Gennady Yuriyovych Kryachko
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
Gennady Yuriyovych Kryachko has a total of 16 co-authors. Here are the top co-authors by number of shared publications:
- Ye. M. Sigarev
Dniprovsky State Technical University (Kamianske, Ukraine)
12 shared publications - M.S. Kuznetsov3 shared publications
- A. A. Pokhvalityi
Dnipro State Technical University (DDTU) (Kamianske, Ukraine)
2 shared publications - Igor Matina
Dniprovsky State Technical University, Kamianske
2 shared publications D. Yeskov
Dniprovsky State Technical University
1 shared publicationD.V. Yeskov
Dniprovsky State Technical University, Kamianske
1 shared publication
Latest Publications
- Open Access
- 15 February 2026
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Science and innovation
- Vol. 22 (1) , 107-122
АНАЛІЗ ПРИЧИН ТА НАСЛІДКІВ РЕЗОНАНСНИХ АВАРІЙ ДОМЕННИХ ПЕЧЕЙ
Вступ. Доменна піч, разом з повітронагрівальною і газоочисною технікою, залишається однією з найнебезпечних металургійних систем. Особливої уваги потребують аварії з катастрофічними наслідками якдля обладнання, так і для техперсоналу. Вони не мають терміну давності й повинні ретельно вивчатисязадля усунення причин їх виникнення та безпечного функціонування.Проблематика. Недостатнє, а іноді й протирічне, висвітлення у технічній літературі інформації про особливо важкі аварії, зокрема вибухи печей, є перепоною для подальшого удосконалення та розробки безпечної технології ведення доменного процесу, тому пошук засобів запобігання та уникнення аварійних ситуацій є актуальним.Мета. Встановити дійсний механізм вибухового руйнування доменної печі №7 Дніпровського металургійного комбінату (ДМК) 07.09.1993 р. з розглядом факторів об’єктивного та суб’єктивного впливів.Матеріали й методи. Для аналізу використано архівні матеріали візуалізації параметрів роботи печі напаперових носіях, фотодокументи, акти й висновки експертних комісій, а також публікації з досліджуваного питання.Результати. Відтворено механізм вибухового руйнування ДП №7 ДМК (Україна). Систематизовано фактори, що спричинили аварійну ситуацію. Виконано порівняння причин і наслідків аварій на досліджуванійпечі і ДП №5 заводу в Port Talbot (Великобританія), що мали однаковий механізм катастрофічного руйнування агрегатів через неконтрольоване потрапляння критичної маси води в робочий простір печі.Висновки. Встановлено, що на ДП №7 ДМК значний масштаб руйнувань з численними людськими жертвами був обумовлений не одним, як вважалося раніше, а двома вибухами різної потужності. Показано динаміку зміни газодуттьового режиму задувального періоду, що призвело при відсутності сходу шихти на колошнику до вибухової аварії. Охарактеризовано важливість дотримання рекомендацій для недопущенняпарових вибухів у доменних печах. Результати дослідження є важливим доповненням до створення нормативних документів для забезпечення безаварійної експлуатації доменних печей.
- 15 February 2026
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Science and innovation
- Vol. 22 (1) , 107-122
Open AccessАНАЛІЗ ПРИЧИН ТА НАСЛІДКІВ РЕЗОНАНСНИХ АВАРІЙ ДОМЕННИХ ПЕЧЕЙ
Вступ. Доменна піч, разом з повітронагрівальною і газоочисною технікою, залишається однією з найнебезпечних металургійних систем. Особливої уваги потребують аварії з катастрофічними наслідками якдля обладнання, так і для техперсоналу. Вони не мають терміну давності й повинні ретельно вивчатисязадля усунення причин їх виникнення та безпечного функціонування.Проблематика. Недостатнє, а іноді й протирічне, висвітлення у технічній літературі інформації про особливо важкі аварії, зокрема вибухи печей, є перепоною для подальшого удосконалення та розробки безпечної технології ведення доменного процесу, тому пошук засобів запобігання та уникнення аварійних ситуацій є актуальним.Мета. Встановити дійсний механізм вибухового руйнування доменної печі №7 Дніпровського металургійного комбінату (ДМК) 07.09.1993 р. з розглядом факторів об’єктивного та суб’єктивного впливів.Матеріали й методи. Для аналізу використано архівні матеріали візуалізації параметрів роботи печі напаперових носіях, фотодокументи, акти й висновки експертних комісій, а також публікації з досліджуваного питання.Результати. Відтворено механізм вибухового руйнування ДП №7 ДМК (Україна). Систематизовано фактори, що спричинили аварійну ситуацію. Виконано порівняння причин і наслідків аварій на досліджуванійпечі і ДП №5 заводу в Port Talbot (Великобританія), що мали однаковий механізм катастрофічного руйнування агрегатів через неконтрольоване потрапляння критичної маси води в робочий простір печі.Висновки. Встановлено, що на ДП №7 ДМК значний масштаб руйнувань з численними людськими жертвами був обумовлений не одним, як вважалося раніше, а двома вибухами різної потужності. Показано динаміку зміни газодуттьового режиму задувального періоду, що призвело при відсутності сходу шихти на колошнику до вибухової аварії. Охарактеризовано важливість дотримання рекомендацій для недопущенняпарових вибухів у доменних печах. Результати дослідження є важливим доповненням до створення нормативних документів для забезпечення безаварійної експлуатації доменних печей.
- Open Access
- 30 June 2025
- Published by SHEI Pryazovskyi State Technical University in Reporter of the Priazovskyi State Technical University. Section: Technical sciences
- No. 50,p. 117-124
Pressure blast melting and blow enrichment with oxygen – process intensifiers or an unfounded tribute to traditions
The fallacy of existing statements about the unfounded expediency of using increased gas pressure in the working space of blast furnaces and enriching the blast with oxygen as intensifiers of the blast furnace process is shown, due to the incorrect comparison of the operation of furnaces of different volumes, which operated under sharply different raw material and operating conditions. Using the example of two blast furnaces of the same enterprise, the volume of which differed by almost two times, it is shown that with an increase in the useful volume of the furnace, the value of increased gas pressure as a means of intensification of melting increases in comparison with units of lower capacity. The main reasons for the increase in the resistance of the charge column are given, which are associated with both a decrease in the volume fraction of coke in the “dry” zone of the furnace and a thinning of the coke “windows” in the cohesion zone with a decrease in the volume fraction of coke, an overestimation of the working height of blast furnaces of Soviet designs, and the need to create powerful tuyeres for the redistribution of tuyeres gas to the centre of the furnace with an increase in the power of the units. It is precisely to overcome the effects of negative factors in order to intensify blast melting that pressure blast furnace melting is widely used. The data obtained from the research results not only indicate the effectiveness of using increased gas pressure, but also indicate its differentiated effect on the intensity of melting in furnaces of different volumes. According to the results of the study, without involving an increase in gas pressure on the top as an intensifier of blast furnace melting, forcing the furnace stroke by blowing can be carried out only by increasing the unevenness of the radial gas distribution with excess coke consumption. It is shown that increasing the gas pressure in the working space of the furnaces and enriching the blow with oxygen are not antagonists, since they are aimed at overcoming negative changes of various nature that arose in the process of improving blast furnace melting
- 30 June 2025
- Published by SHEI Pryazovskyi State Technical University in Reporter of the Priazovskyi State Technical University. Section: Technical sciences
- No. 50,p. 117-124
Open AccessPressure blast melting and blow enrichment with oxygen – process intensifiers or an unfounded tribute to traditions
The fallacy of existing statements about the unfounded expediency of using increased gas pressure in the working space of blast furnaces and enriching the blast with oxygen as intensifiers of the blast furnace process is shown, due to the incorrect comparison of the operation of furnaces of different volumes, which operated under sharply different raw material and operating conditions. Using the example of two blast furnaces of the same enterprise, the volume of which differed by almost two times, it is shown that with an increase in the useful volume of the furnace, the value of increased gas pressure as a means of intensification of melting increases in comparison with units of lower capacity. The main reasons for the increase in the resistance of the charge column are given, which are associated with both a decrease in the volume fraction of coke in the “dry” zone of the furnace and a thinning of the coke “windows” in the cohesion zone with a decrease in the volume fraction of coke, an overestimation of the working height of blast furnaces of Soviet designs, and the need to create powerful tuyeres for the redistribution of tuyeres gas to the centre of the furnace with an increase in the power of the units. It is precisely to overcome the effects of negative factors in order to intensify blast melting that pressure blast furnace melting is widely used. The data obtained from the research results not only indicate the effectiveness of using increased gas pressure, but also indicate its differentiated effect on the intensity of melting in furnaces of different volumes. According to the results of the study, without involving an increase in gas pressure on the top as an intensifier of blast furnace melting, forcing the furnace stroke by blowing can be carried out only by increasing the unevenness of the radial gas distribution with excess coke consumption. It is shown that increasing the gas pressure in the working space of the furnaces and enriching the blow with oxygen are not antagonists, since they are aimed at overcoming negative changes of various nature that arose in the process of improving blast furnace melting
- Open Access
- 26 December 2024
- Published by SHEI Pryazovskyi State Technical University in Reporter of the Priazovskyi State Technical University. Section: Technical sciences
- Vol. 1 (49) , 208-218
Study of the erosion of ladle refractories when gas is injected deep into the bath through a rotating lance
With the use of isothermal modeling, new data were obtained regarding the influence of the movement of gas jets from the nozzles of the tip of the submersible rotating lance on the hydrodynamics and the intensity of mass transfer processes in the ladle bath. It was established that mixing the bath during the rotation of gas jets increases the mass transfer rate, since the tangential stress arising in the liquid causes the gas bubbles to be crushed, which in turn leads to an increase in the volume of the bubbling zones and the reaction surface of the phases. The increase in the total volume of the bubbling zones is 25-35% of the volume of the bath, compared to 8-10% for a stationary nozzle. Peculiarities of erosive wear of the ladle lining during desulfurization by blowing powdered reagents through the nozzles of T-shaped nozzles of lances were investigated. The highest intensity of wear with increasing gas consumption is observed in the upper part of the bucket. With an increase in the rotation speed of the lance and gas consumption, the intensity of wear decreases in the middle horizons from 0.7 to 0.4 mm/min. For the upper areas of the bucket, increasing the gas consumption from 1.0 l/min to 2.2 l/min and the rotation speed to 120 rpm leads to a decrease in intensity by 36.7%, for the middle – by 55.6%, for lower – by 28.5%. Based on the results of a comparative analysis of the wear profile of the working layer of refractories when using stationary and rotating lances and numerical modeling of the dynamics of wear, the rational consumption of the carrier gas and the rotation speed of the lance were determined to minimize the intensity of lining erosion. From the point of view of dispersing the desulfurizing reagents with a simultaneous increase in the gas saturation of the bath, it is advisable to increase the gas consumption and the rotation speed of the lance to the maximum possible values. On the other hand, from the point of view of preventing uneven wear of the lining, it is advisable to limit the speed of rotation of the gun at the level of 60-75 rpm, and gas consumption - by the need to ensure a stable mode of formation of the gas powder flow without clogging the nozzles of the T-shaped tip of the lance
- 26 December 2024
- Published by SHEI Pryazovskyi State Technical University in Reporter of the Priazovskyi State Technical University. Section: Technical sciences
- Vol. 1 (49) , 208-218
Open AccessStudy of the erosion of ladle refractories when gas is injected deep into the bath through a rotating lance
With the use of isothermal modeling, new data were obtained regarding the influence of the movement of gas jets from the nozzles of the tip of the submersible rotating lance on the hydrodynamics and the intensity of mass transfer processes in the ladle bath. It was established that mixing the bath during the rotation of gas jets increases the mass transfer rate, since the tangential stress arising in the liquid causes the gas bubbles to be crushed, which in turn leads to an increase in the volume of the bubbling zones and the reaction surface of the phases. The increase in the total volume of the bubbling zones is 25-35% of the volume of the bath, compared to 8-10% for a stationary nozzle. Peculiarities of erosive wear of the ladle lining during desulfurization by blowing powdered reagents through the nozzles of T-shaped nozzles of lances were investigated. The highest intensity of wear with increasing gas consumption is observed in the upper part of the bucket. With an increase in the rotation speed of the lance and gas consumption, the intensity of wear decreases in the middle horizons from 0.7 to 0.4 mm/min. For the upper areas of the bucket, increasing the gas consumption from 1.0 l/min to 2.2 l/min and the rotation speed to 120 rpm leads to a decrease in intensity by 36.7%, for the middle – by 55.6%, for lower – by 28.5%. Based on the results of a comparative analysis of the wear profile of the working layer of refractories when using stationary and rotating lances and numerical modeling of the dynamics of wear, the rational consumption of the carrier gas and the rotation speed of the lance were determined to minimize the intensity of lining erosion. From the point of view of dispersing the desulfurizing reagents with a simultaneous increase in the gas saturation of the bath, it is advisable to increase the gas consumption and the rotation speed of the lance to the maximum possible values. On the other hand, from the point of view of preventing uneven wear of the lining, it is advisable to limit the speed of rotation of the gun at the level of 60-75 rpm, and gas consumption - by the need to ensure a stable mode of formation of the gas powder flow without clogging the nozzles of the T-shaped tip of the lance
- Open Access
- 3 December 2024
- Published by Dniprovsk State Technical University in Collection of scholarly papers of Dniprovsk State Technical University (Technical Sciences)
- p. 8-21
DEPARTMENT OF METALURGY NAMED AFTER PROFESSOR VOLODIMIR LOGINOV - 95
The article presents the history of creation, development and dynamics of scientific interests of the Department of Metallurgy of the Dnipro State Technical University during the 95-year period of its existence. Reorganization and unification of the Department of Metallurgy of Ferrous Metals with departments of related specialties contributed to the expansion of scientific directions of research and opportunities for the implementation of developments in the practice of metallurgical enterprises. The scientific developments of the department's employees received a positive assessment from experts, were tested and implemented both in Ukraine and abroad.Thanks to the use of proprietary methods and laboratory equipment for isothermal and high-temperature modeling of metallurgical processes, innovative technologies and devices for sintering, blast furnace and steelmaking industries were proposed and mastered. The long-term scientific experience of the department's employees made it possible to substantiate the expediency and carry out a cycle of scientific research in the directions of theoretical and technological foundations of increasing the energy efficiency of agglomeration production and the quality of cast iron; development of methods for selecting slag and optimizing slag modes of blast furnace smelting, including when blowing pulverized coal fuel; substantiation of the priority directions for the further development of the design of devices and equipment for blasting into the blast furnace, improvement of its profile, systems for measuring process parameters and the condition of furnace enclosures;resource-saving technologies and devices for desulfurization and complex refining of recycled cast iron in ladles before converter smelting; dutt devices for conducting converter melting, including using low-slag technology, preliminary heating of scrap metal and elements of liquid-phase recovery of raw materials; new methods and devices for applying slag garnish to the lining of the oxygen converter; methods and devices for optimization of steel deoxidation and pouring technologies.
- 3 December 2024
- Published by Dniprovsk State Technical University in Collection of scholarly papers of Dniprovsk State Technical University (Technical Sciences)
- p. 8-21
Open AccessDEPARTMENT OF METALURGY NAMED AFTER PROFESSOR VOLODIMIR LOGINOV - 95
The article presents the history of creation, development and dynamics of scientific interests of the Department of Metallurgy of the Dnipro State Technical University during the 95-year period of its existence. Reorganization and unification of the Department of Metallurgy of Ferrous Metals with departments of related specialties contributed to the expansion of scientific directions of research and opportunities for the implementation of developments in the practice of metallurgical enterprises. The scientific developments of the department's employees received a positive assessment from experts, were tested and implemented both in Ukraine and abroad.Thanks to the use of proprietary methods and laboratory equipment for isothermal and high-temperature modeling of metallurgical processes, innovative technologies and devices for sintering, blast furnace and steelmaking industries were proposed and mastered. The long-term scientific experience of the department's employees made it possible to substantiate the expediency and carry out a cycle of scientific research in the directions of theoretical and technological foundations of increasing the energy efficiency of agglomeration production and the quality of cast iron; development of methods for selecting slag and optimizing slag modes of blast furnace smelting, including when blowing pulverized coal fuel; substantiation of the priority directions for the further development of the design of devices and equipment for blasting into the blast furnace, improvement of its profile, systems for measuring process parameters and the condition of furnace enclosures;resource-saving technologies and devices for desulfurization and complex refining of recycled cast iron in ladles before converter smelting; dutt devices for conducting converter melting, including using low-slag technology, preliminary heating of scrap metal and elements of liquid-phase recovery of raw materials; new methods and devices for applying slag garnish to the lining of the oxygen converter; methods and devices for optimization of steel deoxidation and pouring technologies.
- Open Access
- 3 December 2024
- Published by Dniprovsk State Technical University in Collection of scholarly papers of Dniprovsk State Technical University (Technical Sciences)
- p. 76-88
SULFIDE CAPACITY AND PROPERTIES OF MODIFIED BUCKET SLAGS
Ladle slag during the entire period of iron refining must have a sufficient degree of ability to hold sulfides while simultaneously ensuring the minimization of iron losses. In ladles with recycled cast iron entering the desulphurization department, slags are formed already during the release of cast iron from the blast furnace or pouring from the mixer, which differ significantly from blast furnace slag in terms of physical and chemical properties. The basicity and sulphide capacity of slags decreases, which due to their active mixing with cast iron is accompanied by an increase in sulfur in the metal.The composition of slags, formed from the remains of blast furnace or mixer slags and products of chemical reactions of sulfur removal by injection of mixtures based on lime and magnesium, needs adjustment to increase the sulfide capacity while simultaneously thinning them to prevent excessive losses of iron with the slag. The use of an additional amount of fluidized lime for adjustment leads to an increase in the processing cost. It is proposed to use a slag modifier based on CaO- and Al2O3-containing steel processing waste to reduce the costs of fluidized lime. The rational specific consumption of modifiers was determined depending on the initial composition of ladle slags and the change in their sulfide capacity was calculated using models based on the concept of optical basicity.The change in melting point, viscosity, and melting point of modified ladle slags was determined, and the concentration path of CaO- and Al2O3-containing waste modified with additives was investigated. It is shown that for the typical composition of the ladle slag of cast iron desulfurization plant of PrJSC «Kamet-Stal», the sulfide capacity values range from 1.0.10-4 to 20.0.10-4, which corresponds to blast furnace slags of the CaO-SiO2-MnO-Al2O3-MgO system with increased desulfurizing ability. The change in the amount of the solid fraction in the final slag in the course of refining and the effect of the basicity of the modified slag on the sulfur distribution coefficient in non-stationary temperature conditions were determined. With the application of the linear programming method, the range of rational chemical composition of ladle slag for the conditions of cast iron desulfurization plant of PrJSC «Kamet-Stal» was determined. Modified ladle slag with a basicity of 1.11-1.41 and a content of 40-51% CaO; 36-51 %SiO2 and 6-21 %Al2O3 are proposed to be considered as satisfying the given range of selected metallurgical properties.
- 3 December 2024
- Published by Dniprovsk State Technical University in Collection of scholarly papers of Dniprovsk State Technical University (Technical Sciences)
- p. 76-88
Open AccessSULFIDE CAPACITY AND PROPERTIES OF MODIFIED BUCKET SLAGS
Ladle slag during the entire period of iron refining must have a sufficient degree of ability to hold sulfides while simultaneously ensuring the minimization of iron losses. In ladles with recycled cast iron entering the desulphurization department, slags are formed already during the release of cast iron from the blast furnace or pouring from the mixer, which differ significantly from blast furnace slag in terms of physical and chemical properties. The basicity and sulphide capacity of slags decreases, which due to their active mixing with cast iron is accompanied by an increase in sulfur in the metal.The composition of slags, formed from the remains of blast furnace or mixer slags and products of chemical reactions of sulfur removal by injection of mixtures based on lime and magnesium, needs adjustment to increase the sulfide capacity while simultaneously thinning them to prevent excessive losses of iron with the slag. The use of an additional amount of fluidized lime for adjustment leads to an increase in the processing cost. It is proposed to use a slag modifier based on CaO- and Al2O3-containing steel processing waste to reduce the costs of fluidized lime. The rational specific consumption of modifiers was determined depending on the initial composition of ladle slags and the change in their sulfide capacity was calculated using models based on the concept of optical basicity.The change in melting point, viscosity, and melting point of modified ladle slags was determined, and the concentration path of CaO- and Al2O3-containing waste modified with additives was investigated. It is shown that for the typical composition of the ladle slag of cast iron desulfurization plant of PrJSC «Kamet-Stal», the sulfide capacity values range from 1.0.10-4 to 20.0.10-4, which corresponds to blast furnace slags of the CaO-SiO2-MnO-Al2O3-MgO system with increased desulfurizing ability. The change in the amount of the solid fraction in the final slag in the course of refining and the effect of the basicity of the modified slag on the sulfur distribution coefficient in non-stationary temperature conditions were determined. With the application of the linear programming method, the range of rational chemical composition of ladle slag for the conditions of cast iron desulfurization plant of PrJSC «Kamet-Stal» was determined. Modified ladle slag with a basicity of 1.11-1.41 and a content of 40-51% CaO; 36-51 %SiO2 and 6-21 %Al2O3 are proposed to be considered as satisfying the given range of selected metallurgical properties.
- Open Access
- 3 December 2024
- Published by Dniprovsk State Technical University in Collection of scholarly papers of Dniprovsk State Technical University (Technical Sciences)
- p. 45-52
THE INFLUENCE OF ADDITIONAL NITROGEN CONTENT IN THE HEATED DUTTY ON THE PERFORMANCE OF THE BLOWING PERIOD OF BLAST FURNACES
An analysis of the effect of heated nitrogen and blowing temperature on the course of the blast furnace process was performed from the point of view of the developers of this technology and the theory of the blast furnace process. It is shown that enriching the blowing with nitrogen reduces the volume of the cavity in case of oxygen deficiency, and increasing the blowing temperature increases the volume and pressure of gases, both in the cavity and outside it. The mutual effect of the two listed factors significantly reduces the gas permeability of the charge, which is an obstacle to its uniform lowering. With regard to the mechanism of nitrogen influence, it is shown that, firstly, the acceleration of heat exchange should accelerate the formation of the primary cohesion zone, in which the processes of sticking together pieces of iron ore materials with the loss of gas permeability and macropores with the formation of a liquid phase will prematurely proceed, and secondly, the dilution of blowing oxygen and reducing agents in the furnace gas does not contribute improving recovery of iron ore materials, especially in the prematurely formed zone of cohesion. Additional nitrogen in the heated blast slows down the process of burning coke on the tuyeres, thereby delaying the start of movement of the charge, increasing its porosity and, accordingly, gas permeability. Focusing attention on the development of the temperature field in the charge column of the blast furnace during the blowing period should not exclude from consideration the dynamics of changes in the mechanics of the movement of the charge and the concentration field, because the problem of nitrogen blowing technology is the lack of relatively uniform lowering of the charge and its treatment with hot reducing gases. In addition, the simultaneous decrease in the mass of coke burning near the nozzles and the reduction in the size of the nozzle cavity, along with the increase in the output of nozzle gas as a result of nitrogen enrichment of the blast, worsens the gas permeability of the charge in the high temperature zone. On the other hand, the depletion of furnace gas by reductants and premature heating of iron ore materials with loss of their fluidity worsen the recovery process. Unprepared iron ore materials, when lowered down, cause an increase in direct recovery and cooling of the furnace. On the basis of the analysis of practical data on the use of nitrogen as an energy additive to atmospheric blasting when blasting blast furnaces, as well as on the basis of the analysis of the compliance of nitrogen blasting technology with the foundations of the theory of the blast furnace process, the negative influence of nitrogen on the course of the blasting period is shown, which calls into question the feasibility of using nitrogen in start-up period of blast furnaces.
- 3 December 2024
- Published by Dniprovsk State Technical University in Collection of scholarly papers of Dniprovsk State Technical University (Technical Sciences)
- p. 45-52
Open AccessTHE INFLUENCE OF ADDITIONAL NITROGEN CONTENT IN THE HEATED DUTTY ON THE PERFORMANCE OF THE BLOWING PERIOD OF BLAST FURNACES
An analysis of the effect of heated nitrogen and blowing temperature on the course of the blast furnace process was performed from the point of view of the developers of this technology and the theory of the blast furnace process. It is shown that enriching the blowing with nitrogen reduces the volume of the cavity in case of oxygen deficiency, and increasing the blowing temperature increases the volume and pressure of gases, both in the cavity and outside it. The mutual effect of the two listed factors significantly reduces the gas permeability of the charge, which is an obstacle to its uniform lowering. With regard to the mechanism of nitrogen influence, it is shown that, firstly, the acceleration of heat exchange should accelerate the formation of the primary cohesion zone, in which the processes of sticking together pieces of iron ore materials with the loss of gas permeability and macropores with the formation of a liquid phase will prematurely proceed, and secondly, the dilution of blowing oxygen and reducing agents in the furnace gas does not contribute improving recovery of iron ore materials, especially in the prematurely formed zone of cohesion. Additional nitrogen in the heated blast slows down the process of burning coke on the tuyeres, thereby delaying the start of movement of the charge, increasing its porosity and, accordingly, gas permeability. Focusing attention on the development of the temperature field in the charge column of the blast furnace during the blowing period should not exclude from consideration the dynamics of changes in the mechanics of the movement of the charge and the concentration field, because the problem of nitrogen blowing technology is the lack of relatively uniform lowering of the charge and its treatment with hot reducing gases. In addition, the simultaneous decrease in the mass of coke burning near the nozzles and the reduction in the size of the nozzle cavity, along with the increase in the output of nozzle gas as a result of nitrogen enrichment of the blast, worsens the gas permeability of the charge in the high temperature zone. On the other hand, the depletion of furnace gas by reductants and premature heating of iron ore materials with loss of their fluidity worsen the recovery process. Unprepared iron ore materials, when lowered down, cause an increase in direct recovery and cooling of the furnace. On the basis of the analysis of practical data on the use of nitrogen as an energy additive to atmospheric blasting when blasting blast furnaces, as well as on the basis of the analysis of the compliance of nitrogen blasting technology with the foundations of the theory of the blast furnace process, the negative influence of nitrogen on the course of the blasting period is shown, which calls into question the feasibility of using nitrogen in start-up period of blast furnaces.
- Open Access
- 6 June 2024
- Published by Dniprovsk State Technical University in Collection of scholarly papers of Dniprovsk State Technical University (Technical Sciences)
- Vol. 1 (44) , 9-15
SOME SPECIFICATIONS REGARDING TEMPERATURES ON HORIZON AIR TUYERES OF THE BLAST FURNACES
The purpose work is to clarify data on temperature changes on horizon air tuyeres of the blast furnaces. Shown that the common idea about similarity of changes in temperature and pressure of gases needs to be clarified. The difference is that the temperature gases in the direction to the centre of the furnace increases to the focus of combustion in front of the tuyeres, and pressure increases to the end of the tuyeres cavity. Accordingly, the temperature decreases starting from combustion focus, and pressure — starting from coke shell of tail part of the tuyeres cavity. The calculation gas temperature variation coefficients Vt based on the DonNDIchormet measurement data showed that Vt decreased from 8 to 3.5 % on average over a distance of 0.5 m as the distance from the tip of the tuyeres increased. This indicates that during peripheral operation of the furnaces, the zone in front of the tuyeres is the most critical in terms of temperature fluctuations. This phenomenon is explained by the characteristic features of the gas mechanics of the tuyere cavity — reduced gas pressure at the tuyere section and discrete deformation of the air-gas jet by coke collapse through dynamically unstable vaults of the tuyere cavity. It is shown that the blast furnace melting conditions determine the effectiveness and efficiency of the blast furnace process, as well as the possible level of reaching the theoretical combustion temperature.
- 6 June 2024
- Published by Dniprovsk State Technical University in Collection of scholarly papers of Dniprovsk State Technical University (Technical Sciences)
- Vol. 1 (44) , 9-15
Open AccessSOME SPECIFICATIONS REGARDING TEMPERATURES ON HORIZON AIR TUYERES OF THE BLAST FURNACES
The purpose work is to clarify data on temperature changes on horizon air tuyeres of the blast furnaces. Shown that the common idea about similarity of changes in temperature and pressure of gases needs to be clarified. The difference is that the temperature gases in the direction to the centre of the furnace increases to the focus of combustion in front of the tuyeres, and pressure increases to the end of the tuyeres cavity. Accordingly, the temperature decreases starting from combustion focus, and pressure — starting from coke shell of tail part of the tuyeres cavity. The calculation gas temperature variation coefficients Vt based on the DonNDIchormet measurement data showed that Vt decreased from 8 to 3.5 % on average over a distance of 0.5 m as the distance from the tip of the tuyeres increased. This indicates that during peripheral operation of the furnaces, the zone in front of the tuyeres is the most critical in terms of temperature fluctuations. This phenomenon is explained by the characteristic features of the gas mechanics of the tuyere cavity — reduced gas pressure at the tuyere section and discrete deformation of the air-gas jet by coke collapse through dynamically unstable vaults of the tuyere cavity. It is shown that the blast furnace melting conditions determine the effectiveness and efficiency of the blast furnace process, as well as the possible level of reaching the theoretical combustion temperature.
- 1 January 2024
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Metal and Casting of Ukraine
- Vol. 32 (3-4)
Unstationary transient modes operation of blast furnaces in the start-up period after construction or reconstruction
The purpose of the presented work is to determine tasks and characteristic features of three periods transition of blast furnaces (BF) from start-up to stationary mode of the smelting, namely blowing, blowing and development of the furnace capacity. It is shown that task of the blowing period is the formation of primary zone of the cohesion and establishment of five-zone column structure of the charge inherent in the stationary mode of blast furnace melting. The task of adjacent blowing and development of the furnace power periods is to achieve the working level of gas blowing parameters – flow rate and blowing temperature together with increased pressure of gases in working space of the furnace. It is shown that completion of the blowing and beginning of the blowing periods is a forced reduction blowing flow rate as a result of the formation of a cohesion zone in column of charge and an increase in its resistance. Visually, the boundary of these periods is characterized by breaks in the curves of changes in furnace gas temperatures and CO and CO2 content over time – the temperature increases after break, and gas content stabilizes at certain levels. It was established that the recommendation to increase the blowing flow in the blowing period at a rate of 30–35 m3/h is not universal, as it does not take into account the dimensions of the blast furnace. It is shown that at the initial relative flow in the inflation period of 1.0 Vd / Vcor . min with an inflation rate of 35 m3/h, the duration of the blowing period of the 1033 m3 BF will be 1.2 days, and the 5000 m3 BF will last 6 days. That is, another well-known recommendation regarding the same duration of the inflation period of 5–6 days needs correction. The modern practice of construction and reconstruction of blast furnaces is aimed at the use of a ceramic glass in the furnace and bottom, therefore, based on the experience of far abroad, the duration of the blowing period can be shortened due to the period of melting of cast iron.Furnaces of large volume require an extended period of power development, in which the condition for each subsequent increase in gas pressure parameters is to maintain stability temperature regime of lining of the furnace, sump and bottom.
- 1 January 2024
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Metal and Casting of Ukraine
- Vol. 32 (3-4)
Unstationary transient modes operation of blast furnaces in the start-up period after construction or reconstruction
The purpose of the presented work is to determine tasks and characteristic features of three periods transition of blast furnaces (BF) from start-up to stationary mode of the smelting, namely blowing, blowing and development of the furnace capacity. It is shown that task of the blowing period is the formation of primary zone of the cohesion and establishment of five-zone column structure of the charge inherent in the stationary mode of blast furnace melting. The task of adjacent blowing and development of the furnace power periods is to achieve the working level of gas blowing parameters – flow rate and blowing temperature together with increased pressure of gases in working space of the furnace. It is shown that completion of the blowing and beginning of the blowing periods is a forced reduction blowing flow rate as a result of the formation of a cohesion zone in column of charge and an increase in its resistance. Visually, the boundary of these periods is characterized by breaks in the curves of changes in furnace gas temperatures and CO and CO2 content over time – the temperature increases after break, and gas content stabilizes at certain levels. It was established that the recommendation to increase the blowing flow in the blowing period at a rate of 30–35 m3/h is not universal, as it does not take into account the dimensions of the blast furnace. It is shown that at the initial relative flow in the inflation period of 1.0 Vd / Vcor . min with an inflation rate of 35 m3/h, the duration of the blowing period of the 1033 m3 BF will be 1.2 days, and the 5000 m3 BF will last 6 days. That is, another well-known recommendation regarding the same duration of the inflation period of 5–6 days needs correction. The modern practice of construction and reconstruction of blast furnaces is aimed at the use of a ceramic glass in the furnace and bottom, therefore, based on the experience of far abroad, the duration of the blowing period can be shortened due to the period of melting of cast iron.Furnaces of large volume require an extended period of power development, in which the condition for each subsequent increase in gas pressure parameters is to maintain stability temperature regime of lining of the furnace, sump and bottom.
- 1 January 2024
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Metal and Casting of Ukraine
- Vol. 32 (2)
The concept of axial movement of blast furnaces and temperature distribution on the horizon of air tuyeres
The purpose of the work is to clarify the data on temperature changes on the horizon of the air tuyeres of blast furnaces. The limitations associated with the implementation of the well-known concept of axial movement of blast furnaces in terms of temperature stabilization in the coke nozzle blast furnace are considered. Based on the comparison of the results of studies on the temperature distribution of coke and its fractional composition at level of air tuyeres, it is shown that on blast furnaces equipped with coneless filling devices and coal dust blowing units, the critical zone in the distribution of temperatures and their fluctuations in time is the intermediate zone between "bird's nest" and the center of the furnace. A temporary, but sufficiently long-term decrease in the temperature of coke to 1000 °C in the intermediate zone of modern blast furnaces is not accompanied by the danger of toterman formation, which is facilitated by the existence of an axial coke vent — a kind of heated core of the coke nozzle and sufficient thermal inertia of the furnace. It has been established that the increase in blowing costs affects distribution of coke temperatures on the horizon of air tuyeres in a similar way to the tendency of the hot strength of coke to deteriorate — the temperatures in the intermediate zone of the coke nozzle decrease. It is recommended to take into account the change in the quality of the loaded coke when choosing dimensions of the coke vent in the center of the furnace and the degree of forcing its course by blowing. In the conditions of using pulverized coal fuel, when working on coke of average quality, the most acceptable mode of organization of the radial gas flow is peripheral-axial with an advantage in the development of axial over peripheral. Despite some conventionality of the examples discussed in the article, it can be argued that a long axial stroke without stroke disturbances can be realized only if the intensity of the peripheral gas flow is maintained for specific conditions. That is, in an ideal form, axial movement of blast furnace melting is practically impossible.
- 1 January 2024
- Published by National Academy of Sciences of Ukraine (Co. LTD Ukrinformnauka) (Publications) in Metal and Casting of Ukraine
- Vol. 32 (2)
The concept of axial movement of blast furnaces and temperature distribution on the horizon of air tuyeres
The purpose of the work is to clarify the data on temperature changes on the horizon of the air tuyeres of blast furnaces. The limitations associated with the implementation of the well-known concept of axial movement of blast furnaces in terms of temperature stabilization in the coke nozzle blast furnace are considered. Based on the comparison of the results of studies on the temperature distribution of coke and its fractional composition at level of air tuyeres, it is shown that on blast furnaces equipped with coneless filling devices and coal dust blowing units, the critical zone in the distribution of temperatures and their fluctuations in time is the intermediate zone between "bird's nest" and the center of the furnace. A temporary, but sufficiently long-term decrease in the temperature of coke to 1000 °C in the intermediate zone of modern blast furnaces is not accompanied by the danger of toterman formation, which is facilitated by the existence of an axial coke vent — a kind of heated core of the coke nozzle and sufficient thermal inertia of the furnace. It has been established that the increase in blowing costs affects distribution of coke temperatures on the horizon of air tuyeres in a similar way to the tendency of the hot strength of coke to deteriorate — the temperatures in the intermediate zone of the coke nozzle decrease. It is recommended to take into account the change in the quality of the loaded coke when choosing dimensions of the coke vent in the center of the furnace and the degree of forcing its course by blowing. In the conditions of using pulverized coal fuel, when working on coke of average quality, the most acceptable mode of organization of the radial gas flow is peripheral-axial with an advantage in the development of axial over peripheral. Despite some conventionality of the examples discussed in the article, it can be argued that a long axial stroke without stroke disturbances can be realized only if the intensity of the peripheral gas flow is maintained for specific conditions. That is, in an ideal form, axial movement of blast furnace melting is practically impossible.