Gábor Gyarmati
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Gábor Gyarmati has a total of 32 co-authors. Here are the top co-authors by number of shared publications:
- Tamás Mende
Institute of Physical Metallurgy, Metal Forming and Nanotechnology, Faculty of Materials and Chemical Engineering, University of Miskolc, 3515 Miskolc, Hungary
6 shared publications György Fegyverneki
Foundry Institute, University of Miskolc, 3515, Miskolc-Egyetemváros, Hungary
5 shared publicationsTamás Mende
Institute of Physical Metallurgy, Metalforming and Nanotechnology, University of Miskolc, Miskolc-Egyetemvaros, Hungary
4 shared publications- György Fegyverneki
Foundry Institute, University of Miskolc, Miskolc-Egyetemváros, Hungary
3 shared publications - Monika Tokár
Foundry Institute, University of Miskolc, 3515 Miskolc-Egyetemváros, Hungary
3 shared publications - László Varga
Tridial Ltd, Budapest Technical University, Budapest, Hungary
2 shared publications
Latest Publications
- Open Access
An Evaluation of the Capability of the Reduced Pressure Test to Assess Liquid Metal Damage in Aluminum Alloy Castings
A systematic study was conducted to determine correlations between reduced pressure testing metrics and tensile results in aluminum alloy castings. The metrics investigated are the density and bifilm indices that have been traditionally used in industry, as well as three other metrics obtained from computed tomography scans. Analysis has shown that reduced pressure testing does not yield reliable results on the quality of aluminum alloy castings. Both density and bifilm indices provide high levels of α- and β-errors, well above those in traditional acceptance sampling plans. There is wide scatter in tensile results at the levels of both indices that are considered to represent “good” melts. The results of the CT scan metrics are similar. Possible reasons for these results and their implications are discussed.
Open AccessAn Evaluation of the Capability of the Reduced Pressure Test to Assess Liquid Metal Damage in Aluminum Alloy Castings
A systematic study was conducted to determine correlations between reduced pressure testing metrics and tensile results in aluminum alloy castings. The metrics investigated are the density and bifilm indices that have been traditionally used in industry, as well as three other metrics obtained from computed tomography scans. Analysis has shown that reduced pressure testing does not yield reliable results on the quality of aluminum alloy castings. Both density and bifilm indices provide high levels of α- and β-errors, well above those in traditional acceptance sampling plans. There is wide scatter in tensile results at the levels of both indices that are considered to represent “good” melts. The results of the CT scan metrics are similar. Possible reasons for these results and their implications are discussed.
- Open Access
- 22 May 2026
- Published by Springer Nature in International Journal of Metalcasting
- p. 1-17
Understanding the Interactions of Grain Refiner Particles and Double Oxide Films in Liquid Aluminum Alloys
Recent studies revealed that the addition of different grain refiner master alloys can affect the sedimentation and thus the spatial distribution of double oxide films in the melt. In this work, the interactions of TiB 2 and (Al,Si) 3 Ti particles with bifilm defects were investigated in the case of a liquid Al-Si-Mg-Cu alloy. The interactions between refiner particles and bifilms were studied by optical and scanning electron microscopy (SEM), while the changes in melt quality were analyzed by the computed tomographic (CT) analysis of reduced pressure test (RPT) specimens. The sedimentation behavior of grain refiner particles was investigated through computational fluid dynamics (CFD) simulations. It was found that TiB 2 particles tend to adhere to double oxide films suspended in the liquid metal, while (Al,Si) 3 Ti particles became attached to bifilms due to the heterogeneous nucleation of (Al,Si) 3 Ti on bifilms and the partial engulfment of oxide film segments during the growth of (Al,Si) 3 Ti particles. The attachment of grain refiner particles to double oxide films leads to the aided sedimentation of bifilms, which results in lowered porosity in RPT specimens. CFD simulations revealed that the experimentally observed fast sedimentation of TiB 2 can only be expected when relatively large particle agglomerates are created.
- 22 May 2026
- Published by Springer Nature in International Journal of Metalcasting
- p. 1-17
Open AccessUnderstanding the Interactions of Grain Refiner Particles and Double Oxide Films in Liquid Aluminum Alloys
Recent studies revealed that the addition of different grain refiner master alloys can affect the sedimentation and thus the spatial distribution of double oxide films in the melt. In this work, the interactions of TiB 2 and (Al,Si) 3 Ti particles with bifilm defects were investigated in the case of a liquid Al-Si-Mg-Cu alloy. The interactions between refiner particles and bifilms were studied by optical and scanning electron microscopy (SEM), while the changes in melt quality were analyzed by the computed tomographic (CT) analysis of reduced pressure test (RPT) specimens. The sedimentation behavior of grain refiner particles was investigated through computational fluid dynamics (CFD) simulations. It was found that TiB 2 particles tend to adhere to double oxide films suspended in the liquid metal, while (Al,Si) 3 Ti particles became attached to bifilms due to the heterogeneous nucleation of (Al,Si) 3 Ti on bifilms and the partial engulfment of oxide film segments during the growth of (Al,Si) 3 Ti particles. The attachment of grain refiner particles to double oxide films leads to the aided sedimentation of bifilms, which results in lowered porosity in RPT specimens. CFD simulations revealed that the experimentally observed fast sedimentation of TiB 2 can only be expected when relatively large particle agglomerates are created.
- Open Access
- 8 May 2026
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 57 (7) , 3826-3839
Characterization of the Melt Quality for an Al–5Mg–2Fe Alloy With and Without the Addition of a Custom-Designed Flux
In this work, the effect of a custom-made, Na- and Ca-free flux on the melt quality of an Al–5Mg–2Fe alloy was studied. The composition of the flux mixture was designed based on thermodynamic calculations as well as previous studies. Melt quality was assessed by using (i) reduced pressure tests with density measurements and Bifilm Index analysis, (ii) microscopic investigation of K-mold samples, and (iii) tensile testing. Defects on fracture surfaces and the microstructure of tensile specimens were investigated by optical and scanning electron microscopy (SEM). Tensile data were analyzed via Weibull statistics. Results indicated that flux addition improved melt quality indices and tensile data only slightly, mainly due to the disappearance of old, coarse oxide films from the fracture surfaces of K-mold and tensile specimens. However, further improvements are needed for a more complete elimination of defects to increase the reliability of mechanical properties. This study provides insight into how fluxing treatments can alleviate the contribution of entrainment defects to the degradation of the mechanical properties of Al–Mg–Fe alloys.
- 8 May 2026
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 57 (7) , 3826-3839
Open AccessCharacterization of the Melt Quality for an Al–5Mg–2Fe Alloy With and Without the Addition of a Custom-Designed Flux
In this work, the effect of a custom-made, Na- and Ca-free flux on the melt quality of an Al–5Mg–2Fe alloy was studied. The composition of the flux mixture was designed based on thermodynamic calculations as well as previous studies. Melt quality was assessed by using (i) reduced pressure tests with density measurements and Bifilm Index analysis, (ii) microscopic investigation of K-mold samples, and (iii) tensile testing. Defects on fracture surfaces and the microstructure of tensile specimens were investigated by optical and scanning electron microscopy (SEM). Tensile data were analyzed via Weibull statistics. Results indicated that flux addition improved melt quality indices and tensile data only slightly, mainly due to the disappearance of old, coarse oxide films from the fracture surfaces of K-mold and tensile specimens. However, further improvements are needed for a more complete elimination of defects to increase the reliability of mechanical properties. This study provides insight into how fluxing treatments can alleviate the contribution of entrainment defects to the degradation of the mechanical properties of Al–Mg–Fe alloys.
- Open Access
Intermetallic Phase Control in Cast Aluminum Alloys by Utilizing Heterogeneous Nucleation on Oxides
With the increasing demand for premium-quality aluminum alloy castings that can be used as safety-critical structural components, as well as the rising urge to utilize sustainable materials during the manufacturing process, novel technologies need to be developed and implemented during the treatment of liquid alloys. Impurity and alloying elements accumulate in recycled aluminum alloys, which frequently results in the formation of coarse intermetallic compound (IMC) particles in the microstructure that have a detrimental effect on the ductility of cast products. One successful approach to alleviate this negative effect relies on affecting the phase selection and refinement of IMC phases. A growing body of literature has shown that the crystallization process of IMCs is affected by the native oxide phases present in the liquid alloys. It has also been demonstrated that by appropriate technologies, harmful oxide inclusion (like oxide bifilms) can be transformed into small-sized oxide particles that can be dispersed throughout the liquid alloy to serve as heterogeneous nucleation sites for different phases. In this way, the adverse effects of oxide inclusions and IMCs are simultaneously mitigated. This contribution aims to review the recent progress of experimental and theoretical work related to intermetallic particle refinement by oxide phases. Emerging technological solutions capable of refining intermetallics through transforming harmful oxide inclusions into numerous, well-dispersed heterogeneous nucleation sites are comprehensively reviewed. Besides analyzing the current state of these techniques, this discussion evaluates their future implications and the potential challenges that may arise in their application and development.
Open AccessIntermetallic Phase Control in Cast Aluminum Alloys by Utilizing Heterogeneous Nucleation on Oxides
With the increasing demand for premium-quality aluminum alloy castings that can be used as safety-critical structural components, as well as the rising urge to utilize sustainable materials during the manufacturing process, novel technologies need to be developed and implemented during the treatment of liquid alloys. Impurity and alloying elements accumulate in recycled aluminum alloys, which frequently results in the formation of coarse intermetallic compound (IMC) particles in the microstructure that have a detrimental effect on the ductility of cast products. One successful approach to alleviate this negative effect relies on affecting the phase selection and refinement of IMC phases. A growing body of literature has shown that the crystallization process of IMCs is affected by the native oxide phases present in the liquid alloys. It has also been demonstrated that by appropriate technologies, harmful oxide inclusion (like oxide bifilms) can be transformed into small-sized oxide particles that can be dispersed throughout the liquid alloy to serve as heterogeneous nucleation sites for different phases. In this way, the adverse effects of oxide inclusions and IMCs are simultaneously mitigated. This contribution aims to review the recent progress of experimental and theoretical work related to intermetallic particle refinement by oxide phases. Emerging technological solutions capable of refining intermetallics through transforming harmful oxide inclusions into numerous, well-dispersed heterogeneous nucleation sites are comprehensively reviewed. Besides analyzing the current state of these techniques, this discussion evaluates their future implications and the potential challenges that may arise in their application and development.
- Open Access
- 4 December 2024
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 56 (1) , 782-797
Analysis of Different Commercial Solid Fluxes Used During the Rotary Degassing Melt Treatment of Casting Aluminum Alloys
This work aimed to get a better understanding of the behavior and melt cleaning efficiency of different commercial solid fluxes used in the foundry industry for the treatment of liquid aluminum alloys. This was realized by combining industrial melt treatment experiments with the application of characterization techniques that can provide information about the phase composition and thermal stability of different fluxes. Rotary degassing treatments coupled with flux addition using 5 different commercial fluxes were conducted on batches of EN AC-46000 alloy (AlSi9Cu3(Fe)) melt. The melt quality was assessed by the Qualiflash technique and Bifilm-Index (BI) analysis of reduced pressure test (RPT) samples. The phase composition and thermal behavior of the fluxes were investigated by X-ray diffraction (XRD) and differential thermal analysis (DTA), respectively. Among the 5 fluxes, two had a rather similar phase composition with the main constituents being NaCl, KCl, CaF2, MgF2, Na2CO3·NaHCO·3H2O, Na2SO4, and K2SiF6. These two fluxes, which contain a relatively high amount of fluoride components (about 11mol pct), and had a melting temperature below 600 °C, proved to be the most efficient in improving the melt quality. The Quality Temperature Index (QTI) values and normalized Bifilm-Index (NBI) results of the RPT samples generally showed a similar tendency, but there was only a loose relationship between the two parameters. Discrepancies between the results of different melt quality evaluation techniques can be traced back to their sensitivity to melt quality changes.
- 4 December 2024
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 56 (1) , 782-797
Open AccessAnalysis of Different Commercial Solid Fluxes Used During the Rotary Degassing Melt Treatment of Casting Aluminum Alloys
This work aimed to get a better understanding of the behavior and melt cleaning efficiency of different commercial solid fluxes used in the foundry industry for the treatment of liquid aluminum alloys. This was realized by combining industrial melt treatment experiments with the application of characterization techniques that can provide information about the phase composition and thermal stability of different fluxes. Rotary degassing treatments coupled with flux addition using 5 different commercial fluxes were conducted on batches of EN AC-46000 alloy (AlSi9Cu3(Fe)) melt. The melt quality was assessed by the Qualiflash technique and Bifilm-Index (BI) analysis of reduced pressure test (RPT) samples. The phase composition and thermal behavior of the fluxes were investigated by X-ray diffraction (XRD) and differential thermal analysis (DTA), respectively. Among the 5 fluxes, two had a rather similar phase composition with the main constituents being NaCl, KCl, CaF2, MgF2, Na2CO3·NaHCO·3H2O, Na2SO4, and K2SiF6. These two fluxes, which contain a relatively high amount of fluoride components (about 11mol pct), and had a melting temperature below 600 °C, proved to be the most efficient in improving the melt quality. The Quality Temperature Index (QTI) values and normalized Bifilm-Index (NBI) results of the RPT samples generally showed a similar tendency, but there was only a loose relationship between the two parameters. Discrepancies between the results of different melt quality evaluation techniques can be traced back to their sensitivity to melt quality changes.
- Open Access
- 11 September 2023
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 18 (2) , 1723-1738
Analysis of the Quality of Incoming AlSi9Mn Alloy Ingots
Previous research revealed that the quality of the ingots produced by different primary or secondary alloy suppliers can differ remarkably. In this way, the quality of the liquid metal and the castings produced from it can be affected by the impurity content of the ingots used as charge material. In this work, a modified reduced pressure test (RPT) technique, which is based on the remelting of samples extracted from ingots, was applied to investigate the quality of primary AlSi9Mn ingots made by horizontal direct-chill (HDC) casting and gravity casting techniques. For the evaluation of metal quality, image analysis of the cross sections was applied. Pore area fraction, number density, normalized bifilm index, and normalized total pore perimeter were determined, and the relationships between the different metrics were analyzed. The results were compared with the melt quality assessment of the as-melted batches made from the ingots. Solidification simulations, thermal analysis, and microstructural investigations were conducted to investigate the solidification conditions of traditional and remelted RPT samples. Based on the results, the HDC cast ingots possess lower oxide and gas concentrations, which can be traced back to the differences in the melt preparation and casting technologies of the ingots. The comparison of the parameters evaluated by image analysis revealed that there is a strong linear relationship between normalized bifilm index and normalized total pore perimeter. The possible sources of error in ingot quality evaluation are highlighted.
- 11 September 2023
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 18 (2) , 1723-1738
Open AccessAnalysis of the Quality of Incoming AlSi9Mn Alloy Ingots
Previous research revealed that the quality of the ingots produced by different primary or secondary alloy suppliers can differ remarkably. In this way, the quality of the liquid metal and the castings produced from it can be affected by the impurity content of the ingots used as charge material. In this work, a modified reduced pressure test (RPT) technique, which is based on the remelting of samples extracted from ingots, was applied to investigate the quality of primary AlSi9Mn ingots made by horizontal direct-chill (HDC) casting and gravity casting techniques. For the evaluation of metal quality, image analysis of the cross sections was applied. Pore area fraction, number density, normalized bifilm index, and normalized total pore perimeter were determined, and the relationships between the different metrics were analyzed. The results were compared with the melt quality assessment of the as-melted batches made from the ingots. Solidification simulations, thermal analysis, and microstructural investigations were conducted to investigate the solidification conditions of traditional and remelted RPT samples. Based on the results, the HDC cast ingots possess lower oxide and gas concentrations, which can be traced back to the differences in the melt preparation and casting technologies of the ingots. The comparison of the parameters evaluated by image analysis revealed that there is a strong linear relationship between normalized bifilm index and normalized total pore perimeter. The possible sources of error in ingot quality evaluation are highlighted.
- Open Access
Grain Refiner Settling and Its Effect on the Melt Quality of Aluminum Casting Alloys
Grain refiner particles, which are intended to induce the formation of fine equiaxed grain structure during the solidification of aluminum alloys, are prone to settling during the holding of the liquid metal, which phenomenon can affect not only the grain size but the spatial distribution of the double oxide films in the melt. In this study, the settling of Al3Ti inoculant particles, as well as its effects on melt quality and grain refinement, were studied. During the experiments, the Ti-concentration of a liquid Al-Si-Mg-Cu alloy was increased to 0.3 wt.% by the addition of Al-10%Ti master alloy at different melt temperatures. Particle settling and grain size evolution were studied by quantitative metallography, while the interactions of grain refiners and bifilms were investigated by scanning electron microscopy (SEM). The evolution of melt quality was assessed by the computed tomographic (CT) analysis of reduced pressure test (RPT) samples. It was found that effective grain refinement was only realized when the introduced blocky Al3Ti particles were dissolved and re-precipitated in the form of (Al,Si)3Ti at a lower temperature. Without dissolving at higher holding temperatures, Al3Ti particle settling has taken place within 10 min. The settling of (Al,Si)3Ti particles improved melt quality by the aided sedimentation of bifilms in the melt.
Open AccessGrain Refiner Settling and Its Effect on the Melt Quality of Aluminum Casting Alloys
Grain refiner particles, which are intended to induce the formation of fine equiaxed grain structure during the solidification of aluminum alloys, are prone to settling during the holding of the liquid metal, which phenomenon can affect not only the grain size but the spatial distribution of the double oxide films in the melt. In this study, the settling of Al3Ti inoculant particles, as well as its effects on melt quality and grain refinement, were studied. During the experiments, the Ti-concentration of a liquid Al-Si-Mg-Cu alloy was increased to 0.3 wt.% by the addition of Al-10%Ti master alloy at different melt temperatures. Particle settling and grain size evolution were studied by quantitative metallography, while the interactions of grain refiners and bifilms were investigated by scanning electron microscopy (SEM). The evolution of melt quality was assessed by the computed tomographic (CT) analysis of reduced pressure test (RPT) samples. It was found that effective grain refinement was only realized when the introduced blocky Al3Ti particles were dissolved and re-precipitated in the form of (Al,Si)3Ti at a lower temperature. Without dissolving at higher holding temperatures, Al3Ti particle settling has taken place within 10 min. The settling of (Al,Si)3Ti particles improved melt quality by the aided sedimentation of bifilms in the melt.
- Open Access
- 17 January 2022
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 53 (2) , 1244-1257
The Effect of Rotary Degassing Treatments with Different Purging Gases on the Double Oxide- and Nitride Film Content of Liquid Aluminum Alloys
Rotary degassing is one of the most frequently used melt treatment technologies used for processing liquid aluminum alloys. Despite this, the information available about the possible effects of this method on the double oxide- and nitride film (bifilm) content, especially when using different purging gases, is quite limited. For this reason, in this study, the effects of multiple rotary degassing treatments conducted with N2 and Ar purging gases on the bifilm quantity of a casting aluminum alloy were compared. The characterization of the melt quality was realized by the computed tomographic (CT) analysis of reduced pressure test (RPT) specimens, image analysis, and scanning electron microscopy (SEM) of the fracture surfaces of K-mold samples. Based on the results, by the application of Ar as a purging gas, relatively low bifilm content can be achieved. On the other hand, while the use of N2 leads to the formation of numerous small-sized nitride bifilms, which significantly increased the pore number density inside the RPT specimens. This can be associated with the nitride formation by the chemical reaction between the liquid aluminum alloy and the N2 purging gas bubbles during the degassing treatments. Graphical abstract
- 17 January 2022
- Published by Springer Nature in Metallurgical and Materials Transactions B
- Vol. 53 (2) , 1244-1257
Open AccessThe Effect of Rotary Degassing Treatments with Different Purging Gases on the Double Oxide- and Nitride Film Content of Liquid Aluminum Alloys
Rotary degassing is one of the most frequently used melt treatment technologies used for processing liquid aluminum alloys. Despite this, the information available about the possible effects of this method on the double oxide- and nitride film (bifilm) content, especially when using different purging gases, is quite limited. For this reason, in this study, the effects of multiple rotary degassing treatments conducted with N2 and Ar purging gases on the bifilm quantity of a casting aluminum alloy were compared. The characterization of the melt quality was realized by the computed tomographic (CT) analysis of reduced pressure test (RPT) specimens, image analysis, and scanning electron microscopy (SEM) of the fracture surfaces of K-mold samples. Based on the results, by the application of Ar as a purging gas, relatively low bifilm content can be achieved. On the other hand, while the use of N2 leads to the formation of numerous small-sized nitride bifilms, which significantly increased the pore number density inside the RPT specimens. This can be associated with the nitride formation by the chemical reaction between the liquid aluminum alloy and the N2 purging gas bubbles during the degassing treatments. Graphical abstract
- Open Access
- 1 November 2021
- Published by Elsevier in Materials Characterization
- Vol. 181, 111467
Controlled precipitation of intermetallic (Al,Si)3Ti compound particles on double oxide films in liquid aluminum alloys
- 1 November 2021
- Published by Elsevier in Materials Characterization
- Vol. 181, 111467
Open AccessControlled precipitation of intermetallic (Al,Si)3Ti compound particles on double oxide films in liquid aluminum alloys
- Open Access
- 5 October 2021
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 16 (3) , 1415-1431
The Influence of Acid Hardener on the Strength and Hot-Distortion Properties of No-Bake Sand Cores
In this research work, the effects of different amounts of acid hardener (30%, 40%, 60%, 80% weighted to the resin) on the hardening characteristics and hot-distortion properties of no-bake furan and no-bake phenolic bonded sand cores were studied. Bending tests were conducted on test bars with storage times of 1, 2, 3, 5, 7, 24h. Hot-distortion tests were carried out on specimens with storage times of 4h and 24h. The bending tests revealed that in the case of the furan binder system, the acid hardener is best utilized in terms of higher bending strength, in an amount of 40–60%, while in the case of the phenolic binder system, the amount of 60–80% acid hardener resulted in higher bending strength of the sand specimens. Too low (30%) acid hardener (catalyst) level produced low bending strength. Too high (80%) amount of acid hardener decreased the strength of the no-bake furan sand samples, and as can be seen from the SEM analysis, it damaged the binder bridges between the sand grains. The hot-distortion tests showed that there is a correlation between the catalyst content and the max. Deformation of the samples both in the furan and in the phenolic no-bake sand cores, which can be described with a maximum curve. Increasing the acid hardener changes the thermoplastic behavior of the phenolic resin, thus the binder bridges become more rigid and brittle. The acid hardener above 40% decreased the thermal stability of the furan and phenolic bonded test pieces. The research work also revealed significant differences between the specimens made with furan and phenolic binder and the effect of the storage time in terms of the bending strength and hot-distortion properties.
- 5 October 2021
- Published by Springer Nature in International Journal of Metalcasting
- Vol. 16 (3) , 1415-1431
Open AccessThe Influence of Acid Hardener on the Strength and Hot-Distortion Properties of No-Bake Sand Cores
In this research work, the effects of different amounts of acid hardener (30%, 40%, 60%, 80% weighted to the resin) on the hardening characteristics and hot-distortion properties of no-bake furan and no-bake phenolic bonded sand cores were studied. Bending tests were conducted on test bars with storage times of 1, 2, 3, 5, 7, 24h. Hot-distortion tests were carried out on specimens with storage times of 4h and 24h. The bending tests revealed that in the case of the furan binder system, the acid hardener is best utilized in terms of higher bending strength, in an amount of 40–60%, while in the case of the phenolic binder system, the amount of 60–80% acid hardener resulted in higher bending strength of the sand specimens. Too low (30%) acid hardener (catalyst) level produced low bending strength. Too high (80%) amount of acid hardener decreased the strength of the no-bake furan sand samples, and as can be seen from the SEM analysis, it damaged the binder bridges between the sand grains. The hot-distortion tests showed that there is a correlation between the catalyst content and the max. Deformation of the samples both in the furan and in the phenolic no-bake sand cores, which can be described with a maximum curve. Increasing the acid hardener changes the thermoplastic behavior of the phenolic resin, thus the binder bridges become more rigid and brittle. The acid hardener above 40% decreased the thermal stability of the furan and phenolic bonded test pieces. The research work also revealed significant differences between the specimens made with furan and phenolic binder and the effect of the storage time in terms of the bending strength and hot-distortion properties.