Zhisheng Wu
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Previous Organizations / Institutes
The organizations / institutes from the scholar's other articles in the past ten years
Research Subjects
Zhisheng Wu has a total of 13 co-authors. Here are the top co-authors by number of shared publications:
- Cuirong Liu
School of Material Science and Engineering, Taiyuan University of Science and Technology, 66 Waliu Road, Taiyuan 030024, China
2 shared publications - Dezhi Yang
School of Material Science and Engineering, Taiyuan University of Science and Technology, 66 Waliu Road, Taiyuan 030024, China
2 shared publications - Ting Wang
State Key Laboratory of Advanced Welding and Joining, Harbin Institute of Technology at Weihai, Weihai 264209, China
2 shared publications - Wenyu Yang
School of Material Science and Engineering, Taiyuan University of Science and Technology, 66 Waliu Road, Taiyuan 030024, China
2 shared publications - Yan Li
School of Material Science and Engineering, Taiyuan University of Science and Technology, 66 Waliu Road, Taiyuan 030024, China
2 shared publications - Cuirong Liu
School of Materials Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030024, China
1 shared publication
Latest Publications
- 4 July 2024
- Published by Springer Nature in Journal of Materials Science
- Vol. 59 (28) , 13234-13250
Mechanical properties and corrosion resistance of TC4 titanium alloy joints by plasma arc welding + gas tungsten arc welding combination welding
- 4 July 2024
- Published by Springer Nature in Journal of Materials Science
- Vol. 59 (28) , 13234-13250
Mechanical properties and corrosion resistance of TC4 titanium alloy joints by plasma arc welding + gas tungsten arc welding combination welding
- Open Access
Effect of Heat Treatment Processes on the Microstructure and Mechanical Properties of High-Strength Aluminum Alloy Deposited Layers Processed by Fused Arc Additive Manufacturing
In this study, 7075 aluminum alloy welding wire with TiB2 nanoparticle reinforcement as an additive together with the variable polarity TIG welding arc as a heat source were applied to produce thin-walled deposited layer samples. Results indicated that the performance of the deposited structure of 7075 aluminum alloy with a TiB2 reinforcement phase was significantly improved compared to the deposited structure of ordinary 7075 aluminum alloy welding wire. Meanwhile, the precipitation of the TiB2 reinforcement phase was insufficient within the structure, and the enhancing effect could not be fully exerted. Moreover, the 7-series aluminum alloy contained a large amount of Zn and Mg elements inside. If the soluble crystalline phase was not fully dissolved, severe stress corrosion could be caused, which inevitably led to a decrease in the mechanical properties. To further improve the performance of the deposited layer, a T6 heat treatment process was performed at 470 °C for 2 h, followed by rapid cooling with distilled water and artificial aging at 120 °C for 24 h. After heat treatment, many second phases appeared in the microstructure of the deposited layer, and the tensile strength increased from (361.8 ± 4.8) MPa to (510.2 ± 5.4) MPa together with the elongation which increased from (9.5 ± 0.5) % to (10.2 ± 0.4) %. The fracture mode of the fracture was a ductile fracture along grain boundaries. The microhardness increased from (145 ± 5) HV to (190 ± 4) HV and exhibited good corrosion resistance in a 3.5% NaCl solution corrosion test.
Open AccessEffect of Heat Treatment Processes on the Microstructure and Mechanical Properties of High-Strength Aluminum Alloy Deposited Layers Processed by Fused Arc Additive Manufacturing
In this study, 7075 aluminum alloy welding wire with TiB2 nanoparticle reinforcement as an additive together with the variable polarity TIG welding arc as a heat source were applied to produce thin-walled deposited layer samples. Results indicated that the performance of the deposited structure of 7075 aluminum alloy with a TiB2 reinforcement phase was significantly improved compared to the deposited structure of ordinary 7075 aluminum alloy welding wire. Meanwhile, the precipitation of the TiB2 reinforcement phase was insufficient within the structure, and the enhancing effect could not be fully exerted. Moreover, the 7-series aluminum alloy contained a large amount of Zn and Mg elements inside. If the soluble crystalline phase was not fully dissolved, severe stress corrosion could be caused, which inevitably led to a decrease in the mechanical properties. To further improve the performance of the deposited layer, a T6 heat treatment process was performed at 470 °C for 2 h, followed by rapid cooling with distilled water and artificial aging at 120 °C for 24 h. After heat treatment, many second phases appeared in the microstructure of the deposited layer, and the tensile strength increased from (361.8 ± 4.8) MPa to (510.2 ± 5.4) MPa together with the elongation which increased from (9.5 ± 0.5) % to (10.2 ± 0.4) %. The fracture mode of the fracture was a ductile fracture along grain boundaries. The microhardness increased from (145 ± 5) HV to (190 ± 4) HV and exhibited good corrosion resistance in a 3.5% NaCl solution corrosion test.
- Open Access
Effects of SiC Content on Wear Resistance of Al-Zn-Mg-Cu Matrix Composites Fabricated via Laser Powder Bed Fusion
In this paper, in situ SiC-reinforced Al-Zn-Mg-Cu composites were fabricated by laser powder bed fusion (LPBF). The effects of SiC content on the microstructure, phase composition, microhardness, and wear resistance of as-printed composites were preliminarily investigated. Results show that the microstructure was regulated, the matrix grains were refined, and the tendency to orientation grain growth was suppressed. SiC particles reacted in situ with the Al matrix to produce Si, Al4C3, and Al4SiC4 phases. The microhardness and wear resistance of as-printed composites increased with SiC content due to the fine grain strengthening of the matrix and the second phase strengthening of precipitates and reinforcements.
Open AccessEffects of SiC Content on Wear Resistance of Al-Zn-Mg-Cu Matrix Composites Fabricated via Laser Powder Bed Fusion
In this paper, in situ SiC-reinforced Al-Zn-Mg-Cu composites were fabricated by laser powder bed fusion (LPBF). The effects of SiC content on the microstructure, phase composition, microhardness, and wear resistance of as-printed composites were preliminarily investigated. Results show that the microstructure was regulated, the matrix grains were refined, and the tendency to orientation grain growth was suppressed. SiC particles reacted in situ with the Al matrix to produce Si, Al4C3, and Al4SiC4 phases. The microhardness and wear resistance of as-printed composites increased with SiC content due to the fine grain strengthening of the matrix and the second phase strengthening of precipitates and reinforcements.
- Open Access
Effect of Annealing Temperature on Microstructure and Properties of Al/Mg Magnetic Pulse Welding Joints
In this investigation, 1060Al/AZ31B welded joints were obtained by magnetic pulse welding technique. In order to test the microstructure and mechanical properties of the joints, the welded joints were annealed at different temperatures and then examined by optical microscopy (OM), scanning electron microscopy (SEM), energy spectrum analysis (EDS) and mechanical properties testing. The testing results of the welded joints annealed at different temperatures showed that the Al-Mg MPW welded joints were well bonded. The changing of the microstructure and mechanical properties of Al/Mg welded joints was not apparent under the temperature of 200 °C. However, Al12Mg17 intermetallic compound layer formed at 200 °C. Al12Mg17 and Al3Mg2 intermetallic compound layers formed at the temperature of 300 °C. The diffusion rate of Mg and Al elements is proportional to the annealing temperature and the intermetallic compounds layer is gradually formed. The microhardness near the interface decreased first and then increased on account of the brittleness of intermetallic compounds. In the tensile shear tests, the fracture mechanism of Al/Mg MPW welded joints were analyzed. When the temperature was lower than 200 °C the joints did not crack. At 200 °C and 250 °C, the joints fracture along the Al12Mg17-Al interface. The joint cracks along the interface of Al12Mg17-Al3Mg2 at the temperature of 300 °C.
Open AccessEffect of Annealing Temperature on Microstructure and Properties of Al/Mg Magnetic Pulse Welding Joints
In this investigation, 1060Al/AZ31B welded joints were obtained by magnetic pulse welding technique. In order to test the microstructure and mechanical properties of the joints, the welded joints were annealed at different temperatures and then examined by optical microscopy (OM), scanning electron microscopy (SEM), energy spectrum analysis (EDS) and mechanical properties testing. The testing results of the welded joints annealed at different temperatures showed that the Al-Mg MPW welded joints were well bonded. The changing of the microstructure and mechanical properties of Al/Mg welded joints was not apparent under the temperature of 200 °C. However, Al12Mg17 intermetallic compound layer formed at 200 °C. Al12Mg17 and Al3Mg2 intermetallic compound layers formed at the temperature of 300 °C. The diffusion rate of Mg and Al elements is proportional to the annealing temperature and the intermetallic compounds layer is gradually formed. The microhardness near the interface decreased first and then increased on account of the brittleness of intermetallic compounds. In the tensile shear tests, the fracture mechanism of Al/Mg MPW welded joints were analyzed. When the temperature was lower than 200 °C the joints did not crack. At 200 °C and 250 °C, the joints fracture along the Al12Mg17-Al interface. The joint cracks along the interface of Al12Mg17-Al3Mg2 at the temperature of 300 °C.
- Open Access
Multiphysics Numerical Simulation of the Transient Forming Mechanism of Magnetic Pulse Welding
Magnetic pulse welding (MPW) is widely used in the connection of dissimilar metals. The welding process involves the coupling of the electromagnetic field and structural field, which is a high-energy transient forming process. Based on the current experimental methods, it is difficult to capture the relevant data in the process of magnetic pulse welding, and the transient forming mechanism of magnetic pulse welding needs to be further studied. Taking the magnetic pulse welding of an Al-Mg sheet as an example, based on the Ansoft Maxwell and ANSYS finite element simulation platform, the loose coupling method was used to analyze an electromagnetic field generated by the discharging capacitor bank and structural field of the Al-Mg sheet under the action of electromagnetic force. The discharge period of the magnetic pulse welding capacitor bank was 62 μs. The current direction in the aluminum sheet changed once half a cycle, and the direction of the electromagnetic force was always consistent with the Z-axis. Under the skin effect, the magnetic induction intensity on the lower surface of the aluminum sheet was the largest. At 16 μs, the induced current, electromagnetic force and magnetic induction intensity in the aluminum sheet reached the peak values, which were 7.89 A/m2, 4.58 N/m3 and 12.6 T, respectively. The maximum electromagnetic force and velocity in the structural field were 2400 KN and 300 m/s. The structure field simulation reproduces the transient forming process of magnetic pulse welding, and clarifies the formation mechanism of the “intermediate zone rebound uncomposite zone-welding bonding zone-unbound zone”. Based on the numerical simulation technology, the research on the transient forming mechanism of magnetic pulse welding under multiphysics simulations can promote the development and application of magnetic pulse welding technology and better guide engineering practices.
Open AccessMultiphysics Numerical Simulation of the Transient Forming Mechanism of Magnetic Pulse Welding
Magnetic pulse welding (MPW) is widely used in the connection of dissimilar metals. The welding process involves the coupling of the electromagnetic field and structural field, which is a high-energy transient forming process. Based on the current experimental methods, it is difficult to capture the relevant data in the process of magnetic pulse welding, and the transient forming mechanism of magnetic pulse welding needs to be further studied. Taking the magnetic pulse welding of an Al-Mg sheet as an example, based on the Ansoft Maxwell and ANSYS finite element simulation platform, the loose coupling method was used to analyze an electromagnetic field generated by the discharging capacitor bank and structural field of the Al-Mg sheet under the action of electromagnetic force. The discharge period of the magnetic pulse welding capacitor bank was 62 μs. The current direction in the aluminum sheet changed once half a cycle, and the direction of the electromagnetic force was always consistent with the Z-axis. Under the skin effect, the magnetic induction intensity on the lower surface of the aluminum sheet was the largest. At 16 μs, the induced current, electromagnetic force and magnetic induction intensity in the aluminum sheet reached the peak values, which were 7.89 A/m2, 4.58 N/m3 and 12.6 T, respectively. The maximum electromagnetic force and velocity in the structural field were 2400 KN and 300 m/s. The structure field simulation reproduces the transient forming process of magnetic pulse welding, and clarifies the formation mechanism of the “intermediate zone rebound uncomposite zone-welding bonding zone-unbound zone”. Based on the numerical simulation technology, the research on the transient forming mechanism of magnetic pulse welding under multiphysics simulations can promote the development and application of magnetic pulse welding technology and better guide engineering practices.