 56, 1-8
Friction and wear properties of Fe7Mo6- and αFeSi2-based alloys in rapeseed oil
- Open Access
- 1 January 2012
- Published by Japan Society of Mechanical Engineers in The Proceedings of Mechanical Engineering Congress, Japan
- Vol. 2012, _S114031-1
S114031 Lubricity of Triolein and Tristearin under High Temperature Condition
We investigated difference of lubricity of triolein, tristearin and rapeseed oil as a reference under high temperature conditions for acceleration of oxidation degradation. Though the triolein consisting of the monounsaturated fatty acid showed superior oxidation durability and oiliness to the rapeseed oil including the polyunsaturated fatty acid, phenomena which might be caused by corrosion and elimination of adsorbed film were observed on both lubricants. On the other hand, there was a possibility that the tristearin consisting of the saturated fatty acid has a superior forming capability of adsorbed film and not be related to corrosion.
- 1 January 2012
- Published by Japan Society of Mechanical Engineers in The Proceedings of Mechanical Engineering Congress, Japan
- Vol. 2012, _S114031-1
Open AccessS114031 Lubricity of Triolein and Tristearin under High Temperature Condition
We investigated difference of lubricity of triolein, tristearin and rapeseed oil as a reference under high temperature conditions for acceleration of oxidation degradation. Though the triolein consisting of the monounsaturated fatty acid showed superior oxidation durability and oiliness to the rapeseed oil including the polyunsaturated fatty acid, phenomena which might be caused by corrosion and elimination of adsorbed film were observed on both lubricants. On the other hand, there was a possibility that the tristearin consisting of the saturated fatty acid has a superior forming capability of adsorbed film and not be related to corrosion.
- 1 October 2011
- Published by Elsevier in Intermetallics
- Vol. 20 (1) , 68-75
Friction and wear properties of Fe–Si intermetallic compounds in ethyl alcohol
- 1 October 2011
- Published by Elsevier in Intermetallics
- Vol. 20 (1) , 68-75
Friction and wear properties of Fe–Si intermetallic compounds in ethyl alcohol
- 4 November 2010
- Published by IOP Publishing in Journal of Physics D: Applied Physics
- Vol. 43 (46)
Tribological properties of nanostripe surface structures—a design concept for improving tribological properties
The tribological properties of nanostripe surface structures were investigated using a pin-on-plate tribometer in order to propose a design concept for improving the tribological properties. The authors used four kinds of nanostripe structures consisting of different combinations of materials (Fe–Au, C–SiC, Al–Al2O3 and Al–Pt) fabricated by a process they had previously proposed. The frictional properties of the nanostripe structures depended on the materials that constituted the nanostripes. When the sliding direction in friction tests was parallel to the microgrooves, nanostripe structures remained on all surfaces even after friction tests. Based on the friction test results, the authors considered a design concept for nanostripe structures in tribological applications.
- 4 November 2010
- Published by IOP Publishing in Journal of Physics D: Applied Physics
- Vol. 43 (46)
Tribological properties of nanostripe surface structures—a design concept for improving tribological properties
The tribological properties of nanostripe surface structures were investigated using a pin-on-plate tribometer in order to propose a design concept for improving the tribological properties. The authors used four kinds of nanostripe structures consisting of different combinations of materials (Fe–Au, C–SiC, Al–Al2O3 and Al–Pt) fabricated by a process they had previously proposed. The frictional properties of the nanostripe structures depended on the materials that constituted the nanostripes. When the sliding direction in friction tests was parallel to the microgrooves, nanostripe structures remained on all surfaces even after friction tests. Based on the friction test results, the authors considered a design concept for nanostripe structures in tribological applications.