Muhammad Haseeb
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Muhammad Haseeb has a total of 32 co-authors. Here are the top co-authors by number of shared publications:
- Hong-Guo Zhang
College of Materials Science and Engineering, Key Laboratory of Advanced Functional Materials, Ministry of Education of China, Beijing University of Technology 1 , Beijing 100124
2 shared publications Hongguo Zhang
2 shared publicationsJunhua Xi
2 shared publicationsMing Yue
2 shared publications- Ming Yue
Beijing University of Technology
2 shared publications Weiqiang Liu
2 shared publications
Latest Publications
- 17 October 2025
- Published by Elsevier in Materials Today Communications
- Vol. 49
Tuning magnetic properties of SrFe12O19 through La–Co substitution: Site-resolved DFT and experimental insights
- 17 October 2025
- Published by Elsevier in Materials Today Communications
- Vol. 49
Tuning magnetic properties of SrFe12O19 through La–Co substitution: Site-resolved DFT and experimental insights
- Open Access
- 1 March 2025
- Published by AIP Publishing in AIP Advances
- Vol. 15 (3)
Effect of initial mixing process and calcination temperature on magnetic properties of La–Ca–Co doped strontium ferrite
This study investigates the significant correlation between preparation techniques, calcination temperatures, and the magnetic properties of La–Ca–Co-doped strontium ferrite. By comparing typical dry mixing and wet mixing processes and investigating the effects of different calcination temperatures, this work reveals detailed insights into how to optimize the magnetic performance of these materials. Results show that dry mixing at 1260 °C produces the largest magnetic energy product (35.4 kJ/m3) when sintered at 1225 °C, with a maximum remanence of 437 mT and coercivity of 384 kA/m. Conversely, wet mixing at 1230 °C produces the optimal magnetic performance as a coercivity of 415 kA/m, remanence of 435 mT and (BH)max of 33.4 kJ m−3 at a sintering temperature of 1215 °C. Wet mixing is better for low-temperature calcination due to reduced particle size, greater specific surface area, and lower energy needs. The dry mixing technique at 1260 °C and the wet mixing process at 1230 °C yield good magnetic characteristics for La–Ca–Co doped strontium ferrite. The importance of calcination temperatures and preparation methods on the magnetic properties of doped ferrite is highlighted in this research.
- 1 March 2025
- Published by AIP Publishing in AIP Advances
- Vol. 15 (3)
Open AccessEffect of initial mixing process and calcination temperature on magnetic properties of La–Ca–Co doped strontium ferrite
This study investigates the significant correlation between preparation techniques, calcination temperatures, and the magnetic properties of La–Ca–Co-doped strontium ferrite. By comparing typical dry mixing and wet mixing processes and investigating the effects of different calcination temperatures, this work reveals detailed insights into how to optimize the magnetic performance of these materials. Results show that dry mixing at 1260 °C produces the largest magnetic energy product (35.4 kJ/m3) when sintered at 1225 °C, with a maximum remanence of 437 mT and coercivity of 384 kA/m. Conversely, wet mixing at 1230 °C produces the optimal magnetic performance as a coercivity of 415 kA/m, remanence of 435 mT and (BH)max of 33.4 kJ m−3 at a sintering temperature of 1215 °C. Wet mixing is better for low-temperature calcination due to reduced particle size, greater specific surface area, and lower energy needs. The dry mixing technique at 1260 °C and the wet mixing process at 1230 °C yield good magnetic characteristics for La–Ca–Co doped strontium ferrite. The importance of calcination temperatures and preparation methods on the magnetic properties of doped ferrite is highlighted in this research.
- Open Access
- 1 February 2024
- Published by AIP Publishing in AIP Advances
- Vol. 14 (2)
Sintering temperature optimization for enhanced magnetic performance in La–Ca–Co doped strontium ferrite
The effectiveness of employing La-Ca-Co co-doping has been demonstrated as the optimal approach for enhancing the magnetic performance of strontium ferrite. However, limited studies have explored the evolution of the magnetoplumbite phase and its correlation with the sintering temperature. In our research, La-Ca-Co doped strontium ferrite permanent magnets were fabricated using a conventional ceramic process and a two-step sintering technique. After sintering at different temperatures, all the samples possess proper c-axis orientation. When the sintering temperature was raised from 1175 °C to 1205 °C, there was an upward trend observed in the remanence Br, increasing from 430 mT to 439 mT. The coercivity Hcj exhibited an increase from 380 kA/m and reached its peak at 397 kA/m at 1185 °C. Although the Br value remained favorable, the coercivity experienced substantial deterioration, reaching its lowest point at 303 kA/m at 1205 °C. Under a sintering temperature of 1195 oC, magnetic performance with optimal energy product was achieved, with Br of 439 mT, Hcj of 379 kA/m, Hcb of 318 kA/m, and (BH)max of 35.5 kJm-3.
- 1 February 2024
- Published by AIP Publishing in AIP Advances
- Vol. 14 (2)
Open AccessSintering temperature optimization for enhanced magnetic performance in La–Ca–Co doped strontium ferrite
The effectiveness of employing La-Ca-Co co-doping has been demonstrated as the optimal approach for enhancing the magnetic performance of strontium ferrite. However, limited studies have explored the evolution of the magnetoplumbite phase and its correlation with the sintering temperature. In our research, La-Ca-Co doped strontium ferrite permanent magnets were fabricated using a conventional ceramic process and a two-step sintering technique. After sintering at different temperatures, all the samples possess proper c-axis orientation. When the sintering temperature was raised from 1175 °C to 1205 °C, there was an upward trend observed in the remanence Br, increasing from 430 mT to 439 mT. The coercivity Hcj exhibited an increase from 380 kA/m and reached its peak at 397 kA/m at 1185 °C. Although the Br value remained favorable, the coercivity experienced substantial deterioration, reaching its lowest point at 303 kA/m at 1205 °C. Under a sintering temperature of 1195 oC, magnetic performance with optimal energy product was achieved, with Br of 439 mT, Hcj of 379 kA/m, Hcb of 318 kA/m, and (BH)max of 35.5 kJm-3.
- 29 October 2023
- Published by Elsevier in Journal of Rare Earths
- Vol. 42 (11) , 2105-2111
Synthesis of size-controlled and dispersible Sm2Fe17N3 magnetic particles by reduction diffusion process using molten salt
- 29 October 2023
- Published by Elsevier in Journal of Rare Earths
- Vol. 42 (11) , 2105-2111
Synthesis of size-controlled and dispersible Sm2Fe17N3 magnetic particles by reduction diffusion process using molten salt
- Open Access
- 1 April 2020
- Published by IOP Publishing in Materials Research Express
- Vol. 7 (4) , 046107
Magnetic performance enhancement in La-Ca-Co doped SrFe12O19 ferrite permanent magnets via cold isostatic pressing
The crystallographic alignment, microstructure and magnetic properties were studied for La0.6Ca0.6Sr0.1Fe12.4Co0.4O19 ferrite permanent magnets prepared with standard ceramic method. The effect of cold isostatic pressing (CIP) and sintering temperature on the structural and magnetic properties of the magnets were investigated. The CIP significantly improves the density of the green compact and final magnets, but undermines the crystallographic alignment of the magnets simultaneously. As a result, the remanence of the magnet achieves optimal value under the compromise between the increased density and the degraded alignment. Moreover, the coercivity of the magnet increases linearly with the increment of the CIP pressure due the fact that CIP processed samples bear more uniform and finer grains in favor of high coercivity. Under optimal CIP pressure and sintering temperature, the magnet obtains best magnetic properties of Br of 0.439 T, Hcj of 396 kA m−1, Hcb of 311 kA m−1, and (BH)maxof 35.8 kJ m−3.
- 1 April 2020
- Published by IOP Publishing in Materials Research Express
- Vol. 7 (4) , 046107
Open AccessMagnetic performance enhancement in La-Ca-Co doped SrFe12O19 ferrite permanent magnets via cold isostatic pressing
The crystallographic alignment, microstructure and magnetic properties were studied for La0.6Ca0.6Sr0.1Fe12.4Co0.4O19 ferrite permanent magnets prepared with standard ceramic method. The effect of cold isostatic pressing (CIP) and sintering temperature on the structural and magnetic properties of the magnets were investigated. The CIP significantly improves the density of the green compact and final magnets, but undermines the crystallographic alignment of the magnets simultaneously. As a result, the remanence of the magnet achieves optimal value under the compromise between the increased density and the degraded alignment. Moreover, the coercivity of the magnet increases linearly with the increment of the CIP pressure due the fact that CIP processed samples bear more uniform and finer grains in favor of high coercivity. Under optimal CIP pressure and sintering temperature, the magnet obtains best magnetic properties of Br of 0.439 T, Hcj of 396 kA m−1, Hcb of 311 kA m−1, and (BH)maxof 35.8 kJ m−3.