Christian Militzer
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Christian Militzer has a total of 23 co-authors. Here are the top co-authors by number of shared publications:
- Henrik Pedersen
Department of Physics, Chemistry and Biology, Linköping University , SE-581 83 Linköping
3 shared publications - Jing-Jia Huang
Department of Physics, Chemistry and Biology, Linköping University 1 , SE-58328 Linköping, Sweden
3 shared publications - Werner Andreas Goedel
Physical Chemistry, Chemnitz University of Technology, Strasse der Nationen 62, 09111 Chemnitz, Germany
3 shared publications - Charles Ajith Wijayawardhana
Department of Chemistry, University of Cincinnati, P.O. Box 210172, Cincinnati, OH 45221-0172, USA
2 shared publications Pauline Dill
Physical Chemistry, Institute of Chemistry, Chemnitz University of Technology 1 , Straße der Nationen 62, 09111 Chemnitz, Germany
2 shared publications- Urban Forsberg
Department of Physics, Chemistry and Biology, Linköping University, SE-581 83 Linköping, Sweden
2 shared publications
Latest Publications
- Open Access
- 27 April 2023
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 41 (3)
Superconformal silicon carbide coatings via precursor pulsed chemical vapor deposition
In this work, silicon carbide (SiC) coatings were successfully grown by pulsed chemical vapor deposition (CVD). The precursors silicon tetrachloride (SiCl4) and ethylene (C2H4) were not supplied in a continuous flow but were pulsed alternately into the growth chamber with H2 as a carrier and a purge gas. A typical pulsed CVD cycle was SiCl4 pulse—H2 purge—C2H4 pulse—H2 purge. This led to growth of superconformal SiC coatings, which could not be obtained under similar process conditions using a constant flow CVD process. We propose a two-step framework for SiC growth via pulsed CVD. During the SiCl4 pulse, a layer of Si is deposited. In the following C2H4 pulse, this Si layer is carburized, and SiC is formed. The high chlorine surface coverage after the SiCl4 pulse is believed to enable superconformal growth via a growth inhibition effect.
- 27 April 2023
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 41 (3)
Open AccessSuperconformal silicon carbide coatings via precursor pulsed chemical vapor deposition
In this work, silicon carbide (SiC) coatings were successfully grown by pulsed chemical vapor deposition (CVD). The precursors silicon tetrachloride (SiCl4) and ethylene (C2H4) were not supplied in a continuous flow but were pulsed alternately into the growth chamber with H2 as a carrier and a purge gas. A typical pulsed CVD cycle was SiCl4 pulse—H2 purge—C2H4 pulse—H2 purge. This led to growth of superconformal SiC coatings, which could not be obtained under similar process conditions using a constant flow CVD process. We propose a two-step framework for SiC growth via pulsed CVD. During the SiCl4 pulse, a layer of Si is deposited. In the following C2H4 pulse, this Si layer is carburized, and SiC is formed. The high chlorine surface coverage after the SiCl4 pulse is believed to enable superconformal growth via a growth inhibition effect.
- Open Access
- 9 August 2022
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 40 (5) , 053402
Conformal and superconformal chemical vapor deposition of silicon carbide coatings
The approaches to conformal and superconformal deposition developed by Abelson and Girolami for a low-temperature, low-pressure chemical vapor deposition (CVD) setting relevant for electronic materials in micrometer or submicrometer scale vias and trenches, are tested here in a high-temperature, moderate pressure CVD setting relevant for hard coatings in millimeter-scale trenches. Conformal and superconformal deposition of polycrystalline silicon carbide (SiC) can be accomplished at deposition temperatures between 950 and 1000 °C with precursor partial pressure higher than 20 Pa and an optional minor addition of HCl as a growth inhibitor. The conformal deposition at low temperatures is ascribed to slower kinetics of the precursor consumption along the trench depth, whereas the impact of high precursor partial pressure and addition of inhibitor is attributable to surface site blocking. With the slower kinetics and the site blocking from precursor saturation leading the growth to nearly conformal and the possibly preferential inhibition effect near the opening than at the depth, a superconformal SiC coating with 2.6 times higher thickness at the bottom compared to the top of a 1 mm trench was achieved.
- 9 August 2022
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 40 (5) , 053402
Open AccessConformal and superconformal chemical vapor deposition of silicon carbide coatings
The approaches to conformal and superconformal deposition developed by Abelson and Girolami for a low-temperature, low-pressure chemical vapor deposition (CVD) setting relevant for electronic materials in micrometer or submicrometer scale vias and trenches, are tested here in a high-temperature, moderate pressure CVD setting relevant for hard coatings in millimeter-scale trenches. Conformal and superconformal deposition of polycrystalline silicon carbide (SiC) can be accomplished at deposition temperatures between 950 and 1000 °C with precursor partial pressure higher than 20 Pa and an optional minor addition of HCl as a growth inhibitor. The conformal deposition at low temperatures is ascribed to slower kinetics of the precursor consumption along the trench depth, whereas the impact of high precursor partial pressure and addition of inhibitor is attributable to surface site blocking. With the slower kinetics and the site blocking from precursor saturation leading the growth to nearly conformal and the possibly preferential inhibition effect near the opening than at the depth, a superconformal SiC coating with 2.6 times higher thickness at the bottom compared to the top of a 1 mm trench was achieved.
- Open Access
- 4 June 2022
- Published by American Chemical Society (ACS) in The Journal of Physical Chemistry C
- Vol. 126 (23) , 9918-9925
Controlled CVD Growth of Highly ⟨111⟩-Oriented 3C-SiC
- 4 June 2022
- Published by American Chemical Society (ACS) in The Journal of Physical Chemistry C
- Vol. 126 (23) , 9918-9925
Open AccessControlled CVD Growth of Highly ⟨111⟩-Oriented 3C-SiC
- 12 August 2021
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 39 (5) , 052406
Atomic layer deposition onto fabrics of carbon and silicon carbide fibers: Preparation of multilayers comprising alumina, titania-furfuryl alcohol hybrid, and titanium phosphate
High temperature-resistant fabrics can be used as a reinforcement structure in ceramic matrix composites. They often need a coating for oxidation protection and mechanical decoupling from the matrix. Atomic layer deposition (ALD) provides very thin conformal coatings even deep down into complex or porous structures and thus might be a suitable technique for this purpose. Carbon fiber fabrics (size 300 mm × 80 mm) and SiC fiber fabrics (size 400 mm × 80 mm) were coated using ALD with a multilayer system: a first layer made of 320 cycles of alumina (Al2O3) deposition, a second layer made of 142 cycles of titania-furfuryl alcohol hybrid (TiO2-FFA), and a third layer made of 360 cycles of titanium phosphate (TixPOy). Scanning electron microscopy reveals that the coatings are uniform and that the thickness of each layer is almost independent of the place in the reactor while coating. Appearance and thickness do not show any dependence on the type of fiber used as a substrate. Energy dispersive x-ray spectroscopy confirmed the expected elemental composition of each layer. Thermogravimetric analysis under oxidizing environment revealed that the first layer increases the onset temperature of fiber oxidation significantly, while the following two layers improve the oxidative protection only to a much smaller degree. Varying the geometry and size of the sample holder and especially the stacking of several fabric specimens on top of each other allowed increasing the total area of coated fabric up to 560 cm2 per batch. It was demonstrated that four-layered fiber coatings could be obtained with high uniformity even on these much more complicated geometries.
- 12 August 2021
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 39 (5) , 052406
Atomic layer deposition onto fabrics of carbon and silicon carbide fibers: Preparation of multilayers comprising alumina, titania-furfuryl alcohol hybrid, and titanium phosphate
High temperature-resistant fabrics can be used as a reinforcement structure in ceramic matrix composites. They often need a coating for oxidation protection and mechanical decoupling from the matrix. Atomic layer deposition (ALD) provides very thin conformal coatings even deep down into complex or porous structures and thus might be a suitable technique for this purpose. Carbon fiber fabrics (size 300 mm × 80 mm) and SiC fiber fabrics (size 400 mm × 80 mm) were coated using ALD with a multilayer system: a first layer made of 320 cycles of alumina (Al2O3) deposition, a second layer made of 142 cycles of titania-furfuryl alcohol hybrid (TiO2-FFA), and a third layer made of 360 cycles of titanium phosphate (TixPOy). Scanning electron microscopy reveals that the coatings are uniform and that the thickness of each layer is almost independent of the place in the reactor while coating. Appearance and thickness do not show any dependence on the type of fiber used as a substrate. Energy dispersive x-ray spectroscopy confirmed the expected elemental composition of each layer. Thermogravimetric analysis under oxidizing environment revealed that the first layer increases the onset temperature of fiber oxidation significantly, while the following two layers improve the oxidative protection only to a much smaller degree. Varying the geometry and size of the sample holder and especially the stacking of several fabric specimens on top of each other allowed increasing the total area of coated fabric up to 560 cm2 per batch. It was demonstrated that four-layered fiber coatings could be obtained with high uniformity even on these much more complicated geometries.
- 21 May 2018
- Published by Wiley in Advanced Materials Interfaces
- Vol. 5 (16)
Atomic Layer Deposition of Titanium Phosphate from Titanium Tetrachloride and Triethyl Phosphate onto Carbon Fibers
A thermal atomic layer deposition (ALD) process for depositing titanium phosphate onto bundles of carbon fibers as well as flat silicon and germanium substrates using titanium tetrachloride and triethyl phosphate as precursors is presented. This process yields conformal coatings on all substrates used while having a growth per cycle of 0.22 nm cycle−1, which is relatively high compared to other metal phosphate ALD processes. The reactions of the precursors with the surface are shown to be self‐limiting at 200 °C. Compositional analysis of the coating is performed using energy‐dispersive X‐ray spectroscopy, X‐ray photoelectron spectroscopy, and Fourier‐transform infrared spectroscopy. It is shown that the as‐deposited coating has a chemical composition of Ti3.0PO8.2 and a residual carbon content of 7%. Upon thermal annealing in air, residual triethyl phosphate and water is lost from the coating and phosphate can be identified up to 1000 °C. At temperatures exceeding 1000 °C, the coating starts to decompose. Thermogravimetric analysis of coated carbon fibers shows that the coating increases the onset temperature of the carbon fiber oxidation, thus providing an oxidation protection to the fibers.
- 21 May 2018
- Published by Wiley in Advanced Materials Interfaces
- Vol. 5 (16)
Atomic Layer Deposition of Titanium Phosphate from Titanium Tetrachloride and Triethyl Phosphate onto Carbon Fibers
A thermal atomic layer deposition (ALD) process for depositing titanium phosphate onto bundles of carbon fibers as well as flat silicon and germanium substrates using titanium tetrachloride and triethyl phosphate as precursors is presented. This process yields conformal coatings on all substrates used while having a growth per cycle of 0.22 nm cycle−1, which is relatively high compared to other metal phosphate ALD processes. The reactions of the precursors with the surface are shown to be self‐limiting at 200 °C. Compositional analysis of the coating is performed using energy‐dispersive X‐ray spectroscopy, X‐ray photoelectron spectroscopy, and Fourier‐transform infrared spectroscopy. It is shown that the as‐deposited coating has a chemical composition of Ti3.0PO8.2 and a residual carbon content of 7%. Upon thermal annealing in air, residual triethyl phosphate and water is lost from the coating and phosphate can be identified up to 1000 °C. At temperatures exceeding 1000 °C, the coating starts to decompose. Thermogravimetric analysis of coated carbon fibers shows that the coating increases the onset temperature of the carbon fiber oxidation, thus providing an oxidation protection to the fibers.
- 3 August 2017
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 100 (12) , 5409-5420
Atomic layer deposition onto carbon fiber fabrics
Carbon fiber fabrics, consisting of interwoven bundles of 3000 single fibers, were coated with Al2O3 using the atomic layer deposition (ALD) process, exposing the fabrics to alternating pulses of trimethyl aluminium and water vapors. The thickness and uniformity of the coatings were investigated using scanning electron microscopy (SEM) and thermogravimetric analysis (TGA). The obtained coatings were conformal, 84 ALD cycles gave rise to approximately 20‐nm‐thick coatings and 168 ALD cycles to approximately 40‐nm‐thick coatings. It was found, that a uniform coating can be obtained at a purge time of 40 seconds. Reducing purge times below 20 seconds gives rise to increased particle growth and thus the coating becomes inhomogeneous. Initially, the samples that were coated had a size of 2×10 cm (thickness 0.3 mm). The size of the fabric was subsequently increased up to 8×20 cm and a uniform coating of the same quality was obtained. By oxidizing the coated fabrics, fabrics composed of interwoven alumina microtubes were obtained. Infiltration of the microtubes with solutions of two distinguishable fluorescent dyes showed that interchange of the dyes between warp and weft microtubes occurs, but is absent at approximately 20% of the crossovers. Taking all our findings into account, we conclude that the majority of the fibers were separated from each other by the coating prior to the oxidation. This work demonstrates that ALD is a suitable method to produce thin, conformal coatings on the surface of carbon fiber fabrics.
- 3 August 2017
- Published by Wiley in Journal of the American Ceramic Society
- Vol. 100 (12) , 5409-5420
Atomic layer deposition onto carbon fiber fabrics
Carbon fiber fabrics, consisting of interwoven bundles of 3000 single fibers, were coated with Al2O3 using the atomic layer deposition (ALD) process, exposing the fabrics to alternating pulses of trimethyl aluminium and water vapors. The thickness and uniformity of the coatings were investigated using scanning electron microscopy (SEM) and thermogravimetric analysis (TGA). The obtained coatings were conformal, 84 ALD cycles gave rise to approximately 20‐nm‐thick coatings and 168 ALD cycles to approximately 40‐nm‐thick coatings. It was found, that a uniform coating can be obtained at a purge time of 40 seconds. Reducing purge times below 20 seconds gives rise to increased particle growth and thus the coating becomes inhomogeneous. Initially, the samples that were coated had a size of 2×10 cm (thickness 0.3 mm). The size of the fabric was subsequently increased up to 8×20 cm and a uniform coating of the same quality was obtained. By oxidizing the coated fabrics, fabrics composed of interwoven alumina microtubes were obtained. Infiltration of the microtubes with solutions of two distinguishable fluorescent dyes showed that interchange of the dyes between warp and weft microtubes occurs, but is absent at approximately 20% of the crossovers. Taking all our findings into account, we conclude that the majority of the fibers were separated from each other by the coating prior to the oxidation. This work demonstrates that ALD is a suitable method to produce thin, conformal coatings on the surface of carbon fiber fabrics.
- 9 November 2016
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 35 (1)
Deposition of an organic–inorganic hybrid material onto carbon fibers via the introduction of furfuryl alcohol into the atomic layer deposition process of titania and subsequent pyrolysis
Exposing bundles of carbon and quartz fibers as well as silicon wafers to sequential pulses of gaseous TiCl4/furfuryl alcohol (FFA) and H2O/TiCl4/furfuryl alcohol, respectively gave rise to conformal organic/inorganic coatings on all of these substrates. The deposition during the FFA pulse is self-limiting and the process shows a linear growth per cycle of (0.65 ± 0.05) nm/cycle in the absence of water pulses and (1.68 ± 0.04) nm/cycle in the presence of water pulses. A possible reaction mechanism comprises classic atomic layer deposition steps as well as a polymerization route of furfuryl alcohol, which leads to the release of water during the furfuryl alcohol pulse and further comprises hydrolytic ring opening of furan rings and/or hydrolytic cleavage of Ti–Cl bonds. Since an additional subsequent water pulse significantly enhances the growth, it seems that without additional water pulse these reactions are limited by the amount of water that is formed or desorbed. Oxidizing the coated carbon fibers at 700 °C gave rise to thin-walled titania microtubes with wrinkled tube walls. Titania/carbon-hybrid microtubes were obtained by coating quartz fibers with TiO2/FFA, pyrolysis at 600 °C under nitrogen atmosphere, and subsequent etching with hydrogen fluoride. Energy dispersive x-ray spectroscopy and x-ray photoelectron spectroscopy (of coated silicon wafers) confirm that the coating consists predominantly of titanium, oxygen, carbon, and comprises residual chlorine. The stoichiometry is TiO2C3.5Cl0.1 before and TiO1.8C1.4 after the pyrolysis. According to XPS and thermogravimetric analysis, the molar ratio of titania to furfuryl alcohol is approximately 1.
- 9 November 2016
- Published by American Vacuum Society in Journal of Vacuum Science & Technology A
- Vol. 35 (1)
Deposition of an organic–inorganic hybrid material onto carbon fibers via the introduction of furfuryl alcohol into the atomic layer deposition process of titania and subsequent pyrolysis
Exposing bundles of carbon and quartz fibers as well as silicon wafers to sequential pulses of gaseous TiCl4/furfuryl alcohol (FFA) and H2O/TiCl4/furfuryl alcohol, respectively gave rise to conformal organic/inorganic coatings on all of these substrates. The deposition during the FFA pulse is self-limiting and the process shows a linear growth per cycle of (0.65 ± 0.05) nm/cycle in the absence of water pulses and (1.68 ± 0.04) nm/cycle in the presence of water pulses. A possible reaction mechanism comprises classic atomic layer deposition steps as well as a polymerization route of furfuryl alcohol, which leads to the release of water during the furfuryl alcohol pulse and further comprises hydrolytic ring opening of furan rings and/or hydrolytic cleavage of Ti–Cl bonds. Since an additional subsequent water pulse significantly enhances the growth, it seems that without additional water pulse these reactions are limited by the amount of water that is formed or desorbed. Oxidizing the coated carbon fibers at 700 °C gave rise to thin-walled titania microtubes with wrinkled tube walls. Titania/carbon-hybrid microtubes were obtained by coating quartz fibers with TiO2/FFA, pyrolysis at 600 °C under nitrogen atmosphere, and subsequent etching with hydrogen fluoride. Energy dispersive x-ray spectroscopy and x-ray photoelectron spectroscopy (of coated silicon wafers) confirm that the coating consists predominantly of titanium, oxygen, carbon, and comprises residual chlorine. The stoichiometry is TiO2C3.5Cl0.1 before and TiO1.8C1.4 after the pyrolysis. According to XPS and thermogravimetric analysis, the molar ratio of titania to furfuryl alcohol is approximately 1.