Marc Schaekers
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Marc Schaekers has a total of 606 co-authors. Here are the top co-authors by number of shared publications:
Sven Van Elshocht
IMEC, Kapeldreef 75, B-3001 Leuven, Belgium
15 shared publications- Hao Yu
IMEC
12 shared publications - Jorge Adrian Kittl
Imec, Kapeldreef 75, B3001 Leuven, Belgium
12 shared publications - Christoph Adelmann
IMEC
11 shared publications Christophe Detavernier
Department of Solid State Sciences, Ghent University, Conformal Coating of Nanostructures (CoCooN), Ghent, Belgium
9 shared publicationsK. De Meyer
IMEC, Kapeldreef 75, B-3001 Leuven, Belgium
9 shared publications
Latest Publications
- 1 December 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 22.4.1-22.4.4
Comprehensive study of Ga activation in Si, SiGe and Ge with 5 × 10−10Ω·cm2contact resistivity achieved on Ga doped Ge using nanosecond laser activation
Ga diffusion and activation in Si, SWGe 0.6 and Ge are studied comprehensively. Optimal Ga activation conditions for Si 0.4 Ge 0.6 and Ge feature a low thermal budget: Ga is highly activated at 400°C in Ge and at 500°C in SWGe 0.6 using a 1min rapid thermal annealing (RTA); the activation is further boosted using short-duration high-temperature nanosecond laser activation (NLA). A low Ti/p-Ge contact resistivity (pc) of 1.2×10 -9 Q-cm 2 is approached using Ga doping and 400°C RTA activation, while a record-low pc for p-Ge down to 5×10 -10 Qcm 2 is achieved using NLA for Ga activation.
- 1 December 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 22.4.1-22.4.4
Comprehensive study of Ga activation in Si, SiGe and Ge with 5 × 10−10Ω·cm2contact resistivity achieved on Ga doped Ge using nanosecond laser activation
Ga diffusion and activation in Si, SWGe 0.6 and Ge are studied comprehensively. Optimal Ga activation conditions for Si 0.4 Ge 0.6 and Ge feature a low thermal budget: Ga is highly activated at 400°C in Ge and at 500°C in SWGe 0.6 using a 1min rapid thermal annealing (RTA); the activation is further boosted using short-duration high-temperature nanosecond laser activation (NLA). A low Ti/p-Ge contact resistivity (pc) of 1.2×10 -9 Q-cm 2 is approached using Ga doping and 400°C RTA activation, while a record-low pc for p-Ge down to 5×10 -10 Qcm 2 is achieved using NLA for Ga activation.
- 9 November 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Electron Device Letters
- Vol. 39 (1) , 83-86
Thermal Stability of TiN/Ti/p+-Si0.3Ge0.7 Contact With Ultralow Contact Resistivity
In this letter, the contact properties and thermal stability of TiN/Ti/p + -Si 0.3 Ge 0.7 contacts are investigated. We demonstrate that the insertion of an ultra-thin Ti interlayer is necessary to reduce the contact resistivity (ρc) as compared with a standard TiN/p + -Si 0.3 Ge 0.7 direct contact. However, the Ti interlayer has to be thin enough to avoid degradation of the contact morphology after 500 °C annealing. This letter reveals further that the Ti encroachment into grooved SiGe regions under the contact interface is responsible for the ρ c increase seen after this annealing.
- 9 November 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Electron Device Letters
- Vol. 39 (1) , 83-86
Thermal Stability of TiN/Ti/p+-Si0.3Ge0.7 Contact With Ultralow Contact Resistivity
In this letter, the contact properties and thermal stability of TiN/Ti/p + -Si 0.3 Ge 0.7 contacts are investigated. We demonstrate that the insertion of an ultra-thin Ti interlayer is necessary to reduce the contact resistivity (ρc) as compared with a standard TiN/p + -Si 0.3 Ge 0.7 direct contact. However, the Ti interlayer has to be thin enough to avoid degradation of the contact morphology after 500 °C annealing. This letter reveals further that the Ti encroachment into grooved SiGe regions under the contact interface is responsible for the ρ c increase seen after this annealing.
- 2 May 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Electron Device Letters
- Vol. 38 (7) , 843-846
Lanthanum and Lanthanum Silicide Contacts on N-Type Silicon
In this letter, we investigate contacts of a low work function rare-earth metal, La, and its silicides on n-Si. LaSi x /n - -Si contacts show low Schottky barrier height (φ b ) of around 0.25-0.4 eV and promisingly low contact resistivity (ρ c ) on moderately doped n + -Si. However, on highly doped n ++ -Si, we find Pc of LaSi x near one order higher than the TiSi x control. This experiment indicates that low φ b does not guarantee low Pc on highly doped substrates. We further discuss reasons behind this phenomenon.
- 2 May 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Electron Device Letters
- Vol. 38 (7) , 843-846
Lanthanum and Lanthanum Silicide Contacts on N-Type Silicon
In this letter, we investigate contacts of a low work function rare-earth metal, La, and its silicides on n-Si. LaSi x /n - -Si contacts show low Schottky barrier height (φ b ) of around 0.25-0.4 eV and promisingly low contact resistivity (ρ c ) on moderately doped n + -Si. However, on highly doped n ++ -Si, we find Pc of LaSi x near one order higher than the TiSi x control. This experiment indicates that low φ b does not guarantee low Pc on highly doped substrates. We further discuss reasons behind this phenomenon.
- 1 May 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-3
Ultralow resistive wrap around contact to scaled FinFET devices by using ALD-Ti contact metal
We report on Atomic Layer Deposition Titanium (ALD Ti) for FinFET source/drain contact applications. On planar test structures, we accurately benchmark contact resistivity (ρc) of ALD Ti, ~1.4 × 10-9 Ω · cm 2 on Si:P and ~2.0 × 10-9 Ω·cm 2 on SiGe:B, among to lowest reported values in literature. Ultralow ρc is resulting from enhanced Ti/Si(Ge) reactivity originating in the ALD process. We also demonstrate capability of this process to significantly lower Rc on FinFETs by allowing a lateral contact into the S/D area effectively maximizing the contacting area.
- 1 May 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-3
Ultralow resistive wrap around contact to scaled FinFET devices by using ALD-Ti contact metal
We report on Atomic Layer Deposition Titanium (ALD Ti) for FinFET source/drain contact applications. On planar test structures, we accurately benchmark contact resistivity (ρc) of ALD Ti, ~1.4 × 10-9 Ω · cm 2 on Si:P and ~2.0 × 10-9 Ω·cm 2 on SiGe:B, among to lowest reported values in literature. Ultralow ρc is resulting from enhanced Ti/Si(Ge) reactivity originating in the ALD process. We also demonstrate capability of this process to significantly lower Rc on FinFETs by allowing a lateral contact into the S/D area effectively maximizing the contacting area.
- 5 January 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Electron Devices
- Vol. 64 (2) , 500-506
TiSi(Ge) Contacts Formed at Low Temperature Achieving Around $2 \,\, \times \,\, 10^{-{9}}~\Omega $ cm2 Contact Resistivities to p-SiGeThis paper reports ultralow contact resistivities (ρ c ) achieved on highly doped p-SiGe with two low-temperature contact formation methods. One method combines precontact amorphization implantation with ~500 °C rapid thermal processing (RTP)-based Ti germano-silicidation; ρ c achieved was ~2.9 × 10 -9 Ω·cm 2 . The other method combines codeposited TiSi-Ti:Si = 1:1-with ~450 °C RTP-based Ti silicidation; ρ c achieved was ~1.7 × 10 -9 Ω·cm 2 . When Pc reaches minimum, the TiSi(Ge) alloy is generally amorphous with embedded small crystallites, similar to the previous observations on pure Si substrates.
- 5 January 2017
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Electron Devices
- Vol. 64 (2) , 500-506
TiSi(Ge) Contacts Formed at Low Temperature Achieving Around $2 \,\, \times \,\, 10^{-{9}}~\Omega $ cm2 Contact Resistivities to p-SiGeThis paper reports ultralow contact resistivities (ρ c ) achieved on highly doped p-SiGe with two low-temperature contact formation methods. One method combines precontact amorphization implantation with ~500 °C rapid thermal processing (RTP)-based Ti germano-silicidation; ρ c achieved was ~2.9 × 10 -9 Ω·cm 2 . The other method combines codeposited TiSi-Ti:Si = 1:1-with ~450 °C RTP-based Ti silicidation; ρ c achieved was ~1.7 × 10 -9 Ω·cm 2 . When Pc reaches minimum, the TiSi(Ge) alloy is generally amorphous with embedded small crystallites, similar to the previous observations on pure Si substrates.
- 1 December 2016
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 25.1.1-25.1.4
Heterostructure at CMOS source/drain: Contributor or alleviator to the high access resistance problem?
This work investigates the interface resistivity of several heterostructures. Theoretical simulations suggest that, apart from the doping impact, the band offset and the difference in density of states (DOS) increase significantly the heterostructure interface resistivity. This conclusion corresponds well to our experiments that 1) high interface resistances are observed between (high-Ge content) p-SiGe/p-Si, n-InAs/n-Si, and n-InAs/n-Ge; and that 2) a TiSix/12nm Si:P/n-Ge contact with favorable band alignment between Si:P/n-Ge approaches low effective contact resistivity of 1.4×10-8 Ω cm2, close to a record-low value for n-Ge contacts.
- 1 December 2016
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 25.1.1-25.1.4
Heterostructure at CMOS source/drain: Contributor or alleviator to the high access resistance problem?
This work investigates the interface resistivity of several heterostructures. Theoretical simulations suggest that, apart from the doping impact, the band offset and the difference in density of states (DOS) increase significantly the heterostructure interface resistivity. This conclusion corresponds well to our experiments that 1) high interface resistances are observed between (high-Ge content) p-SiGe/p-Si, n-InAs/n-Si, and n-InAs/n-Ge; and that 2) a TiSix/12nm Si:P/n-Ge contact with favorable band alignment between Si:P/n-Ge approaches low effective contact resistivity of 1.4×10-8 Ω cm2, close to a record-low value for n-Ge contacts.
- 31 October 2016
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Electron Devices
- Vol. 63 (12) , 4632-4641
Titanium Silicide on Si:P With Precontact Amorphization Implantation Treatment: Contact Resistivity Approaching $1 \times 10^{-9}$ Ohm-cm2In recent CMOS technology, extreme shrinking of contact area at source/drain regions raises serious concerns of high metal/semiconductor contact resistance. Confronting this problem, we introduce a precontact amorphization implantation plus Ti silicidation technique (PCAI + TiSi x ) and achieve ultralow contact resistivity (ρ c ) of (1.3 - 1.5) × 10 -9 Ω · cm 2 on Si:P. This PCAI + TiSi x technique utilizes light amorphization (low-energy implantation), thin Ti and TiSi x film, and moderate thermal budget (500°C-550°C): these features are compatible with modern CMOS manufacturing. Moreover, the PCAI + TiSi x -induced ρ c reduction is proved universal on both n- and p-Si. With additional characterizations, we find that the silicidation-induced ρ c variation is not merely a Schottky barrier height tuning effect. The electrical and physical characterizations suggest that the low ρ c is strongly correlated with the formation of interfacial TiSi x crystallites between amorphous TiSi alloy and Si.
- 31 October 2016
- Published by Institute of Electrical and Electronics Engineers (IEEE) in IEEE Transactions on Electron Devices
- Vol. 63 (12) , 4632-4641
Titanium Silicide on Si:P With Precontact Amorphization Implantation Treatment: Contact Resistivity Approaching $1 \times 10^{-9}$ Ohm-cm2In recent CMOS technology, extreme shrinking of contact area at source/drain regions raises serious concerns of high metal/semiconductor contact resistance. Confronting this problem, we introduce a precontact amorphization implantation plus Ti silicidation technique (PCAI + TiSi x ) and achieve ultralow contact resistivity (ρ c ) of (1.3 - 1.5) × 10 -9 Ω · cm 2 on Si:P. This PCAI + TiSi x technique utilizes light amorphization (low-energy implantation), thin Ti and TiSi x film, and moderate thermal budget (500°C-550°C): these features are compatible with modern CMOS manufacturing. Moreover, the PCAI + TiSi x -induced ρ c reduction is proved universal on both n- and p-Si. With additional characterizations, we find that the silicidation-induced ρ c variation is not merely a Schottky barrier height tuning effect. The electrical and physical characterizations suggest that the low ρ c is strongly correlated with the formation of interfacial TiSi x crystallites between amorphous TiSi alloy and Si.
- 1 October 2016
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 525-527
Observation of contact resistivity independence from Schottky barrier height on heavily doped p-type SiGe
The electrical characteristics of Ti/p-SiGe contacts with Ti thicknesses of 3nm and 5nm have been investigated in this paper. TiN was used as a cap layer on Ti. It is observed that as Ti film becomes thinner, Ti/p-SiGe contact resistivity (ρc) increases, but its Schottky barrier height (SBH) decreases, which does not coincide with the regular ρc-SBH dependence. Using TiN/p-SiGe as a control sample, it is concluded that when Ti film is thinned down to nm scale, the contact property is strongly influenced by TiN cap layer.
- 1 October 2016
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 525-527
Observation of contact resistivity independence from Schottky barrier height on heavily doped p-type SiGe
The electrical characteristics of Ti/p-SiGe contacts with Ti thicknesses of 3nm and 5nm have been investigated in this paper. TiN was used as a cap layer on Ti. It is observed that as Ti film becomes thinner, Ti/p-SiGe contact resistivity (ρc) increases, but its Schottky barrier height (SBH) decreases, which does not coincide with the regular ρc-SBH dependence. Using TiN/p-SiGe as a control sample, it is concluded that when Ti film is thinned down to nm scale, the contact property is strongly influenced by TiN cap layer.
- 22 September 2016
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-2
Ultralow-resistivity CMOS contact scheme with pre-contact amorphization plus Ti (germano-)silicidation
Following the previous study on Si:P [1], we also achieve ultralow contact resistivities (ρc) of ~2×10-9 Ω·cm2 on Si0.3Ge0.7:B using the same Ti based pre-contact amorphization (PCAI) plus post-metal anneal (PMA) technique. Similar as on Si:P, low-energy PCAI provides the lowest ρc on SiGe:B. By increasing the B concentration, the PMA temperature required on SiGe:B also matches with that on Si:P. A simple Ti based CMOS contact flow is thus proposed. Several B doping and activation methods on SiGe:B are also compared in this work.
- 22 September 2016
- Published by Institute of Electrical and Electronics Engineers (IEEE)
- p. 1-2
Ultralow-resistivity CMOS contact scheme with pre-contact amorphization plus Ti (germano-)silicidation
Following the previous study on Si:P [1], we also achieve ultralow contact resistivities (ρc) of ~2×10-9 Ω·cm2 on Si0.3Ge0.7:B using the same Ti based pre-contact amorphization (PCAI) plus post-metal anneal (PMA) technique. Similar as on Si:P, low-energy PCAI provides the lowest ρc on SiGe:B. By increasing the B concentration, the PMA temperature required on SiGe:B also matches with that on Si:P. A simple Ti based CMOS contact flow is thus proposed. Several B doping and activation methods on SiGe:B are also compared in this work.