K. E. Smetanina
Current Organizations / Institutes
The organizations/institutes from the scholar's latest article
Research Subjects
Research Interests
K. E. Smetanina has a total of 14 co-authors. Here are the top co-authors by number of shared publications:
- Aleksey Vladimirovich Nokhrin
National Research Lobachevsky State University of Nizhny Novgorod, Nizhny Novgorod, Russia
3 shared publications - Eugeniy A. Lantsev
Materials Science Department, Physico-Technical Research Institure, Lobachevsky State University of Nizhny Novgorod, 603022 Nizhny Novgorod, Russia
3 shared publications - Maksim Sergeevich Boldin
National Research Lobachevsky State University of Nizhny Novgorod, Nizhny Novgorod, Russia
3 shared publications - Pavel V. Andreev
Lobachevsky State University of Nizhny Novgorod, Nizhny Novgorod, Russia
3 shared publications - Yuriy V Blagoveshchenskiy
Baikov Institute of Metallurgy and Materials Science, Russian Academy of Sciences, Moscow, Russia
3 shared publications - Nataliya Malekhonova
National Research Lobachevsky State University of Nizhny Novgorod, Nizhny Novgorod, Russia
2 shared publications
Latest Publications
- 1 May 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 12 (3) , 650-663
Investigation of Aspects of High-Speed Sintering of Plasma-Chemical Nanopowders of Tungsten Carbide with Higher Content of Oxygen
The special aspects of spark plasma sintering (SPS) of plasma-chemical nanopowders of tungsten carbide with higher oxygen content were investigated. It was demonstrated that shrinkage rate of the WC nanopowders during SPS is limited by the rate of grain-boundary diffusion with the abnormally low values of activation energy. Decrease in the activation energy of SPS is caused by the influence of oxygen on the diffusion permeability of boundaries of the tungsten carbide grains at the stage of intense densification, as well as by abnormal grain growth. Kinetics of SPS of the WC-W2C-WO3-W nanopowder compositions at the stage of severe densification is controlled by the rate of sticking together the oxide particles, with their simultaneous transformation into W2C particles, and then by the plastic flow of W2C particles in the presence of the tungsten particles at the stage of high-temperature sintering. Ceramics with a high density ratio (98–99%) and ultra-fine-grained structure (the mean grain size less than 0.3 μm) with higher hardness HV = 30.5 GPa and fracture toughness of ~6.5 MPa m1/2 were obtained using the SPS method.
- 1 May 2021
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 12 (3) , 650-663
Investigation of Aspects of High-Speed Sintering of Plasma-Chemical Nanopowders of Tungsten Carbide with Higher Content of Oxygen
The special aspects of spark plasma sintering (SPS) of plasma-chemical nanopowders of tungsten carbide with higher oxygen content were investigated. It was demonstrated that shrinkage rate of the WC nanopowders during SPS is limited by the rate of grain-boundary diffusion with the abnormally low values of activation energy. Decrease in the activation energy of SPS is caused by the influence of oxygen on the diffusion permeability of boundaries of the tungsten carbide grains at the stage of intense densification, as well as by abnormal grain growth. Kinetics of SPS of the WC-W2C-WO3-W nanopowder compositions at the stage of severe densification is controlled by the rate of sticking together the oxide particles, with their simultaneous transformation into W2C particles, and then by the plastic flow of W2C particles in the presence of the tungsten particles at the stage of high-temperature sintering. Ceramics with a high density ratio (98–99%) and ultra-fine-grained structure (the mean grain size less than 0.3 μm) with higher hardness HV = 30.5 GPa and fracture toughness of ~6.5 MPa m1/2 were obtained using the SPS method.
- 1 May 2020
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 11 (3) , 586-597
Kinetics of Spark Plasma Sintering of WC–10% Co Ultrafine-Grained Hard Alloy
The effect of the carbon content on the kinetics of spark plasma sintering of nanopowder and submicron powder of WC–10% Co compositions was studied. Free carbon in the graphite form was introduced into nanopowders and submicron powders by mixing. The activation energy of solid-phase sintering at isothermal holding and continuous heating was determined. It is shown that increase in the carbon content leads to decrease in the volume fraction of the η phase and shift of the shrinkage curve into the region of low temperatures. It is established that an increase in the carbon content does not have a significant effect on the sintering activation energy of nanopowders and submicron powders in the region of “average” heating temperatures, the value of which is close to the activation energy of grain boundary diffusion in cobalt. It is shown that an increase in the carbon content leads to a significant decrease in the activation energy of consolidation of WC–Co powders in the region of “high” sintering temperatures owing to a decrease in the concentration of tungsten atoms in the γ phase based on cobalt. The sintering kinetics of fine-grained WC–Co alloys is limited by the rate of Coble diffusion creep of cobalt.
- 1 May 2020
- Published by Pleiades Publishing Ltd in Inorganic Materials: Applied Research
- Vol. 11 (3) , 586-597
Kinetics of Spark Plasma Sintering of WC–10% Co Ultrafine-Grained Hard Alloy
The effect of the carbon content on the kinetics of spark plasma sintering of nanopowder and submicron powder of WC–10% Co compositions was studied. Free carbon in the graphite form was introduced into nanopowders and submicron powders by mixing. The activation energy of solid-phase sintering at isothermal holding and continuous heating was determined. It is shown that increase in the carbon content leads to decrease in the volume fraction of the η phase and shift of the shrinkage curve into the region of low temperatures. It is established that an increase in the carbon content does not have a significant effect on the sintering activation energy of nanopowders and submicron powders in the region of “average” heating temperatures, the value of which is close to the activation energy of grain boundary diffusion in cobalt. It is shown that an increase in the carbon content leads to a significant decrease in the activation energy of consolidation of WC–Co powders in the region of “high” sintering temperatures owing to a decrease in the concentration of tungsten atoms in the γ phase based on cobalt. The sintering kinetics of fine-grained WC–Co alloys is limited by the rate of Coble diffusion creep of cobalt.
- 1 January 2020
- Published by Intercontact Science in Physics and Chemistry of Materials Treatment
- Vol. 6
An investigation of the peculiarities of high-speed sintering of plasma chemically synthesized tungsten carbide nanopowders with increased oxygen content
Spark plasma sintering (SPS) of plasma-chemical nanopowders tungsten carbide with a high oxygen content are studied. The results show that the nanopowder WC shrinkages during SPS is limited by grain boundary diffusion with abnormally low activation energies. It is established that the decrease in the activation energy can be caused by the influence of oxygen on the diffusion permeability of the tungsten carbide grain boundaries at the stage of intense compaction, as well as by abnormal grain growth at the stage of high-temperature sintering. The SPS kinetics of WC-W2C-WO3-W nanopowder compositions at the stage of intense compaction is controlled by the rate of oxide particle sintering with their simultaneous transformation into W2C particles, and then, by the plastic flow of W2C particles in the presence of W particles at the stage of high-temperature sintering. Using the SPS method, we obtained ceramics with a high density (98-99%), ultrafine-grained structure (the average grain size is less than 0.3 mm), having an increased hardness HV = 30.5 GPa with a Palmquist crack resistance of ~6.5 MPa·m1/2.
- 1 January 2020
- Published by Intercontact Science in Physics and Chemistry of Materials Treatment
- Vol. 6
An investigation of the peculiarities of high-speed sintering of plasma chemically synthesized tungsten carbide nanopowders with increased oxygen content
Spark plasma sintering (SPS) of plasma-chemical nanopowders tungsten carbide with a high oxygen content are studied. The results show that the nanopowder WC shrinkages during SPS is limited by grain boundary diffusion with abnormally low activation energies. It is established that the decrease in the activation energy can be caused by the influence of oxygen on the diffusion permeability of the tungsten carbide grain boundaries at the stage of intense compaction, as well as by abnormal grain growth at the stage of high-temperature sintering. The SPS kinetics of WC-W2C-WO3-W nanopowder compositions at the stage of intense compaction is controlled by the rate of oxide particle sintering with their simultaneous transformation into W2C particles, and then, by the plastic flow of W2C particles in the presence of W particles at the stage of high-temperature sintering. Using the SPS method, we obtained ceramics with a high density (98-99%), ultrafine-grained structure (the average grain size is less than 0.3 mm), having an increased hardness HV = 30.5 GPa with a Palmquist crack resistance of ~6.5 MPa·m1/2.