Yan Li
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Yan Li has a total of 11 co-authors. Here are the top co-authors by number of shared publications:
- Cuirong Liu
School of Material Science and Engineering, Taiyuan University of Science and Technology, 66 Waliu Road, Taiyuan 030024, China
2 shared publications - Dezhi Yang
School of Material Science and Engineering, Taiyuan University of Science and Technology, 66 Waliu Road, Taiyuan 030024, China
2 shared publications - Wenyu Yang
School of Material Science and Engineering, Taiyuan University of Science and Technology, 66 Waliu Road, Taiyuan 030024, China
2 shared publications - Zhisheng Wu
School of Materials Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030024, China
2 shared publications Cuirong Liu
Instrumental Analysis Center, School of Material Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030024, P. R. China
1 shared publication- Dengkui Zhang
School of Materials Science and Engineering, Taiyuan University of Science and Technology, Taiyuan, China
1 shared publication
Latest Publications
- Open Access
Effect of Annealing Temperature on Microstructure and Properties of Al/Mg Magnetic Pulse Welding Joints
In this investigation, 1060Al/AZ31B welded joints were obtained by magnetic pulse welding technique. In order to test the microstructure and mechanical properties of the joints, the welded joints were annealed at different temperatures and then examined by optical microscopy (OM), scanning electron microscopy (SEM), energy spectrum analysis (EDS) and mechanical properties testing. The testing results of the welded joints annealed at different temperatures showed that the Al-Mg MPW welded joints were well bonded. The changing of the microstructure and mechanical properties of Al/Mg welded joints was not apparent under the temperature of 200 °C. However, Al12Mg17 intermetallic compound layer formed at 200 °C. Al12Mg17 and Al3Mg2 intermetallic compound layers formed at the temperature of 300 °C. The diffusion rate of Mg and Al elements is proportional to the annealing temperature and the intermetallic compounds layer is gradually formed. The microhardness near the interface decreased first and then increased on account of the brittleness of intermetallic compounds. In the tensile shear tests, the fracture mechanism of Al/Mg MPW welded joints were analyzed. When the temperature was lower than 200 °C the joints did not crack. At 200 °C and 250 °C, the joints fracture along the Al12Mg17-Al interface. The joint cracks along the interface of Al12Mg17-Al3Mg2 at the temperature of 300 °C.
Open AccessEffect of Annealing Temperature on Microstructure and Properties of Al/Mg Magnetic Pulse Welding Joints
In this investigation, 1060Al/AZ31B welded joints were obtained by magnetic pulse welding technique. In order to test the microstructure and mechanical properties of the joints, the welded joints were annealed at different temperatures and then examined by optical microscopy (OM), scanning electron microscopy (SEM), energy spectrum analysis (EDS) and mechanical properties testing. The testing results of the welded joints annealed at different temperatures showed that the Al-Mg MPW welded joints were well bonded. The changing of the microstructure and mechanical properties of Al/Mg welded joints was not apparent under the temperature of 200 °C. However, Al12Mg17 intermetallic compound layer formed at 200 °C. Al12Mg17 and Al3Mg2 intermetallic compound layers formed at the temperature of 300 °C. The diffusion rate of Mg and Al elements is proportional to the annealing temperature and the intermetallic compounds layer is gradually formed. The microhardness near the interface decreased first and then increased on account of the brittleness of intermetallic compounds. In the tensile shear tests, the fracture mechanism of Al/Mg MPW welded joints were analyzed. When the temperature was lower than 200 °C the joints did not crack. At 200 °C and 250 °C, the joints fracture along the Al12Mg17-Al interface. The joint cracks along the interface of Al12Mg17-Al3Mg2 at the temperature of 300 °C.
- Open Access
Multiphysics Numerical Simulation of the Transient Forming Mechanism of Magnetic Pulse Welding
Magnetic pulse welding (MPW) is widely used in the connection of dissimilar metals. The welding process involves the coupling of the electromagnetic field and structural field, which is a high-energy transient forming process. Based on the current experimental methods, it is difficult to capture the relevant data in the process of magnetic pulse welding, and the transient forming mechanism of magnetic pulse welding needs to be further studied. Taking the magnetic pulse welding of an Al-Mg sheet as an example, based on the Ansoft Maxwell and ANSYS finite element simulation platform, the loose coupling method was used to analyze an electromagnetic field generated by the discharging capacitor bank and structural field of the Al-Mg sheet under the action of electromagnetic force. The discharge period of the magnetic pulse welding capacitor bank was 62 μs. The current direction in the aluminum sheet changed once half a cycle, and the direction of the electromagnetic force was always consistent with the Z-axis. Under the skin effect, the magnetic induction intensity on the lower surface of the aluminum sheet was the largest. At 16 μs, the induced current, electromagnetic force and magnetic induction intensity in the aluminum sheet reached the peak values, which were 7.89 A/m2, 4.58 N/m3 and 12.6 T, respectively. The maximum electromagnetic force and velocity in the structural field were 2400 KN and 300 m/s. The structure field simulation reproduces the transient forming process of magnetic pulse welding, and clarifies the formation mechanism of the “intermediate zone rebound uncomposite zone-welding bonding zone-unbound zone”. Based on the numerical simulation technology, the research on the transient forming mechanism of magnetic pulse welding under multiphysics simulations can promote the development and application of magnetic pulse welding technology and better guide engineering practices.
Open AccessMultiphysics Numerical Simulation of the Transient Forming Mechanism of Magnetic Pulse Welding
Magnetic pulse welding (MPW) is widely used in the connection of dissimilar metals. The welding process involves the coupling of the electromagnetic field and structural field, which is a high-energy transient forming process. Based on the current experimental methods, it is difficult to capture the relevant data in the process of magnetic pulse welding, and the transient forming mechanism of magnetic pulse welding needs to be further studied. Taking the magnetic pulse welding of an Al-Mg sheet as an example, based on the Ansoft Maxwell and ANSYS finite element simulation platform, the loose coupling method was used to analyze an electromagnetic field generated by the discharging capacitor bank and structural field of the Al-Mg sheet under the action of electromagnetic force. The discharge period of the magnetic pulse welding capacitor bank was 62 μs. The current direction in the aluminum sheet changed once half a cycle, and the direction of the electromagnetic force was always consistent with the Z-axis. Under the skin effect, the magnetic induction intensity on the lower surface of the aluminum sheet was the largest. At 16 μs, the induced current, electromagnetic force and magnetic induction intensity in the aluminum sheet reached the peak values, which were 7.89 A/m2, 4.58 N/m3 and 12.6 T, respectively. The maximum electromagnetic force and velocity in the structural field were 2400 KN and 300 m/s. The structure field simulation reproduces the transient forming process of magnetic pulse welding, and clarifies the formation mechanism of the “intermediate zone rebound uncomposite zone-welding bonding zone-unbound zone”. Based on the numerical simulation technology, the research on the transient forming mechanism of magnetic pulse welding under multiphysics simulations can promote the development and application of magnetic pulse welding technology and better guide engineering practices.
- Open Access
Effects of the Substitution of 20% Nd for La or Doping with 20% C on the Magnetic Properties and Magnetocaloric Effect in LaFe11.5Si1.5 Compound
The effects of element substitution and element doping on the magnetic properties and magnetocaloric effect of the LaFe11.5Si1.5 compound were investigated. The crystals of the LaFe11.5Si1.5, La0.8Nd0.2Fe11.5Si1.5, and LaFe11.5Si1.5C0.2 compounds all showed cubic NaZn13-type structures, but the lattice of the La0.8Nd0.2Fe11.5Si1.5 shrank and the lattice of the LaFe11.5Si1.5C0.2 expanded. All three compounds had the characteristic of first-order magnetic transition due to the obvious itinerant-electron metamagnetic (IEM) transition occurring above Curie temperature (TC). For the LaFe11.5Si1.5, La0.8Nd0.2Fe11.5Si1.5, and LaFe11.5Si1.5C0.2 compounds, the TC were approximately 194 K, 188 K, and 232 K, respectively. Meanwhile, the maximum magnetic entropy changes (−ΔSM) under a magnetic field change of 0–3 T were approximately 18.7 J/kg·K, 22.8 J/kg·K, and 16.4 J/kg·K, respectively. The TC was mainly affected by the lattice constant. Furthermore, the −ΔSM was mainly affected by the latent heat of the first-order magnetic transition.
Open AccessEffects of the Substitution of 20% Nd for La or Doping with 20% C on the Magnetic Properties and Magnetocaloric Effect in LaFe11.5Si1.5 Compound
The effects of element substitution and element doping on the magnetic properties and magnetocaloric effect of the LaFe11.5Si1.5 compound were investigated. The crystals of the LaFe11.5Si1.5, La0.8Nd0.2Fe11.5Si1.5, and LaFe11.5Si1.5C0.2 compounds all showed cubic NaZn13-type structures, but the lattice of the La0.8Nd0.2Fe11.5Si1.5 shrank and the lattice of the LaFe11.5Si1.5C0.2 expanded. All three compounds had the characteristic of first-order magnetic transition due to the obvious itinerant-electron metamagnetic (IEM) transition occurring above Curie temperature (TC). For the LaFe11.5Si1.5, La0.8Nd0.2Fe11.5Si1.5, and LaFe11.5Si1.5C0.2 compounds, the TC were approximately 194 K, 188 K, and 232 K, respectively. Meanwhile, the maximum magnetic entropy changes (−ΔSM) under a magnetic field change of 0–3 T were approximately 18.7 J/kg·K, 22.8 J/kg·K, and 16.4 J/kg·K, respectively. The TC was mainly affected by the lattice constant. Furthermore, the −ΔSM was mainly affected by the latent heat of the first-order magnetic transition.
- 20 April 2020
- Published by American Chemical Society (ACS) in The Journal of Physical Chemistry C
- Vol. 124 (19) , 10530-10540
TiO2 Ultrathin Coating of SBA-15/Au by Atomic Layer Deposition for Enhanced Catalytic Performance in Epoxidation of Styrene
Metal-oxide interfaces play an important role in heterogeneous catalysis. However, the inherent ultrahigh aspect ratios of nanoporous catalytic system severely limit the precise coating of the porous inner surfaces to engineer the metal-oxide interfaces. Herein, atomic layer deposition (ALD) was used to deposit different thickness (cycle numbers) of TiO2 from sub-monolayer to multi-layers into a porous catalyst (SBA-15/Au) to maximize the Au-TiO2 interfaces. The catalytic activity of the optimized TiO2 coating sample is nearly 4 times higher than that of SBA-15/Au for styrene epoxidation. Moreover, the activity as a function of the cycle numbers of ALD TiO2 shows a volcano-like behavior, indicating that only the optimized interfaces of the porous catalyst can result in the maximized activity. This result demonstrates the superiority of the ALD ultrathin coating to improve the catalytic performance of nanoporous catalysts.
- 20 April 2020
- Published by American Chemical Society (ACS) in The Journal of Physical Chemistry C
- Vol. 124 (19) , 10530-10540
TiO2 Ultrathin Coating of SBA-15/Au by Atomic Layer Deposition for Enhanced Catalytic Performance in Epoxidation of Styrene
Metal-oxide interfaces play an important role in heterogeneous catalysis. However, the inherent ultrahigh aspect ratios of nanoporous catalytic system severely limit the precise coating of the porous inner surfaces to engineer the metal-oxide interfaces. Herein, atomic layer deposition (ALD) was used to deposit different thickness (cycle numbers) of TiO2 from sub-monolayer to multi-layers into a porous catalyst (SBA-15/Au) to maximize the Au-TiO2 interfaces. The catalytic activity of the optimized TiO2 coating sample is nearly 4 times higher than that of SBA-15/Au for styrene epoxidation. Moreover, the activity as a function of the cycle numbers of ALD TiO2 shows a volcano-like behavior, indicating that only the optimized interfaces of the porous catalyst can result in the maximized activity. This result demonstrates the superiority of the ALD ultrathin coating to improve the catalytic performance of nanoporous catalysts.