Neelima Paul
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Neelima Paul has a total of 96 co-authors. Here are the top co-authors by number of shared publications:
- Ralph Gilles
Technical University of Munich, Heinz Maier-Leibnitz Zentrum
8 shared publications - Amitesh Paul
Technische Universität München, Physik-Department, Lehrstuhl für Neutronenstreuung, James-Franck-Strasse 1, D-85748, Garching, Germany
4 shared publications - Peter Müller-Buschbaum
Technical University of Munich James-Franck-Str. 1
4 shared publications - Thomas Waldmann
ZSW—Zentrum für Sonnenenergie- und Wasserstoff-Forschung Baden-Württemberg, 89081 Ulm, Germany
4 shared publications - Margret Wohlfahrt-Mehrens
Zentrum für Sonnenenergie- und Wasserstoff-Forschung Baden-Württemberg (ZSW), Lise-Meitner-Straße 24, 89081 Ulm, Germany
3 shared publications - Marius Flügel
ZSW—Zentrum für Sonnenenergie- und Wasserstoff-Forschung Baden-Württemberg, Helmholtzstrasse 8, D-89081 Ulm, Germany
3 shared publications
Latest Publications
- Open Access
- 9 September 2025
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry A
- Vol. 13 (41) , 35435-35446
Measuring the buried interphase between solid electrolytes and lithium metal using neutrons
Neutrons allow one to probe interfaces in next generation high-energy batteries including solid-state Li metal batteries. Understanding these interfaces is key to enabling these batteries to reach their potential.
- 9 September 2025
- Published by Royal Society of Chemistry (RSC) in Journal of Materials Chemistry A
- Vol. 13 (41) , 35435-35446
Open AccessMeasuring the buried interphase between solid electrolytes and lithium metal using neutrons
Neutrons allow one to probe interfaces in next generation high-energy batteries including solid-state Li metal batteries. Understanding these interfaces is key to enabling these batteries to reach their potential.
- Open Access
- 24 February 2025
- Published by American Physical Society (APS) in Physical Review B
- Vol. 111 (5)
Tungsten oxide thin films probed by depth-resolved positron annihilation spectroscopy
Tungsten oxide ( WO x ) films grown on tungsten (W) are characterized by depth-resolved Doppler-broadening spectroscopy (DBS) and positron-annihilation lifetime spectroscopy (PALS) as primary analytical methods. The WO x films are prepared on W(111) monocrystals using either exposure to air, electrochemical, or thermal oxidation procedures, chosen according to the desired thickness. We calculate the lifetime of positrons in the bulk of WO x and in different types of vacancies using the atomic superposition (AtSup) method. These give the size required for a multivacancy in WO x needed for it to be identifiable by PALS. In our experiments, we identified a distinct positron lifetime of 325 p s in the thin oxide layer on W exposed to air. This value overlaps with that of multivacancy sites in W and, hence, should be taken into account in future PALS studies of radiation-induced defects in W. Published by the American Physical Society 2025
- 24 February 2025
- Published by American Physical Society (APS) in Physical Review B
- Vol. 111 (5)
Open AccessTungsten oxide thin films probed by depth-resolved positron annihilation spectroscopy
Tungsten oxide ( WO x ) films grown on tungsten (W) are characterized by depth-resolved Doppler-broadening spectroscopy (DBS) and positron-annihilation lifetime spectroscopy (PALS) as primary analytical methods. The WO x films are prepared on W(111) monocrystals using either exposure to air, electrochemical, or thermal oxidation procedures, chosen according to the desired thickness. We calculate the lifetime of positrons in the bulk of WO x and in different types of vacancies using the atomic superposition (AtSup) method. These give the size required for a multivacancy in WO x needed for it to be identifiable by PALS. In our experiments, we identified a distinct positron lifetime of 325 p s in the thin oxide layer on W exposed to air. This value overlaps with that of multivacancy sites in W and, hence, should be taken into account in future PALS studies of radiation-induced defects in W. Published by the American Physical Society 2025
- 28 October 2024
- Published by American Chemical Society (ACS) in ACS Materials Letters
- Vol. 6 (12) , 5216-5221
Comparative Analysis of Reactivity of Al and Ga Doped Garnet Solid State Electrolyte at the Interface with Li Metal
- 28 October 2024
- Published by American Chemical Society (ACS) in ACS Materials Letters
- Vol. 6 (12) , 5216-5221
Comparative Analysis of Reactivity of Al and Ga Doped Garnet Solid State Electrolyte at the Interface with Li Metal
- Open Access
- 1 July 2024
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 171 (7) , 070526
Efficient Workflows for Detecting Li Depositions in Lithium-Ion Batteries
Lithium deposition on anode surfaces can lead to fast capacity degradation and decreased safety properties of Li-ion cells. To avoid the critical aging mechanism of lithium deposition, its detection is essential. We present workflows for the efficient detection of Li deposition on electrode and cell level. The workflows are based on a variety of complementary advanced physico-chemical methods which were validated against each other for both graphite and graphite/Si electrodes: Electrochemical analysis, scanning electron microscopy, glow discharge-optical emission spectroscopy and neutron depth profiling, ex situ optical microscopy, in situ optical microscopy of cross-sectioned full cells, measurements in 3-electrode full cells, as well as 3D microstructurally resolved simulations. General considerations for workflows for analysis of battery cells and materials are discussed. The efficiency can be increased by parallel or serial execution of methods, stop criteria, and design of experiments planning. An important point in case of investigation of Li depositions are rest times during which Li can re-intercalate into the anode or react with electrolyte. Three workflows are presented to solve the questions on the occurrence of lithium deposition in an aged cell, the positions of lithium deposition in a cell, and operating conditions which avoid lithium depositions in a cell.
- 1 July 2024
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 171 (7) , 070526
Open AccessEfficient Workflows for Detecting Li Depositions in Lithium-Ion Batteries
Lithium deposition on anode surfaces can lead to fast capacity degradation and decreased safety properties of Li-ion cells. To avoid the critical aging mechanism of lithium deposition, its detection is essential. We present workflows for the efficient detection of Li deposition on electrode and cell level. The workflows are based on a variety of complementary advanced physico-chemical methods which were validated against each other for both graphite and graphite/Si electrodes: Electrochemical analysis, scanning electron microscopy, glow discharge-optical emission spectroscopy and neutron depth profiling, ex situ optical microscopy, in situ optical microscopy of cross-sectioned full cells, measurements in 3-electrode full cells, as well as 3D microstructurally resolved simulations. General considerations for workflows for analysis of battery cells and materials are discussed. The efficiency can be increased by parallel or serial execution of methods, stop criteria, and design of experiments planning. An important point in case of investigation of Li depositions are rest times during which Li can re-intercalate into the anode or react with electrolyte. Three workflows are presented to solve the questions on the occurrence of lithium deposition in an aged cell, the positions of lithium deposition in a cell, and operating conditions which avoid lithium depositions in a cell.
- Open Access
- 1 July 2024
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 171 (7) , 070503
Lithium Redistribution Mechanism within Silicon-Graphite Electrodes: Multi-Method Approach and Method Validation
Li redistribution processes within Si-graphite composite (SiG) electrodes are analyzed using in situ and operando X-ray diffraction (XRD), ex situ light microscopy (LM), in situ optical microscopy of cross-sectioned full cells (CS-IOM), and 3D microstructure-resolved simulations of full cells. First, the lithiation behavior of graphite and SiG full cells (Si content 20.8 wt.-%) is analyzed. The results are used as validation of the methods (XRD, LM, CS-IOM, simulation). Second, the Li redistribution between the graphite component and Si component within SiG electrodes is investigated: By operando XRD measurements during charging in comparison with relaxed cells, a higher lithiation degree in the graphite component is found during charging compared to the relaxed state, indicating Li redistribution from graphite to Si during relaxation. The Li redistribution is directly observed by in situ and ex situ optical microscopy, where the golden LiC6 phase disappears during a 24 h relaxation period. The results are supported by simulations showing the variation in the Li concentration, not only in graphite but also within the Si component. Furthermore, all methods find that the Li redistribution is more pronounced at a higher C-rate of 0.5 C, suggesting a preference for graphite lithiation over Si lithiation.
- 1 July 2024
- Published by The Electrochemical Society in Journal of the Electrochemical Society
- Vol. 171 (7) , 070503
Open AccessLithium Redistribution Mechanism within Silicon-Graphite Electrodes: Multi-Method Approach and Method Validation
Li redistribution processes within Si-graphite composite (SiG) electrodes are analyzed using in situ and operando X-ray diffraction (XRD), ex situ light microscopy (LM), in situ optical microscopy of cross-sectioned full cells (CS-IOM), and 3D microstructure-resolved simulations of full cells. First, the lithiation behavior of graphite and SiG full cells (Si content 20.8 wt.-%) is analyzed. The results are used as validation of the methods (XRD, LM, CS-IOM, simulation). Second, the Li redistribution between the graphite component and Si component within SiG electrodes is investigated: By operando XRD measurements during charging in comparison with relaxed cells, a higher lithiation degree in the graphite component is found during charging compared to the relaxed state, indicating Li redistribution from graphite to Si during relaxation. The Li redistribution is directly observed by in situ and ex situ optical microscopy, where the golden LiC6 phase disappears during a 24 h relaxation period. The results are supported by simulations showing the variation in the Li concentration, not only in graphite but also within the Si component. Furthermore, all methods find that the Li redistribution is more pronounced at a higher C-rate of 0.5 C, suggesting a preference for graphite lithiation over Si lithiation.
- 19 August 2023
- Published by Elsevier in Journal of Magnetism and Magnetic Materials
- Vol. 585
Exchange coupling due to spin-imbalance in Er magnetic sublattice within Er/Tb multilayers
- 19 August 2023
- Published by Elsevier in Journal of Magnetism and Magnetic Materials
- Vol. 585
Exchange coupling due to spin-imbalance in Er magnetic sublattice within Er/Tb multilayers
- 17 February 2023
- Published by American Chemical Society (ACS) in Journal of the American Chemical Society
- Vol. 145 (8) , 4450-4461
Dynamic Structure Evolution of Extensively Delithiated High Voltage Spinel Li1+xNi0.5Mn1.5O4 x < 1.5
High voltage spinel is one of the most promising next-generation cobalt-free cathode materials for lithium ion battery applications. Besides the typically utilized compositional range of LixNi0.5Mn1.5O4 0 < x < 1 in the voltage window of 4.90-3.00 V, additional 1.5 mol of Li per formula unit can be introduced into the structure, in an extended voltage range to 1.50 V. Theoretically, this leads to significant increase of the specific energy from 690 to 1190 Wh/kg. However, utilization of the extended potential window leads to rapid capacity fading and voltage polarization that lack a comprehensive explanation. In this work, we conducted potentiostatic entropymetry, operando XRD and neutron diffraction on the ordered stoichiometric spinel LixNi0.5Mn1.5O4 within 0 < x < 2.5 in order to understand the dynamic structure evolution and correlate it with the voltage profile. During the two-phase reaction from cubic (x < 1) to tetragonal (x > 1) phase at ∼2.8 V, we identified the evolution of a second tetragonal phase with x > 2. The structural evaluation during the delithiation indicates the formation of an intermediate phase with cubic symmetry at a lithium content of x = 1.5. Evaluation of neutron diffraction data, with maximum entropy method, of the highly lithiated phase LixNi0.5Mn1.5O4 with 2 < x < 2.5 strongly suggests that lithium ions are located on octahedral 8a and tetrahedral 4a positions of the distorted tetragonal phase I41amd. Consequently, we were able to provide a conclusive explanation for the additional voltage step at 2.10 V, the sloping voltage profile below 1.80 V, and the additional voltage step at ∼3.80 V.
- 17 February 2023
- Published by American Chemical Society (ACS) in Journal of the American Chemical Society
- Vol. 145 (8) , 4450-4461
Dynamic Structure Evolution of Extensively Delithiated High Voltage Spinel Li1+xNi0.5Mn1.5O4 x < 1.5
High voltage spinel is one of the most promising next-generation cobalt-free cathode materials for lithium ion battery applications. Besides the typically utilized compositional range of LixNi0.5Mn1.5O4 0 < x < 1 in the voltage window of 4.90-3.00 V, additional 1.5 mol of Li per formula unit can be introduced into the structure, in an extended voltage range to 1.50 V. Theoretically, this leads to significant increase of the specific energy from 690 to 1190 Wh/kg. However, utilization of the extended potential window leads to rapid capacity fading and voltage polarization that lack a comprehensive explanation. In this work, we conducted potentiostatic entropymetry, operando XRD and neutron diffraction on the ordered stoichiometric spinel LixNi0.5Mn1.5O4 within 0 < x < 2.5 in order to understand the dynamic structure evolution and correlate it with the voltage profile. During the two-phase reaction from cubic (x < 1) to tetragonal (x > 1) phase at ∼2.8 V, we identified the evolution of a second tetragonal phase with x > 2. The structural evaluation during the delithiation indicates the formation of an intermediate phase with cubic symmetry at a lithium content of x = 1.5. Evaluation of neutron diffraction data, with maximum entropy method, of the highly lithiated phase LixNi0.5Mn1.5O4 with 2 < x < 2.5 strongly suggests that lithium ions are located on octahedral 8a and tetrahedral 4a positions of the distorted tetragonal phase I41amd. Consequently, we were able to provide a conclusive explanation for the additional voltage step at 2.10 V, the sloping voltage profile below 1.80 V, and the additional voltage step at ∼3.80 V.
- Open Access
- 1 January 2023
- Published by Elsevier in SSRN Electronic Journal
Ultrathin Single-Ion Conducting Polymer Enabling a Stable Li|Li1.3al0.3ti1.7(Po4)3 Interface
NASICON-type Li1+xAlxTi2−x(PO4)3 (LATP) solid electrolytes have attracted great attention because of their high ionic conductivity, wide electrochemical stability window, pronounced chemical resistance, and low cost. However, the chemical instability of LATP against metallic lithium (Li0) poses a major challenge and hinders its application in solid-state lithium batteries. Herein, an ultrathin polysiloxane-based single-ion conductor (PSiO) serves as multifunctional protection interlayer to enhance the interfacial stability between LATP and Li0. PSiO effectively blocks the direct contact between Li0 and LATP, regulates the homogeneous Li+ flux at the Li|electrolyte interface, promotes the intimate contact between PSiO and Li0 by forming Si−O−Li bonds, and generates an LiF-enriched Li|electrolyte interphase. As a result, it enables more than 2,000 h of stable cycling in symmetric PSiO@Li‖PSiO@Li cells and superior rate capability and cycling stability in high-energy PSiO@Li‖LiNi0.88Co0.09Mn0.03O2 cells. The realization of well performing 2-layer bipolar stacked cells eventually demonstrates the great potential of this approach.
- 1 January 2023
- Published by Elsevier in SSRN Electronic Journal
Open AccessUltrathin Single-Ion Conducting Polymer Enabling a Stable Li|Li1.3al0.3ti1.7(Po4)3 Interface
NASICON-type Li1+xAlxTi2−x(PO4)3 (LATP) solid electrolytes have attracted great attention because of their high ionic conductivity, wide electrochemical stability window, pronounced chemical resistance, and low cost. However, the chemical instability of LATP against metallic lithium (Li0) poses a major challenge and hinders its application in solid-state lithium batteries. Herein, an ultrathin polysiloxane-based single-ion conductor (PSiO) serves as multifunctional protection interlayer to enhance the interfacial stability between LATP and Li0. PSiO effectively blocks the direct contact between Li0 and LATP, regulates the homogeneous Li+ flux at the Li|electrolyte interface, promotes the intimate contact between PSiO and Li0 by forming Si−O−Li bonds, and generates an LiF-enriched Li|electrolyte interphase. As a result, it enables more than 2,000 h of stable cycling in symmetric PSiO@Li‖PSiO@Li cells and superior rate capability and cycling stability in high-energy PSiO@Li‖LiNi0.88Co0.09Mn0.03O2 cells. The realization of well performing 2-layer bipolar stacked cells eventually demonstrates the great potential of this approach.
- 8 October 2020
- Published by Pleiades Publishing Ltd in Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques
- Vol. 14 (S1) , S156-S160
Combining SANS and VSANS to Extend Q-Range for Morphology Investigation of Silicon-Graphite Anodes
Silicon-based electrodes are attractive candidates as anodes for Li-ion batteries due to their high theoretical specific capacity. However, repeated lithiation/delithiation causes significant morphological changes in the silicon particles, which results in formation of highly porous silicon structures and severe side reactions at the silicon–electrolyte interface. To quantify such morphological changes on both the micrometer and nanometer scales, we combine the techniques of very small-angle neutron scattering (VSANS) and small-angle neutron scattering (SANS). While conventional and contrast-matched SANS data provide insight into the solid–electrolyte-interphase coverage around silicon particles and the filling of evolving porosity within the electrode, VSANS data provide information on the micrometer-sized graphite particles.
- 8 October 2020
- Published by Pleiades Publishing Ltd in Journal of Surface Investigation: X-Ray, Synchrotron and Neutron Techniques
- Vol. 14 (S1) , S156-S160
Combining SANS and VSANS to Extend Q-Range for Morphology Investigation of Silicon-Graphite Anodes
Silicon-based electrodes are attractive candidates as anodes for Li-ion batteries due to their high theoretical specific capacity. However, repeated lithiation/delithiation causes significant morphological changes in the silicon particles, which results in formation of highly porous silicon structures and severe side reactions at the silicon–electrolyte interface. To quantify such morphological changes on both the micrometer and nanometer scales, we combine the techniques of very small-angle neutron scattering (VSANS) and small-angle neutron scattering (SANS). While conventional and contrast-matched SANS data provide insight into the solid–electrolyte-interphase coverage around silicon particles and the filling of evolving porosity within the electrode, VSANS data provide information on the micrometer-sized graphite particles.