Hui Xiao
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Hui Xiao has a total of 17 co-authors. Here are the top co-authors by number of shared publications:
Bingxi Li
Guangdong Univ Technol, State Key Lab High Performance Tools, Guangzhou 510006, Peoples R China
1 shared publicationDaodao Zhang
Jiangxi Mech Sci Inst, Nanchang 330000, Jiangxi, Peoples R China
1 shared publication- Junbin Zeng
Guangdong Provincial Key Laboratory of Industrial Intelligent Inspection Technology, Foshan University, Foshan 528000, China
1 shared publication - Kuanfang He
School of mechanical and electrical engineering and automation, Foshan University, Foshan, China
1 shared publication Lijun Song
State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body, Hunan University, Changsha, China
1 shared publication- Lijun Song
State Key Laboratory of Advanced Design and Manufacturing for Vehicle Bodies, Hunan university, Changsha 410082, China
1 shared publication
Latest Publications
- Open Access
Microstructure Control and Hot Cracking Prevention During Laser Additive Manufacturing of Cobalt-Based Superalloy
Hot cracking is a frequent and severe defect that occurs during laser additive manufacturing of superalloys. In this work, a pulsed-wave (PW) laser modulation process was employed to control the solidification microstructure and reduce the hot cracking susceptibility of laser additive manufactured cobalt-based superalloy. The effects of continuous-wave (CW) and PW laser processing modes on the dendrite morphology, element segregation, eutectic phase, and hot cracking of fabricated Co-based superalloys were investigated. Optical microscopy, scanning electron microscopy, and energy-dispersive X-ray spectroscopy were used to characterize the microstructural characteristics of samples. A two-color pyrometer was used to measure the molten pool temperature variation under different laser processing modes. The results show that coarse columnar dendrites, chain-like eutectic carbides, and hot cracks were observed in the CW sample. In contrast, the fine equiaxed crystals, discrete eutectic carbides, and low-level residual stresses were obtained to avoid hot cracks, owing to the high cooling rate and the periodic melting and solidification of the molten pool under the PW laser processing mode. This work provides a new method for controlling solidification structure and hot cracking of laser additive manufactured Co-based superalloy.
Open AccessMicrostructure Control and Hot Cracking Prevention During Laser Additive Manufacturing of Cobalt-Based Superalloy
Hot cracking is a frequent and severe defect that occurs during laser additive manufacturing of superalloys. In this work, a pulsed-wave (PW) laser modulation process was employed to control the solidification microstructure and reduce the hot cracking susceptibility of laser additive manufactured cobalt-based superalloy. The effects of continuous-wave (CW) and PW laser processing modes on the dendrite morphology, element segregation, eutectic phase, and hot cracking of fabricated Co-based superalloys were investigated. Optical microscopy, scanning electron microscopy, and energy-dispersive X-ray spectroscopy were used to characterize the microstructural characteristics of samples. A two-color pyrometer was used to measure the molten pool temperature variation under different laser processing modes. The results show that coarse columnar dendrites, chain-like eutectic carbides, and hot cracks were observed in the CW sample. In contrast, the fine equiaxed crystals, discrete eutectic carbides, and low-level residual stresses were obtained to avoid hot cracks, owing to the high cooling rate and the periodic melting and solidification of the molten pool under the PW laser processing mode. This work provides a new method for controlling solidification structure and hot cracking of laser additive manufactured Co-based superalloy.
- 22 May 2022
- Published by Springer Nature in Applied Physics A
- Vol. 128 (6) , 1-10
Solidification structure and aging response of laser additive manufactured Inconel 718
- 22 May 2022
- Published by Springer Nature in Applied Physics A
- Vol. 128 (6) , 1-10
Solidification structure and aging response of laser additive manufactured Inconel 718
- Open Access
Enhancing Hardness and Wear Performance of Laser Additive Manufactured Ti6Al4V Alloy Through Achieving Ultrafine Microstructure
Refining microstructure is an important issue for laser additive manufacturing (LAM) of titanium alloy. In the present work, the microstructures of LAM-fabricated Ti6Al4V alloy were refined using a low energy density with the combination of a small spot diameter, a low laser power, and a high scanning speed. The microstructure, hardness, wear performance, and molten pool thermal behavior of LAM-fabricated Ti6Al4V coatings were studied. The results show that the grain sizes of both prior β and α phases are strongly dependent on the cooling rate of the molten pool. The fine prior β grains and submicron-scale acicular α phases were obtained under a low energy density of 75 J mm−2 due to the high cooling rate of the molten pool. In addition, the as-fabricated Ti6Al4V sample with submicron-scale acicular α phase showed a very high hardness of 7.43 GPa, a high elastic modulus of 133.6 GPa, and a low coefficient of friction of 0.48. This work provides a good method for improving the microstructure and mechanical performance of LAM-fabricated Ti6Al4V alloy.
Open AccessEnhancing Hardness and Wear Performance of Laser Additive Manufactured Ti6Al4V Alloy Through Achieving Ultrafine Microstructure
Refining microstructure is an important issue for laser additive manufacturing (LAM) of titanium alloy. In the present work, the microstructures of LAM-fabricated Ti6Al4V alloy were refined using a low energy density with the combination of a small spot diameter, a low laser power, and a high scanning speed. The microstructure, hardness, wear performance, and molten pool thermal behavior of LAM-fabricated Ti6Al4V coatings were studied. The results show that the grain sizes of both prior β and α phases are strongly dependent on the cooling rate of the molten pool. The fine prior β grains and submicron-scale acicular α phases were obtained under a low energy density of 75 J mm−2 due to the high cooling rate of the molten pool. In addition, the as-fabricated Ti6Al4V sample with submicron-scale acicular α phase showed a very high hardness of 7.43 GPa, a high elastic modulus of 133.6 GPa, and a low coefficient of friction of 0.48. This work provides a good method for improving the microstructure and mechanical performance of LAM-fabricated Ti6Al4V alloy.